Refine
Labor/Institute
Keywords
- Femtosekundenlaser (35)
- Bragg-Reflektor (29)
- Laserschneiden (22)
- Laserbearbeitung (16)
- Faserlaser (15)
- Ultrakurzzeitlaser (15)
- Lumineszenzdiode (14)
- Laser (9)
- Quarzglas (8)
- Dünne Schicht (7)
Year of publication
Document Type
- Article (108)
- Conference Proceeding (60)
- Other (3)
- Part of a Book (1)
This contribution quantifies the birefringence within injection-molded cyclic olefin copolymer plates and discusses its impact on the mechanical properties of the plates. It also focuses on the impact of birefringence on integrated waveguides and Bragg gratings and provides fabrication guidelines for such structures. The anisotropy in all three dimensions of the workpiece is examined by means of polarimetry and a prism coupler. It is found that the birefringence is inhomogenously distributed within the workpieces, whereas the maximum birefringence not only varies locally, but also depends on the observation direction. Overall, a maximum birefringence of 10 × 10−4 is found at the plate’s surface near the injection gate. The anisotropy then reduces exponentially towards the center of the workpiece and saturates at 1.8 × 10−4, in a depth of 0.4 mm. Thus, the birefringence strongly affects near-surface photonic structures. It is found that, depending on their orientation and the local birefringence of the substrate, waveguides and Bragg gratings fabricated with comparable parameters behave completely differently in terms of polarization-dependent optical attenuation, cross-sectional intensity distribution and Bragg reflection signal. For example, the support of the TM mode can vary between total loss and an optical attenuation of 0.9 dB × cm−1. In consequence, this study underlines the importance of quantifying the birefringent state of an injection-molded cyclic olefin copolymer workpiece if it is supposed to serve as a substrate for integrated photonic structures. The study furthermore demonstrates that birefringence effects can be omitted by burying the photonic structures deeper into the volume of the thermoplastic.
This contribution demonstrates and discusses the preparation of finely dispersed copper(II) oxide nanosuspensions as precursors for reductive laser sintering (RLS). Since the presence of agglomerates interferes with the various RLS sub-processes, fine dispersion is required, and oversized particles must be identified by a measurement methodology. Aside from the established method of scanning electron microscopy for imaging individual dried particles, this work applies the holistic and statistically more significant laser diffraction in combination with dynamic image analysis in wet dispersion. In addition to direct ultrasonic homogenization, high-energy ball milling is introduced for RLS, to produce stable nanosuspensions with a high fine fraction, and, above all, the absence of oversize particles. Whereas ultrasonic dispersion stagnates at particle sizes between 500 nm and 20 μm, even after 8 h, milled suspension contains a high proportion of finest particles with diameters below 100 nm, no agglomerates larger than 1 μm and a trimodal particle size distribution with the median at 50 nm already, after 100 min of milling. The precursor layers produced by doctor blade coating are examined for their quality by laser scanning microscopy. The surface roughness of such a dry film can be reduced from 1.26 μm to 88 nm by milling. Finally, the novel precursor is used for femtosecond RLS, to produce homogeneous, high-quality copper layers with a sheet resistance of 0.28 Ω/sq and a copper mass concentration of 94.2%.
Evaluation of an ultrashort pulsed laser robot system for flexible and large-area micromachining
(2023)
We report for the first time on the realization, characterization and application of an ultrashort pulsed laser robot system for flexible and large-area 2D and 3D laser micromachining with 6 articulated axes. To characterize the dynamic positioning of the laser beam during and after axes movement, CMOS image sensors were integrated into the beam path. A method introduced for the alignment of the optical axes allows a reduction of the deviations in laser beam positioning to less than 141.8 ± 92.9 μm within a 110° rotation range of axis 4. In addition, a high laser beam positioning repeatability of less than 102.2 μm is demonstrated over a total period of 14 h for a movement of axis 5 within a range of 0° to 90°. Initial laser cutting, laser structuring and laser marking applications on automotive dashboards and glass substrates are presented for flexible and large area 2D and 3D manufacturing. By applying a special laser cutting strategy for processing AF 32 eco thin glass, high cutting quality is achieved with a taper of up to 96.3% without the generation of cracks, demonstrating the innovative potential of the high-precision laser robot system. Nonetheless, different identified inherent influences of each axis 1–5 during robot axis movement demand for an innovative beam stabilization concept to achieve high precision in laser beam positioning.
We report on an experimental study of laser microvia percussion drilling of Ajinomoto build-up film (ABF) material using an ultrashort pulsed laser in the ultraviolet region. In order to optimize the drilling quality in terms of the fabricated taper and microvia diameter, the
MHz burst mode is used in combination with both a Gaussian and a top-hat laser intensity distribution. To evaluate the influence of the top-hat beam shape on defocusing, microvias were drilled at different z-positions in the range of 200 μm evenly distributed around the focal plane. The drilling quality was evaluated by laser scanning microscopy and metallography. When using a top-hat beam shape, a reduced taper of down to 26.8 % on average is achieved compared to a Gaussian beam. For the application of 3 intra-burst pulses, we find an improvement of the taper by 11.6% compared to the single pulse mode due to the increasing heat accumulation. Using a top-hat beam shape in combination with the MHz burst mode, an 18.2 % reduction in laser drilling time for a microvia with a similar taper is remarkable, demonstrating the high potential for scaling throughput in electronics manufacturing.
We demonstrate and discuss the integration of Bragg gratings in aerosol-jetted polymer optical waveguides, produced in the optical assembly and connection technology for component-integrated bus systems (OPTAVER) process. By using a femtosecond laser and adaptive beam shaping, an elliptical focal voxel generates different types of single pulse modification by nonlinear absorption in the waveguide material, which are arranged periodically to form Bragg gratings. Integration of a single grating structure or, alternatively, an array of Bragg grating structures in the multimode waveguide yields a pronounced reflection signal with typical multimodal properties, i.e., a number of reflection peaks with non-Gaussian shapes. However, the main wavelength of reflection, located around 1555 nm, is evaluable by means of an appropriate smoothing algorithm. When loaded by mechanical bending, a pronounced Bragg wavelength shift of this reflected peak up to 160 pm is detected. This demonstrates that the additively manufactured waveguides can be used not only for signal transmission but also as a sensor.
We report on ultraviolet ultrashort pulsed laser processing of silicon carbide. Laser ablated cavities are evaluated with respect to their ablation rates, surface roughness and overall quality by varying the laser pulse fluence. Using this type of laser, high edge quality and surface roughness down to 107 nm can be achieved with an ablation efficiency of up to 0.228 mm 3 W −1 min −1. Functional surfaces are produced by generating laser induced periodic surface structures. The comparison with infrared wavelength underlines the advantages of the ultraviolet wavelength for laser micro machining this material. Significant differences with respect to the measured ablation depths and roughness as well as generated micro-and nanostructures appear. While infrared ablation is dominated by a chipping mechanism above a critical fluence of 9.93 Jcm −2 , higher ablation rates are observed with strong quality losses at the same time. In comparison to the infrared emission wavelength, in general , a significantly higher processing quality is achieved with the ultraviolet emission wavelength. In addition, the influence of spot size and repetition rate in UV processing is investigated. By increasing these parameters, a process acceleration without quality losses is enabled. The generation of a sophisticated microstructure exemplifies the advantages of processing silicon carbide with the UV laser reported here.
We report on the acceleration of femtosecond reductive laser sintering of copper (II) oxide on the surface of transparent cyclic olefin copolymers (COC) by varying the focus size to generate metallic copper (Cu) layers. By using different focusing conditions, different process speeds are achieved, and the structural accuracies are controlled. The formation of Cu lines is observed for different focus sizes at various scan speeds, which is attributed to laser exposure duration and chemical reaction time. The formed lines are categorized and measured by optical microscopy and provide the basis for two-dimensional Cu surfaces. By hatching, high quality conductive films are produced with an increased focus diameter of up to 400 µm at a scan speed of 400 mm/s and a hatch distance of 250 µm resulting in a multiple increased process speed by a factor of thirteen compared to previous research. Using 4-tip measurement , a low sheet resistance of 0.165 Ω/sq was validated on these Cu films, which have an atomic Cu content of 89.5%.
While sapphire is one of the most durable materials, its properties entail that high-precision machining, especially in the sub-millimeter regime, is still challenging. This contribution demonstrates and discusses novel femtosecond laser-based micromachining approaches for the fabrication of rotational-symmetric sapphire workpieces, specifically the generation of optical fibers by means of laser lathe of sapphire rods and the practical realization of windmill fibers. In addition, volume refractive index modification in planar sapphire substrates is presented to induce photonic crystal waveguides. The micromachined structures are comprehensively examined with respect to geometric fidelity, surface roughness, refractive index modification, and potential optical waveguiding properties. All micromachining approaches are done by means of frequency-doubled or frequency-tripled femtosecond laser radiation. Different laser optical setups including laser scanning head, spatial beam profilers including a spatial light modulator and axial rotatory movement of the specimen are employed for micro structuring and in-depth refractive index modifications. In particular for laser lathe, a sophisticated scanning pattern, in combination with an incremental axial rotatory movement of the specimen, allows for the precise diameter reduction of sapphire rods with 250 µm diameter to fibers with outer diameters of 25 µm. By supporting the workpiece with a V-groove fixture, multi-mode fibers with lengths up to 20 cm can be processed with an average surface roughness of 250 nm. Additionally, an adapted ablation scanning sequence enables the first practical demonstration of sapphire windmill fibers. Furthermore, using a spatial light modulator allows for the adaption of the laser propagation properties as to enable volume refractive index modifications with free-form arrangement. Hexagonal patterns of refractive index modifications surrounding a pristine waveguide core are fabricated and single-mode waveguiding at 1550 nm is verified. Finally, the possibility of integrating Bragg gratings into this photonic waveguide type is demonstrated
While Bragg grating-based optical devices have shown promising performances for pressure sensing applications, their sensitivity, especially in the low-pressure regime, is unsatisfying and needs to be optimized by elaborate designs, such as cantilevers or other extrinsic mechanical transducers. This contribution demonstrates and discusses a novel concept for optical pressure sensors based on polymer planar Bragg gratings. Waveguide and Bragg grating are fabricated underneath the surface of a temperature-stable and humidity-insensitive cyclic olefin copolymer substrate by means of a femtosecond laser. Based on the employed direct-writing procedure, in combination with adaptive, in-situ beam shaping with a spatial light modulator, writing depth, i.e., location of the photonic structures within the substrate, as well as Bragg grating periodicity and positioning can be deliberately chosen. Afterwards, the polymer substrate is post-processed with a high-precision micro mill, so a diaphragm comprising the integrated photonic structures is generated. The resulting diaphragm exhibits a thickness of 300 µm and a diameter of 10 mm. Finally, the optical sensor is packaged and sealed to form an air-filled gas pocket underneath the diaphragm. Deformations of the diaphragm by external pressure changes translate to strain variations along the waveguide axis and thus perturb the Bragg grating period. This leads to changes in the grating’s wavelength of main reflection, which can be evaluated in order to quantify the relative external pressure. With this straightforward optical sensor concept, pressure sensitivities up to 39 pm kPa-1, within relative pressures ranges from 78 kPa to 372 kPa, are achieved.
We report on a comprehensive study of laser percussion microvia drilling of Ajinomoto build-up film (ABF) material using an ultrashort pulsed laser in MHz burst mode. After laser processing, microvia drilling quality is being evaluated by the fabricated diameter and taper using laser scanning microscopy and metallography. The influences of the incubation effect, heat accumulation and shielding effects as a result of pulse to pulse interactions are being discussed on the ablation threshold, penetration depth and laser microvia drilling quality. We find that an increasing heat accumulation in MHz burst mode processing is responsible for the void formation and delamination of the insulating ABF layer. Therefore, the parameter clearance is introduced to evaluate these effects on the microvia sidewalls. For a comparable clearance, applying 2 intra-burst pulses achieves an average reduced taper of down to 19.5% compared to single pulse mode. At the same time, a reduced laser drilling time of 16.7% per microvia highlights the enormous potential of the MHz burst mode for laser drilling of ABF material in printed circuit board fabrication.
This article discusses the process of the laser turning of rotational symmetric, cylindrical components using ultrashort laser pulses with respect to the geometrical conditions and the resulting energy distribution during the laser turning process. As a result, process predictions and potential process optimizations are feasible. Particular attention is drawn to the laser spot formation on the cylindrical surface of the work piece in conjunction with the positioning of the laser beam relative to the rotation axis of the specimen. Based on fundamental calculations and experimental results, an optimum processing strategy is discussed, whereat the use of a trepanning optic in the laser turning process and the forming of a particular surface structure is additionally being issued.
The creation of aligning layers for the uniform orientation of liquid crystals is significant for both research and the application of liquid crystals. For all applications, the creation of aligning layers possessing controllable characteristics such as azimuthal and polar anchoring energies, easy-axis of director alignment and pretilt angle, in the same way as it is achieved by using photoaligning layers processed by light, is very important. Here, aligning properties of hybrid aligning layers created on the basis of sapphire surfaces additionally coated by photoaligning layer of PVCN-F are studied. These hybrid layers possess the properties of the nano-structured sapphire layer and the photosensitive PVCN-F layer, and complement each other. The irradiation time dependence of the azimuthal anchoring energy of the hybrid layers is studied. By using certain experimental conditions during irradiation of hybrid layers, e.g., polarization of light and irradiation time, a minimum value of the azimuthal anchoring energy, close to zero, was obtained. Atomic force microscope studies of the irradiated hybrid layers were also carried out. It was found that the behavior of the contact angle of nematic droplets placed on treated sapphire surfaces are in good agreement with properties of hybrid aligning layers and parameters of structuring surface obtained from AFM images.
We report on a comprehensive study of the mechanical properties of maraging steel
body-centred cubic lattice structures fabricated by a hybrid additive manufacturing technology that combines laser powder bed fusion with in situ high-speed milling. As the mechanical properties of additive manufactured components are inferior to, e.g., cast components, surface modifications can improve the mechanical behaviour. Different hybrid additive manufacturing technologies have been designed using additive and subtractive processes, improving process quality. Following this, mechanical testing is performed with respect to static tensile properties and dynamic stress, hardness, and porosity, comparing specimens manufactured by laser powder bed fusion only to those manufactured by the hybrid approach. In addition, the influence of different heat-treatment techniques on the mechanical behaviour of the lattice structures is investigated, namely solution and aging treatment as well as hot isostatic pressing. Thus, the influence of the superior surface quality due to the hybrid approach is evaluated, leading to, e.g., an offset of about 14–16% for the static testing of HIP lattice structures. Furthermore, the dynamic load behaviour can be improved with a finished surface, heading to a shift of the different zones of fatigue behaviour in the testing of hybrid-built specimens.
Axicon generated Bessel beams are a popular tool for high aspect ratio precision laser drilling. Spot diameter and working distance are given by the geometric parameters of the axicon and the wavelength used. Thus, it is difficult to manipulate the beam shape of a Bessel beam for a given setup. Spatial light modulators (SLMs) overcome limitations in flexibility. However, due to the limited phase shift of SLMs, only Bessel beams with flat cone angles and large focal length can be generated. In this contribution, an approach for generating Bessel beams with a shorter, but tunable focal length is presented. A physical axicon was combined with an SLM. A holographic image of a negative axicon is put on the SLM to generate a ring beam, which is focused by a subsequent physical axicon to get a small focal diameter. Thus, different sized high aspect ratio micro holes can be drilled without using any moving components.
We report on laser drilling borehole arrays using ultrashort pulsed lasers with a particular focus on reducing the inadvertent heat accumulation across the workpiece by optimizing the drilling sequence. For the optimization, evolutionary algorithms are used and their results are verified by thermal simulation using Comsol and experimentally evaluated using a thermal imaging camera. To enhance process efficiency in terms of boreholes drilled per second, multi-spot approaches are employed using a spatial light modulator. However, as higher temperatures occur across the workpiece when using simultaneous multi-spot drilling as compared to a single-spot process, a subtle spatial distribution and sequence of the multi-spot approach has to be selected in order to limit the
resulting local heat input over the processing time. Different optimization approaches based on evolutionary algorithms aid to select those drilling sequences which allow for the combination of a high efficiency of multi-spot profiles, a low-generated process temperature and a high-component quality. In particular, using a 4 x 4 laser spot array allows for the drilling of 40,000 boreholes in less than 76 s (526 boreholes/s) with a reduced temperature increase by about 35%, as compared to a single spot process when employing an optimized drilling sequence.
Multi-Bessel Beams Generated by an Axicon and a Spatial Light Modulator for Drilling Applications
(2023)
We report on an optical setup to generate multi-Bessel beam profiles combining a refractive axicon and a spatial light modulator. Based on their particular beam profile, Bessel beams offer advantageous properties for micro drilling processes and internal volume processing, especially for transparent materials. In addition, the laser power of industrial, ultrashort pulsed lasers has increased significantly over the last few years, offering the possibility for highly efficient processes using multi-spot profiles. Our optical concept combines the dynamic possibilities of beam splitting using a spatial light modulator with the benefits of Bessel beams, which facilitates multi-Bessel beam processing. Beside the simulation and experimental evaluation of the generated multi-Bessel beams, we exemplify the applicability of the developed module for the perforation of thin metal foils by micro drilling.
We report on milling and tool wear characteristics of hybrid additive manufacturing comprising laser powder bed fusion and in situ high-speed milling, a particular process in which the cutter mills inside the powder bed without any cooling lubricant being applicable. Flank wear is found to be the dominant wear characteristic with its temporal evolution over utilization period revealing the typical s-shaped dependence. The flank wear land width is measured by microscopy and correlated to the achievable surface roughness of milled 3D-printed parts, showing that for flank wear levels up to 100 μm a superior surface roughness below 3 μm is accessible for hybrid additive manufacturing. Further, based on this correlation recommended tool, life scenarios can be deduced. In addition, by optimizing the finishing tool start position and the number of afore-built layers, the milling process is improved with respect to the maximum millable angle for undercut surfaces of 3D-printed parts to 30° for the roughing process and to 40° for the entire machining process including finishing
Sapphire is a robust and wear-resistant material. However, efficient and high-quality micromachining is still a challenge. This contribution demonstrates and discusses two novels, previously unreported approaches for femtosecond laser-based micromachining of rotational-symmetric sapphire workpieces, whereas both methods are in principal hybrids of laser scanning and laser turning or laser lathe. The first process, a combination of a sequential linear hatch pattern in parallel to the workpiece’s main axis with a defined incremental workpiece rotation, enables the fabrication of sapphire fibers with diameters of 50 µm over a length of 4.5 mm. Furthermore, sapphire specimens with a diameter of 25 µm over a length of 2 mm can be fabricated whereas an arithmetical mean height, i.e., Sa parameter, of 281 nm is achieved. The second process combines a constant workpiece feed and orthogonal scanning with incremental workpiece rotation. With this approach, workpiece length limitations of the first process are overcome and sapphire fibers with an average diameter of 90 µm over a length of 20 cm are manufactured. Again, the sapphire specimen exhibits a comparable surface roughness with an average Sa value of 249 nm over 20 cm. Based on the obtained results, the proposed manufacturing method paves an innovative and flexible, all laser-based way towards the fabrication or microstructuring of sapphire optical devices, and thus, a promising alternative to chemical processes.