BAM Dissertationsreihe
Filtern
Erscheinungsjahr
- 2016 (15) (entfernen)
Dokumenttyp
- Dissertation (15)
Referierte Publikation
- nein (15)
Schlagworte
- Brandschutz (2)
- Zuverlässigkeit (2)
- zerstörungsfreie Prüfung (2)
- Abbruch (1)
- Abplatzungen (1)
- Alkali-Kieselsäure-Reaktion (1)
- Antibody (1)
- Aufbereitung (1)
- Automation bias (1)
- Beton (1)
144
This thesis addresses numerical simulations of self-compacting concrete (SCC) castings and suggests a novel modelling approach that treats reinforcement zones in a formwork as porous media.
As a relatively new field in concrete technology, numerical simulations of fresh concrete flow can be a promising aid to optimise casting processes and to avoid on-site casting incidents by predicting the flow behaviour of concrete during the casting process. The simulations of fresh concrete flow generally involve complex mathematical modelling and time-consuming computations. In case of a casting prediction, the simulation time is additionally significantly increased because each reinforcement bar occurring in succession has to be considered one by one. This is particularly problematic when simulating SCC casting, since this type of concrete is typically used for heavily reinforced structural members. However, the wide use of numerical tools for casting prediction in practice is possible only if the tools are user-friendly and simulations are time-saving.
In order to shorten simulation time and to come closer to a practical tool for casting prediction, instead to model steel bars one by one, this thesis suggests to model zones with arrays of steel bars as porous media. Consequently, one models the flow of SCC through a reinforcement zone as a free-surface flow of a non-Newtonian fluid, propagating through the medium. By defining characteristic parameters of the porous medium, the influence on the flow and the changed (apparent) behaviour of concrete in the porous matrix can be predicted. This enables modelling of any reinforcement network as a porous zone and thus significantly simplifies and fastens simulations of reinforced components’ castings.
Within the thesis, a computational model for SCC flow through reinforced sections was developed. This model couples a fluid dynamics model for fresh concrete and the macroscopic approach for the influence of the porous medium (formed by the rebars) on the flow. The model is implemented into a Computational Fluid Dynamics software and validated on numerical and experimental studies, among which is a large-scale laboratory casting of a highly reinforced beam. The apparent rheology of concrete within the arrays of steel bars is studied and a methodology to determine unknown input parameters for the porous medium is suggested. Normative tables defining characteristic porous medium parameters as a function of the topology of the rebar zone for different reinforcement cases are generated. Finally, the major contribution of this work is the resulting numerical package, consisting of the numerical solver and the parameter library. The thesis concludes on the ability of the porous medium analogy technique to reliably predict the concrete casting behaviour, while being significantly easier to use and far less time consuming than existing tools.
142
Die Schädigung von Gefahrgutbehältern während ihres Transports durch Korrosion und Ermüdungsrisswachstum sind Ursache von Unfällen, die Menschenleben gefährden, die Umwelt schädigen und hohe Sachschäden verursachen. Um solchen Unfällen vorzubeugen, werden präventive Intervallprüfungen durchgeführt. Diese sind jedoch kostenintensiv, unter anderem durch die Standzeit der Transportmittel. Eine Alternative bietet die Idee einer kontinuierlichen Zustandsüberwachung mittels Schallemissionsprüfung (SEP). So sollen Materialfehler sofort nach dem Entstehen entdeckt und repariert werden können. Die Schallemissionsprüfung ist eine online Methode der Familie der zerstörungsfreien Prüfung. Schallemission (SE) wird durch Veränderungen im Material erzeugt und durch elastische Wellen als Körperschall transportiert. Erzeugt das Schallemissionsereignis genug Energie, damit sich eine elastische Welle bis zum Rand eines Bauteils ausbreiten kann, entsteht dort eine Oberflächenverschiebung im Pikometer-Bereich, die mithilfe von piezoelektrischen Sensoren detektiert werden kann. Der Sensor gibt ein elektrisches Signal aus. Aus diesem transienten SE-Signal lassen sich SE-Parameter wie die Maximalamplitude oder die Frequenz extrahieren. Durch Methoden der Signalanalyse können Signalgruppen in der Zeit- und Frequenzebene untersucht werden. Durch Wellenmodenanalysen lassen sich beispielsweise Aussagen über die Art der Quelle machen. Diese Methoden werden angewendet, um aus dem SE-Signal Rückschlüsse auf die Quelle der Schallemission zu ziehen. Werden definierte Schadensmechanismen erkannt, können Hinweise auf den Schadenszustand des Bauteils gegeben werden. Durch Schallemission, die durch den Rissfortschritt erzeugt wird, kann beispielsweise ein Zusammenhang zur Rissfortschrittsrate und zum Spannungsintensitätsfaktor geschlossen werden. Eine neue Entwicklung im Bereich der Schallemissionsprüfung ist die Mustererkennung von SESignalen. Aus den Signalen werden spezifische Merkmale extrahiert, die sie ihren Schadensmechanismen zuordnen sollen. Für die Schadensmechanismen Korrosion und Ermüdungsrisswachstum findet in dieser Arbeit eine vergleichende Analyse von SE-Signalen statt. Die Schadensmechanismen werden anwendungsnah auf großen Platten in der Wärmeeinflusszone einer Schweißnaht generiert und ihre SE-Signale definiert aufgenommen. Dafür werden Resonanzsensoren verwendet, die auf der einen Seite durch ihre Frequenzabhängigkeit sehr empfindlich die kleinste Oberflächenbewegungen reagieren und somit auch für die Anwendung in einer Zustandsüberwachung geeignet sind, jedoch andererseits frequenzbasierte Methoden der Signalanalyse erschweren. Es werden reines Ermüdungsrisswachstum, Ermüdungsrisswachstum unter dem Einfluss von Korrosion sowie reine Oberflächenkorrosion generiert. Die Signalgruppen der Schadensmechanismen werden anhand ihrer Parameter verglichen; anhand von Wellenmodenanalysen können erste Unterschiede, trotz des starken Sensoreinflusses im Frequenzbereich, festgestellt werden. Der Schadenszustand der Proben wird durch bruchmechanische Kenngrößen in Zusammenhang mit SE-Parametern der Signalgruppen gebracht. Ferner findet eine Mustererkennung der SE-Signale statt. Dafür werden zwei Methoden des überwachten Lernens verwendet: eine automatisierte Merkmalsauswahl mithilfe eines kommerziellen Mustererkennungssystems, bei dem hauptsächlich frequenzabhängige Merkmale generiert werden sowie eine parameterbasierte Mustererkennung. Bei der parameterbasierten Mustererkennung wird die Einteilung in Signalklassen aufgrund der Häufigkeitsverteilung der SE-Parameter aus den Signalen der untersuchen Schadensmechanismen vorgenommen. Dabei ergeben beide Methoden, insbesondere für die Schädigung durch Korrosion, eine gute Zuordnung der SE-Signale in die richtige Schädigungsklasse. Abschließend findet unter Berücksichtigung der Nachweisbarkeit von SE-Ereignissen und der Klassifizierbarkeit von SE-Signalen eine Einschätzung zu Chancen und Risiken der permanenten Zustandsüberwachung mittels Schallemissionsprüfung statt. Dazu werden unter anderem eigene Messungen an Tankfahrzeugen hinzugezogen sowie Ergebnisse aus zyklischer und statischer Belastung verglichen. Es wird eine Abschätzung zur Wahl der Überwachungsmethode an Gefahrgutbehältern gegeben.
147
Einfluss der Porosität von Beton auf den Ablauf einer schädigenden Alkali-Kieselsäure-Reaktion
(2016)
This thesis deals with the question of how the porosity of concrete influences the process of a damaging alkali-silica-reaction (“ASR”). In particular, it is examined whether the use of slip form pavers and the reduced porosity resulting from this use have an effect on the process of a damaging ASR.
Since the 1980s slip form pavers have been used, which modifies the structure of concrete. However, these modifications have not yet been taken into consideration in the relevant technical guidelines. The use of slip form pavers instead of conventional concrete pavers results in a denser structure. Due to the denser structure the ductility and the porosity of the concrete decrease. Thus it is more difficult for the tensile stress to be reduced. Moreover, the space for the ASR gel to expand is reduced. These consequences promote the ASR. By contrast, the permeability of the concrete is lower. Hence, the penetration of external alkalis is reduced and the diffusion of the alkalis to the potentially reactive aggregate slowed down. Against this background the question arises whether the use of slip form pavers and the reduced porosity of the concrete increase the risk of a damaging ASR.
An innovative non-destructive testing methodology is applied to answer this question. Based on variations of the porosity it is examined which damage parameters influence the process and intensity of a damaging ASR. The damaging parameters taken into consideration are the mechanical properties of the concrete, the expansion space and the transport processes within the concrete. In order to determine the influence of the relevant damaging parameters two categories of tests are conducted: one category is based on a high internal potential for damages due to ASR, the other one on a high external potential. In both cases alkali-reactive slow/late aggregates are tested. The different porosities of the concrete mainly result from a variation of the w/c-ratio. In case of a high internal potential for ASR-damages the mechanical properties and the expansion space play the most important role. Furthermore; the influence of an air-entraining agent on the process of a damaging ASR is taken into account. The high internal potential for ASR-damages is provoked by the use of cement with a high amount of alkalises for the production of the concrete samples. These samples are stored in the 40 °C fog chamber storage and the 60 °C concrete prisms test. On the one hand the expansion and the change in mass as well as the eigenfrequency are measured discontinuously in the conventional way. On the other hand the innovative testing methodology applied to these ASR-provoked stored concrete samples serves to continuously measure the expansion and the hardening as well as crack formation processes. This methodology comprises a determination of the ultrasonic velocity and of acoustic emissions as well as 3-dimensional micro X-ray computed tomography (μ-3D-CT). The high external potential for ASR-damages is provoked by the cyclic climate storage, designed by FIB. The analysis of these concretes focuses on transportation processes.
140
Im Mittelpunkt der vorliegenden Arbeit steht das Ermüdungsverhalten von Beton unter hochzyklischen Druckschwellbeanspruchungen. Der aktuelle Wissensstand bezüglich des Ermüdungsverhaltens ist nach wie vor sehr lückenhaft. Ganz besonders trifft das auf den eigentlichen Ermüdungsprozess zu, der dem abschließenden Ermüdungsversagen vorausgeht. Dem Defizit im Wissen um das Ermüdungsverhalten steht allerdings eine zunehmende Bedeutung der Thematik in der Baupraxis gegenüber. Daher wurde im Rahmen dieser Arbeit eine systematische Untersuchung des Ermüdungsprozesses vorgenommen. Damit wird ein Beitrag geleistet, um einen tieferen Einblick und ein besseres Verständnis für den Schädigungsprozess und die damit verbundenen Vorgänge innerhalb des Betons zu gewinnen.
Die experimentellen Untersuchungen bestehen im Wesentlichen aus einstufigen Dauerschwingversuchen im Druckschwellbereich an zylindrischen Probekörpern aus Normalbeton. Verwendet wurden zwei verschiedene Ermüdungslastniveaus, die Bruchlastzyklen zwischen 10⁶ und 10⁷ sowie zwischen 10³ und 10⁴ erzeugten. Die Untersuchung des Ermüdungsvorgangs erfolgte durch den Einsatz verschiedener ZfP- und ZP-Methoden, wie der Dehnungsmessung, der Messung flächiger Oberflächenverformungen, der Ultraschallmessung, der Schallemissionsmessung, der Lichtmikroskopie und des Rasterelektonenmikroskops. Zur Bewertung einiger Einflussgrößen im Zusammenhang mit dem Ermüdungsverhalten fanden zudem ergänzende Versuche zum Kriecheinfluss sowie zum Einfluss der Probengröße statt.
Es konnte festgestellt werden, dass es sich bei dem Ermüdungsvorgang um eine von Beginn an einsetzende Schädigungsevolution innerhalb des Betons handelt. Diese beeinflusst die verschiedenen Materialeigenschaften des Betons in vielfältiger und sehr unterschiedlicher Weise. Die wesentlichste Feststellung in diesem Zusammenhang ist, dass die ermüdungsbedingte Materialschädigung zu einer Veränderung der gesamten Spannungs-Dehnungs-Beziehung führt, die sich ebenfalls in einem fortlaufenden Evolutionsprozess äußert.
Aus den Untersuchungen konnten als entscheidende Ursache für die beobachteten Veränderungen im makroskopischen Materialverhalten Veränderungen in der Mikrorissstruktur nicht festgestellt werden. Vielmehr weisen die Ergebnisse der Untersuchungen darauf hin, dass die ermüdungsbedingten Veränderungen speziell in den Phasen I und II vorrangig das Resultat von viskosen Prozessen innerhalb des Zementsteins sind. Darüber hinaus geht aus den Versuchen hervor, dass auch das Kriechen zu relativ ähnlichen, aber weniger stark ausgeprägten Veränderungen im Material führt. Ein Einfluss der Probengröße auf das resultierende Verhalten konnte sowohl im statischen als auch im zyklischen Fall beobachtet werden.
Aus den gewonnenen experimentellen Erkenntnissen wird eine Beschreibung der Vorgänge abgeleitet, die während des Ermüdungsprozesses im Materialgefüge ablaufen und zu den beobachteten makroskopischen Veränderungen führen. In diesem Zusammenhang hat sich herausgestellt, dass eine Erfassung der ermüdungsbedingten Schädigung anhand einer skalaren Größe über die Steifigkeit der tatsächlichen Veränderung der Spannungs-Dehnungs-Beziehung nicht gerecht wird. Eine Betrachtung im Hinblick auf einen zuverlässigen Schädigungsindikator im Zusammenhang mit den gemessenen Größen liefert zudem einen Überblick über die Eignung verschiedener Größen zur Erfassung des Ermüdungsschädigungsgrades im Beton. Abschließend wird ein Ansatz vorgestellt, der die beobachteten Entwicklungen entscheidender Größen im Ermüdungsvorgang abzubilden vermag.
145
Non-destructive testing (NDT) is regarded as one of the key elements in ensuring quality of engineering systems and their safe use. A failure of NDT to detect critical defects in safetyrelevant components, such as those in the nuclear industry, may lead to catastrophic consequences for the environment and the people. Therefore, ensuring that NDT methods are capable of detecting all critical defects, i.e. that they are reliable, is of utmost importance. Reliability of NDT is affected by human factors, which have thus far received the least amount of attention in the reliability assessments. With increased use of automation, in terms of mechanised testing (automation-assisted inspection and the corresponding evaluation of data), higher reliability standards are believed to have been achieved. However, human inspectors, and thus human factors, still play an important role throughout this process, and the risks involved in this application are unknown. The overall aim of the work presented in this dissertation was to explore for the first time the risks associated with mechanised NDT and find ways of mitigating their effects on the inspection performance. Hence, the objectives were to (1) identify and analyse potential risks in mechanised NDT, (2) devise measures against them, (3) critically address the preventive measures with respect to new potential risks, and (4) suggest ways for the implementation of the preventive measures. To address the first two objectives a risk assessment in form of a Failure Modes and Effects Analysis (FMEA) was conducted (Study 1). This analysis revealed potential for failure during both the acquisition and evaluation of NDT data that could be assigned to human, technology, and organisation. Since the existing preventive measures are insufficient to defend the system from identified failures, new preventive measures were suggested. The conclusion of the study was that those preventive measures need to be carefully considered with respect to new potential risks, before they can be implemented, thus serving as a starting point for further empirical studies. To address the final two objectives, two preventive measures, i.e. human redundancy and the use of automated aids in the evaluation of NDT data, were critically assessed with regard to potential downfalls arising from the social interaction between redundant individuals and the belief in the high reliability of automated aids. The second study was concerned with the potential withdrawal of effort in sequential redundant teams when working collectively as opposed to working alone, when independence between the two redundant individuals is not present. The results revealed that the first redundant inspector, led to believe someone else will conduct the same task afterwards, invested the same amount of effort as when working alone. The redundant checker was not affected by the information about the superior experience of his predecessor and—instead of expected withdrawal of effort—exhibited better performance in the task. Both results were in contradiction to the hypotheses, the explanations for which can be found in the social loafing and social compensation effects and in the methodological limitations. The third study examined inappropriate use of the aid measured in terms of (a) agreement with the errors of the aid in connection to the frequency of verifying its results and in terms of (b) the overall performance in the task. The results showed that the information about the high reliability of the aid did not affect the perception of that aid’s performance and, hence, no differences in the actual use of the aid were to be expected. However, the participants did not use the aid appropriately: They misused it, i.e. agreed with the errors committed by the aid and disused it, i.e. disagreed with the correct information provided by the aid, thereby reducing the overall reliability of the aid in terms of sizing ability. Whereas aid’s misuse could be assigned to low propensity to take risks and reduced verification behaviour because of a bias towards automation, the disuse was assigned to the possible misunderstanding of the task. The results of these studies raised the awareness that methods used to increase reliability and safety, such as automation and human redundancy, can backfire if their implementation is not carefully considered with respect to new potential risks arising from the interaction between individuals and complex systems. In an attempt to minimise this risk, suggestions for their implementation in the NDT practice were provided.
148
Low-alloyed heat-resistant steels have a fundamental contribution to the currently applied steel grades in pressurized and temperature loaded components like membrane walls(water walls)or pressure vessels. Here, the main advantages of the low-alloy concept can be used in terms of superior high temperature mechanical properties, workability and decreased amounts of expensive alloy elements. The main challenge for the future is to further increase the power plant thermal efficiency independent of the type of power plant concept, i.e. fossil-fired or nuclear power plant, where the material selection can directly affect reduction of CO2 emissions.
In power plant design, welding is the most applied manufacturing technique in component construction. The necessary weld heat input causes metallurgical changes and phase transitions in the heat affected zone (HAZ) of the base materials and in the deposited weld metal. The weld joint can absorb hydrogen during welding or in later service - This absorption can cause degradation of mechanical properties of the materials, and in certain loading conditions, hydrogen-assisted cold cracks can occur. This cracking phenomenon can appear time delayed due to the temperature dependency of the hydrogen diffusion and
the presence of a “critical” hydrogen concentration. Additionally, each specific weld microstructure shows a certain hydrogen diffusion and solubility that contribute to susceptibility of the cracking phenomenon. Therefore hydrogen cannot be neglected as possible failure effect, which was identified recently in the case of T24 creep-resistant tubeto-tube weld joints. It is necessary to identify and assess the hydrogen effect in weld joints of low-alloyed steel grades for to improve further early detection of possible failures.
For each specific weld joint microstructure, it is necessary to separate the interdependencies between mechanical load and the hydrogen concentration. The
diffusivity and solubility must be considered to identify hydrogen quantities in the material at any given time. In this case, the effects of mechanical loading were dealt with independently. For the characterization of the mechanical properties, hydrogen charged tensile specimens were investigated for the base materials and thermally simulated HAZ
microstructures. The hydrogen diffusion was characterized with the permeation technique at room temperature and at elevated temperature ranges up to 400°C - It was investigated by interpreting the hydrogen effusion behavior with carrier gas hot extraction technique (CGHE). For realistic determination of the hydrogen diffusion coefficients, an improved
method was developed encompassing accelerated specimen heating and hydrogen determination via mass spectrometer (MS). Simultaneously, the corresponding temperature
dependent trapped and total hydrogen concentrations were determined.
The determined experimental results showed increased susceptibility to the hydrogen affected
degradation of the HAZ compared to the base material, which is independent of the investigated alloy composition. In particular, the martensitic coarse grain HAZ is the most susceptible microstructure to hydrogen-affected degradation. The results of the tensile
tests allowed the definition of consistent microstructure specific failure criteria (envelope curves) versus quantified hydrogen concentrations for the reactor pressure vessel 16MND5 steel (20MnMoNi-5-5) and the creep-resistant T24 steel (7CrMoVTiB10-10). The procedure of quantifying hydrogen concentrations in HAZ microstructures is novel and supports a new method of analysis for hydrogen degradation effects. Further investigations with the T22
steel (10CrMo9-10), as compared to the creep-resistant T24 steel (7CrMoVTiB10-10),
confirmed the beneficial effect of Vanadium as an alloying element to improve the resistance to degradation. In general, Mn-Mo-Ni base material grades show a higher resistance compared to Cr-Mo steels that do not include Vanadium alloying.
The investigations showed the decreased diffusion coefficient of the HAZ microstructure compared to the base material microstructure. This is caused by the stronger trapping effects that are present which simultaneously increase the hydrogen solubility as well. In
general, trapping effects above 100°C are negligible. It is noted that after testing the T24 grade, these trapping effects were observed above 100°C and must be considered. At elevated temperatures, the calculated hydrogen diffusion coefficients are sometimes greater than those in literature. This is primarily due to the unique applied specimen heating procedure resulting in a varied hydrogen effusion from the specimen.
The significance of the obtained results can be characterized in three perspectives. First, the direct comparison of the degradation was possible in terms of microstructure-specific hydrogen effects on the mechanical properties. Second, consistent failure criteria were established to quantify degradation vs. the hydrogen concentration. Third, the determination of more accurate hydrogen diffusion coefficients is now available.
From a scientific point of view, important contributions were made to further interpret the hydrogen effects on the macroscopic mechanical properties, with respect to the alloy composition and the microstructure. From a procedural standpoint, the mentioned deviation in the elevated temperature diffusion coefficients can be caused by the calculation method. This can be an explanation for the reported data scatter in the references.
In terms of an economic view, the presented experimental results contribute to a safe and reliable weld workability of the steel grades. Thus, the identified temperature levels of hydrogen trapping can be applied in the definition of minimum preheat, interpass or postheat temperatures. In addition, recommendations for suitable dehydrogenation heat treatment (DHT) procedures, with accurate temperature values and holding times, can be derived from these results. In the future, the application of the mechanical and diffusion data is intended to support numerical analysis methods to provide an improved prediction of hydrogen effects on material degradation in weld microstructures.
154
Pharmacologically active compounds are omnipresent in contemporary daily life, in our food and in our environment. The fast and easy quantification of those substances is becoming a subject of global importance. The fluorescence polarization immunoassay (FPIA) is a homogeneous mix-and-read format and a suitable tool for this purpose that offers a high sample throughput. Yet, the applicability to complex matrices can be limited by possible interaction of matrix compounds with antibodies or tracer.
Caffeine is one of the most frequently consumed pharmacologically active compounds and is present in a large variety of consumer products, including beverages and cosmetics. Adverse health effects of high caffeine concentrations especially for pregnant women are under discussion. Therefore, and due to legal regulations, caffeine should be monitored. Automated FPIA measurements enabled the precise and accurate quantification of caffeine in beverages and cosmetics within 2 min. Samples could be highly diluted before analysis due to high assay sensitivity in the low μg/L range. Therefore, no matrix effects were observed.
The antiepileptic drug carbamazepine (CBZ) is discussed as a marker for the elimination efficiency of wastewater treatment plants and the dispersion of their respective effluents in surface water. The development of a FPIA for CBZ included the synthesis and evaluation of different tracers. Using the optimum tracer CBZ-triglycine-5-(aminoacetamido) fluorescein, CBZ concentrations in surface waters could be measured on different platforms: one sample within 4 min in tubes or 24 samples within 20 min on microtiter plates (MTPs). For this study, a commercially available antibody was used, which led to overestimations with recovery rates up to 140% due to high cross-reactivities towards CBZ metabolites and other pharmaceuticals.
For more accurate CBZ determination, a new monoclonal antibody was produced. In this attempt, methods for improving the monitoring during the production process were successfully applied, including feces screening and cell culture supernatant screening with FPIA. The new monoclonal antibody is highly specific for CBZ and showed mostly negligible cross-reactivities towards environmentally relevant compounds. Measurements at non-equilibrium state improved the sensitivity and selectivity of the developed FPIA due to slow binding kinetics of the new antibody. Additionally, this measure enables for CBZ determination over a measurement range of almost three orders of magnitude. The comprehensively characterized antibody was successfully applied for the development of sensitive homogeneous and heterogeneous immunoassays.
The new antibody made the development of an on-site measurement system for the determination of CBZ in wastewater possible. After comprehensive optimization, this automated FPIA platform allows the precise quantification of CBZ in wastewater samples only pre-treated by filtration within 16 min. Recovery rates of 61 to 104% were observed. Measurements in the low μg/L range are possible without the application of tedious sample preparation techniques.
Different FPIA platforms including MTPs, cuvettes and tubes were successfully applied. For the choice of the right format, the application field should be considered, e.g. desired sample throughput, usage for optimization or characterization of antibodies or if a set-up for routine measurements is sought for. For high sample throughput and optimization, FPIA performance on MTPs is advantageous. The best results for the application to real samples were obtained using kinetic FP measurements in cuvettes.
152
Trans-Zearalenone(ZEN)is a non-steroidal estrogenic mycotoxin which frequently contaminates cereal grains worldwide. Ingestion of food and feed containing ZEN causes numerous mycotoxicoses in animals and possibly humans with pronounced estrogenic effects. Due to the trans-configurated double bond, ZEN isomerizes to the cis-configuration upon the influence of light. This work investigates the instrumental analysis, metabolism and toxicity of ZEN and cis- ZEN. The first part focused on the determination of ZEN in edible oils. Due to a maximum level of 400 µg/kg ZEN in the European Union (EU), reliable analytical methods are needed. A comprehensive method comparison proved dynamic covalent hydrazine chemistry (DCHC) to be the most suitable approach. Thus, an automated solid phase extraction (SPE) coupled online to high performance liquid chromatography (HPLC) was developed with the novelty of a covalent SPE step comprising the DCHC principle. The automated online system allows an accurate, selective and reliable quantification of ZEN in edible oils in compliance with EU performance criteria while significantly reducing workload and thereby personnel costs. In contrast to ZEN, reference standards and analytical methods are missing for cis- ZEN which causes a lack of data on the occurrence, fate and risks of cis-ZEN. Therefore, a native and an isotopically labeled cis-ZEN standard were synthesized and implemented in an existing stable isotope dilution analysis HPLC tandem mass spectrometry (HPLC-MS/MS) method. Using this method, a large extent of cis-ZEN formation was observed for ZEN contaminated maize germ oils when exposed to daylight which confirms that cis-ZEN can be a relevant food contaminant and should be considered in the analysis of food and feed. Furthermore, this work investigated the in vitro phase I metabolism of ZEN and cis-ZEN in rat and human liver microsomes by using HPLC-MS and -MS/MS analyses. The metabolic pathways of cis-ZEN were found to be essentially similar to ZEN including reduction and oxidation reactions generating α- and β-cis- zearalenol as well as 13- and 15-OH-cis-ZEN. A previously unidentified oxidative metabolic pathway for both isomers of ZEN results in the formation of cis-ZEN-11,12-oxide and ZEN-11,12-oxide in human liver microsomes. The estrogenicity of cis-ZEN and its reductive metabolites was assessed using the E-Screen assay. cis-ZEN proved to be slightly more estrogenic than ZEN. Biotransformation of cis-ZEN to β-cis-ZEL corresponds to a detoxification, whereas metabolism to α-cis-ZEL resembles a metabolic activation as its estrogenicity considerably exceeds that of cis-ZEN. The catecholic metabolites can be expected to show a decreased estrogenicity as demonstrated for 15-OH- ZEN. Independent of the estrogenic effects, the catecholic and epoxidic metabolites identified in this work can be expected to act genotoxic and carcinogenic. The epoxides in particular could fundamentally change the widely accepted view of ZEN causing adverse effects exclusively through endocrine disrupting actions.
151
Konzept zur ganzheitlichen Nachhaltigkeitsbewertung des Abbruchs und der Aufbereitung von Mauerwerk
(2016)
Mit der vorliegenden Arbeit wurde ein methodisches Konzept zur ganzheitlichen Nachhaltigkeitsbewertung des Abbruchs und der Aufbereitung von Mauerwerk bereitgestellt. Das Bewertungskonzept ermöglicht einen ganzheitlichen Vergleich verschiedener Szenarien für den Abbruch und die Aufbereitung von Mauerwerk unter Berücksichtigung der Anwendung von Mauerwerkbruch und aussortierter Fremdstoffe zur Verwertung. Es kombiniert die Kosten-Wirksamkeitsanalyse, die Stoffflussanalyse, die Ökobilanzierung, die Betrachtung sozialer Aspekte und Wirtschaftlichkeitsbetrachtungen bei gleichzeitiger Berücksichtigung der Materialqualitäten. Das Bewertungskonzept basiert im Kern auf der Kosten-Wirksamkeitsanalyse (KWA) mit der Erweiterung um das Gesamtwirksamkeitswert-Kosten-Verhältnis. Hiermit können sowohl monetäre als auch nicht monetäre Effekte beurteilt werden. Ausgangspunkt der KWA ist ein klar definiertes Zielsystem. Im vorliegenden Fall wurden aus der EU-Abfallrahmenrichtlinie, dem Kreislaufwirtschaftsgesetz und der EU-Bauproduktenverordnung die vier Generalziele „Mensch und Umwelt“, „Ressourcenschonung“, „Ausreichende Materialqualität“ sowie „Wirtschaftlichkeit“ abgeleitet. Die Generalziele "Mensch und Umwelt" und "Ressourcenschonung" wurden weiter in Hauptziele, Ziele und Unterziele unterteilt. Die Quantifizierung und Beurteilung dieser beiden Generalziele erfolgt im Rahmen der Wirksamkeitsanalyse. Zur Quantifizierung der abstrakten Ziele wurden konkrete und messbare Zielkriterien ausgewählt, die üblicherweise bei der Ökobilanzierung und sozialorientierten Betrachtungen verwendet werden, z. B. Umweltauswirkungen, Material- und Energieverbrauch.
Nach Ermittlung einer Gesamtwirksamkeit und den anfallenden Kosten für jedes Szenario wird das Gesamtwirksamkeit-Kosten-Verhältnis je Szenario errechnet. Dieses Verhältnis bildet die Grundlage für die abschließende Reihung der untersuchten Szenarien entsprechend ihrer nachhaltigkeitsbezogenen Wertigkeit im Sinne der europäischen und deutschen Kreislaufwirtschaft.
Mit dem Konzept wird zukünftigen Nutzern eine strukturierte und methodische Bewertungsgrundlage als Planungsinstrument für Abbruchprojekte an die Hand gegeben. Gleichzeitig werden die Nutzer für bestehende Gestaltungsvarianten für den Abbruch und die Aufbereitung von Mauerwerk sowie für die vielfältigen Anwendungsmöglichkeiten von Mauerwerkbruch sensibilisiert.
141
In der vorliegen Arbeit wird ein kurzglasfaserverstärktes Polyamid 6 unter zweiachsiger mechanischer Belastung charakterisiert. Die Analyse umfasst das einachsige und zweiachsige Ermüdungsverhalten unter Zug-, Torsions- und Zug-Torsionslast sowie die dabei auftretende charakteristische Mikroschädigungsentwicklung.
Zur Beschreibung des Ermüdungsverhaltens unter zweiachsiger Axial-Torsionslast kann das auf Ermüdungslasten angepasste, nicht-differenzierende Tsai-Hill-Kriterium angewendet werden.
Die Mikroschädigungsanalyse erfolgt begleitend zu den mechanischen Belastungsversuchen mit der zerstörungsfreien Prüfmethode der Röntgenrefraktionsanalyse. Durch fraktographische Analysen des Werkstoffes wird das qualitative Auftreten der im Modell angenommenen Schädigungsmechanismen abgesichert.
Prinzipiell ist die Mikroschädigung kurzfaserverstärkter Werkstoffe durch Faser-Matrix-Ablösungen beziehungsweise Faserbrüche und Matrix-Mikrorissbildung geprägt. Abhängig von Faserlängenkonfiguration sowie Belastungsart und -richtung ändert sich das Auftreten beziehungsweise die quantitative Ausprägung der einzelnen Mechanismen. So tritt Matrix-Mikrorissbildung lediglich im Zusammenhang mit Zuglasten auf, während Faser-Matrix-Ablösungen unabhängig von der Belastungsart im geschädigten Werkstoff vorliegen. Die Mikroschädigungsmechanismen Faser-Matrix-Ablösung und Matrix-Mikrorissbildung korrelieren linear mit den nichtlinearelastischen Verzerrungen unter statischen und schwellenden Ermüdungslasten (R = 0;1).