TY - JOUR A1 - Gamisch, Bernd A1 - Gaderer, Matthias A1 - Dawoud, Belal T1 - On the Development of Thermochemical Hydrogen Storage: An Experimental Study of the Kinetics of the Redox Reactions under Different Operating Conditions T2 - Applied Sciences N2 - This work aims at investigating the reduction/oxidation (redox) reaction kinetics on iron oxide pellets under different operating conditions of thermochemical hydrogen storage. In order to reduce the iron oxide pellets (90% Fe2O3, 10% stabilizing cement), hydrogen (H2) is applied in different concentrations with nitrogen (N2), as a carrier gas, at temperatures between between 700 ∘C and 900 ∘C, thus simulating the charging phase. The discharge phase is triggered by the flow of a mixture out of steam (H2O) and N2 at different concentrations in the same temperature range, resulting in the oxidizing of the previously reduced pellets. All investigations were carried out in a thermo-gravimetric analyzer (TGA) with a flow rate of 250mL/min. To describe the obtained kinetic results, a simplified analytical model, based on the linear driving force model, was developed. The investigated iron oxide pellets showed a stable redox performance of 23.8% weight reduction/gain, which corresponds to a volumetric storage density of 2.8kWh/(L bulk), also after the 29 performed redox cycles. Recalling that there is no H2 stored during the storage phase but iron, the introduced hydrogen storage technology is deemed very promising for applications in urban areas as day-night or seasonal storage for green hydrogen. KW - hydrogen storage KW - iron/iron oxide KW - reaction kinetics KW - redox reactions Y1 - 2021 UR - https://opus4.kobv.de/opus4-oth-regensburg/frontdoor/index/index/docId/2649 N1 - Corresponding author: Belal Dawoud VL - 11 IS - 4 SP - 1 EP - 15 PB - MDPI CY - Basel ER -