Refine
Year of publication
Document Type
- Article (10)
- conference proceeding (article) (7)
Has Fulltext
- no (17)
Reviewed
- Begutachtet/Reviewed (10)
Keywords
- Laser ablation (1)
- Laser applications (1)
- Laser direct joining; metal-polymer connections; surface texturing; transmission joining; (1)
- Laser drill (1)
- Laser micromachining (1)
- Liquid-vapor interface (1)
- Surface micromachining (1)
- laser transmission welding; adapted wavelength; melt pool geometry; gap bridging (1)
- laser transmission welding; polymers; residual stresses; environmental stress cracking (1)
- laser transmission welding; quasi-simultaneous welding; irradiation strategies; offset-scanning technique; thermal degradation (1)
Institute
The use of electrophotographic polymer powder transfer for the preparation of patterned powder layers is discussed with respect to a possible multimaterial application in powder bed-based additive manufacturing technologies such as selective laser sintering (SLS). Therefore, an experimental setup with a two-chamber design was realized, enabling the electrophotographic transfer of SLS powder materials at typical process conditions. The powder development (pick-up) step was investigated thoroughly for different powder materials to provide deep understanding of the underlying electrostatic effects and the influence of distinct powder properties. While using two different development modes, differences in the development results were correlated to differences in their particle size distribution, bulk density, and relative permittivity. Moreover, a new strategy was invented, allowing the residual electrophotographic powder deposition to be in general independent from the already produced part height. This is known to be a huge challenge but is mandatory for the buildup of three-dimensional multimaterial components.
High-speed observation of melt pool-vapor interactions in long-pulsed laser ablation of metals
(2025)
Laser ablation of metals can be performed using cost-effective and efficient continuous wave fiber lasers using the fast power modulation capabilities of these beam sources. Single-pulse laser ablation of steel with pulse durations in the microsecond to millisecond time scale is observed using a high-speed camera setup to investigate the dynamic interactions between the generated melt pool and the vapor phase. Distinct processing regimes were identified depending on the pulse duration, temporal pulse shape, and power density. Pulse durations in the microsecond range can lead to beneficial processing conditions for ablation processes. In this regime, phase explosion and dynamic melt expulsion by melt uplift and coaxial droplet ejection due to the rapid drop in vapor pressure after the laser pulses were observed as desirable mechanisms, leading to effective material removal and high processing quality with little melt adhesion.
Laser direct joining of metals and plastics is a promising process for producing strong and reliable joints for lightweight hybrid structures without the need for adhesives, primers or mechanical fasteners. Commonly this process consists of two separate steps using at least two processing stations: the surface of the metal part is textured to achieve an increased surface roughness and improved mechanical interlock between the components. In another step, the thermoplastic components or the matrix of thermoplastic fiber reinforced composites are selectively heated to allow the melt to flow into the prepared metal structures. In this work, a new method is presented that combines highly efficient laser surface texturing of metallic parts and the selective laser heating of the joining zone in a transmission joining process using a single laser beam source running in different operation modes. This enables a very compact and cost-efficient processing station.
Residual stresses in welded parts can limit the mechanical performance and reliability of the components. In polymers, especially in amorphous thermoplastics, tensile residual stresses in the presence of certain media can lead to environmental stress cracking, which can result in catastrophic failure of the connection. In this work the mechanisms of stress generation in welding of plastics is compared to metallic materials and methods for evaluating residual stresses are discussed in terms of suitability to polymer materials. The application of solvents in liquid and vapor phase is shown to be a useful tool for intentionally inducing stress cracking in laser-welded parts to evaluate and compare residual stress levels and orientations in the weld zones. Appropriate process parameters are examined for reducing welding stresses.
The usage of laser transmission welding of polymers as a joining technique in industrial applications is often limited by the optical properties of the joining partners and the limited gap-bridging capability. By using alternative laser wavelengths or multiple beam sources it is possible to adjust the radiation to the properties of the materials and increase the weld seam quality. Especially for scattering materials, parts without specific laser absorbing additives and in applications where relatively large gaps occur due to manufacturing tolerances of the parts, adapted wavelengths can lead to improved results. In this work, the gap bridging during quasi-simultaneous laser transmission welding is investigated in welding experiments and thermomechanical FE-simulations. Usage of a laser wavelength in the range of 2.0 μm is found to be beneficial in terms of gap-bridging, compared to usually applied diode or solid state lasers emitting at about 1 μm due to the higher intrinsic absorption in unmodified thermoplastic materials. This leads to increased temperatures in the transparent joining partner and therefore greater thermal expansion. Furthermore the radiation shows an increased penetration depth in carbon black filled, laser absorbing materials, also leading to increased thermal expansion and improved gap bridging. The wavelength of 2.0 μm is also found to improve the strength of weld seams when turbid materials or materials with scattering additives are used as laser transparent parts, since scattering at small particles is strongly wavelength dependent, so the longer wavelength features better control of the resulting intensity distribution in the joining zone.
Laser direct joining of metals and plastics is a promising process for producing hybrid material joints without the need for adhesives, fasteners or additional materials [1,2]. In this process, a metallic part is structured by laser radiation to increase the surface roughness and to create undercuts. A thermoplastic or thermoplastic composite material is then brought into contact with the metal component and melted in the contact zone. The melt flows into the structures and, after cooling, a stable joint is formed.
The properties of such joints strongly depend on the properties of these structures. So far, two main approaches have been used for the structuring process: By repeated irradiation with continuous laser radiation, linear grooves or grid structures can be introduced at high removal rates [3]. More complex structures with high aspect ratios can be generated with short and ultra-short pulsed laser radiation [2]. Such structures can lead to higher bond strengths, but due to the limited average power and high cost per watt of those laser systems, the process is usually much slower than with cw beam sources [2]. Modern high-power and comparatively inexpensive cw-fiber lasers feature fast optical modulation capability with modulation frequencies in the range of up to 100 kHz [4], enabling increased temporal control of the laser-material interaction by using pulses in the μs range and temporal pulse shaping. As shown in Fig. 1, surface structuring using fast modulated laser radiation was found to lead to increased melt expulsion and therefore higher removal rates compared to remote ablation cutting with continuous wave laser radiation at the same average and peak power levels. Therefore, shorter processing times and in some cases a single irradiation can be sufficient to achieve the desired structuring depth. In addition, the lower overall heat input reduces distortion in thin-walled specimens.
References
[1] A. Klotzbach; M. Langer; R. Pautzsch; J. Standfuß; E. Beyer; Thermal direct joining of metal to fiber reinforcedthermoplastic components. J. Laser Appl. 2017, 29, 22421.
[2] K. van der Straeten; C. Engelmann; A. Olowinsky; A. Gillner; Comparison of laser-based joining approaches forplastic-metal-hybrids - Strength vs. process speed. In Proceedings of the 3rd Hybrid Conference, Bremen,Germany, 2018, pp. 203–309.
[3] C. Engelmann, D. Meier, A. Olowinsky; M. Kielwasser, Metal meets Composite - Hybrid Joining for AutomotiveApplications, Lasers in Manufacturing Conference 2015, 2015.
[4] D. A. V. Kliner et al.; Next-generation industrial fiber lasers enabled by high-performance components, Proc.SPIE 10513, Components and Packaging for Laser Systems IV, 2018, 105130S.
Laser transmission welding of polymers is a widely used joining technique for automotive components, consumer products, medical applications and others. The process is strongly dependent on the transmission properties of one of the joining partners to ensure a suitable laser intensity distribution in the joining zone between the two components. Scattering at crystalline structures, additives or reinforcements in composites as well as the absorptivity of the matrix can compromise the transmitted beam profile [1, 2, 3]. Successful welding of these materials is therefore often limited to thin parts.
This work describes methods for measuring the spectral absorption, transmission and scattering properties to assess the weldability of scattering materials. Since many of these materials show anisotropic properties due to the manufacturing processes and the fiber orientation, the transmission properties are influenced by the polarization state of the laser beam.
An experimental setup shown in Fig. 1, using a commercially available Spectrophotometer with integrating sphere, is used to measure direct transmission, forward and backward directed scattering and the reflection of linearly polarized light after interaction with amorphous and semicrystalline polymers as well as particle and fiber reinforced thermoplastic composites. The spectral measurements reveal that compared to commonly used lasers emitting at about 1.0 μm the application of laser wavelengths in the range of 1.3 to 2.0 μm can lead to increased transmission and reduced scattering losses within the materials. Variation of the polarization adds an additional degree of freedom to influence the transmission properties, especially in highly anisotropic materials or composites. For validation of the spectrometric results welding experiments using a conventional diode laser beam source and a unpolarised and a linearly polarized 2.0-μm single-mode Tm-fiber [4] were carried out. Additionally the resulting laser beam profiles after transmission through different amorphous and semicrystalline polymeric materials were measured using a scanning slit beam profiler.
Using a suitable laser wavelength and adjusted polarization successful welding was achieved for highly scattering materials that could not be welded using a conventional diode laser beam source.
[1] X. F. Xu, A. Parkinson, P. J. Bates and G. Zak, Effect of part thickness, glass fiber and crystallinity on light scattering during laser transmission welding of thermoplastics, Optics & Laser Technology 75, pp. 123-131, 2015.
[2] V. Mamuschkin, A. Roesner, M. Aden, Laser Transmission Welding of White Thermoplastics with Adapted Wavelengths, Physics Procedia, 41, p. 172-179, (2013).
[3] T. Frick and A. Schkutow, Laser transmission welding of polymers–Irradiation strategies for strongly scattering materials. Procedia CIRP, 74, p. 538-543, (2018).
[4] K. Scholle, M. Schäfer, S. Lamrini, M. Wysmolek, M. Steinke, J. Neumann, P. Fuhrberg, All-fiber linearly polarized high power 2-μm single mode Tm-fiber laser for plastic processing and Ho-laser pumping applications, Proc. SPIE 10512, Fiber Lasers XV: Technology and Systems, 105120O, (2018).
Laser surface texturing of metals is usually performed using pulsed laser sources. Short and ultrashort pulsed laser systems offer the highest machining quality and processing flexibility. Most of these beam sources however feature relatively low average powers or high system prices. Continuous wave fiber lasers in comparison feature high average powers at moderate costs. In this work the laser power of a continuous-wave fiber laser is rapidly modulated to investigate the possibilities to improve laser surface texturing processes by periodically changing the interaction between the sur-face tension in the melt pool and the vapor pressure created during high power laser processing. It was found that the intermittent nature of modulated continuous wave laser radiation can improve the melt expulsion from the processing area, leading to high material removal rates and ablation ef-ficiencies while also limiting the heat input into the substrate material.
Remote ablation cutting with continuous wave laser radiation is a process commonly used for the surface pretreatment of large area metallic parts before joining of metal-polymer hybrid structures, due to their cost-effectiveness and high average powers when compared to short-pulsed lasers. The process requires high power-densities and multiple irradiations at high scanning speeds to achieve the desired kerf depth. In this work a fast modulated cw fiber laser is used to investigate the possibilities of increasing the material removal rate by periodically dropping the laser power and therefore modifying the recoil pressure at the vapor-liquid interface in the interaction zone to assist in melt expulsion. It was found that power modulation with frequencies in excess of 10 kHz can lead to an increased material removal rate when compared to continuous wave processing at comparable average and peak power levels, enabling higher kerf aspect ratios in a single irradiation.
2.0 μm fiber lasers provide a high beam quality and a high‐power output, which makes them ideal for welding and cutting a wide variety of commercially used plastics, as well as marking plastics, metals or even food. At 2.0 μm wavelength the intrinsic absorption of most thermoplastics is high enough to weld or cut without applying any absorbent additives or coatings. Compared to commonly used near‐infrared systems, welding with 2.0 μm lasers can improve heat distribution and gap bridging and enable transmission welding for challenging materials.