Over the past decades research on the molecular dynamics of miscible polymer blends is of topical interest in the literature, to understand the segmental mobility of individual components, as it is affected by blending. In general, miscible polymer blends exhibit a complex dynamic behavior. For an A/B blend the relaxation times of component A and component B are affected by the spatial local compositional heterogeneity, present in binary systems on a microscopic level, regardless of the macroscopic homogeneity. Here, a combination of broadband dielectric and specific heat spectroscopy was employed to study the dynamically asymmetric PVME/PS blend with seven different compositions, focusing on samples with high PS contents. Considering that PS is dielectrically invisible, BDS is a powerful technique to study the response of PVME, as it is affected by PS segments. Here, three separate relaxation processes were found by dielectric investigations, related to confined or constrained PVME segments due to the spatial local compositional heterogeneities, which is in contrary to the previous literature findings [1]. Moreover, the dielectric data was compared with results obtained by specific heat spectroscopy, where a fourth relaxation process was found, due to the cooperative fluctuations of PVME and PS.
[1] Colmenero, J., Arbe, A. Soft Matter, 2007, 3, 1474.
The molecular mobility of the highly asymmetric miscible blend poly(vinyl methyl ether)/polystyrene was investigated by broadband dielectric (frequency range 10^-1 Hz – 10^9 Hz) and specific heat spectroscopy (frequency range 10^1 Hz – 10^4 Hz). The dielectric spectra revealed a complex molecular dynamic behavior, where three different relaxation processes were observed. At temperatures below the glass transition temperature an α´-relaxation was found, with an Arrhenius-like temperature dependence of its relaxation rates. It is assigned to localized fluctuations of the confined PVME segments within a frozen glassy matrix dominated by PS. Above the thermal glass transition temperature two processes with a VFT behavior of their relaxation rates were detected called α1- and α2-relaxation, both originating from PVME dipoles fluctuating in PS-rich environments, however with diverse PS concentrations. The relevant length scales for the processes are assumed to be different, corresponding to the Kuhn segment length for the former relaxation and to the CRR for the latter one. The observed multiple glassy dynamics result from spatial local compositional heterogeneities on a microscopic level. Additionally, SHS investigations were performed for the first time for this system, proving an existence of a fourth relaxation process (α3-relaxation) due to the cooperative fluctuations of both PS and PVME segments. The separation between the thermal α3- and dielectric α2-relaxation increases dramatically with increasing polystyrene concentration, proving that the thermal response is dominated by PS.
Broadband dielectric spectroscopy in the frequency range from 10-1 to 109 Hz is employed to revisit the segmental dynamics of the miscible blend system poly(vinyl methyl ether)/polystyrene (PVME/PS) in dependence on the composition firstly in the bulk state. Here especially the case of high polystyrene concentrations is considered. It is important to note that only the molecular dynamics of PVME segments as affected by PS is observed because the dipole moment of polystyrene is negligible. Three relaxation processes are found which are due to fluctuations of differently constrained or confined PVME segments. The degree of the confinement of PVME segments due to PS is discussed in dependence on the composition.
Further a spatial confinement is considered by investigating thin films of the PVME/PS blend where the film thickness was varied from 100 nm down to 5 nm. Two concentrations of PVME/PS (50/50 wt% and 25/75 wt%) are investigated. To measure nanometer thick films a novel electrode system based on nanostructured electrodes was employed. Nanostructured electrodes can be considered as a cut-edge technology in dielectric spectroscopy. The relaxation spectra of the films showed multiple processes which are discussed in dependence on the film thickness.