Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
Dokumenttyp
- Vortrag (89)
- Zeitschriftenartikel (51)
- Posterpräsentation (36)
- Beitrag zu einem Tagungsband (30)
- Sonstiges (13)
- Buchkapitel (1)
- Dissertation (1)
- Forschungsbericht (1)
Sprache
- Englisch (207)
- Deutsch (13)
- Italienisch (1)
- Mehrsprachig (1)
Schlagworte
- Corrosion (222) (entfernen)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (105)
- 7.6 Korrosion und Korrosionsschutz (105)
- 5 Werkstofftechnik (51)
- 5.1 Mikrostruktur Design und Degradation (48)
- 6 Materialchemie (35)
- 6.2 Material- und Oberflächentechnologien (26)
- 4 Material und Umwelt (18)
- 4.1 Biologische Materialschädigung und Referenzorganismen (16)
- 6.3 Strukturanalytik (7)
- 1 Analytische Chemie; Referenzmaterialien (4)
- 5.0 Abteilungsleitung und andere (4)
- 5.6 Glas (3)
- 6.1 Oberflächen- und Dünnschichtanalyse (3)
- 9 Komponentensicherheit (3)
- 9.0 Abteilungsleitung und andere (3)
- 1.4 Prozessanalytik (2)
- 3 Gefahrgutumschließungen; Energiespeicher (2)
- 3.2 Gefahrguttanks und Unfallmechanik (2)
- 4.2 Material-Mikrobiom Wechselwirkungen (2)
- 1.1 Anorganische Spurenanalytik (1)
- 1.2 Biophotonik (1)
- 4.5 Kunst- und Kulturgutanalyse (1)
- 5.2 Metallische Hochtemperaturwerkstoffe (1)
- 5.4 Multimateriale Fertigungsprozesse (1)
- 6.0 Abteilungsleitung und andere (1)
- 6.6 Physik und chemische Analytik der Polymere (1)
- 6.7 Materialsynthese und Design (1)
- 7.4 Baustofftechnologie (1)
- 8 Zerstörungsfreie Prüfung (1)
- 8.5 Röntgenbildgebung (1)
- 9.2 Versuchsanlagen und Prüftechnik (1)
Eingeladener Vortrag
- nein (89)
Corrosion fatigue specimen with different surfaces (technical surfaces after machining and polished surfaces) of high alloyed martensitic stainless steel X46Cr13 (1.4043) and duplex stai nless steel X2CrNiMoN22 3 2 (1.4462) were compared at load amplitudes from 175 MPa to 325 MPa in the geothermal brine of the N orthern German Basin at 98 °C. Surface corrosion layers and pits reveal carbonate corrosion products on the surface such as FeCO 3 and FeOOH as the main precipitation phases with no dependence on the original surface roughness . At high stress amplitudes above 275 MPa technical surfaces (P50% at σa 300 MPa=5 × 10 5 ) resulted in more cycles to failure than polished (P50% at σa 300 MPa=1.5 × 10 5 ). The greater slope coefficient for technical surfaces k = 19.006 compared to polished surfaces k =8.78 demonstrate s earlier failure at given stress amplitude σa .
In service, most materials are operated under simultaneous corrosive and mechanical load and there are very few methods capable for testing material degradation under these conditions, especially when it comes to high resolution analysis. For this purpose, in this work, a tensile module capable of uniaxial stretching and compression with up to 5 kN force was integrated into an AFM stage. The elimination of the need for sample unmounting and remounting and the resulting possibility of keeping the sample under constant mechanical load during AFM measurements not only enables a precise positioning of the area of interest but also allows for the analysis of processes in the elastic deformation regime.
This methodology was demonstrated for two case studies. Scanning Kelvin Probe Force Microscopy (SKPFM) was used as the main tool to characterize the deformation behavior. Moreover, a flexible electrochemical measurement cell was used to enable electrochemical analysis by means of electrochemical impedance spectroscopy (EIS) and Linear Sweep Voltammetry (LSV) during AFM measurements at different levels of strain. The in situ AFM results are complemented by microstructure analysis by means of electron backscatter diffraction (EBSD).
In the first case study, the deformation induced delamination of a thin organic coating on AA2024 T3 aluminium alloy was investigated as a function of alloy surface treatment. The formation of cracks in the insulating passive film enabled an early detection of deformation processes by means of SKPFM. The second case study focused on the comparison of corrosion and deformation behavior of conventional and additively manufactured 316 stainless steels. In comparison to the conventional 316 stainless steel, the effect of processing was clearly detectable on the additively manufactured material as zones of inhomogeneous potential, which also affected the initiation of local corrosion processes. The contribution will provide detailed information on the new AFM setup and summarize our results from both case studies.
The performance of functional coatings and adhesively joined hybrid components relies strongly on the stability of the polymer-metal interface. With the increasing utilization of multi-material structures in the automotive and aerospace industry, it is of great scientific and technical interest to understand the processes leading to interface degradation and to develop novel strategies to increase corrosion and delamination resistance.
The aim of this project is to develop thin epoxy-based films and their carbon nanofiller loaded composites on aluminium alloy AA2024-T3 as a model system and to investigate their interfacial stability under corrosive and coupled corrosive-mechanical load. Spin coating was used for the layer-by-layer deposition of poly[(o-cresyl glycidyl ether)-co-formaldehyde] and poly-(ethylenimine) bi-layers. Atomic force microscopy (AFM) results indicate a very homogeneous and dense film with low surface roughness. Carbon nanofillers were introduced either by mixing into the coating components or in between individual layers to control the separation between the carbon nanofillers and alloy surface. The film chemistry and barrier properties were characterized by means of spectroscopic and electrochemical methods, respectively. The degradation and delamination behavior of the epoxy-based films was characterized by means of in situ AFM corrosion experiments. The quantitative imaging (QI) mode allowed the observation of hydrogen-generation induced blister formation during exposure to corrosive electrolyte and how the local corrosion processes evolved with exposure time. Complementary energy dispersive X-ray spectroscopy (EDX) analysis was performed to correlate the corrosion behavior with the different intermetallic particle chemistries and distributions. The presentation will summarize our results on the effect of interface chemistry and carbon nanofiller – alloy separation on the initiation of local corrosion processes on thin film covered AA2024-T3 aluminium alloys.
The presentation summarizes our recent results on the coupled electrochemical methods for high resolution corrosion studies. The combination of Scanning Electrochemical Microscopy (SECM) and multielectrode (MMA) based real-time corrosion monitoring was presented as a new method for achieving high time resolution in local electrochemical analysis. Correlative imaging by means of Atomic Force Microscopy (AFM) and Scanning Electron Microscopy (SEM) was demonstrated as a tool for the investigation of local corrosion processes initiated by the intermetallic particles (IMPs) on AA2024-T3 aluminium alloy.
Roaldite – Fe4N – has been identified in the São Julião de Moreira iron meteorite using electron backscatter diffraction (EBSD) and simultaneously acquired energy-dispersive x-ray spectroscopy (EDS). Mean-periodic-number images derived from raw EBSD patterns confirm this phase by an even higher spatial resolution compared to EDS.
Roaldite appears in the form of systematically and repetitively aligned plates. Despite the locally heavy plastic deformation, it is shown that the origin of the oriented precipitation of roaldite is linked to the orientation of the kamacite matrix. Roaldite can be considered to be precipitated from kamacite using an inverse Kurdjumov-Sachs (K-S) or Nishiyama-Wassermann (N-W) orientation relationship. A more accurate discrimination is impossible due to the accumulated shock deformation, which blurs the local reference orientation of kamacite. The habit plane of roaldite is found to be {112}R, which is most likely parallel to {120}K of kamacite. Some of the roaldite plates contain two orientation variants which repeatedly alternate. Their misorientation angle is about 12°.
The second edition of this textbook on physical electrochemistry, written by two experienced teachers of physical chemistry, corrosion engineering and materials science and engineering, covers the current knowledge which should be transferred to students of these fields.
In 20 chapters the fundamentals of electrochemistry, the most important electrochemical measurement techniques and applications of electrochemistry are covered.
It can be concluded that this study fulfills its intension of “serving as a key textbook in undergraduate courses” dealing with electrochemistry and being “a reference source for graduated students, researchers and engineers” interested in this field. Teachers will find sufficient content for preparing lectures on this topic. Even self‐learning is well supported by the clear structure, presented content and provided sources for further reading.