Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2019 (118) (entfernen)
Dokumenttyp
- Vortrag (52)
- Beitrag zu einem Tagungsband (30)
- Zeitschriftenartikel (25)
- Posterpräsentation (9)
- Forschungsbericht (2)
Schlagworte
- Additive manufacturing (12)
- Laser implantation (12)
- Additive Manufacturing (11)
- Laser beam welding (11)
- TiB2 (11)
- Thermography (10)
- Surface texturing (9)
- Additive Fertigung (8)
- AISI D2 (7)
- Laser Metal Deposition (7)
Organisationseinheit der BAM
- 9.3 Schweißtechnische Fertigungsverfahren (118) (entfernen)
Eingeladener Vortrag
- nein (52)
The deep penetration laser beam welding (LBW) has developed to one of the most promising metal joining methods in the modern manufacturing industry. It has well-known advantages of good penetration capacity, low heat input, high reachable welding speed and low welding distortion in comparison to conventional arc welding techniques. However, there are still challenges in LBW making the realization of the advantages difficult, such as porosity or inhomogeneous element distribution when using filler material. The magnetohydrodynamics technique is a promising way to solve these issues by introducing a suitable electromagnetic field, and correspondingly Lorentz force, to control the Transport phenomena in the weld pool.
The underlying physics in wire feed laser beam welding with electromagnetic stirring were investigated numerically and experimentally. A three-dimensional transient heat transfer and fluid flow model coupled with dynamic keyhole, magnetic induction and element transport was developed for the first time. The electromagnetic behaviour as well as the temperature and velocity profiles, solidification parameters, keyhole evolution and element transport are calculated.
The model is well tested against the experimental results. The beneficial effects from electromagnetic stirring (element homogenization and grain refinement) are explained quantitatively using the numerical data and the results from high-speed imaging, OM, EDX and EBSD.
Das DED Auftragschweißen ist ein additives Fertigungsverfahren für Metalle, bei dem das Material schichtweise auf ein Substrat aufgetragen wird. Die schnellen Temperaturzyklen rufen Spannungsgradienten im Bauteil hervor. Der schichtweise Aufbau der Bauteile verursacht eine anisotrope Mikrostruktur. Mittels nachgelagerter Wärmebehandlung können diese Effekte verringert werden. Im anschließenden Schritt der Prozesskette wird das additiv hergestellte Bauteil mittels Drahterodieren von dem Substrat abgetrennt.
In diesem Beitrag wird eine thermo-mechanische Simulation der gesamten Prozesskette vorgestellt, welche den additiven Aufbau, Wärmebehandlung und das Abtrennen vom Substrat beinhaltet. Anstelle der in der Literatur üblichen schichtweisen Modellierungsstrategie für die DED Simulation wird das gesamte Bauteil in einem Stück vernetzt und der vollständig transiente, schichtweise Materialauftrag über Elementgruppen realisiert. Im Gegensatz zu früheren Simulationen muss der nichtlineare Kontakt zwischen den Schichten nicht berücksichtigt werden, was die Rechenzeiten deutlich verkürzt.
Das Modell wurde validiert mittels Abgleiches des Verzugs aus Simulation und Experiment.
Die Proben, bestehend aus DIN 1.4404 (AISI 316L), wurden nach jedem Prozessschritt 3D gescannt um den Verzug zu quantifizieren. Zusätzlich wurden Querschnitte und Härtetests nach Vickers von unterschiedlich behandelten Proben durchgeführt, um den Effekt der Wärmebehandlung auf die Mikrostruktur und die Härte des Bauteils zu untersuchen.
Die Präsentation gibt einen Überblick bezüglich der von der BAM im Rahmen des SimCoLas Verbundprojekts durchgeführten Arbeiten zum Thema "Photonische Prozessketten". Die numerisch abgebildete Prozesskette Tiefziehen/Laserstrahlschweißen wird darsgestellt und diskutiert. Fokus der Diskussion ist die entwickelte Methodik zur konsistenten Abbildung numerischer Prozessketten mit der Applikation Heissrisskritikalität beim Laserstrahlschweißen.
Der Vortrag gibt einen Überblick über Arbeiten im Rahmen der Themenstellung "photonische Prozessketten" des SimCoLas Projekts. Es werden Ergebnisse zur Datendurchgängigkeit der Prozesskette Umformen/Laserstrahlschweißen sowie erste Ergebnisse zu numerischen Schweißstruktursimulationen zur Bewertung der Heissrisskritikalität eines tiefgezogenen Napfes beim Laserstrahlschweißen gegeben.
The potential of lowered surface features as well as the application of wear resistant coatings have been known for many years to improve the tribological behavior of forming tools. More recent studies also discuss the capability of protruded microfeatures for adjusting the tribological behavior between contacting surfaces. The demand for a high wear resistance of such structures as well as their economical and reliable production, however, often limits the industrial application. The laser implantation process can overcome these limitations. In contrast to conventional cw-laser dispersing processes, where the formation of uniform metal matrix composite layers is intended, this surface engineering technique aims to improve the tribological behavior of contacting surfaces by a localized dispersing of pre-placed hard ceramic particles. This enables the formation of deterministic textures composed of separated wear resistant dome- or ring-shaped microstructures (implants).
Since TaC shows very promising material properties for improving the wear resistance of tools exposed to severe operating conditions, this paper analyzes its suitability for pulsed laser implantation on X38CrMoV5-3 tool steel for the first time. In the experiments, the influence of the particles and the laser parameters (pulse power, pulse duration and focal diameter) on the material properties of the localized dispersed zones was studied by optical microscopy, scanning electron microscopy, energy dispersive X-ray spectroscopy and X-ray diffraction. The composite´s (micro-) hardness was measured and calculated by using a rule of mixture. Additionally, the influence of the laser parameters and the TaC particles on the geometrical properties of the implants was studied by optical microscopy and white light interferometry.
The results showed that defect-free implants with hardness values of ~900 HV1 can be obtained at the focal spot, since a localized dispersing of the TaC particles is possible using a pulsed millisecond laser. However, in dependence of the laser intensity, also a partial dissolution of the initial particles occurs. This leads to the precipitation of new dendritic TaC nanoparticles and to varying contents of retained austenite in the matrix. Both effects have a strong influence on the implant hardness and must be considert by the rule of mixture. Regarding the geometrical response it was pointed out that protruded microfeatures with heights up to 10 µm can be created. In comparison to laser remelted zones, the implanted zones showed significantly altered weld pool profiles due to the influence of the particles on the melt convection. A transition of the implant shape from predominantly dome-shaped to predominantly ring-shaped was observed for intensities >1.7∙106 W/cm2 due to the onset of the keyhole effect.
Laser beam welding of aluminum die casting is challenging. A large quantity of gases (in particular hydrogen) is absorbed by aluminum during the die-cast manufacturing process and is contained in the base material in solved or bound form. After re-melting by the laser, the gases are released and are present in the melt as pores. Many of these metallurgic pores remain in the weld seam as a result of the high solidification velocities. The natural (Archimedean) buoyancy is not sufficient to remove the pores from the weld pool leading to process instabilities and poor mechanical properties of the weld. Therefore, an electromagnetic (EM) system is used to apply an additional buoyancy component to the pores. The physical mechanism is based on the generation of Lorentz forces, whereby an electromagnetic pressure is introduced into the weld pool. The EM system exploits the difference in electrical conductivity between poorly conducting pores (inclusions) and the comparatively better conducting aluminum melt to increase the resulting buoyancy velocity of the pores. Within the present study, the electromagnetic supported degassing is investigated in dependence on the laser beam power, welding velocity and electromagnetic flux density. By means of a design of experiments a systematic variation of these parameters is carried out for partial penetration laser beam welding of 6 mm thick sheets of wrought aluminum alloy AlMg3 and die-cast aluminum alloy AlSi12(Fe) where the wrought alloy serves as a reference. The proportion of pores in the weld seams is determined using X-ray images, computed tomography (CT-) images and cross-section images. The results prove a significant reduction of the porosity up to 70 % for both materials as a function of the magnetic flux density
The paper describes a systematic investigation of the EM influenced laser beam welding of the aluminum die casting alloy AlSi12(Fe) in comparison to a reference material, a wrought aluminum alloy AlMg3. By using of a face centred CCD test plan, the influencing variables laser power, welding velocity and magnetic flux density are varied with regard to their influence on the remaining porosity. The global pore fraction of the weld seams was analyzed by X-ray images with ImageJ. This enabled a qualitatively very good regression model to be derived for the respective material, which identifies the dominant influencing variables. The results prove, statistically verified, for the investigated parameter range, that
- the magnetic flux density is the main cause for the porosity reduction,
- the porosity rises with increasing laser power the porosity in the weld seams rises,
- the influence of the welding velocity is negligible,
- the pore quantity in wrought alloy is more strongly minimized by the magnetic flux density than in die casting,
- the porosity decreases due to the EM influence by approx. 70 % compared to the unaffected welds. This effect is emphasized by the contour line charts, which illustrate the relationship between laser power and magnetic flux density.
With the exception of the quadratic influence of B at the wrought alloy, the statistical correlation shows a linear development of the respective influence variables for both aluminum alloys. In order to investigate these deviations, further simulations with a focus on weld pool geometry and weld pool flow are to be performed. In addition, the welding results can be classified in accordance with DIN EN ISO 13919-2 in the highest evaluation group B for AlMg3 and in evaluation group C for AlSi12(Fe) by applying a magnetic flux density of 350 mT. The analysis of the CT images at constant laser power and welding velocity allows a direct comparison both between the two alloys and also as a function of the magnetic flux density with regard to the number and size of pores. An increase in the magnetic flux density leads to a significant decrease in the number and volume of pores, which can be seen more clearly in wrought alloy than in die casting. Very acceptable results can be achieved for both materials and different welding parameters. This successfully demonstrates the desired process robustness and functionality of the EM system for practical applications. For subsequent investigations of overlap joints, the lowest possible laser power and a high magnetic flux density are recommended.
The laser-based direct energy deposition (DED) as a technology for additive manufacturing allows the production of near net shape components. Industrial applications require a stable process to ensure reproducible quality. Instabilities in the manufacturing process can lead to faulty components which do not meet the required properties.
The DED process is adjusted by various parameters such as laser power, velocity, powder mass flow and spot diameter, which interact with each other. A frequently used comparative parameter in welding is the energy per unit length and is calculated from the laser power and the velocity in laser welding. The powder per unit length comparative parameter in the DED process has also be taken into account, because this filler material absorbs energy in addition to the base material.
This paper deals with the influence of mass energy as a comparative parameter for determining the properties of additively manufactured parts. The same energy per unit length of 60 J/mm as well as the same powder per unit length of 7.2 mg/mm can be adjusted with different parameter sets. The energy per unit length and the powder per unit length determine the mass energy. The laser power is varied within the experiments between 400 W and 900 W. Energy per unit length and powder per unit length are kept constant by adjusting velocity and powder mass flow. Using the example of Inconel 718, experiments are carried out with the determined parameter sets. In a first step, individual tracks are produced and analyzed by means of micro section. The geometry of the tracks shows differences in height and width. In addition, the increasing laser power leads to a higher dilution of the base material. To determine the suitability of the parameters for additive manufacturing use, the individual tracks are used to build up parts with a square base area of 20x20 mm². An investigation by Archimedean principle shows a higher porosity with lower laser power. By further analysis of the micro sections, it can be seen that at low laser power, connection errors occur between the tracks.
The results show that laser power, velocity and powder mass flow have to be considered in particular, because a constant mass energy can lead to different geometric as well as microscopic properties.
Im Vortrag werden Ergebnisse eines Forschungsvorhabens des DVS vorgestellt, in dem ein Verfahren zur Vermeidung von Schweißimperfektionen im Überlappbereich einer laserstrahlhybridgeschweißten Rundnaht entwickelt wird. Die Strategie der Prozessführung beim Schließen der Rundnaht sieht hervor, dass ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG-Schweißprozess realisiert. Es konnte gezeigt werden, dass eine Defokussierung des Laserstrahls von bis zu 40 mm über den Weg von max. 15 mm während der Bewegung des Schweißkopfes zu einer deutlich besseren Nahtausbildung im Überlappbereich führt. Es konnte eine günstige kelchförmige Schweißnahtform ohne eine Tendenz zur Rissbildung erzielt werden.
Localized laser surface treatments are able to produce tailor-made surface properties to fulfill requirements of a variety of technical applications. Especially micrometric surface topologies can be beneficial for optimizing tribological contact situations. Structures with lowered surface features are already utilized for bearings or cylinders of combustion engines. There are also other fields of application, where the potential of protruding surface features is known, e. g. for metal forming tools.
A promising approach for a tailored surface treatment working in the microsecond range is the localized dispersing of hard ceramic particles by pulsed laser radiation, the so-called laser implantation. This technique is able to produce micrometric surface structures and to improve simultaneously the wear resistance by creating metal matrix composites.
In this talk, the laser implantation technique is described and compared to the state of the art. The potential to adjust the geometry as well as the mechanical properties of laser implanted surfaces is demonstrated by means of microstructural and topographical investigations of different ceramic materials and steel substrates. Finally, results of research projects are presented aiming on the application of such structured surfaces. Their capability to change and optimize friction and wear are demonstrated for fully lubricated contacts, tools for hot sheet metal forming and tools for cold rolling of sheets for automotive applications.