In this paper shortwave infrared (SWIR) thermographic measurements of the manufacturing of thin single-line walls via laser metal deposition (LMD) are presented. As the thermographic camera is mounted fixed to the welding arm, an acceleration sensor was used to assist in reconstructing the spatial position from the predefined welding path. Hereby we could obtain data sets containing the size of the molten pool and the oxide covered areas as functions of the position in the workpiece. Furthermore, the influence of the acquisition wavelength onto the thermograms was investigated in a spectral range from 1250 nm to 1550 nm. All wavelengths turned out to be usable for the in-situ process monitoring of the LMD process. The longer wavelengths are shown to be beneficial for the lower temperature range, while shorter wavelengths show more details within the molten pool.
Laser Metal Deposition (LMD) as a technology for additive manufacturing allows the production of large components outside of closed working chambers. Industrial applications require a stable process as well as a constant deposition of the filler material in order to ensure uniform volume growth and reproducible mechanical properties. This paper deals with the influence of travel path strategies on temperature profile and material deposition. Meandering and spiral hatching strategies are used in the center as well as in the edge of a specimen. The temperature is measured with thermocouples attatched to the backside of the specimen. The tests are carried out on the materials S235JR and 316L. The results show a strong dependence of the maximum temperatures on the travel path strategy and the welding position on the component.