The creation of thermochemical models to forecast the dependent variables governing the bloatability of lightweight aggregates (LWAs) is the goal of this work. Laser particle size analysis, XRD, XRF, IR, TGA-DTA, SEM-EDX, Laser imaging system, µ-CT, hot-stage microscope and Factsage (8.3) thermodynamic software were used for clays and LWAs characterization in the temperature range 900–1250°C. It was found that the LWAs bloating zone occurs at 1050–1250°C with a minimum bulk density (BD) of (0.74 g/cm3) at 1250°C. During the LWAs pyroplastic state, the crystallization of anorthite from the silicate melt lowers its viscosity due mainly to the alkalis’ uptake into the anorthite lattice. However, the silicate melt is still viscous enough to trigger the reduction of hematite and consequently guarantees the evolution of bloating gases. The simultaneous association of higher evolved gas with less melt content of higher viscosity would promote the LWAs bloatability. The higher the gas that accompanied with low melt of lower viscosity would loosen the LWAs their consistency and sphericity upon their sudden cooling. Based on the LWAs bulk density and lab experimental observations, the production window limits of successful LWAs are ≥40 wt% silicate melt of 103-107 Pa.s viscosity that accompanied with (0.50–4.00 wt%) gas content. This production window has been verified by Liapor industrial kiln feed. The LWAs pyroplastic and post-quenching characteristics are all statistically significant variables (<0.05) for prediction modeling. The forecasting models are statistically verified by the multi-collinearity testing that shows VIF values <10 indicating the absence of any multi-collinearity among the models’ explanatory variables.
This study valorizes granite sawing waste and kaolin through production of durable ceramics tiles. FactSage (8.4) thermochemical software was integrated with petrography, XRD, XRF, DTA-TGA, SEM-EDX, physico-mechanical, hot-stage microscopy, dilatometry, chemical durability tests and Raman spectroscopy to investigate the green materials and ceramics sintered at 900-1250 °C/h. Results show that Al/Si, Ca/Si, and Ca/Al ratios and impurities levels control feldspar crystallization, glassy phase formation, and the development of silicate melt with variable viscosities. The optimum composition (40 wt% granite waste at 1200 °C/h) has a compact, interlocked microstructure with ∼47 wt% melt and suitable viscosity (2.41 × 105 PaS), yielding negligible water absorption (0.19%), low porosity (0.46%), high flexural strength (52 MPa), controlled thermal expansion (5.42 × 10−6 C−1), and excellent acidic/alkali durability (0.48, 0.06 wt%) as well as acceptable geometric stability. However, 50 wt% granite waste involvement caused deformation at 1200 °C, and bloating occurring at 1250 °C. Ceramic tiles at 1200 °C are promising for heavy-duty industrial flooring applications.