Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2023 (734) (entfernen)
Dokumenttyp
- Vortrag (284)
- Zeitschriftenartikel (260)
- Posterpräsentation (79)
- Forschungsdatensatz (56)
- Beitrag zu einem Tagungsband (34)
- Buchkapitel (6)
- Sonstiges (5)
- Dissertation (2)
- Video (2)
- Monografie (1)
Sprache
- Englisch (734) (entfernen)
Schlagworte
- Additive manufacturing (40)
- Automation (25)
- Nanoparticles (24)
- SEM (23)
- X-ray scattering (23)
- XPS (22)
- Additive Manufacturing (21)
- HAXPES (21)
- SAXS (20)
- Laser beam welding (18)
Organisationseinheit der BAM
- 6 Materialchemie (317)
- 9 Komponentensicherheit (150)
- 5 Werkstofftechnik (130)
- 6.1 Oberflächen- und Dünnschichtanalyse (86)
- 8 Zerstörungsfreie Prüfung (73)
- 6.3 Strukturanalytik (71)
- 6.0 Abteilungsleitung und andere (66)
- 9.4 Integrität von Schweißverbindungen (64)
- 7 Bauwerkssicherheit (60)
- 6.6 Physik und chemische Analytik der Polymere (57)
Paper des Monats
- ja (27)
The presentation gives an overview of two slurry-based additive manufacturing (AM) technologies specifically developed for advanced ceramic materials.
The “Layerwise Slurry Deposition” (LSD-print) is a modification of Binder Jetting making use of a ceramic slurry instead of a dry powder as a feedstock. In this process, a slurry is deposited layer-by-layer by means of a doctor blade and dried to achieve a highly packed powder layer, which is then printed by jetting a binder. The LSD-print technology combines the high-speed printing of binder jetting with the possibility of producing a variety of high-quality ceramics with properties comparable to those achieved by traditional processing.
The Laser Induced Slip casting (LIS) technology follows a novel working principle by locally drying and selectively consolidating layer-by-layer a ceramic green body in a vat of slurry, using a laser as energy source. LIS combines elements of Vat Photopolymerization with the use of water-based feedstocks containing a minimal amount of organic additives. The resulting technology can be directly integrated into a traditional ceramic process chain by manufacturing green bodies that are sintered without the need of a dedicated debinding.
Both technologies offer high flexibility in the ceramic feedstock used, especially concerning material and particle size. Advantages and disadvantages are briefly described to outline the specific features of LSD-print and LIS depending on the targeted application.
Additive Manufacturing for dental restorations by layerwise slurry deposition (LSD-print) technology
(2023)
The growing market of custom-made dental restorations offers a major potential for an application of ceramic additive manufacturing (AM).
The possibility to individualize patient specific design and to establish new efficient workflows, from model generation to manufacturing, can be fully exploited by AM technologies. However, for mass customization to be truly envisioned, ceramic AM needs to achieve a level of maturity, aesthetic quality, and productivity comparable to established manufacturing processes.
In this presentation, the potential of the “layerwise slurry deposition” LSD-print technology for dental applications will be explored. It has been shown in the past years that the LSD-print can be applied to advanced ceramic materials such as alumina and silicon-infiltrated silicon carbide. For these materials, the LSD-print technology combines the high-speed printing of binder jetting with the possibility of producing a variety of high-quality ceramics.
The current development deals with the challenges of applying this technology to a feldspar dental material, comparing the quality of AM restorations with the equivalent material for an established CAD/CAM workflow.
Preliminary results not only indicate that the AM material produced by LSD-print can be competitive in terms of mechanical properties, but also that aesthetically satisfactory restorations can be manufactured for veneers, inlays and onlays as well as single unit fixed dental prostheses (FDPs).
The presentation focuses on the material and technological challenges alongside the process chain, from the printing process, to debinding, firing and finishing the restorations.
Aero-engine turbine disks are safety-relevant components which are operated under high thermal and mechanical stress conditions. The actual part qualification and certification procedures make use of spin-tests conducted on production-similar disks. While these tests provide, on the one hand, a reliable definition of the critical conditions for real components, on the other hand they represent a relevant cost item for engine manufacturers. The aim of this work is to present two alternative burst speed assessment methods under development based on the Failure Assessment Diagram (FAD) and a global stability criterion, respectively. In the scope of the fracture mechanics assessment, the failure modes hoop-burst and rim-peeling are investigated with semicircular surface cracks modelled at the critical regions on the turbine disk. The comparison of the predicted critical rotational speed shows good agreement between the assessment methods.
Friction stir welding (FSW) has the capacity to join the Al/Ti dissimilar structures with superior mechanical properties. The microstructures and mechanical characteristics of Al/Ti dissimilar FSW joints are determined by the heat and mass transfer during the welding process. However, a quantitative study of the Al/Ti dissimilar FSW process is lacking. Therefore, using the computational fluid dynamics (CFD) and volume of fluid (VOF) approach, a multi-phase model was constructed for quantitatively analyzing the heat and mass transfer behaviour in dissimilar FSW of TC4 titanium alloy and AA2024-T4 aluminium alloy. The mixed material was treated as a functionally graded material (FGM) to compute the thermophysical characteristics at the weld nugget zone (WNZ). Due to the vast disparity in the thermophysical characteristics of aluminum and titanium alloy, the temperature field in Al/Ti dissimilar FSW was severely asymmetric. The temperature of titanium alloy on the advancing side (AS) was higher than that of aluminium alloy on the retreating side (RS) at the same distance from the tool centre line near the tool shoulder, but it was lower than that of aluminium alloy on the RS without the influence of the shoulder. Due to the high flow stress of titanium alloy, plastic material flow mostly occurred on the RS of aluminium alloy in the Al/Ti dissimilar FSW, with its percentage exceeding 80%. This model was validated by experiment results.
Effect of Polycarboxylate Superplasticizer in Ordinary Portland Cement and Sulfate Resistant Cement
(2023)
Polycarboxylate superplasticizers (PCE) are the most widely used admixtures in today’s cementitious construction materials. The molecular structure has a decisive influence on the effectiveness of PCE, which also can be tailored to serve in a different cementitious system.
The current study investigates the influence of the backbone charge density of PCE on the rheology, hydration kinetics, and adsorption behavior of ordinary Portland cement (OPC) and sulfate-resistant cement (SRC). The results indicate that regardless of the PCE type, OPC requires a higher amount of PCE to be adsorbed to induce changing of rheological parameters and hydration kinetics. Regardless of the cement type, the PCE with a higher charge density exhibits higher adsorption behavior, corresponding to lower viscosity measurement.
Compared to OPC, SRC is more sensitive to the introduction of both PCEs and has a lower saturation dosage, indicating that SRC generally provides better workability properties regardless of the PCE.
In the maritime context of offshore operation, corrosion, in combination with the materials used, poses a particular challenge to ensure safe operation over long indefinite periods and to minimise susceptibility to failure. Until today, only a few corrosion protection systems have proven themselves for the interaction of efficiency, installation, and maintenance in the offshore sector. In addition, available corrosion test methods sometimes have major deficits about conclusions of the durability. Therefore, there is more research and development needed.
The flagship project H2Mare of the Federal Ministry of Education and Research aims to enable the production of green hydrogen and PtX products at high seas. Research is being driven forward by the partners in four individual projects, where BAM is involved in two.
In PtX-Wind, major kinds of corrosion attacks at offshore constructions are characterized and investigated, and suitable corrosion protection measures determined. In TransferWind, attention focusses on transferring scientific results into standardization.
This poster at the H2Mare Conference 2023 presents an overview of the investigation methods and contribution of the department “Corrosion and Corrosion Protection”.
An observation of the fracture process in front of the crack tip inside a dentin sample by means of ex-situ X-ray computed tomography after uniaxial compression at different deformation values was carried out in this work. This ex-situ approach allowed the microstructure and fracturing process of human dentin to be observed during loading. No cracks are observed up to the middle part of the irreversible deformation in the samples at least visible at 0.4μm resolution. First cracks appeared before the mechanical stress reached the compression strength. The growth of the cracks is realized by connecting the main cracks with satellite cracks that lie ahead of the main crack tip and parallel its trajectory. When under the stress load the deformation in the sample exceeds the deformation at the compression strength of dentin, an appearance of micro-cracks in front of the main cracks is observed. The micro-cracks are inclined (~60°) to the trajectory of the main cracks. The further growth of the main cracks is not realized due to the junction with the micro-cracks; we assume that the micro-cracks dissipate the energy of the main crack and suppressed its growth. These micro-cracks serve as additional stress accommodations, therefore the samples do not break apart after the compression test, as it is usually observed under bending and tension tests.
Understanding the mechanical behavior of silicon nanowires is essential for the implementation of advanced nanoscale devices. Although bending tests are predominantly used for this purpose, their findings should be properly interpreted through modeling. Various modeling approaches tend to ignore parts of the effective parameter set involved in the rather complex bending response. This oversimplification is the main reason behind the spread of the modulus of elasticity and strength data in the literature. Addressing this challenge, a surface-based nanomechanical model is introduced in this study. The proposed model considers two important factors that have so far remained neglected despite their significance: (i) intrinsic stresses composed of the initial residual stress and surface-induced residual stress and (ii) anisotropic implementation of surface stress and elasticity. The modeling study is consolidated with molecular dynamics-based study of the native oxide surface through reactive force fields and a series of nanoscale characterization work through in situ threepoint bending test and Raman spectroscopy. The treatment of the test data through a series of models with increasing complexity demonstrates a spread of 85 GPa for the modulus of elasticity and points to the origins of ambiguity regarding silicon nanowire properties, which are some of the most commonly employed nanoscale building blocks. A similar conclusion is reached for strength with variations of up to 3 GPa estimated by the aforementioned nanomechanical models. Precise consideration of the nanowire surface state is thus critical to comprehending the mechanical behavior of silicon nanowires accurately. Overall, this study highlights the need for a multiscale theoretical framework to fully understand the size-dependent mechanical behavior of silicon nanowires, with fortifying effects on the design and reliability assessment of future nanoelectromechanical systems.
Overview of ongoing research and future prospects on polyethylene neutron shielding materials at bam
(2023)
The extension of the interim storage period of radioactive waste before disposal will cause additional challenges for the nuclear waste management in Germany, so that an extensive knowledge of the long-term performance of casks, including their components and inventories, will be required for future extended storage licenses.
Ultra-high and high molecular weight polyethylenes ((U)HMW-PE) are used for neutron shielding purposes in casks for storage and transport of spent fuel and high-level waste due to their extremely high hydrogen content. During their service life of several decades as cask components, the PE materials are exposed to neutron and gamma radiation from the radioactive inventory of the casks, mechanical assembling stresses and temperature. All these combined effects affect the material properties of such components which in turn may be crucial for some possible accident scenarios.
At the Bundesanstalt für Materialforschung und -prüfung (BAM), the effects of high temperature exposure in combination with subsequent or previous irradiation were investigated with a comprehensive aging program including thermal aging at 125 °C for different aging periods up to 5 years and irradiation with doses ranging from 50 to 600 kGy.
This contribution provides an overview of the ongoing research related to the structural changes of (U)HMW-PE induced by gamma irradiation and high temperature exposure and focuses on current research perspectives at BAM with regard to the prediction of the dynamic behavior of the material during extended interim storage in case of an accident scenario. First results of the coupled effect of temperature, radiation and mechanical loading will be presented. The effect of microstructural changes induced by gamma irradiation and high temperature on the mechanical behavior of (U)HMW-PE will be assessed.
Recovery is an important measure for seal applications representing to which extent the elastomer regains its initial shape after deformation and release of an applied force. Compression set (CS) indicates the degree of recovery. Ethylene propylene diene rubber (EPDM) was aged at 75 ◦C, 100 ◦C, 125 ◦C and 150 ◦C for different ageing times up to five years and compression set measurements were performed at different times after disassembly and after additional tempering. Short- and long-term recovery up to one year after release for samples aged at 125 ◦C and 150 ◦C was also studied. To assess the curvature in the Arrhenius diagram that may occur due to non-sufficiently aged specimens, a degradation-rate based model was fitted to the CS data after tempering. For each ageing temperature, two decay fit functions were proposed, each with an activation energy and a corresponding degradative process. The influence of ageing on the leak-tightness after fast small partial release is investigated and estimated through the analysis of the shift factors from time temperature superposition (TTS) of CS measurements at different times after disassembly. Shift factors of CS measurement after 1 s and after additional tempering are in good agreement.