@article{YahyaAbdel-KaderOgilaetal.2026, author = {Yahya, Ahmed and Abdel-Kader, Noha and Ogila, Waleed and Moustafa, Ahmed and Hegazy, Ahmed A. and Abd-El-Raoof, Fawzia and Raab, Bastian and Hofmeister, Sebastian and Soltan, AbdelMonem and Abdel-Maksoud, Yasmen G.}, title = {Sustainable ceramic tile production: Thermochemical, microstructural, and physico-mechanical characterization of valorized granite sawing waste}, journal = {Ceramics International}, publisher = {Elsevier BV}, issn = {0272-8842}, doi = {10.1016/j.ceramint.2026.04.370}, institution = {Fakult{\"a}t Werkstofftechnik}, year = {2026}, abstract = {This study valorizes granite sawing waste and kaolin through production of durable ceramics tiles. FactSage (8.4) thermochemical software was integrated with petrography, XRD, XRF, DTA-TGA, SEM-EDX, physico-mechanical, hot-stage microscopy, dilatometry, chemical durability tests and Raman spectroscopy to investigate the green materials and ceramics sintered at 900-1250 °C/h. Results show that Al/Si, Ca/Si, and Ca/Al ratios and impurities levels control feldspar crystallization, glassy phase formation, and the development of silicate melt with variable viscosities. The optimum composition (40 wt\% granite waste at 1200 °C/h) has a compact, interlocked microstructure with ∼47 wt\% melt and suitable viscosity (2.41 × 105 PaS), yielding negligible water absorption (0.19\%), low porosity (0.46\%), high flexural strength (52 MPa), controlled thermal expansion (5.42 × 10-6 C-1), and excellent acidic/alkali durability (0.48, 0.06 wt\%) as well as acceptable geometric stability. However, 50 wt\% granite waste involvement caused deformation at 1200 °C, and bloating occurring at 1250 °C. Ceramic tiles at 1200 °C are promising for heavy-duty industrial flooring applications.}, language = {en} }