Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2019 (118) (entfernen)
Dokumenttyp
- Vortrag (52)
- Beitrag zu einem Tagungsband (30)
- Zeitschriftenartikel (25)
- Posterpräsentation (9)
- Forschungsbericht (2)
Schlagworte
- Additive manufacturing (12)
- Laser implantation (12)
- Additive Manufacturing (11)
- Laser beam welding (11)
- TiB2 (11)
- Thermography (10)
- Surface texturing (9)
- Additive Fertigung (8)
- AISI D2 (7)
- Laser Metal Deposition (7)
- Numerical simulation (7)
- Laserstrahlschweißen (6)
- Thermografie (6)
- 3D printing (5)
- Hybrid Laser Arc Welding (5)
- X38CrMoV5-3 (5)
- 3D Druck (4)
- Direct energy deposition (4)
- Duplex (4)
- Highspeed-plasma-laser-cladding (4)
- Keyhole mode welding (4)
- Low Cycle Fatigue (4)
- Mechanical properties (4)
- Open data (4)
- Open science (4)
- Solidification cracking (4)
- Ti-6Al-4V (4)
- Additive Manufacturing (AM) (3)
- Computed Tomography (3)
- Deposition welding (3)
- Digitalization (3)
- Electromagnetic Weld Pool Support (3)
- Element transport (3)
- End crater (3)
- Full Penetration (3)
- Heat conduction (3)
- High power laser beam welding (3)
- Hot-Stamping (3)
- Hybrid laser-arc welding (3)
- Inconel 718 (3)
- LPA (3)
- Laser Powder Bed Fusion (L-PBF) (3)
- Laser Pulver Auftragsschweißen (3)
- Laser metal deposition (3)
- Laserimplantation (3)
- Magnetohydrodynamics (3)
- Microstructure (3)
- Process monitoring (3)
- Research data management (3)
- Thick Materials (3)
- Weld pool shape (3)
- Welding (3)
- Advanced high strength steel (2)
- Aerosol measurements (2)
- Auftragschweißen (2)
- Boundary element method (2)
- Bulging effect (2)
- CT (2)
- Computed tomography (2)
- DED (2)
- Defokussierung (2)
- Direct Energy Deposition (2)
- Direct Laser Metal Deposition (2)
- Dual phase steel (2)
- End-crater (2)
- Endkrater (2)
- Fatigue (2)
- Fume (2)
- High Temperature Testing (2)
- Hot cracking (2)
- Keyhole mode laser beam welding (2)
- Korrosionsschutz (2)
- LCF (2)
- LMD (2)
- LME (2)
- Laser (2)
- Laser Beam Welding (2)
- Laser Powder Bed Fusion (2)
- Laser beam melting (2)
- Laser dispersing (2)
- Laserhybridschweißen (2)
- MHD (2)
- Mikrostruktur (2)
- Molten pool dynamics (2)
- NDT (2)
- NiCrBSi (2)
- Online Process Monitoring (2)
- Optical Tomography (2)
- Partial penetration (2)
- Particle gas emission (2)
- Pipeline steel X120 (2)
- Plasma (2)
- Plasma-Transferred-Arc (2)
- Plume (2)
- Porosity (2)
- Powder Bed Fusion (2)
- Presshärten (2)
- Process simulation (2)
- Prozesskette (2)
- Pufferschichten (2)
- RSW (2)
- Residual stress (2)
- Resistance spot welding (2)
- Rundnaht (2)
- Selected Laser Melting (2)
- Selective Laser Melting (2)
- Simulation (2)
- Solidification (2)
- Spatter (2)
- Stainless Steel (2)
- Superelliptic Lamé curves (2)
- Temperature field (2)
- Tensile Properties (2)
- Testing method (2)
- Ti64 (2)
- TiAl5V4 (2)
- Titan (2)
- Titanium (2)
- Tribologie (2)
- Tungsten carbide (2)
- Wear resistance (2)
- Weld pool behavior (2)
- Weld pool shape approximation (2)
- Zinc coated steel (2)
- Zugeigenschaften (2)
- Überlappbereich (2)
- AGIL (1)
- AM (1)
- Acoustic Emission (1)
- Advanced high strength steels (1)
- Aluminium-Druckguss (1)
- Artungleiche Werkstoffe (1)
- Auftriebskräfte (1)
- Bewegtes Gitter (1)
- Bulge (1)
- Bulging (1)
- Calculation time (1)
- Characterisation (1)
- Circumferential weld (1)
- Circumferential welds (1)
- Coarse-grained heat-affected zone (1)
- Computed tomography (CT) (1)
- Crack (1)
- Crack propagation (1)
- Cracking (1)
- Critical strain (1)
- Cryogenic Steel (1)
- Crystal Plasticity Modelling (1)
- DED-L (1)
- Data fusion (1)
- Digitalisierung (1)
- Directed Energy Deposition (1)
- Directed energy deposition (1)
- Dissimilar metal weld overlays (1)
- Distortion (1)
- Distortion simulation (1)
- Efficient modelling (1)
- Electro-thermomechnical model (1)
- Electrode geometry (1)
- Electromagnetic stirring (1)
- Electromagnetic weld pool support (1)
- Elektromagnetische Porenreduktion (1)
- Elektromagnetische Schmelzbadunterstützung (1)
- Elektromagnetsiche Schmelzbadbeeinflussung (1)
- Elemenet transport (1)
- Environment (1)
- Equivalent heat source (1)
- Fatigue tests (1)
- Fine-grained Steel (1)
- Finite element method (1)
- Forschungsdatenmanagement (1)
- Full penetration (1)
- Fusion zone (1)
- Fügetechnologie (1)
- Grain size (1)
- Grain structure (1)
- Heat saturation function (1)
- Heissrisse (1)
- High-power laser beam (1)
- Highspeed plasma (1)
- Hochleistungslaserstrahlschweißen (1)
- Hot crack (1)
- Hot stamping (1)
- Hybrid components (1)
- Hybrid laser arc welding (1)
- In situ Monitoring (1)
- In-situ Process Monitoring (1)
- Infrared Thermography (1)
- Infrared thermography (1)
- Knotenweise Zwangsbedingungen (1)
- Kurz- und Langriss-Ermüdungsbruchmechanik (1)
- L-PBF (1)
- Lack-of-fusion (1)
- Laser cladding (1)
- Laser hybrid welding (1)
- Laser surface texturing (1)
- Laser welding (1)
- Laser-Hybridschweißen (1)
- Laser-Pulver-Auftragschweißen (1)
- Laserdispergieren (1)
- Laserpulverauftragschweißen (1)
- Laserstrahlhybridschweißen (1)
- Liquid metal embrittlement (1)
- Local fatigue spproaches (1)
- Localized Laser Dispersing (1)
- Low Temperature Toughness (1)
- Low heat input GMA welding (1)
- Magnetic field (1)
- Mechanical Properties (1)
- Mechanical property (1)
- Melt pool behaviour (1)
- Melting (1)
- Microstructure characterisation (1)
- Mittelrippendefekt (1)
- Moving mesh (1)
- NbC (1)
- Neutron Diffraction (1)
- Neutron diffraction (1)
- Nickel alloys (1)
- Non-destructive Materials (1)
- Non-destructive testing (1)
- Numerical analysis (1)
- Numerical modelling (1)
- Numerische ISmulation (1)
- Numerische Simulation (1)
- Optical Emission Spectroscopy (1)
- Optical emission spectroscopy (1)
- Optical measurment technique (1)
- Optical tomography (1)
- Optische Tomografie (1)
- Oscillating magnetic field (1)
- Parabolic flight (1)
- Partial penetration laser hybrid welding (1)
- Path planning (1)
- Primär- und Sekundärspannungen (1)
- Process development (1)
- Prozessmonitoring (1)
- Prozesssimulation (1)
- Prozessüberwachung (1)
- Radiological inspections (1)
- Residual stresses (1)
- Rundnähte (1)
- SLM (1)
- Safety (1)
- Schweißeigenspannungen (1)
- Schweißeigenspannungs-Tiefen-Profile (1)
- Schweißen (1)
- Schweißen von kaltzähen Stählen (1)
- Schweißstruktursimulation (1)
- Selective Laser Melting (SLM) (1)
- SimCoLas (1)
- Stabilität von Eigenspannungen (1)
- Stahl und Aluminium (1)
- Standardisation (1)
- Steel (1)
- TaC (1)
- Tantalum carbide (1)
- Technical crack detection (1)
- Tensile testing (1)
- Themral cycles (1)
- Thermo-fluid dynamics (1)
- Thermo-fluid flow (1)
- Thermograhy (1)
- Thick materials (1)
- Thick-walled Structures (1)
- Thick-walled steel (1)
- Thick-walled steels (1)
- Tool steel (1)
- Toughness (1)
- Transient heat transfer (1)
- Tubular X-joints (1)
- Weld pool (1)
- Welding process simulation (1)
- X8Ni9 (1)
- deposition welding (1)
- digital image correlation (1)
- dual phase steel (1)
- highspeed plasma laser cladding (1)
- resistance spot welding (1)
- µ-gravity (1)
- Äquivalente Wärmequelle (1)
- кратер шва (1)
- кристаллизация, (1)
- плавление, (1)
- сварочная ванна (1)
- температурное поле (1)
- функция теплонасыщения (1)
Organisationseinheit der BAM
- 9.3 Schweißtechnische Fertigungsverfahren (118) (entfernen)
Eingeladener Vortrag
- nein (52)
Additive Fertigungsverfahren gewinnen aufgrund der schnellen, flexiblen und kosten-günstigen Fertigung von Bauteilen zunehmend an Bedeutung. Das Laserpulverauf-tragschweißen (LPA) wurde anfangs hauptsächlich als Beschichtungsverfahren ein-gesetzt. Diese Technologie bewerkstelligt aber auch das Reparieren von verschlisse-nen Bauteilen, sodass diese zeitsparend und ressourcenschonend erneuert werden können. Die hohe Aufbaurate, die flexible Pulverzusammensetzung sowie die hohe Endkonturnähe ermöglichen heutzutage die Entwicklung und additive Fertigung von neuen Materialien, wie zum Beispiel Nickel-Titan-Formgedächtnislegierungen.
The determination of mechanical properties of welded Steel structures such as strength or ductility is a subject of high interest for the majority of Companies in the area of metal Processing. The material Parameters can be obtained by performing the tensile test on the samples made from a part of a component. In some cases, it is highly expensive to produce the tensile specimens especially from the weld metal, which contains different type of microstructure such as weld seam or heat affected zone in an extremely small area. Therefore, a method is described in this paper to determine the material Parameters of high strength Steel structures and welded joints locally and without any additional effort to perform the tensile test. In this method, instrumented indentation technique (IIT), an indenter is pushed on the flat surface of a specimen in a certain period of time and simultaneously the applied force and the corresponding indentation path are measured. The data related to the force-indentation diagram is given as input to an artificial neural network (ANN) to obtain the material Parameters. The ANN can be trained by generating the large qualitative data sets with numerical Simulation of the IIT procedure. The Simulation must be run several times with the different material model parameter sets to generate the numerous
force-indentation diagrams as the inputs of ANN. Then, the trained ANN is validated by performing the IIT on the welded joints and comparing the obtained material Parameters from ANN with the tensile test.
Consequently, the mechanical properties of welded joints can be determined by performing the IIT and evaluating the resulting data by the ANN.
To increase the competitiveness of jacket substructures compared to monopiles a changeover from an individual towards a serial jacket production based on automated manufactured tubular joints combined with standardized pipes has to be achieved. Therefore, this paper addresses fatigue tests of automatically welded tubular X-joints focusing on the location of the technical fatigue crack. The detected location of the technical crack is compared to numerical investigations predicting the most fatigue prone notch considering the structural stress approach as well as the notch stress approach. Besides, the welding process of the automated manufactured tubular X-joints is presented.
Over the last years, the weight of modern car bodies has risen significantly due to the increasing customers’ demand for comfort and safety equipment. However, this ongoing trend leads to an increasing fuel consumption and thus to higher carbon dioxide emissions. In order to counteract these problems, hot stamping has been established in the automotive industry as a key technolo-gy for lightweight construction, regarding the manufacturing of safety-relevant car body compo-nents. Hot stamped parts are commonly made out of boron-manganese steel 22MnB5, which is initially austenized and subsequently formed and quenched in one process step. As a result, geo-metrical complex structures with an ultimate tensile strength of 1500 MPa are generated. The surfaces of the workpieces are coated with an Al-Si layer to avoid oxide scale formation and to ensure corrosion protection. However, the coating system leads to an increased adhesive wear on the tool surface due to the high thermo-mechanical tool stresses. Therefore, a time and cost con-suming rework of the hot stamping tools is required. The aim of this study is to increase the tribological performance of hot stamping tools by using a laser implantation process. This tech-nique allows the ma-nufacturing of separated, elevated and dome-shaped microstructures on the tool surface in consequence of a localized dispersing of hard ceramic particles by pulsed laser radiation. The generated surface features offer great potential for reducing the tribological load, due to their high hardness and wear resistance. For this purpose, the friction coefficient of un-modified and laser implanted tool surfaces were examined and compared by using a modified pin-on-disk test. In addition, the surfaces were analyzed by optical measurements in order to quantify the amount of wear.
Plasma-Transferred-Arc (PTA) welding is a process that enables high deposition rates, but also causes increased thermal load on the component. Laser metal deposition (LMD) welding, on the other hand, reaches a high level of precision and thus achieves comparatively low deposition rates, which can lead to high processing costs. Combining laser and arc energy aims to exploit the respective advantages of both technologies. In this study, a novel approach of this process combination is presented using a PTA system and a 2 kW disk laser. The energy sources are combined in a common process zone as a high-speed plasma laser cladding technology (HPLC), which achieves process speeds of 10 m/min at deposition rates of 6.6 kg/h and an energy per unit length of 39 J/mm.
Resistance spot welding (RSW) is widely used in the automotive industry
as the main joining method. Generally, an automotive body contains
around 2000 to 5000 spot welds. Therefore, it is of decisive importance to characterize the mechanical properties of these areas for the further optimization and improvement of an automotive body structure. The present paper aims to introduce a novel method to investigate the mechanical properties and microstructure of the resistance spot weldment of DP1000 sheet steel. In this method, the microstructure of RSW of two sheets was reproduced on one sheet and on a bigger area by changing of the welding parameters, e. g. welding current, welding time, electrode force and type. Then, tensile tests in combination with digital Image correlation (DIC) measurement were performed on the notched tensile specimens to determine the mechanical properties of the weld metal.
The notch must be made on the welded tensile specimen to force the fracture and elongation on the weld metal, enabling the characterization of its properties. Additionally, the parameters of a nonlinear isotropic material model can be obtained and verified by the simulation of the tensile specimens. The parameters obtained show that the strength of DP1000 steel and the velocity of dislocations for reaching the Maximum value of strain hardening, are significantly increased after RSW. The effect of sample geometry and microstructural inhomogeneity of the welded joint on the constitutive property of the weld metal are presented and discussed.
Effect of Inter-Layer Dwell Time on Distortion and Residual Stresses of Laser Metal Deposited Wall
(2019)
The laser metal deposition is an advanced manufacturing technology enabling the production of large-sized parts and partially or completely elimination of machining and welding. The process is characterised by non-uniform local heating of the buildup leading to a stress distribution, which may exceed the yield strength of the material and leads to loss of dimensional accuracy. The interlayer dwell time has a strong influence on the temperature field. The effect of the interlayer dwell time on the distortion and the stress distribution during laser metal deposition of a single-pass wall on the edge of 2 mm thick plate was studied experimentally and numerically. The deposited material was IN625 and the substrate material was AISI 316. A decrease of the residual displacement, due to a uniform shrinkage after the deposition of the last layer and a lower level of the residual compressive longitudinal plastic strain, has been observed in the studies without dwell time. The peak increment of the free edge displacement corresponds to the first layer and hence the subsequent layers will be deposited on the already plastically deformed buildup. The tensile residual longitudinal stress near the top of the buildup and transverse stress near the edges of the buildup is higher than yield strength in the studies with dwell time.
Some zinc coated advanced high strength steels (AHSS), under certain manufacturing conditions, are known to be prone to liquid metal embrittlement (LME) during resistance spot welding. LME is an undesired phenomenon, which can cause both surface and internal cracks in a spot weld, potentially influencing its strength. An effort is made to understand influencing factors of LME better, and evaluate geometry-material combinations regarding their LME susceptibility. Manufacturers benefit from such knowledge because it improves the processing security of the materials. The experimental procedure of welding under external load is performed with samples of multiple AHSS classes with strengths up to 1200 MPa, including dual phase, complex phase and TRIP steels. This way, externally applied tensile load values are determined, which cause liquid metal embrittlement in the samples to occur. In the future, finite element simulation of this procedure gives access to in-situ stress and strain values present during LME formation. The visualization improves the process understanding, while a quantification of local stresses and strains allows an assessment of specific welded geometries.
Among the various welding technologies, resistance spot welding (RSW) and laser beam welding (LBW) play a significant role as joining methods for the automobile industry. The application of RSW and LBW for the automotive body alters the microstructure in the welded areas. It is necessary to identify the mechanical properties of the welded material to be able to make a reliable statement about the material behavior and the strength of welded components. This study develops a method by which to determine the mechanical properties for the weldment of RSW and LBW for two dual phase (DP) steels, DP600 and DP1000, which are commonly used for the automotive bodies. The mechanical properties of the resistance spot weldment were obtained by performing tensile tests on the notched tensile specimen to cause an elongation of the notched and welded area in order to investigate its properties. In order to determine the mechanical properties of the laser beam weldment, indentation tests were performed on the welded material to calculate its force-penetration depth-curve. Inverse numerical simulation was used to simulate the indentation tests to determine and verify the parameters of a nonlinear isotropic material model for the weldment of LBW. Furthermore, using this method, the parameters for the material model of RSW were verified. The material parameters and microstructure of the weldment of RSW and LBW are compared and discussed. The results show that the novel method introduced in this work is a valid approach to determine the mechanical properties of welded high-strength steel structures. In addition, it can be seen that LBW and RSW lead to a reduction in ductility and an increase in the amount of yield and tensile strength of both DP600 and DP1000.
Vermeidung von Schweißimperfektionen im Überlappbereich bei laserstrahlhybridgeschweißten Rundnähten
(2019)
Die Laserstrahl-Hybrid-Schweißtechnologie erweist sich in der schweißtechnischen Fertigung immer mehr als innovative Alternative gegenüber anderen Schweißverfahren. Obwohl das Laserstrahl-Hybridschweißverfahren viele wirtschaftliche Vorteile gegenüber herkömmlichen Schweißverfahren aufweist, wie z.B. große Einschweißtiefe und dadurch eine reduzierte Anzahl von Schweißlagen, geringe thermische Belastung des Grundwerkstoffes aufgrund reduziertem Wärmeeintrag, konnte das Schweißverfahren überwiegend für das Schweißen von Längsnähten demonstriert werden. Eine Vielzahl von Schweißaufgaben, z.B. beim Schweißen von Segmenten von Windkraftanlagen oder dem Orbitalschweißen beim Verlegen von Großrohrleitungen sieht vor, dass die zu schweißenden Bauteile mit einer Rundnaht zusammengefügt werden. Die schweißtechnische Herausforderung ist hier, dass beim Schließen einer Rundnaht mit der Entstehung eines fehlerbehafteten Überlappbereiches zu rechnen ist. Ein zentrales Problem im Überlappbereich einer laserstrahl- sowie laserhybridgeschweißten Rundnaht ist die Bildung von Imperfektionen wie Poren, Rissen sowie die Bildung eines Endkraters, welcher als geometrische Kerbe wirkt. Bisher liegen keine universellen Lösungen zur fehlerfreien Ausführung von geschlossenen Rundnähten beim Laserstrahl-Hybridschweißen vor. Diese Studie befasst sich mit der Entwicklung eines Verfahrens, mit dem die Entstehung von o.g. Schweißimperfektionen vermieden wird. Die Strategie der Prozessführung beim Schließen der Rundnaht sieht hervor, dass ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht werden kann. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG-Schweißprozess realisiert.
Im Rahmen dieser Arbeit wurde eine Serie von Schweißversuchen an 9,5 mm dicken Rohabschnitten aus hochfestem Pipelinestahl X100Q mit Variation der Prozessparameter wie der Laserleistung, der Defokussierung des Laserstrahls sowie der Endkraterfüllzeit im Überlappbereich der Rundnaht durchgeführt. Nachfolgend werden die erzielten Ergebnisse dargestellt und diskutiert.
The introduction of electromagnetic stirring to laser beam welding can bring several beneficial effects e.g. element homogenization and grain refinement. However, the underlying physics has not been fully explored due to the absence of quantitative data of heat and mass transfer in the molten pool. In this paper, the influence of electromagnetic stirring on the thermo-fluid flow and element transport in the wire feed laser beam welding is studied numerically and experimentally. A three-dimensional transient heat transfer and fluid flow model coupled with dynamic keyhole, magnetic induction and element Transport is developed for the first time. The results suggest that the Lorentz force produced by an oscillating magnetic field and its induced eddy current shows an important influence on the thermo-fluid flow and the keyhole stability. The melt flow velocity is increased by the electromagnetic stirring at the rear and lower regions of molten pool. The keyhole collapses more frequently at the upper part. The additional Elements from the filler wire are significantly homogenized because of the enhanced forward and downward flow. The model is well verified by fusion line shape, high-speed images of molten pool and measured element distribution. This work provides a deeper understanding of the transport phenomena in the laser beam welding with magnetic field.
The additional element from the filler wire in the laser beam welding is usually distributed inhomogeneously in the final weld due to the high solidification rate of weld pool. It has been found that the electromagnetic stirring produced by an external oscillating magnetic field can enhance the material mixing in the weld pool to achieve a more uniform element distribution. However, the magnetic field has a highly non-linear and multi-coupled interaction with the weld pool behavior, which makes the quantitative explanation of the physical mechanism difficult. In this study, the effect of electromagnetic stirring on the transport phenomena in the wire feed laser beam welding is investigated by a numerical modelling. A 3D transient multi-physical model considering the magnetohydrodynamics, heat transfer, fluid flow, keyhole dynamics and element transport is developed. The multiple reflections and the Fresnel absorption of the laser on the keyhole wall are calculated using the ray tracing method. The numerical results show that a Lorentz force produced by the oscillating magnetic field and its induced eddy current gives significant influence on the transport phenomena in the molten pool. The forward and downward flow is enhanced by the electromagnetic stirring, which homogenizes the distribution of the additional elements from a nickel-based filler wire in a steel weld pool. The numerical results show a good agreement with the high-speed images of the molten pool, the fusion line from the optical micrograph and the element distribution from the energy dispersive X-ray spectroscopy. This work provides a physical base for the electromagnetic-controlled laser beam welding and some guidance for the selection of electromagnetic parameters.
The control of friction and wear is a major concern in many industrial applications. A promising method for a tailored surface modification is the so-called laser implantation technique. This method combines surface texturing and material optimization in one processing step by a localized dispersing of hard ceramic particles using pulsed laser radiation. Wear resistant, protruding micrometric features (implants) with defined geometry can be created in deterministic pattern where needed on highly stressed surfaces, i.e. on forming or cutting tools. However, in order to maintain the implants over the tool’s lifetime, a suitable selection of hard ceramic particles is a prerequisite. They must provide a defect-free Metal Matrix Composite with a high share of homogeneously distributed particles and especially a high implant hardness.
In this study TiN, TiC and TiB2 hard particles were compared as implant materials for the first time. By a systematic variation of the pulse power and pulse duration, their dispersing behavior and influence on the material properties of AISI D2 tool steel was investigated. Although all powder materials had grain sizes smaller than 10 µm, it was possible to disperse them by pulsed laser radiation and to obtain defect-free protruding implants. The highest share of dispersed particles (~64 %) was observed for TiB2. By scanning electron microscopy and energy dispersive X-ray spectroscopy, it was also shown that a significant share of the pre-placed particles was dissolved by the laser beam and precipitated as nanometer sized particles within the matrix during solidification. These in-situ formed particles have a decisive influence on the material properties. While the TiN and TiC implants have shown maximum hardness values of 750 HV1 and 850 HV1, the TiB2 implants have shown the highest hardness values with more than 1600 HV1. By X-ray diffraction, it was possible to ascribe the lower hardness values of TiC and TiN implants to high amounts of retained austenite in the metal matrix. By implanting TiB2, the formation of retained austenite was successfully suppressed due to the in-situ formation of TiC particles, which was proven by electron backscatter diffraction. In conclusion, all the implant materials are basically suitable for laser implantation on AISI D2 tool steel. However, TiB2 has shown the most promising results.
The control of friction and wear is a major concern in many industrial applications. A promising method for a tailored surface modification is the so-called laser implantation technique. This method combines surface texturing and material optimization in one processing step by a localized dispersing of hard ceramic particles using pulsed laser radiation. Wear resistant, protruding micrometric features (implants) with defined geometry can be created in deterministic pattern where needed on highly stressed surfaces, i.e. on forming or cutting tools. However, in order to maintain the implants over the tool’s lifetime, a suitable selection of hard ceramic particles is a prerequisite. They must provide a defect-free Metal Matrix Composite with a high share of homogeneously distributed particles and especially a high implant hardness.
In this study TiN, TiC and TiB2 hard particles were compared as implant materials for the first time. By a systematic variation of the pulse power and pulse duration, their dispersing behavior and influence on the material properties of AISI D2 tool steel was investigated. Although all powder materials had grain sizes smaller than 10 µm, it was possible to disperse them by pulsed laser radiation and to obtain defect-free protruding implants. The highest share of dispersed particles (~64 %) was observed for TiB2. By scanning electron microscopy and energy dispersive X-ray spectroscopy, it was also shown that a significant share of the pre-placed particles was dissolved by the laser beam and precipitated as nanometer sized particles within the matrix during solidification. These in-situ formed particles have a decisive influence on the material properties. While the TiN and TiC implants have shown maximum hardness values of 750 HV1 and 850 HV1, the TiB2 implants have shown the highest hardness values with more than 1600 HV1. By X-ray diffraction, it was possible to ascribe the lower hardness values of TiC and TiN implants to high amounts of retained austenite in the metal matrix. By implanting TiB2, the formation of retained austenite was successfully suppressed due to the in-situ formation of TiC particles, which was proven by electron backscatter diffraction. In conclusion, all the implant materials are basically suitable for laser implantation on AISI D2 tool steel. However, TiB2 has shown the most promising results.
Gut kombiniert: Laser-Plasma-Auftragschweißen
Für den Schutz vor starkem abrasiven Verschleiß (Panzern) oder vor korrosiven Medien (Plattieren) sowie für das Auftragen einer Pufferlage können das Laser-Pulver-Auftragschweißen oder das Plasma-Pulver-Auftragschweißen zum Einsatz kommen. Während das Laser-Pulver-Auftragschweißen eine geringe thermische Belastung verspricht, ermöglicht das Plasma-Pulver-Auftragschweißen hohe Auftragraten. Wissenschaftler des Fraunhofer IPK erarbeiten neuartige Verfahrenskombinationen und Düsenkonzepte, die die jeweiligen Vorteile dieser bestehenden Verfahren vereinen und somit eine hohe Qualität und Effizienz garantieren. So kann beispielsweise die punktgenaue Energie der Laserstrahlung den Plasmalichtbogen stabilisieren und den Wärmeeintrag in das Bauteil besser kontrollieren.
Plasma-Transferred-Arc (PTA) welding is a process that enables high deposition rates, but also causes increased thermal 9 load on the component. Laser based Direct Energy Deposition (DED) welding, on the other hand, achieves a high level of 10 precision and thus comparatively low deposition rates, which can lead to high processing costs. Combining laser and arc 11 energy aims to exploit the respective advantages of both technologies. 12 In this study, different possibilities of this process combination are presented using a PTA system and a 2 kW disk laser. 13 This includes the combination in a common process zone as a highspeed plasma laser cladding technology (HPLC), which 14 achieves process speeds of 10 m/min. Besides that it is being examined whether a pre-running plasma arc can be used to 15 coat difficult-to-weld rail steel with a carbon content of 0.8 % due to a preheating effect. Furthermore, a smoothing of the 16 coating by a plasma arc following the laser is investigated.
The geometrical characteristics of the weld end crater are commonly used for the validation of numerical results in welding simulation. A semi-analytical model calculating the cooling stage of the welding process after the moving energy source is turned off has been developed. A solution for various combinations of heat sources and workpieces has been found. The theoretical limits for the heat transfer of the absorbed energy during cooling in a thin plate and a semi-infinite body were studied. It is shown that after turning off the energy source, an additional melting of the base material in longitudinal direction may occur. The developed technique is applied to complete-penetration keyhole laser beam welding of a 2 mm thick austenitic chromium-nickel 316L steel plate at a welding speed of 20 mm/s and a laser power of 2.3 kW. The results show a theoretical increase of the weld end crater length in comparison to the length of the steady-state weld pool of up to 19 %. A shift of the centre of the end crater, in which the solidification of the liquid metal ends, towards the tail of the end crater relative to the axis of the heat source at the time of its termination, was computed. The speed and the direction of crystallization of the molten material in the weld pool and the end crater were found to be different. A good agreement between the computational results and the welding experiments was achieved.
Rapid localized heating and cooling during additive manufacturing using laser deposition method (LMD) lead to loss of dimensional accuracy as well as cracking of built parts. Finite-Element welding simulations allow prediction of geometrical deviations and accumulated residual stresses as well as their optimization before conducting experiments. Due to the great length of stacked welds, calculation times for fully transient thermomechanical simulations are currently long, the calculation stability suffers from the high number of contact bodies in the model and the modelling effort is high, as the geometries need to be sliced and positioned layer-wise.
In this contribution, an integrated modelling approach is demonstrated for a thin-walled LMD component made from 30 layers of 1.4404 (316L) stainless steel: Instead of the layer-by-layer modelling strategy commonly found in the literature, the whole component mesh is kept in one piece and the fully transient, layer-by-layer material deposition is implemented via element sets. In contrast to prior simulations, nonlinear contact between the layers does not have to be considered, significantly decreasing calculation times. The calculated distortions are compared to recently published, in-situ digital image correlation (DIC) measurements as well as numerical simulations conducted with the established layer-wise modelling strategy to judge result quality. Finally, the improvement in calculation time and ease-of-use is compared between both modelling approaches and conclusions regarding future usage for industrial-scale components are drawn.
A novel approach for the reconstruction of an equivalent volumetric heat source from a known weld pool shape is proposed. It is based on previously obtained weld pool geometries from a steady-state thermo-fluid dynamics simulation. Hereby the weld pool dimensions are obtained under consideration of the most crucial physical phenomena, such as phase transformations, thermo-capillary convection, natural convection and temperature-dependent material properties. The algorithm provides a time and calibration efficient way for the reproduction of the weld pool shape by local Lamé curves. By adjusting their parameters, the identification of the finite elements located within the weld pool is enabled. The heat input due to the equivalent heat source is assured by replacing the detected nodes’ temperature by the melting temperature.
The model offers variable parameters making it flexible and adaptable for a wide range of workpiece thicknesses and materials and allows for the investigation of transient thermal effects, e.g. the cooling stage of the workpiece. The calculation times remain acceptably short especially when compared to a fully coupled process simulation. The computational results are in good agreement with performed complete-penetration laser beam welding experiments.
A novel approach for the reconstruction of an equivalent volumetric heat source from a known weld pool shape is proposed. It is based on previously obtained weld pool geometries from a steady-state thermo-fluid dynamics simulation. Hereby the weld pool dimensions are obtained under consideration of the most crucial physical phenomena, such as phase transformations, thermo-capillary convection, natural convection and temperature-dependent material properties. The algorithm provides a time and calibration efficient way for the reproduction of the weld pool shape by local Lamé curves. By adjusting their parameters, the identification of the finite elements located within the weld pool is enabled. The heat input due to the equivalent heat source is assured by replacing the detected nodes’ temperature by the melting temperature.
The model offers variable parameters making it flexible and adaptable for a wide range of workpiece thicknesses and materials and allows for the investigation of transient thermal effects, e.g. the cooling stage of the workpiece. The calculation times remain acceptably short especially when compared to a fully coupled process simulation. The computational results are in good agreement with performed complete-penetration laser beam welding experiments.
The weld pool dynamics and shape play a fundamental role in keyhole mode welding. The presented work aims the experimental and numerical investigation of the influence of the weld pool characteristics on the formation of hot cracking. The experimental procedure allows recording the molten pool in the longitudinal section of a butt joint configuration of 15 mm thick structural steel and transparent quartz glass by using a high-speed video camera and two thermal imaging cameras. The observations show that the dimensions of the weld pool vary depending on the depth. The regions close to the surface form a teardrop-shaped weld pool. A bulge-region and its temporal evolution are observed approximately in the middle of the depth of the weld pool, where hot cracking appears. A numerical framework including models for the weld pool dynamics, global temperature field, transient stress state, crystal growth, diffusion and macro-segregation and subroutines for their one-way couplings is developed. The numerically obtained and experimentally observed results are in a good agreement. It is shown that the bulge-region leads to a delay in the solidification behavior, increased temporal tensile stresses and accumulation of impurities in the defect region and hence enhance the probability of hot cracking formation.
The geometrical characteristics of the weld end crater are commonly used for the validation of numerical results in welding simulation. A semi-analytical model calculating the cooling stage of the welding process after the moving energy source is turned off has been developed. A solution for various combinations of heat sources and workpieces has been found. The theoretical limits for the heat transfer of the absorbed energy during cooling in a thin plate and a semi-infinite body were studied. It is shown that after turning off the energy source, an additional melting of the base material in longitudinal direction may occur. The developed technique is applied to complete-penetration keyhole laser beam welding of a 2 mm thick austenitic chromium-nickel 316L steel plate at a welding speed of 20 mm/s and a laser power of 2.3 kW. The results show a theoretical increase of the weld end crater length in comparison to the length of the steady-state weld pool of up to 19 %. A shift of the centre of the end crater, in which the solidification of the liquid metal ends, towards the tail of the end crater relative to the axis of the heat source at the time of its termination, was computed. The speed and the direction of crystallization of the molten material in the weld pool and the end crater were found to be different. A good agreement between the computational results and the welding experiments was achieved.
Die Entstehung von Erstarrungsrissen stellt ein in der Schweißtechnik lange bekanntes Problem dar. Diese prozessseitige Herausforderung ist selbst nach dem heutigen Wissenstand schwer zu beherrschen und gefährdet die Sicherheit der gefügten Bauteile. Dieses Problem erweist sich als besonders schwierig beim einlagigen Hochleistungslaserstrahlschweißen von Metallteilen hoher Blechstärke, welche eine essentielle Rolle in vielerlei industriellen Anwendungen spielen.
Gegenstand des hier bearbeiteten Forschungsprojekts war die numerische Untersuchung der Entstehungsmechanismen des Mittelrippendefekts beim Laserstrahlschweißen niedriglegierter Stähle. Mittels mehrerer gekoppelter Simulationen, für welche sowohl kommerziellen Softwares, wie COMSOL Multiphysics und ANSYS, als auch in-house entwickelte Programme eingesetzt worden sind, wurden die am stärksten ausgeprägten Mechanismen der Erstarrungsrissbildung und deren Zusammenspiel aufgeklärt. Begleitend zur Simulation wurden mehrere experimentelle Untersuchungen für den niedriglegierten Baustahl S355 an den Blechdicken 12 mm und 15 mm zu deren Validierung durchgeführt. Die Ergebnisse der Simulation des Kristallwachstums, der Diffusion und der Makroseigerung von Schwefel zeigen, dass die Risse für bestimmte Werkstoffe mit einer hohen Konzentration an Verunreinigungen
hauptsächlich metallurgisch bedingt entstehen können. Allerdings zeigte die Untersuchung des Einflusses der Ausbauchung (Bulging) im Mittenbereich der Schweißnaht auf das transiente Temperaturfeld und die transienten Transversalspannungen im risskritischen Bereich auch, dass die Rissbildung nicht nur metallurgisch bedingt und insbesondere auch für aus metallurgischer Sicht eigentlich rissunkritische Materialien auftreten kann.
Der Bulging-Bereich hat sich in der Untersuchung als besonders kritisch in allen Teilen der Simulationskette gezeigt. Die Einflüsse dieser geometrischen Besonderheit konnten bei allen physikalischen Teilaspekten der Problematik als heißrissinduzierend identifiziert werden. Von besonderer Bedeutung wird an dieser Stelle das erkannte Zusammenspiel dieser Einflüsse hervorgehoben. Bisher wurde die Bildung der Erstarrungsrisse hauptsächlich durch einen einzelnen physikalischen Aspekt, wie z.B. rein metallurgisch oder rein thermomechanisch bedingt, isoliert betrachtet. Die gewonnen Erkenntnisse über die Einflüsse des Bulgings auf die unterschiedlichen Teilaspekte zeigen deutlich, dass alle Entstehungsmechanismen auch die Schmelzbadgeometrie als Ursprung haben. Von dieser hängen die transienten Temperatur- und Spannungsfelder, die Kristallwachsrichtung, die Erstarrungsgeschwindigkeit und die Konzentration von Verunreinigungen, welche zur Entstehung von niedrigschmelzenden Phasen führt, ab.
Die Ergebnisse des Forschungsvorhabens sind vielfach in referierten Zeitschriften und auf Fachtagungen veröffentlicht worden. Hervorzuheben dabei ist der „Best Presentation Award“ auf der LANE Conference 2018 in Fürth, wodurch die Thematik einem breiten Publikum bekannt gemacht werden konnte.
The talk will give an overview of past, ongoing and future activities at BAM welding divisions, specifically those regarding prospects and challenges of the ongoing digital transformation and the move to more accessible research data (open science) with concerns to welding research. We will discuss current ways to publish and share research results inside the welding community and highlight approaches and advancements from other scientific fields to improve accessibility and reproducibility. We would also like to discuss the feasibility of integrating open science principles into the current IIW landscape of meetings, publications and education. In Addition we will introduce our upcoming series of workshops organized by BAM focusing on defining and implementing an open source file format specifically designed to publish and exchange high quality welding research data.
WelDX is a newly started research project at BAM publicly funded by the German Federal Ministry of Education and Research. Over the course of three years the project aims to build the foundation for a publicly accessible file format and to foster research collaboration in arc welding on a national and international level.
The talk will motivate benefits and discuss challenges of using a common file format designed to describe, store and share arc welding research data in the scope of "Open Science". By using common open source software and tools, welding data will be made more accessible and reusable so that new scientific practices may emerge.
The proposed file format aims to be easy to use for common welding applications while also offering the possibility to describe complex experiments for state of the art welding research.
In addition the talk will illustrate how in the future other facilities and researchers will be able to use experimental arc welding data generated at BAM for their own research, for example to conduct their own data analysis or welding process and thermo-mechanical simulations.
The WelDX research project aims to foster the exchange of scientific data inside the welding community by developing and establishing a new open source file format suitable for documentation of experimental welding data and upholding associated quality standards. In addition to fostering scientific collaboration inside the national and international welding community an associated advisory committee will be established to oversee the future development of the file format. The proposed file format will be developed with regards to current needs of the community regarding interoperability, data quality and performance and will be published under an appropriate open source license.
By using the file format objectivity, comparability and reproducibility across different institutes and experimental setups can be improved.
Ziel des WelDX Forschungsvorhabens ist es, den Austausch wissenschaftlicher Forschungsdaten aus dem Bereich der Schweißtechnik auf Basis eines einheitlichen Open Source Dateiformates zu ermöglichen und damit die Einhaltung und Dokumentation geeigneter Qualitätsstandards zu fördern. Im Zuge der Projektarbeit wird die Zusammenarbeit und der Wissenstransfer schweißtechnischer Institute zunächst auf nationaler Ebene gefördert und die Bildung eines von der Fachcommunity getragenen Kuratoriums zur Betreuung und Weiterentwicklung des Dateiformates und der Ausarbeitung zugehöriger Qualitätsstandards angestrebt.
Zunächst erfolgt die Erstellung und Veröffentlichung eines geeigneten Dateiformates zum Austausch großvolumiger, detaillierter Forschungsdaten im Bereich mechanisierter und automatisierter Schweißverfahren. Durch die Nutzung des Dateiformates zur Dokumentation der Forschungsarbeiten soll auch für komplexe Schweißaufgaben und Versuchsaufbauten eine deutlich gesteigerte objektive Vergleichbarkeit der Messdaten und Ergebnisse im Sinne der guten wissenschaftlichen Praxis zwischen den Instituten erzielt werden.
Der Vortrag gibt einen Überblick über Arbeiten im Rahmen der Themenstellung "photonische Prozessketten" des SimCoLas Projekts. Es werden Ergebnisse zur Datendurchgängigkeit der Prozesskette Umformen/Laserstrahlschweißen sowie erste Ergebnisse zu numerischen Schweißstruktursimulationen zur Bewertung der Heissrisskritikalität eines tiefgezogenen Napfes beim Laserstrahlschweißen gegeben.
Die Präsentation gibt einen Überblick bezüglich der von der BAM im Rahmen des SimCoLas Verbundprojekts durchgeführten Arbeiten zum Thema "Photonische Prozessketten". Die numerisch abgebildete Prozesskette Tiefziehen/Laserstrahlschweißen wird darsgestellt und diskutiert. Fokus der Diskussion ist die entwickelte Methodik zur konsistenten Abbildung numerischer Prozessketten mit der Applikation Heissrisskritikalität beim Laserstrahlschweißen.
The deep penetration laser beam welding (LBW) has developed to one of the most promising metal joining methods in the modern manufacturing industry. It has well-known advantages of good penetration capacity, low heat input, high reachable welding speed and low welding distortion in comparison to conventional arc welding techniques. However, there are still challenges in LBW making the realization of the advantages difficult, such as porosity or inhomogeneous element distribution when using filler material. The magnetohydrodynamics technique is a promising way to solve these issues by introducing a suitable electromagnetic field, and correspondingly Lorentz force, to control the Transport phenomena in the weld pool.
The underlying physics in wire feed laser beam welding with electromagnetic stirring were investigated numerically and experimentally. A three-dimensional transient heat transfer and fluid flow model coupled with dynamic keyhole, magnetic induction and element transport was developed for the first time. The electromagnetic behaviour as well as the temperature and velocity profiles, solidification parameters, keyhole evolution and element transport are calculated.
The model is well tested against the experimental results. The beneficial effects from electromagnetic stirring (element homogenization and grain refinement) are explained quantitatively using the numerical data and the results from high-speed imaging, OM, EDX and EBSD.
Laser beam welding of aluminum die casting is challenging. A large quantity of gases (in particular hydrogen) is absorbed by aluminum during the die-cast manufacturing process and is contained in the base material in solved or bound form. After re-melting by the laser, the gases are released and are present in the melt as pores. Many of these metallurgic pores remain in the weld seam as a result of the high solidification velocities. The natural (Archimedean) buoyancy is not sufficient to remove the pores from the weld pool leading to process instabilities and poor mechanical properties of the weld. Therefore, an electromagnetic (EM) system is used to apply an additional buoyancy component to the pores. The physical mechanism is based on the generation of Lorentz forces, whereby an electromagnetic pressure is introduced into the weld pool. The EM system exploits the difference in electrical conductivity between poorly conducting pores (inclusions) and the comparatively better conducting aluminum melt to increase the resulting buoyancy velocity of the pores. Within the present study, the electromagnetic supported degassing is investigated in dependence on the laser beam power, welding velocity and electromagnetic flux density. By means of a design of experiments a systematic variation of these parameters is carried out for partial penetration laser beam welding of 6 mm thick sheets of wrought aluminum alloy AlMg3 and die-cast aluminum alloy AlSi12(Fe) where the wrought alloy serves as a reference. The proportion of pores in the weld seams is determined using X-ray images, computed tomography (CT-) images and cross-section images. The results prove a significant reduction of the porosity up to 70 % for both materials as a function of the magnetic flux density
The potential of lowered surface features as well as the application of wear resistant coatings have been known for many years to improve the tribological behavior of forming tools. More recent studies also discuss the capability of protruded microfeatures for adjusting the tribological behavior between contacting surfaces. The demand for a high wear resistance of such structures as well as their economical and reliable production, however, often limits the industrial application. The laser implantation process can overcome these limitations. In contrast to conventional cw-laser dispersing processes, where the formation of uniform metal matrix composite layers is intended, this surface engineering technique aims to improve the tribological behavior of contacting surfaces by a localized dispersing of pre-placed hard ceramic particles. This enables the formation of deterministic textures composed of separated wear resistant dome- or ring-shaped microstructures (implants).
Since TaC shows very promising material properties for improving the wear resistance of tools exposed to severe operating conditions, this paper analyzes its suitability for pulsed laser implantation on X38CrMoV5-3 tool steel for the first time. In the experiments, the influence of the particles and the laser parameters (pulse power, pulse duration and focal diameter) on the material properties of the localized dispersed zones was studied by optical microscopy, scanning electron microscopy, energy dispersive X-ray spectroscopy and X-ray diffraction. The composite´s (micro-) hardness was measured and calculated by using a rule of mixture. Additionally, the influence of the laser parameters and the TaC particles on the geometrical properties of the implants was studied by optical microscopy and white light interferometry.
The results showed that defect-free implants with hardness values of ~900 HV1 can be obtained at the focal spot, since a localized dispersing of the TaC particles is possible using a pulsed millisecond laser. However, in dependence of the laser intensity, also a partial dissolution of the initial particles occurs. This leads to the precipitation of new dendritic TaC nanoparticles and to varying contents of retained austenite in the matrix. Both effects have a strong influence on the implant hardness and must be considert by the rule of mixture. Regarding the geometrical response it was pointed out that protruded microfeatures with heights up to 10 µm can be created. In comparison to laser remelted zones, the implanted zones showed significantly altered weld pool profiles due to the influence of the particles on the melt convection. A transition of the implant shape from predominantly dome-shaped to predominantly ring-shaped was observed for intensities >1.7∙106 W/cm2 due to the onset of the keyhole effect.
In additive manufacturing (AM) Laser Metal Deposition (LMD), parts are built by welding layers of powder feedstock onto a substrate. Applications for steel powders include forging tools and structural components for various industries. For large parts, the choice of tool-paths influences the build-rate, the part performance and the distortions in a highly geometry-dependent manner. With weld-path lengths in the range of hundreds of meters, a reliable, automated tool path generation is essential for the usability of LMD processes.
In this contribution, automated tool-path generation approaches are shown and their results are discussed for arbitrary geometries. The investigated path strategies are the classical approaches: “Zig-zag-” and “contour-parallel-strategies”. After generation, the tool-paths are automatically formatted into g-code for experimental build-up and ASCII for a numerical simulation model. Finally, the tool paths are discussed in regards to volume-fill, microstructure and porosity for the experimental samples.
This work presents a part of the IGF project 18737N “Welding distortion simulation” (FOSTA P1140)
Das DED Auftragschweißen ist ein additives Fertigungsverfahren für Metalle, bei dem das Material schichtweise auf ein Substrat aufgetragen wird. Die schnellen Temperaturzyklen rufen Spannungsgradienten im Bauteil hervor. Der schichtweise Aufbau der Bauteile verursacht eine anisotrope Mikrostruktur. Mittels nachgelagerter Wärmebehandlung können diese Effekte verringert werden. Im anschließenden Schritt der Prozesskette wird das additiv hergestellte Bauteil mittels Drahterodieren von dem Substrat abgetrennt.
In diesem Beitrag wird eine thermo-mechanische Simulation der gesamten Prozesskette vorgestellt, welche den additiven Aufbau, Wärmebehandlung und das Abtrennen vom Substrat beinhaltet. Anstelle der in der Literatur üblichen schichtweisen Modellierungsstrategie für die DED Simulation wird das gesamte Bauteil in einem Stück vernetzt und der vollständig transiente, schichtweise Materialauftrag über Elementgruppen realisiert. Im Gegensatz zu früheren Simulationen muss der nichtlineare Kontakt zwischen den Schichten nicht berücksichtigt werden, was die Rechenzeiten deutlich verkürzt.
Das Modell wurde validiert mittels Abgleiches des Verzugs aus Simulation und Experiment.
Die Proben, bestehend aus DIN 1.4404 (AISI 316L), wurden nach jedem Prozessschritt 3D gescannt um den Verzug zu quantifizieren. Zusätzlich wurden Querschnitte und Härtetests nach Vickers von unterschiedlich behandelten Proben durchgeführt, um den Effekt der Wärmebehandlung auf die Mikrostruktur und die Härte des Bauteils zu untersuchen.
Приведено аналитическое решение задачи теплопроводности после прекращения действия подвижного источника теплоты для различных комбинаций источника и свариваемого тела. Показано, что после выключения источника возможно дополнительное плавление основного металла за счет перегретого жидкого металла сварочной ванны. Например, при лазерной сварке со сквозным проплавлением стальной пластины толщиной 2 мм длина кратера шва может быт на 19% больше установившейся длины сварочной ванны. Установлено, что центр кратера, в котором заканчивается затвердевание жидкого металла, смещен в сторону хвостовой части кратера относительно оси теплового источника в момент прекращения его действия. Скорость и направление кристаллизации металла сварочной ванны и кратера различны.
The introduction of an external magnetic field in laser beam welding can bring a lot of beneficial effects e. g. a homogeneous element distribution and grain refinement. However, the physical mechanism has not been fully revealed because it is difficult to describe the weld pool behavior quantitatively. In this work, the influence of an oscillating magnetic field in wire feed laser beam welding is studied using a three-dimensional transient multi-physical model. The magnetohydrodynamics, heat transfer, fluid flow, keyhole dynamics and element transport are all taken into consideration. Under suitable electromagnetic parameters, a significant electromagnetic stirring can be produced in the weld pool by the induced Lorentz force. It shows important influence on the keyhole stability and the fluid flow. The keyhole collapses more frequently at the upper part under the oscillating magnetic field. The forward and downward flow along the central plane of the weld pool is enhanced, which can bring the additional element from the filler wire to the root of the weld pool. There is a good agreement between the numerical results and the experiment results from the high-speed imaging, the optical micrograph and the energy dispersive X-ray spectroscopy. This work provides a fundamental understanding of the relationship between electromagnetic control, weld pool behavior and weld property.
Die Laserimplantation erlaubt die Herstellung verschleißbeständiger, erhabener Mikrostrukturen (Implants) auf Stahloberflächen durch ein diskontinuierliches Dispergieren von keramischen Partikeln mittels gepulster Laserstrahlung. Durch die flexible Anordnung separierter Implants zu komplexen Mustern erlaubt das Verfahren eine gezielte Oberflächenstrukturierung zur Beeinflussung des Reibungs- und Verschleißverhaltens. Insbesondere erwies sich Titandiborid (TiB2) als Implantationsmaterial für geeig-net, da eine Manipulation der Implantgeometrie in einem breiten Bereich vorgenommen werden konnte, ohne dass Materialdefekte wie Risse oder Poren auftraten.
Ziel der Untersuchungen war es, den Einfluss implantierter TiB2-Partikel auf die Materialeigenschaften von X153CrMoV12 zu ermitteln. Hierfür wurden im Rahmen der Arbeit die Laserparameter (Pulsleistung und -dauer) in einem breiten Parameterfeld variiert und vergleichende Untersuchungen an TiB2 implan-tierten Zonen sowie an punktuell umschmelzstrukturierten Zonen durchgeführt. Die Ergebnisse zeigen, dass eine reine Umschmelzstrukturierung zu einer deutlichen Reduktion der Oberflächenhärte aufgrund erhöhter Restaustenitgehalte (γR) führt. Im Gegensatz dazu führt das Laserimplantieren von TiB2-Partikeln zu einer deutlichen Härtesteigerung in den kuppel- oder ringförmigen Implants. Härtewerte von bis zu 1800 HV1 resultieren aus dispergierten TiB2-Primärpartikeln sowie in-situ ausgeschiedenen Se-kundärphasen, durch die der Restaustenitanteil zudem deutlich reduziert wird.
The shape of the parts, created by the technology of direct laser metal deposition (DLMD), is influenced by various parameters, for example, the power and diameter of the laser source spot. The contribution of energy from the laser affects the temperature distribution in the formed layers. The changing temperature in the working area entails a change in the geometry of the layers and affects the stability of the process. In this paper, experiments on the measurement of temperature cycles in the DLMD process with different directions of the filling track are carried out. An infrared camera was used to measure thermal cycles. The calibration of the acquired data (i.e. correspondence table between the intensity of thermal radiation of the material and the absolute temperature) was done with help of two-color pyrometer ex situ and in situ measurements. The experiments are carried out on two materials 316L and Inconel 718. The effect of the maximum temperature on the layer height is shown, and thermal cycles in the formation of layers for different filling strategies are presented.
The shape of the parts, created by the technology of direct laser metal deposition (DLMD), is influenced by various parameters, for example, the power and diameter of the laser source spot. The contribution of energy from the laser affects the temperature distribution in the formed layers. The changing temperature in the working area entails a Change in the geometry of the layers and affects the stability of the process. In this paper, experiments on the measurement of temperature cycles in the DLMD process with different directions of the filling track are carried out. An infrared camera was used to measure thermal cycles. The calibration of the acquired data (i.e. correspondence table between the intensity of thermal radiation of the material and the absolute temperature) was done with help of two-color pyrometer ex situ and in situ measurements. The experiments are carried out on two materials 316L and Inconel 718. The effect of the maximum temperature on the layer height is shown, and thermal cycles in the formation of layers for different filling strategies are presented.
Plasma-Transferred-Arc (PTA) welding is a process that enables high deposition rates, but also causes increased thermal load on the component. Laser based Direct Energy Deposition (DED) welding, on the other hand, achieves a high level of precision and thus comparatively low deposition rates, which can lead to high processing costs. Combining laser and arc energy aims to exploit the respective advantages of both technologies.
In this study, different possibilities of this process combination are presented using a PTA system and a 2 kW disk laser. This includes the combination in a common process zone as a highspeed plasma laser cladding technology (HPLC), which achieves process speeds of 10 m/min. Besides that it is being examined whether a pre-running plasma arc can be used to coat difficult-to-weld rail steel with a carbon content of 0.8 % due to a preheating effect. Furthermore, a smoothing of the coating by a plasma arc following the laser is investigated.
This work aims to find the thermal cycles during and after fusion welding through simulation by first calculating the resulting local temperature field in the quasi-stationary part of the process. Here complete-penetration keyhole laser beam welding with a laser power of 18 kW on a 15 mm thick slab of a low-alloyed steel at a welding speed of 2 m/min is considered. In order to physically depict the laser material interaction a multi-physics numerical model including the effects of phase transformation, thermo-capillary convection, natural convection and temperature-dependent material properties up to evaporation temperature is developed. It uses a fixed keyhole geometry with a right truncated circular cone shape to introduce the laser beam energy to the workpiece. In a subsequent study, the resulting local temperature field is then used as an equivalent heat source in order to predict the unsteady thermal cycle during and after fusion welding. The translational movement of the laser beam through the workpiece is represented by a moving mesh approach. For the simulation, stationary heat transfer and fluid dynamics are described by a system of strongly coupled partial differential equations. These are solved with the commercial finite element software COMSOL Multiphysics 5.0. The results of the numerical simulation are validated by experiments, where the weld bead shapes and the thermal cycles show good correlation.
In this study, the influence of the welding speed and the arc power on the solidification crack formation for partial penetration laser hybrid welded Thick-Walled plates were investigated. Experimentally, a linear correlation between the welding velocity and the crack number was observed. That is by reducing the welding velocity the crack number was reduced.
The reduced welding velocity showed a strong impact on stress, as the model demonstrated a very lower stress amount in comparison to the reference case. The reduction of the welding speed could be a helpful technique to reduce the hot cracking. The wire feed speed showed a very slight influence on the crack formation. That can be returned to the large distance between the critical region for cracking and the arc region.
In this study, the influence of the welding speed and the arc power on the solidification crack formation for partial penetration laser hybrid welded Thick-Walled plates were investigated. Experimentally, a linear correlation between the welding velocity and the crack number was observed. That is by reducing the welding velocity the crack number was reduced.
The reduced welding velocity showed a strong impact on stress, as the model demonstrated a very lower stress amount in comparison to the reference case. The reduction of the welding speed could be a helpful technique to reduce the hot cracking. The wire feed speed showed a very slight influence on the crack formation. That can be returned to the large distance between the critical region for cracking and the arc region.
In this study, the influence of the welding speed, the arc power and the laser focal position on the solidification crack formation for partial penetration laser hybrid welded thick-walled plates were investigated. Experimentally, a direct correlation between the welding speed and the crack number was observed. That is by reducing the welding velocity the crack number was decreased. The focal position shows also a significant influence on the crack number. Since by focusing the laser on the specimen surface, the crack number has been significantly diminished.
The wire feed speed showed a very slight influence on the crack formation. That is due to the large distance between the critical region for cracking and the arc region.
The numerical model shows a high-stress concentration in the weld root for both components (vertical and transversal).
Numerically, the reduced welding speed showed a strong impact on stress, as the model demonstrated a lower stress amount by decreasing the welding speed. The solidification cracking in the weld root is a result of interaction between metallurgical and geometrical and thermomechanical factors.
Hybrid laser-arc welding offers many advantages, such as deep penetration, good gap bridge-ability, and low distortion due to reduced heat input. The filler wire which is supplied to the process is used to influence the microstructure and mechanical properties of the weld seam.
A typical problem in deep penetration high-power laser beam welding with filler wire and hybrid laser-arc welding is an insufficient mixing of filler material in the weld pool, leading to a non-uniform element distribution in the seam. In this study, oscillating magnetic fields were used to form a non-conservative component of the Lorentz force in the weld pool to improve the element Distribution over the entire thickness of the material. Full penetration hybrid laser-arc welds were performed on 20-mm-thick S355J2 steel plates with a nickel-based wire for different arrangements of the oscillating magnetic field. The Energy-dispersive X-ray spectroscopy (EDS) data for the distribution of two tracing elements (Ni and Cr) were used to analyze the homogeneity of dilution of the filler wire.
With a 30° turn of the magnetic field to the welding direction, a radical improvement in the filler material distribution was demonstrated. This would lead to an improvement of the mechanical properties with the use of a suitable filler wire.
The advantage of selective laser melting (SLM) is its high accuracy and geometrical flexibility.
Because the maximum size of the components is limited by the process chamber, possibilities must be found to combine several parts manufactured by SLM. An application where this is necessary, is, for example, the components of gas turbines, such as burners or oil return pipes, and inserts, which can be joined by circumferential welds. However, only a few investigations to date have been carried out for the welding of components produced by SLM. The object of this paper is, therefore, to investigate the feasibility of laser beam welding for joining SLM tube connections made of nickel-based alloys.
For this purpose, SLM-manufactured Inconel 625 and Inconel 718 tubes were welded with a Yb:YAG disk laser and subsequently examined for residual stresses and defects. The results showed that the welds had no significant influence on the residual stresses. A good weld quality could be achieved in the seam circumference. However, pores and pore nests were found in the final overlap area, which meant that no continuous good welding quality could be accomplished. Pore formation was presumably caused by capillary instabilities when the laser power was ramped out.
The presented study deals with the performing and mechanical testing of single pass hybrid laser-arc welds (HLAW) on 25 mm thick plates made of steel grade S355J2. One of the challenges have to be solved at full penetration HLAW of thick plates is the drop formation occurring due to the disbalances of the forces acting in the keyhole and on the melt pool surface. Such irregularities mostly limit the use of high-power laser beam welding or HLAW of thick-walled constructions. To overcome this problem, an innovative concept of melt pool support based on generating Lorentz forces in the weld pool is used in this work. This method allows to perform high quality welds without sagging even for welding of 25 mm thick plates in flat position at a welding speed of 0.9 m min-1. For the obtain of full penetrated welds a laser beam power of 19 kW was needed. A high V-impact energy of up to 160 J could be achieved at the test temperature of 0 °C. Even at the most critical part in the weld root an impact energy of 60 J in average could be reached. The tensile strength of the weld reaches that of the base material. An introduce of the HLAW process with electromagnetic support of the melt pool in the industrial practice is an efficient alternative to the time- and cost-intensive arc-based multi-layer welding techniques which are established nowadays for joining of thick-walled constructions.
With global increases in clean energy demand, the natural gas is gaining in importance. Pipelines are the safest and most cost-effective way of transporting natural gas. Due to high transport volume and resulting high operation pressure, the demand for ultra-high strength steel grades such as X120 is very strong. As a result of the fact that these steels are produced by thermo-mechanical controlled processing, the welding process must be selected accordingly. Based on investigations, a high heat input such as by submerged arc welding process leads to softening in the weld metal and loss of strength whereas pure laser beam welding results in high cooling rates and deteriorate toughness of the weld metal. The objective of this research is to investigate the influence of heat input to mechanical properties of hybrid laser-arc welded pipeline steels of grade X120. Test specimens with a thickness of 20 mm could be welded without preheating in a single-pass with different welding velocities to observe the largest possible parameter window of the heat input. The achieved V-notch impact energy for hybrid laser-arc welded samples was 144±37 J at a testing temperature of -40 °C. With a tensile strength of 930±4 MPa the requirements of API 5L was achieved. To prevent gravity drop-outs at the slow welding speeds, an electromagnetic weld pool support system was used, which works contactless and is based on generating Lorentz forces. It was therefore possible to control the cooling rate in order to meet the requirements of the mechanical properties. By adapting the electromagnetic weld pool support to the laser and laser hybrid welding process, the application potential of these technologies for industrial implementation can be drastically increased.
Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support
(2019)
Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
Results of experimental investigations of the relationship between laser-hybrid welding process parameters, type of the filler metal and the mechanical properties of the welds made from 9% nickel cryogenic steel X8Ni9 are discussed. The results contribute to the development and conversion in the industrial practice a new laser beam-based welding technology for the automated manufacturing of LNG tanks. The remarkable heterogeneity in the chemical composition of the weld metal as well as an insufficient impact toughness could be indicated by using austenitic filler wire. The most promising results were achieved by applying 11%Ni filler wire, which is similar to the base material. A correlation between impact toughness and wire feeding speed could be shown. The highest impact toughness was 134 J at -196°C. The laser-hybrid welds passed the tensile test. The failure stress of 720 MPa with a fracture location in the base metal was achieved for all samples tested.