Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Dokumenttyp
- Vortrag (12)
- Zeitschriftenartikel (6)
- Posterpräsentation (5)
- Beitrag zu einem Tagungsband (4)
- Dissertation (1)
- Forschungsbericht (1)
Schlagworte
- Aluminium (29) (entfernen)
Organisationseinheit der BAM
- 5 Werkstofftechnik (11)
- 5.2 Metallische Hochtemperaturwerkstoffe (11)
- 7 Bauwerkssicherheit (4)
- 7.6 Korrosion und Korrosionsschutz (4)
- 6 Materialchemie (3)
- 8 Zerstörungsfreie Prüfung (2)
- 8.5 Röntgenbildgebung (2)
- 4 Material und Umwelt (1)
- 4.2 Material-Mikrobiom Wechselwirkungen (1)
- 6.2 Material- und Oberflächentechnologien (1)
Eingeladener Vortrag
- nein (12)
The performance of adhesively joined hybrid components relies strongly on the stability of the adhesive-material interface. With the increasing utilization of multi-material structures in the automotive and aerospace industry, it is of great scientific and technical interest to understand the processes leading to adhesive failure and to develop novel strategies to increase corrosion and delamination resistance of adhesive joints.
The aim of this study is to develop thin epoxy based films and their carbon nanofiller loaded composites on aluminium alloy AA2024-T3 and to investigate their interfacial stability under corrosive and coupled corrosive-mechanical load. Spin coating was used for the layer-by-layer deposition of poly[(o-cresyl glycidyl ether)-co-formaldehyde] and poly-(ethylenimine) bi-layers. Carbon nanofillers are introduced either by mixing into the coating components or in between individual layers. Cyclic voltammetry (CV) and electrochemical impedance spectroscopy (EIS) analysis was performed to investigate the porosity and water uptake of the model films, respectively. Atomic force microscopy (AFM) results indicated a very homogeneous and dense film with low surface roughness. The bi-layer thickness ranged between 30 to 40 nm. Electrochemical measurements show a higher corrosion resistance with the increase of the bi-layer number.
The main novelty of this contribution is the in-situ AFM investigations under coupled corrosive-mechanical load. For this purpose, a tensile module capable of uniaxial stretching and compression with up to 5 kN force was integrated into the AFM stage. Stretching experiments were performed to investigate the mechanical properties and adhesion of the films, as well as structural changes of the film morphology during uniaxial deformation. The contribution will provide detailed information on the new AFM setup and summarize our results on the stability of model epoxy and nanocomposite films on AA2024-T3.
The influence of heat treatment and creep loading on the microstructure of an Al-Cu-Li alloy was investigated. Especially the formation of different precipitates (T1 and Theta') were characterized and the microstructural changes under different ageing conditions (with and without external strain) were investigated to determine the effect od stress on the ageing process.
The influence of heat treatment and creep loading on the microstructure of an Al-Cu-Li alloy was investigated. Especially the formation of different precipitates (T1 and Theta') were characterized and the microstructural changes under different ageing conditions (with and without external strain) were investigated to determine the effect od stress on the ageing process.
The fabrication and characteristics of amorphous silica reinforced Al matrix composites are studied in this paper. The major starting materials were commercial Al powder and extracted nanoparticle SiO2 (NPS) powder from Indonesian silica sands. Two different active solutions,namely N-butanol and tetramethylammonium hydroxide (TMAH), were introduced during synthesis. Characterisations in terms of physical, mechanical, microstructural and corrosion rate examinations were also employed. Introducing the SiO2 nanoparticles into the Al matrix has decreased the density and increased the porosity of the composites. The addition of N-butanol into Al/SiO2(Al/SiO2(B)) led to broader and lower X-ray diffraction profiles than the addition of TMAH (Al/SiO2(T)). From the microstructural analysis, we found that the SiO2 particles enter and agglomerate into the opening gap of the Al sheets. Furthermore, yield strength, ultimate compression strength and modulus of elasticity tended to reduce the addition of SiO2. The corrosion rate of Al/SiO2(T) was lower than that of Al/SiO2(B) composites.