Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
Dokumenttyp
- Vortrag (40)
- Zeitschriftenartikel (19)
- Beitrag zu einem Tagungsband (12)
- Posterpräsentation (11)
- Buchkapitel (1)
- Beitrag zu einem Sammelband (1)
Sprache
- Englisch (84)
Schlagworte
- Hydrogen (84) (entfernen)
Organisationseinheit der BAM
- 9 Komponentensicherheit (63)
- 9.0 Abteilungsleitung und andere (36)
- 9.4 Integrität von Schweißverbindungen (22)
- 9.5 Tribologie und Verschleißschutz (16)
- 6 Materialchemie (8)
- 5 Werkstofftechnik (7)
- 5.1 Mikrostruktur Design und Degradation (7)
- 6.1 Oberflächen- und Dünnschichtanalyse (6)
- 9.2 Versuchsanlagen und Prüftechnik (6)
- 6.2 Material- und Oberflächentechnologien (2)
Paper des Monats
- ja (2)
Modeling of Hydrogen-Assisted Cracking (HAC) in Duplex Stainless Steels (DSS):
- Hydrogen causes significant degradation in DSS and consequently HAC
- Mechanisms of HAC have not been fully understood in two-phase microstructures
- Mesoscale numerical modeling for HAC in DSS was created, coupled to the macroscale, enabling simulation of HAC in both phases independent from predefined crack paths
The steel grade 20MnMoNi5-5 (according to German DIN standard or 16MND5 according to French AFNOR standard) is widely applied in (weld) fabrication of reactor pressure vessel components. Thus, a wide range of welding technologies (like submerged arc welding (SAW) or tungsten inert gas (TIG)) is used resulting in different heat affected zone (HAZ) microstructures. During weld fabrication, the weld joints may take up hydrogen. Especially, the HAZ shows an increased susceptibility for a degradation of the mechanical properties in presence of hydrogen. In addition, the hydrogen-assisted degradation of mechanical properties is influenced by three main local factors: hydrogen concentration, microstructure, and load condition. Hence, the base material (BM) and two different simulated non-tempered as-quenched HAZ microstructures were examined using hydrogen-free and hydrogen-charged tensile specimens. The results indicate that the effect of hydrogen on the degradation is significantly increased in case of the HAZ compared to the BM. In addition, hydrogen has remarkable effect in terms of reduction of ductility. It was ascertained that the degradation of the mechanical properties increases in the order of BM, bainitic HAZ, and the martensitic HAZ. Scanning electron microscope (SEM) investigation showed a distinct change of the fracture topography depended on the microstructure with increasing hydrogen concentration in case of the as-quenched HAZ microstructures.
Neutron imaging
(2016)
Neutron imaging methods are appropriate to investigate hydrogen distributions in several metallic systems. The large total neutron cross section of hydrogen compared to those of elements or isotopes, respectively, in usual structural materials like steels or zirconium alloys allows the detection even of small amounts of hydrogen in such materials. The dependence of the total macroscopic neutron cross section of the sample or component on the hydrogen concentration can be determined experimentally by means of calibration specimens with known hydrogen concentrations. Such a calibration allows for a full quantitative determination of the local hydrogen concentration with a spatial resolution better than 20 μm. Because neutron radiography is fast and non-destructive, in situ investigations of time-dependent processes like hydrogen absorption and release or hydrogen bulk diffusion can be performed. This chapter gives an introduction into the main neutron imaging methods, radiography and tomography, and gives as examples results of neutron imaging investigations of hydrogen in different steels and in zirconium alloys,respectively.
The polymer chemical structure of the polyimide has a major influence on the tribological behaviour. The addition of graphite in PI2 has a beneficial effect in hydrogen on the friction and wear. The low friction of graphite is associated with a lubricant film in hydrogen. The influence of hydrogen on graphite is more effective than humidity. CNTs have a similar effect to that of graphite in PEEK composites. TiO2 particles improve significantly the wear rate both in vacuum and hydrogen environment. In LH2 friction and wear decrease for unfilled polymers. Friction of graphite filled composites increases slightly and wear rate is stable.