This study valorizes granite sawing waste and kaolin through production of durable ceramics tiles. FactSage (8.4) thermochemical software was integrated with petrography, XRD, XRF, DTA-TGA, SEM-EDX, physico-mechanical, hot-stage microscopy, dilatometry, chemical durability tests and Raman spectroscopy to investigate the green materials and ceramics sintered at 900-1250 °C/h. Results show that Al/Si, Ca/Si, and Ca/Al ratios and impurities levels control feldspar crystallization, glassy phase formation, and the development of silicate melt with variable viscosities. The optimum composition (40 wt% granite waste at 1200 °C/h) has a compact, interlocked microstructure with ∼47 wt% melt and suitable viscosity (2.41 × 105 PaS), yielding negligible water absorption (0.19%), low porosity (0.46%), high flexural strength (52 MPa), controlled thermal expansion (5.42 × 10−6 C−1), and excellent acidic/alkali durability (0.48, 0.06 wt%) as well as acceptable geometric stability. However, 50 wt% granite waste involvement caused deformation at 1200 °C, and bloating occurring at 1250 °C. Ceramic tiles at 1200 °C are promising for heavy-duty industrial flooring applications.