Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (270) (entfernen)
Sprache
- Englisch (241)
- Deutsch (28)
- Französisch (1)
Schlagworte
- Lithium-ion battery (8)
- Glass (6)
- SAXS (6)
- Additive manufacturing (5)
- Crystallization (5)
- Lithium (5)
- Nanocomposite (5)
- Raman spectroscopy (5)
- Thermal runaway (5)
- Corrosion (4)
Organisationseinheit der BAM
- 6 Materialchemie (52)
- 1 Analytische Chemie; Referenzmaterialien (40)
- 5 Werkstofftechnik (36)
- 8 Zerstörungsfreie Prüfung (34)
- 8.5 Röntgenbildgebung (28)
- 6.3 Strukturanalytik (23)
- 7 Bauwerkssicherheit (17)
- 5.6 Glas (16)
- 1.4 Prozessanalytik (15)
- 3 Gefahrgutumschließungen; Energiespeicher (14)
Paper des Monats
- ja (6)
Porous carbons are promising anode materials for next generation lithium batteries due to their large lithium storage capacities. However, their highsloping capacity during lithiation and delithiation as well as capacity fading due to intense formation of solid electrolyte interphase (SEI) limit their gravimetric and volumetric energy densities. Herein we compare a microporous carbide-derived carbon material (MPC) as promising future anode for all solid-state batteries with a commercial high-performance hard carbon anode. The MPC obtains high and reversible lithiation capacities of 1000 mAh g−1carbon in half-cells exhibiting an extended plateau region near 0 V vs. Li/Li+ preferable for full-cell application. The well-defined microporosity of the MPC with a specific surface area of >1500 m2 g−1 combines well with the argyrodite-type electrolyte (Li6PS5Cl) suppressing extensive SEI formation to deliver high coulombic efficiencies. Preliminary full-cell measurements vs. nickel-rich NMC-cathodes (LiNi0.9Co0.05Mn0.05O2) provide a considerably improved average potential of 3.76 V leading to a projected energy density as high as 449 Wh kg−1 and reversible cycling for more than 60 cycles. 7Li Nuclear Magnetic Resonance spectroscopy was combined with ex-situ Small Angle X-ray Scattering to elucidate the storage mechanism of lithium inside the carbon matrix. The formation of extended quasi-metallic lithium clusters after electrochemical lithiation was revealed.
The ability to track electrode degradation, both spatially and temporally, is fundamental to understand performance loss during operation of lithium batteries. X-ray computed tomography can be used to follow structural and morphological changes in electrodes; however, the direct detection of electrochemical processes related to metallic lithium is difficult due to the low sensitivity to the element. In this work, 4-dimensional neutron computed tomography, which shows high contrast for lithium, is used to directly quantify the lithium diffusion process in spirally wound Li/SOCl2 primary cells. The neutron dataset enables the quantification of the lithium transport from the anode and the accumulation inside the SOCl2 cathode to be locally resolved. Complementarity between the collected neutron and X-ray computed tomographies is shown and by applying both methods in concert we have observed lithium diffusion blocking by the LiCl protection layer and identified all cell components which are difficult to distinguish using one of the methods alone.
The understanding of dynamic processes in Li-metal batteries is an important consideration to enable the full capacity of cells to be utilised. These processes, however, are generally not directly observable using X-ray techniques due to the low attenuation of Li; and are challenging to visualise using neutron imaging due to the low temporal resolution of the technique. In this work, complementary X-ray and neutron imaging are combined to track the dynamics of Li within a primary Li/SOCl2 cell. The temporal challenges posed by neutron imaging are overcome using the golden ratio imaging method which enables the identification of Li diffusion in operando. This combination of techniques has enabled an improved understanding of the processes which limit rate performance in Li/SOCl2 cells and may be applied beyond this chemistry to other Li-metal cells.
Additive manufacturing (AM) of alkali-activated materials is a promising method for producing ceramic precursors, construction elements and other parts. A recently introduced AM process is laser-induced slip casting of lithium aluminate/microsilica slurries, which yields parts with excellent mechanical strengths. To clarify the underlying mechanisms, μ-Raman spectroscopy was applied to parts produced by the process, and the dissolution and hydration of lithium aluminate was studied inter alia using conventional and in-situ X-ray diffraction. The results show that significant dissolution of lithium aluminate occurs, particularly at increased temperatures during laser interaction, which leads to an increase of pH and precipitation of an akopovaite-like Li-Al-CO3 layered double hydroxide. The increase of the pH is likely to induce dissolution of the microsilica and possibly formation of a hydrous lithium aluminosilicate gel. These observations explain the strength evolution of the studied parts and can also aid the development and improvement of related AM methods.
Meta-analysis of heat release and smoke gas emission during thermal runaway of lithium-ion batteries
(2023)
Herein a meta-analysis of 76 experimental research papers from 2000 to 2021 is given about possible effects on the thermal runaway of lithium-ion battery cells. Data on the hazards of gas emissions and released heat are related to each other and differentiated by cell properties such as, cell geometry, cathode type or state of charge. Quantitative information on the total heat release in the range of 2.0–112.0 kJ Wh−1, the peak heat release rate in the range of 0.006–2.8 kW Wh−1and the smoke gas emission were extracted, normalized in terms of cell energy (Wh), combined in a data library and compared graphically. The total amount of gas emitted (3–48 mmol Wh−1) as well as the released amount of carbon monoxide (1–161 mg Wh−1) and hydrogen fluoride (2–197 mg Wh−1) were investigated as a function of the state of charge and cell geometry. The analysis reveals that the measured values are significantly influenced by the types of calorimeters and smoke gas analyzers used as well as by the type of thermal runaway trigger. This meta-analysis can serve as an important basis for any risk assessment of lithium-ion batteries.
Adopting X-ray computed tomography (XCT) for ex-situ characterization of battery materials has gained interest in the past decade. The main goal of this paper is to demonstrate the effectiveness of several X-ray computer tomography techniques to study commercial batteries. General guidelines are provided to select the most suitable imaging equipment and parameters for investigations of lithium-ion batteries, spanning the length scales from cell to electrode, down to particle level. Relevantly, such parameters would also be suitable for operando experiments.
Safety mechanisms and manufacturing inconsistencies at cell level as well as defects and inhomogeneity in cathode and anode is illustrated and quantified. Furthermore, relation of beam energy and sample-detector-distance on contrast retrieved from attenuation and phase shift is inspected using Synchrotron XCT.
Composition and Explosibility of Gas Emissions from Lithium-Ion Batteries Undergoing Thermal Runaway
(2023)
Lithium-based batteries have the potential to undergo thermal runaway (TR), during which mixtures of gases are released. The purpose of this study was to assess the explosibility of the gaseous emission from LIBs of an NMC-based cathode during thermal runaway. In the current project, a series of pouch lithium-based battery cells was exposed to abuse conditions (thermal) to study the total amount of gases released and the composition of the gas mixture. First, the battery cells were placed in a closed vessel, and the pressure and temperature rise inside the vessel were measured. In a second step, the composition of gases was analysed using a Fourier transform Infrared (FTIR) spectrometer.
We found that the amount of released gases was up to 102 ± 4 L, with a clear dependence on the battery capacity. This study showed that the concentration of gaseous emissions such as carbon monoxide (CO), methane (CH4), ethylene (C2H4), ethane (C2H6), and hydrogen cyanide (HCN) increased with higher cell capacity. Of the five studied flammable gases, the maximum concentrations of carbon monoxide (16.85 vol%), methane (7.6 vol%), and ethylene (7.86 vol%) were identified to be within their explosible range. Applying Le Chatelier’s law, a calculated lower explosion limit (LEL) of 7% in volume fraction was obtained for the gas mixture. The upper explosion limit (UEL) of the gas mixture was also found to be 31% in volume. A filter comprising pyrobubbles was used for the removal of the studied gas components released during the thermal abuse. The investigation revealed that the pyrobubbles filter was highly effect in the removal of HCN (up to 94% removal) and CO2 (up to 100% removal). Herein, we report the dependency of the method of thermal runaway trigger on the measured maximum temperature.
Herein, we present a detailed investigation of the electrochemically triggered formation and dissolution processes of α- and β-sulfur crystals on a monolithic carbon cathode using operando high-resolution synchrotron radiography (438 nm/pixel).
The combination of visual monitoring with the electrical current response during cyclic voltammetry provides valuable insights into the sulfur formation and dissolution mechanism. Our observations show that the crystal growth process is mainly dictated by a rapid equilibrium between long-chain polysulfides on one side and solid sulfur/short-chain polysulfides on the other side, which is consistent with previous studies in this field. The high temporal and spatial resolution of synchrotron imaging enables the observation of different regimes during the sulfur formation and dissolution process. The appearance of short-chain polysulfides after the first anodic CV peak initiates a rapid dissolution process of α-sulfur crystals on the cathode. The increase in the long-chain lithium polysulfide concentration at the cathode surface during charge results in an increased crystal growth rate, which in turn produces imperfections in α- and β-sulfur crystals. There are strong indications that these defects are fluid inclusions, which may trap dissolved polysulfides and therefore reduce the electrochemical cell capacity.
Additive manufacturing of alkali-activated materials currently attracts a lot of attention, because of the possibility to produce customized high-performance elements for a range of applications, potentially being more resource-efficient than conventionally produced parts. Here, we describe a new additive manufacturing process for alkali-activated materials that is based on selective laser-heating of lithium aluminate/microsilica slurries. The new process-material combination allows to manufacture elements with complex geometries at high building rates and high accuracy. The process is versatile and transferrable to structures of sizes differing by orders of magnitude. The mechanical strength of the obtained materials was in the range of values reported for conventional metakaolin-based geopolymers, and superior to what has been hitherto reported for alkali-activated materials produced by additive manufacturing. This mechanical performance was obtained despite the fact that the degree of reaction of the lithium aluminate and the microsilica was low, suggesting that significant reactions took place only at the surface of the microsilica particles.
The application of lithium-sulfur (Li-S) batteries is still limited by their rapid capacity fading. The pulverization of the sulfur positive electrode after the lithiation and the consequence dissolution of long chain polysulfides in organic solvents lead to the shuttle effect. To address these issues, here we report the mechanochemical preparation of ZIF-8 (Zeolitic Imidazole Framework-8)-based composites as sulfur hosts for positive electrodes in Li-S batteries. We studied different methods for the incorporation of conductive carbon. Also, the replacement of Zn2+ metal centers by other bivalent metals (Cu2+, Co2+ and Ni2+), enabled the preparation of other ZIF-8-based materials. The positive electrode ZIF-8/C/S8 showed initial discharges of 772 mA h g−1 while the pristine one, ZIF-8/S8, displayed 502 mA h g−1. The enhanced performance of 54% for ZIF-8/C/S8 indicates that the direct mechanochemical synthesis of ZIF-8 with conductive carbon is beneficial at initials charge/discharge process in comparison to traditional slurry preparation (ZIF-8/S8). Also, the Li2S6 absorption tests shows 87% of discoloration with ZIF-8/C/S8, confirming the better polysulfides absorption.