Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
Dokumenttyp
- Beitrag zu einem Tagungsband (30)
- Vortrag (27)
- Sonstiges (24)
- Zeitschriftenartikel (6)
- Posterpräsentation (1)
Sprache
- Englisch (88) (entfernen)
Referierte Publikation
- nein (88) (entfernen)
Schlagworte
- Corrosion (50)
- Geothermal (17)
- Coating (11)
- CCS (10)
- Steel (10)
- Geothermal energy (9)
- CO2 (8)
- Copper (8)
- CCUS (7)
- Polyaniline (7)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (69)
- 7.6 Korrosion und Korrosionsschutz (69)
- 5 Werkstofftechnik (22)
- 5.1 Mikrostruktur Design und Degradation (21)
- 3 Gefahrgutumschließungen; Energiespeicher (2)
- 3.2 Gefahrguttanks und Unfallmechanik (2)
- 5.6 Glas (2)
- 6 Materialchemie (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.4 Prozessanalytik (1)
Eingeladener Vortrag
- nein (27)
The collaborative project “Impacts of impurities in CO2 streams captured from different emitters in a regional cluster on transport, injection and storage (CLUSTER)” aimed to set up recommendations on how to define “reasonable minimum composition thresholds” that CO2 streams should meet when accessing CO2 transport pipeline networks. Within CLUSTER, we investigated potential impacts of CO2 streams with different and temporally variable compositions and mass flow rates along the whole CCS chain. Investigations included, amongst others, impacts on:
• corrosion of pipeline steel,
• pipeline network design and related transport costs,
• alteration of well bore cements,
• pressure development and rock integrity,
• geochemical reactions, and
• petrophysical and geomechanical rock properties.
All investigations are based on a generic CCS chain scenario. In this scenario, CO2 streams are captured from a spatial cluster of eleven emitters and collected in a regional pipeline network. Emitters comprise seven fossil fuel-fired power plants equipped with different capture technologies, two cement plants, one refinery and one integrated iron and steel plant. In total, 19.78 Mio t CO2 (including impurities) are captured in the emitter cluster annually. The combined CO2 stream is transported in a trunk line with a length of 400 km (100 km of these offshore) and is injected into five generic storage structures. The storage reservoirs are saline aquifers of the Buntsandstein.
The investigations revealed beneficial and deteriorating impacts of different impurities and combinations thereof. Overall, no fundamental technical obstacles for transporting, injecting and storing CO2 streams of the modelled variable compositions and mass flow rates were observed. Based on the results, the CLUSTER project team recommends not to define “minimum composition thresholds” for CO2 streams as strict threshold values for each individual impurity in the stream. Instead, CO2 stream compositions and variabilities for specific CCS projects should be constrained with regard to a set of parameters including i) the overall CO2 content, ii) maximum contents of relevant impurities or elements, iii) acceptable variability of CO2 stream composition, and iv) impurity combinations to be avoided.
The collaborative project “Impacts of impurities in CO2 streams captured from different emitters in a regional cluster on transport, injection and storage (CLUSTER)” aimed to set up recommendations on how to define “reasonable minimum composition thresholds” that CO2 streams should meet when accessing CO2 transport pipeline networks. Within CLUSTER, we investigated potential impacts of CO2 streams with different and temporally variable compositions and mass flow rates along the whole CCS chain. Investigations included, amongst others, impacts on: Corrosion of pipeline steel, pipeline network design and related transport costs, alteration of well bore cements, pressure development and rock integrity, geochemical reactions, and petrophysical and geomechanical rock properties.
All investigations are based on a generic CCS chain scenario. In this scenario, CO2 streams are captured from a spatial cluster of eleven emitters and collected in a regional pipeline network. Emitters comprise seven fossil fuel-fired power plants equipped with different capture technologies, two cement plants, one refinery and one integrated iron and steel plant. In total, 19.78 Mio t CO2 (including impurities) are captured in the emitter cluster annually. The combined CO2 stream is transported in a trunk line with a length of 400 km (100 km of these offshore) and is injected into five generic storage structures. The storage reservoirs are saline aquifers of the Buntsandstein.
The investigations revealed beneficial and deteriorating impacts of different impurities and combinations thereof. Overall, no fundamental technical obstacles for transporting, injecting and storing CO2 streams of the modelled variable compositions and mass flow rates were observed. Based on the results, the CLUSTER project team recommends not to define “minimum composition thresholds” for CO2 streams as strict threshold values for each individual impurity in the stream. Instead, CO2 stream compositions and variabilities for specific CCS projects should be constrained with regard to a set of parameters including i) the overall CO2 content, ii) maximum contents of relevant impurities or elements, iii) acceptable variability of CO2 stream composition, and iv) impurity combinations to be avoided.
According to the results of the experiments carried out, the following points can be concluded:
1. Exposure tests showed that specimens with the addition of SiO2 particles and polyaniline particles exhibit better corrosion resistance than specimens with the addition of only polyaniline particles or binder only.
2. Open circuit potential measurements showed that in the beginning of the experiments, both coatings had an open circuit potential 100 mV higher than carbon steel. Within one day of immersion, the potential of carbon steel increased significantly, indicating the formation of oxide layer. After extended exposure the carbon steel potential sat between PS1 (which had higher potential) and PS2 (which had a lower potential) and all three were in the range –600 mV to –500 mV vs Ag/AgCl.
3. Both coatings PS-1 and PS-2 were degraded with increasing exposure time, shown by the decrease of absolute impedance value at low frequency range after 2, 4, and 6 days exposure.
4. Potentiodynamic test was performed after 3 hours and 6 days exposure, and it was shown that the coating in the initial stage exhibited more passive behavior than the specimens exposed for 6 days.
Synergistic effects of impurities in the condensate on the corrosion of CO2 transport pipeline
(2017)
For the reliability of transport pipelines the corrosion resistance of the materials used needs to be determined in conditions, which are possible during the transport process. In some situations condensation of components out of the CO2 stream can occur. To study the effect of condensate on transport pipeline steel, a “worst-case scenario” gas mixture, containing 2.5 % H2O, 1.8 % O2, 1000 ppmv NO2, and 220 ppmv SO2, was proposed, fed (1.5 L/min) into a glass reactor containing coupon-shaped specimens for 120 600 h at 278 K (to simulate the underground pipeline transport), and resulted in the condensate containing 0.114 M H2SO4 and 0.0184 M HNO3 (pH 2.13). Basing on this “original” condensate, exposure tests and electrochemical characterization together with pH and conductivity in CO2 saturated condition at the same temperature were carried out. The role of each gas impurity and the combination of them, when the condensate is formed, was studied by investigating the role of individual and varying combination of acidic components in the condensate on the corrosion behaviors of the commercial pipeline-steel (L360NB). It can be concluded that although the condensation of NOx in form of HNO3 causes faster corrosion rate, it is the condensation of SOx or the combination of SOx and NOx that may cause much more severe problems in form of localized and pitting corrosions. Different to the corrosion products formed in CO2 atmosphere without impurities (mainly iron carbonate) the corrosion products resulted from these acidic condensation have no protectability, indicating the need of controlling gas quality during the transportation within the pipeline network.
Within the last years the use of feasible alternative energy sources has risen and is going to replace fossil resources more and more. Nevertheless, service conditions in solar facilities are due to the chemical composition of heat transmission media and temperatures, in many cases, extreme in terms of corrosion. Since the construction of power plants shall be economical with maximum life service, materials selection based on preliminary material qualification is essential to guarantee a secure and reliable operation of those facilities.
The materials selection depends on the operation temperature of a power plant on the chemical composition of the transmission fluid used. In high corrosive environments Ni-based alloys are often used as an all-round solution for the construction of corrosion resistant parts, because of their good corrosion properties. However, there might be limits for their use regarding their corrosion behavior, with which this contribution deals.
By means of electrochemical measurements and exposure tests the suitability of two high alloyed materials X8NiCrSi38 18 and NiCr25FeAlYB in molten nitrate salt (60 % NaNO3/40 % KNO3) was characterized at 600 °C.
Within the last years the use of feasible alternative energy sources has risen and is going to replace fossil resources more and more. Nevertheless, service conditions in solar facilities are due to the chemical composition of heat transmission media and temperatures, in many cases, extreme in terms of corrosion. Since the construction of power plants shall be economical with maximum life service, materials selection based on preliminary material qualification is essential to guarantee a secure and reliable operation of those facilities.
The materials selection depends on the operation temperature of a power plant on the chemical composition of the transmission fluid used. In high corrosive environments Ni-based alloys are often used as an all-round solution for the construction of corrosion resistant parts, because of their good corrosion properties. However, there might be limits for their use regarding their corrosion behavior, with which this contribution deals.
By means of electrochemical measurements and exposure tests the suitability of two high alloyed materials X8NiCrSi38-18 and NiCr25FeAlYB in molten nitrate salt (60 % NaNO3/40 % KNO3) was characterized at 600 °C.
Study of Polyaniline/Silicon Dioxide based Coating on Carbon Steel in Artificial Geothermal Brine
(2021)
Geothermal brines are corrosive in nature because of their salt contents and high temperatures. Therefore, they pose a major challenge to geothermal power-plants, which are mostly built of low alloyed steels, e.g., carbon steel. Carbon steel is susceptible to uniform and localized corrosion when exposed to geothermal brines having acidic-saline properties. To overcome this limitation, geothermal power plants should be built by either high alloyed materials or by integrating protection systems on carbon steel, such as coatings and inhibitors. We studied a coating system containing polyaniline/silicon dioxide basing on locally available resources that provides protection against corrosion of carbon steel and enhance the thermal resistance in geothermal environments. Here, exposure and electrochemical tests of coated carbon steels were performed in an artificial geothermal brine. The solution had a pH of 4, with the composition of 1,500 mg/L of chlorides, which is based on the chemical analysis of geothermal brine found in Sibayak, Indonesia. All exposure tests were conducted using autoclaves at 150 °C with a total pressure of 1 MPa, which was performed for up to six months to evaluate the durability of the coating system. Post-experimental analyses were performed by assessing the surface of specimens using optical and electron microscopes. On the other hand, electrochemical tests were performed for seven days at 25 °C and 150 °C to investigate the kinetics of electrochemical reactions by measuring open circuit potential and electrochemical impedance spectra. Experimental results showed the corrosion resistance of PANI/SiO2 composite coatings, where polyaniline and SiO2 play their roles as stabilizers.
Study of Polyaniline/Silicon Dioxide based Coating on Carbon Steel in Artificial Geothermal Brine
(2021)
By using the available resources in Indonesia, such as silicon dioxide and marine coating base, the PANI/SiO2 modified alkyd coating was able to protect carbon steel in a deaerated artificial geothermal water. The screening of coatings shows that the modification by adding individual pigment was not sufficient to protect carbon steel even during a short-term exposure, indicated by the discoloration after only seven days of exposure. Electrochemical tests indicated that there was no significant change in the Ecorr between the coated and uncoated carbon steel at room temperature. At 150 °C, the coated carbon steel has a lower potential than that of carbon steel, indicating that the coating is protecting carbon steel cathodically or slowing down the corrosion reaction. Finally, a long-term exposure test confirmed that the PANI/SiO2 modified coating successfully protects the carbon steel in the Sibayak artificial geothermal water up to 150 °C for 6 months.
The suitability of an Al2O3 coating for corrosion protection on X20Cr13 was evaluated in various artificial geothermal brines, focusing on the influence of different pH (4, 6 and 8) and their chemical compositions on the coating properties. All experiments were performed in the laboratory using autoclaves at 150 ◦C and 1 MPa in deaerated condition for 1 and 7 days. Results showed that the pH of geothermal waters is the most detrimental factor in the transformation of ɣ-Al2O3 and its protective abilities. Delaminations were found in the Coating exposed to geothermal brines with pH 4. FTIR spectra indicated a transformation of ɣ-Al2O3 to boehmite AlOOH after exposure to pH 4 and 6, and bayerite Al(OH)3 was formed after exposure to pH 8. Different Crystal structures of the hydrated Al2O3 also contribute to the stability of the coatings, observed by the SEM- EDX of the surface and cross-section of coatings. This study indicated that ɣ-Al2O3 sol-gel coating presents a promising aspect of corrosion protection in geothermal environment with a neutral pH.
Often 3D‐printing and additive manufacturing are mentioned as the 3rd industrial revolution. In this conjunction this book provides a brief overview on additively manufactured metal pieces.
This book fulfills its intension to serve as an educational guide, providing a holistic picture encompassing science, technology and applications for the real‐life use of Metal Additive Manufacturing.
This book grew out of a course on polymer coatings held by the author at the university. It shall serve as an introduction to the wide field of polymer coatings. It is not intended to cover completely all facts on polymer coatings.
All chapters are well structured. Selected figures and formulas illustrate the content and contribute to a good understandability. At the end of each chapter some hints for further reading are provided.
Finally, the book fulfills its intention to introduce into the topic by providing basics on science and technology of polymer coatings, suitable for chemists in industry, materials scientists, polymer chemists and physical chemists.
The second edition of this textbook on physical electrochemistry, written by two experienced teachers of physical chemistry, corrosion engineering and materials science and engineering, covers the current knowledge which should be transferred to students of these fields.
In 20 chapters the fundamentals of electrochemistry, the most important electrochemical measurement techniques and applications of electrochemistry are covered.
It can be concluded that this study fulfills its intension of “serving as a key textbook in undergraduate courses” dealing with electrochemistry and being “a reference source for graduated students, researchers and engineers” interested in this field. Teachers will find sufficient content for preparing lectures on this topic. Even self‐learning is well supported by the clear structure, presented content and provided sources for further reading.
Since nanoscience has a tremendous impact on the development of electrochemistry, Wiley‐VCH paid attention to that by publishing thisbook as volume 17 within the series “Advances in Electrochemical Science and Engineering”.
This collection of “nanoaspects”on electrodes provides a helpful overview on principles and current findings to readers interested in such applications. It fulfills its intention of being “a valuable resource for researchers working in such fields as electrochemistry, materials science, spectroscopy, analytical and medicinal chemistry”.
Since data processing has now also found its way into materials science, there has been a great demand from users for a corresponding textbook. This book provides a guide to the latest advances of materials informatics and data mining for materials science. 46 authors introduce readers to methods, present tools and case studies to illustrate the power of materials informatics within this new field of application.
This concise reference book,consisting of 2 volumes, provides “key scientific and technical properties and data” for “materials scientists, metallurgists, engineers,chemists, and physicists as well as academic staff, technicians, and students” dealing with such kind of materials.
Within its 3rd edition the previous work was extended by a chapter on occupational health and safety issues of materials, beside of the update of whole content. Within 22 chapters materials properties and data are summarized in many tables. Some facts are illustrated by drawings and diagrams for better understandability. Each chapter ends with a part on further reading arranged accordingly.
The first edition of this book, published within the series “Materials Science – Metals and Alloys”, provides broad knowledge of this interesting and widely applied metal from manufacturing and production to finishing and application in 13 chapters, written by 29 contributors. Each chapter is separately concluded and ends with references used.
This book fulfills its intention of conveying comprehensive and cutting‐edge knowledge of magnesium alloys. It is useful for practicing engineers, researchers and students searching for an instructional and reference source.
Since materials play an important role when designing and servicing industrial facilities. Also, for energy systems there is no way around. Selection of appropriate materials is an essential aspect for successful application and reliable service life. Future engineers must be made aware on the importance of this fact. So, they may prevail in techno‐economic discussions.
The book fulfills its intension of providing to students in science and engineering a comprehensive understanding of different energy processes and what role materials play in this conjunction. Also, it gives interested engineers and scientists an insight in this matter. After being introduced the user should dig deeper in the existing detailed knowledge available for materials selection within these special conditions to assure a reliable operation of the energy production facility.
Currently, storage of electric energy is becoming more and more interesting in terms of applicability and efficiency. One way is the electrochemical storage by already well‐developed battery‐systems. This textbook provides an introduction into physical and chemical processes necessary for battery application.
This book fulfills its intension to serve graduate students of electrical engineering as an introduction into the field of batteries. Even students and interested readers of other faculties might find an introduction in physical and chemical background of batteries.
This book introduces to aspects to be considered when dealing with coatings and linings. Philip A. Schweitzer covers and compares a variety of specific coatings and their applications. In 18 chapters he divided the content into two main parts: linings and coatings.
All professionals involved in design and maintenance processes get by this book a compact survey of necessary considerations which needs to be done when applying surface protection measures. The literature references at the end of some chapters support the readers finding additional information about the special topic, mainly written by the author himself. Since this newly issued paperback edition is a 1:1 re‐print of the 2001 hardcover version, neither current publications are referenced, nor revisions were made.
This paperback issue of the 2007 hardcover version within the “Corrosion Engineering Handbook” series presents various materials and methods for controlling and protecting against corrosion instead of using expensive alloys to construct a tank or processing vessel.
This book is a very comprehensive collection of the current knowledge about applied linings and coatings. So, it fulfills its intension, “that regardless of what is being built, … information for … whoever is responsible for the selection of material of construction will be found in this book to enable them to avoid unnecessary loss of material through corrosion”, to a very large extent.
This edition, published as first issue within the series “Corrosion Atlas”, provides 181 corrosion case studies, collected from 29 contributors.
These Corrosion Atlas Case Studies provide a helpful tool required for engineers in their daily life to quickly determine and solve their equipment's corrosion problems by compact theoretical background and vivid examples. It fulfills the intension of the editors to be “the first centralized collection of case studies containing challenges paired directly with solutions together in one location”.
his fully updated examination of sustainable processes for gaseous and liquid biofuels production, published for the second time within the series “Biomass, Biofuels, Biochemicals”, provides 33 contributions made by 120 authors. They present a holistic view of biofuels in research, operation, scale‐up and application. Comparing to the first edition, all chapters have been updated and new chapters covering topics of current interest, including sustainability and biohydrogen have been added.
By its wide overview on existing technologies, this book provides state‐of‐the‐art information and knowledge to the desired readership, like post‐graduates, researchers in the area of biofuels, wastewater treatment, alternate energy sources, renewable energy from biomass, chemical and biochemical engineers, microbiologists, biotechnologists working in academic and research institutes as well as in industry and governmental agencies.
This book by Scrivener Publishing contains 14 chapters written by 82 leading scientists, experienced in the field of coatings. They demonstrate mechanisms, usage and manipulation of cutting‐edge coating methods. Each chapter is well structured and ends with a conclusion, highlighting the content. The book is divided into 3 parts: “Materials and Methods”, “Coating Materials Nanotechnology” and “Advanced Coating Technology and Applications”.
Finally, this book provides a comprehensive insight into innovative research in advanced coating materials and state‐of‐the‐art technologies, without being a real textbook. It fulfills its intension of being beneficial both for technicians and scientists.
Al2O3 coatings are often used as protective layers on steels against electrochemical and high-temperature corrosion because they are chemically inert and stable at elevated temperatures. This study presents preliminary work on the possibilities of using Al2O3 sol-gel coatings for corrosion protection of martensitic stainless steels in geothermal environments. Al2O3 sol-gel coatings were applied on UNS S42000, which is known to be susceptible to uniform and localized corrosion. The coated steel specimens were then tested in two types of artificial geothermal water, which simulate the geothermal fluids found in Sibayak (SBY), Indonesia, and North German Basin (NGB), Germany, respectively. SBY has pH 4 and 1.5 g/L of chloride ions, whereas NGB has a pH of 6 and 166 g/L of chloride ions. All experiments were carried out in autoclaves at 150 °C and 1 MPa under the deaerated condition. Evaluations were performed by investigating the surface profiles of both uncoated and coated steels before and after the corrosion test using a Laser Scanning Microscope (LSM) and Scanning Electron Microscope (SEM). Finally, Electrochemical Impedance Spectroscopy (EIS) was performed to compare the corrosion resistance of Al2O3 coated steels in SBY and NGB solutions. It was observed from the corrosion test that Al2O3 coatings are more suitable for use in the geothermal water with a higher pH.
Al2O3 coatings are often used as protective layers on steels against electrochemical and high-temperature corrosion because they are chemically inert and stable at elevated temperatures. This study presents preliminary work on the possibilities of using Al2O3 sol-gel coatings for corrosion protection of martensitic stainless steels in geothermal environments. Al2O3 sol-gel coatings were applied on UNS S42000, which is known to be susceptible to uniform and localized corrosion. The coated steel specimens were then tested in two types of artificial geothermal water, which simulate the geothermal fluids found in Sibayak (SBY), Indonesia, and North German Basin (NGB), Germany, respectively. SBY has pH 4 and 1.5 g/L of chloride ions, whereas NGB has a pH of 6 and 166 g/L of chloride ions. All experiments were carried out in autoclaves at 150 °C and 1 MPa under the deaerated condition. Evaluations were performed by investigating the surface profiles of both uncoated and coated steels before and after the corrosion test using a Laser Scanning Microscope (LSM) and Scanning Electron Microscope (SEM). Finally, Electrochemical Impedance Spectroscopy (EIS) was performed to compare the corrosion resistance of Al2O3 coated steels in SBY and NGB solutions. It was observed from the corrosion test that Al2O3 coatings are more suitable for use in the geothermal water with a higher pH.
Geothermal brine is a complex system containing a wide variety of dissolved salts resulting from the condition s in a geothermal well. These fluids lead to corrosion in pipes and other parts of geothermal system construction and necessitate intense research efforts in finding new suitable materials. Carbon steel is susceptible to corrosion in geothermal brine especially when it is exposed to a high temperature and high-pressure medium, which is considered to be an aggressive environment. An artificial geothermal water, bas ed on a brine composition found in Indonesia, was used to investigate the performance of high alloyed materials. The electrolyte has pH 4 and contains 1,500 mg/l Cl-, 20 mg/l SO4 2-, 15 mg/l HCO3 -, 200 mg/l Ca 2+, 250 mg/l K+, and 600 mg/l Na+. In order to protect the bare material in geothermal application, it is necessary to either use high alloyed material s or coatings. In this research, a coating system consisting of polyaniline and silicon dioxide was investigated regarding its behavior to protect carbon steel. In detail, the effect of SiO2 and polyaniline (PANi) addition was evaluated by exposure and electrochemical tests for 7 days, i.e. electrochemical impedance spectroscopy (EIS) and open circuit potential (OCP ) at room temperature and 150 °C with 1 MPa pressure .
Carbon Capture, Utilization and Storage (CCUS) has been proposed as a promising technology for the mitigation of CO2 emissions into the atmosphere from fossil-fuel-operated power generation plants. As the reliability and cost effectiveness of the pipeline transport network is crucial to the overall operability and resilience of the CCUS system, it is vital to realize the possible corrosion risks of the employed pipeline steels corresponding to the impurity level of the gas source.
Recent studies have shown that even the high alloyed materials might be susceptible to general and/or localized corrosion by the condensates forming from the impurities such as SOx, NOx, CO, O2 and water [1]. Up to now, however, there is no regulation procedure which defines the maximum acceptable level of impurities and the combination of them for each employed pipeline steels. Herein, systematic experiment series were conducted by mixing pure CO2 gas with varying concentration of each impurity and with the varying combination of them. Each time, the mixture was then fed (1 L/min) into the reactor containing 12 specimens for 120-600 h at 5°C (to simulate the sub-level pipeline transport). The resulted condensate was collected and analyzed by ionic chromatography and atomic absorption spectroscopy to determine the chemical composition. In this study, the “worst-case scenario” gas mixture, containing 2.5 % H2O, 1.8 % O2, 1000 ppm NO2, and 220 ppm SO2 as impurities, resulted in the condensate containing H2SO4 0.114 M and HNO3 0.0184 M (pH 2.13). This “original” condensate was then re-produced to carry out exposure tests and electrochemical characterization including corrosion potentials and impedance spectroscopy in CO2 saturated condition for 7-14 days at the same temperature. The corrosion rate was also measured by mass loss method.
We can conclude that, at the initial stage, HNO3 plays the dominant role in Fe dissolution process, while H2SO4 is responsible for the pit initiation followed by pitting corrosion. Future studies will be focused on the combination effect from the impurities and the exposure test under the regularly changing condensate to mimic the real CO2 pipeline system.
Carbon Capture, Utilization and Storage (CCUS) has been proposed as a promising technology for the mitigation of CO2 emissions into the atmosphere from fossil-fuel- operated power generation plants. As the reliability and cost effectiveness of the Pipeline transport network is crucial to the Overall operability and resilience of the CCUS system, it is vital to realize the possible corrosion risks of the employed Pipeline steels corresponding to the impurity Level of the gas source. Recent studies have shown that even the high alloyed materials might be susceptible to General and/or localized corrosion by the condensates forming from the impurities such as SOx, NOx, CO, O2 and water.
Up to now, however, there is no regulation procedure which defines the maximum acceptable level of impurities and the combination of them for each employed pipeline steels. Herein, systematic experiment series were conducted by mixing pure CO2 gas with varying concentration of each impurity and with the varying combination of them. Each time, the mixture was then fed (1 L/min) into the reactor containing 12 specimens for 120-600 h at 5°C (to simulate the sub-level Pipeline transport). The resulted condensate was collected and analyzed by ionic chromatography and atomic Absorption spectroscopy to determine the chemical composition. In this study, the “worstcase scenario” gas mixture, containing 2.5 % H2O, 1.8 % O2, 1000 ppm NO2, and 220 ppm SO2 as impurities, resulted in the condensate containing H2SO4 0.114 M and HNO3 0.0184 M (pH 2.13).
This “original” condensate was then reproduced to carry out exposure tests and electrochemical characterization including corrosion potentials and impedance spectroscopy in CO2 saturated condition for 7-14 days at the same temperature. The corrosion rate was also measured by mass loss method.
We can conclude that, at the initial stage, HNO3 plays the dominant role in Fe dissolution process, while H2SO4 is responsible for the pit initiation followed by pitting corrosion. Future studies will be focused on the combination effect from the impurities and the exposure test under the regularly changing condensate to mimic the real CO2 pipeline system.
Carbon Capture and Storage (CCS) is identified as an excellent technology to reach the target of CO2 reduction. However, the safety issue and cost-effectiveness hinder the future of CCS. For the reliability and safety issues of injection wells, the corrosion resistance of the materials used needs to be determined.
In this study, representative low-cost materials including carbon steel 1.8977 and low alloyed steel 1.7225 were investigated in simulated pore water at 333 K and under CO2 saturation condition to represent the worst-case scenario: CO2 diffusion and aquifer fluid penetration. These simulated pore waters were made from relevant cement powder to mimic the realistic casing-cement interface. Electrochemical studies were carried out using the pore water made of cement powder dissolved in water in comparison with those dissolved in synthetic aquifer fluid, to reveal the effect of cement as well as formation water on the steel performance. Two commercially available types of cement were investigated: Dyckerhoff Variodur® and Wollastonite. Variodur® is a cement containing high performance binder with ultra-fine blast furnace slag which can be used to produce high acid resistance concrete. On the other hand, Wollastonite is an emerging natural material mainly made of CaSiO3 which can be hardened by converting to CaCO3 during CO2 injection.
The results showed the pH-reducing effect of CO2 on the simulated pore water/aquifer (from more than 10 to less than 5) leading to the active corrosion process that happened on both 1.8977 and 1.7225. Electrochemical characterization showed negative free corrosion potential and polarisation curves without passive behaviors. The tested coupons suffered from pitting corrosion, which was confirmed by surface analysis. Interestingly, basing on the pit depth measurements from the tested coupons and the hardness of cement powder, it is suggested that Variodur® performed better than Wollastonite in both aspects. The electrochemical data was compared to that resulted from exposure tests to give a recommendation on material selection for bore-hole construction.
The aim of the work presented was the evaluation of corrosion resistance
of various materials in geothermal Waters as a base to create a catalogue of suitable materials for applications in (not only) German geothermal power plants.
Users shall be enabled to have a basis for designing such facilities. High alloyed corrosion resistant alloys are suitable and do not cause copper or lead deposition. They shall be chosen for future design of the piping system, either in massive or in cladded form, if crevices formation with non-metallic materials can be prevented!
The fabrication and characteristics of amorphous silica reinforced Al matrix composites are studied in this paper. The major starting materials were commercial Al powder and extracted nanoparticle SiO2 (NPS) powder from Indonesian silica sands. Two different active solutions,namely N-butanol and tetramethylammonium hydroxide (TMAH), were introduced during synthesis. Characterisations in terms of physical, mechanical, microstructural and corrosion rate examinations were also employed. Introducing the SiO2 nanoparticles into the Al matrix has decreased the density and increased the porosity of the composites. The addition of N-butanol into Al/SiO2(Al/SiO2(B)) led to broader and lower X-ray diffraction profiles than the addition of TMAH (Al/SiO2(T)). From the microstructural analysis, we found that the SiO2 particles enter and agglomerate into the opening gap of the Al sheets. Furthermore, yield strength, ultimate compression strength and modulus of elasticity tended to reduce the addition of SiO2. The corrosion rate of Al/SiO2(T) was lower than that of Al/SiO2(B) composites.
Finally, this book fulfills its intension of facilitating the materials selection regarding current technical and normative aspects for all users, recyclers, test personnel and byers of Cu-materials in all kinds of applications. The well-structured data provide a reliable help for making decisions when applying or using Cu-alloys within the daily business. It shall not be missed in their book-shelfs.
This book provides an overview on research‐topics who need to be investigated when dealing with this topic, basing on the symposium in 2014. It addresses the key challenges involved in CCS materials design, processing and modelling. Readers can get an overview on topics one should consider when working in these field and selecting current Journal articles.
By exposure and electrochemical tests in the laboratory the Cu-effect on corrosion behavior of carbon steel, high-alloyed steels and Ti-alloy can be assessed.
Critical materials specific properties were determined by static exposure and electrochemical tests in an artificial geothermal water with high salinity and low pH, containing Cu. Conclusions were drawn using characteristic potential values.
It could be shown that significant Cu-deposition and -precipitation only occurred in combination with carbon steel. High-alloyed materials (S31603, S31653, S31700, S31703, S31803 and N08904) prevent the disturbing Cu-agglomeration. Therefore, they are suitable to be chosen for future design of the piping system, either in massive or in cladded form, if formation of crevices with non-metallic materials can be excluded.
From the interactions and pitting corrosion point of view, R50400 seems to be most favorable.
By exposure and electrochemical tests in the laboratory the Cu-effect on corrosion behavior of carbon steel, high-alloyed steels and Ti-alloy can be assessed.
Critical materials specific properties were determined by static exposure and electrochemical tests in an artificial geothermal water with high salinity and low pH, containing Cu. Conclusions were drawn using characteristic potential values.
It could be shown that significant Cu-deposition and -precipitation only occurred in combination with carbon steel. High-alloyed materials (S31603, S31653, S31700, S31703, S31803 and N08904) prevent the disturbing Cu-agglomeration. Therefore, they are suitable to be chosen for future design of the piping system, either in massive or in cladded form, if formation of crevices with non-metallic materials can be excluded.
From the interactions and pitting corrosion point of view, R50400 seems to be most favorable.
Since 2016 ISO Technical Committee (TC) 265 is working on standardization the whole CCS-process chain. Around 30 countries are working together to provide international guidelines. As ISO 27913 was the first standard finished within these activities it is already in the stage of first revision.
The objective of ISO 27913 is “to provide specific requirements and recommendations on certain aspects of safe and reliable design, construction and operation of pipelines intended for the large-scale transportation of CO2 that are not already covered in existing pipeline standards such as ISO 13623, ASME B31.8, EN 1594, AS 2885 or other standards. Existing pipeline standards cover many of the issues related to the design and construction of CO2 pipelines; however, there are some CO2 specific issues that are not adequately covered in these standards. The purpose of this document is to cover these issues consistently. Hence, this document is not a standalone standard, but is written to be a supplement to other existing pipeline standards for natural gas or liquids for both onshore and offshore pipelines.”
This contribution shall provide information on the content, the current stage of the revision process, encourage to contribute to this standard and make listeners aware to consider the influence of ISO standard on documents currently in draft.
Since 2016 ISO Technical Committee (TC) 265 is working on standardization the whole CCS-process chain. Around 30 countries are working together to provide international guidelines. As ISO 27913 was the first standard finished within these activities it is already in the stage of first revision.
The objective of ISO 27913 is “to provide specific requirements and recommendations on certain aspects of safe and reliable design, construction and operation of pipelines intended for the large-scale transportation of CO2 that are not already covered in existing pipeline standards such as ISO 13623, ASME B31.8, EN 1594, AS 2885 or other standards. Existing pipeline standards cover many of the issues related to the design and construction of CO2 pipelines; however, there are some CO2 specific issues that are not adequately covered in these standards. The purpose of this document is to cover these issues consistently. Hence, this document is not a standalone standard, but is written to be a supplement to other existing pipeline standards for natural gas or liquids for both onshore and offshore pipelines.”
This contribution shall provide information on the content, the current stage of the revision process, encourage to contribute to this standard and make listeners aware to consider the influence of ISO standard on documents currently in draft.
Specific amounts of oxidizing and reductive impurities as well as some moisture were added to dense phase CO2 to replicate CO2 streams from sources in a CCS pipeline network. Due to the moisture content being only 50 ppmV no visible acid condensation took place. To simulate stress conditions at the inside pipeline surface due to fluid pressure (10 MPa) specimens were preloaded using a load frame. Experiments conducted at 278 K and at 313 K revealed the highest corrosion rate at lower temperature. Corrosive effect of impurities was strongest applying mixed atmosphere, containing oxidizing and reductive components, closely followed by CO2 streams with pure oxidizing character. By far, the lowest corrosion rate (10x lower) resulted from reductive atmosphere. In general, at constant temperature and pressure the CO2 stream composition strongly influences the morphology, thickness and composition of the corrosion products. Applying oxidizing or mixed impurities, iron hydroxides or oxides (e.g. goethite, hematite) occur as dominating corrosion products, capable to incorporate different amounts of sulfur. In contrast, using reductive atmosphere very thin corrosion layers with low crystallinity were developed, and phase identification by XRD was unfeasible. SEM/EDX analysis revealed the formation of Fe-O compounds, most likely attributed to the oxygen partial pressure in the system induced by CO2 (≥0.985 volume fraction) and volatile H2O. In addition to the surface covering corrosion layer, secondary phases had grown locally distributed on top of the layer. These compounds are characteristic for the applied atmosphere and vary in number, shape and chemical composition.
Carbon Capture Utilization and Storage (CCUS) is a promising technology for the reduction of CO2 emissions, e.g. from fossil-fuel operated power plants or cement mills. Crucial points for a sustainable and future-proof CCUS procedure are reliability and cost efficiency of the pipeline transport network. Due to the absence of certified benchmarks for upper limits, systematic experiments with impurities in the CO2 stream were carried out. For oxidation processes SO2 and NO2 acted as corrosive components, and for reductive atmosphere H2S. Carbon steel L485MB (pipeline), martensitic steel 1.4313 (compression) and austenitic steel 1.4562 (injection) were selected as specimens. Experiments were performed at 0 bar or 100 bar and within a temperature range 278 K ≤ T ≤ 313 K. High-alloyed Cr-Ni steels revealed no corrosion (1.4562, 1.4313), while for carbon steel considerable corrosion was observed. The type and intensity of corrosion was strongly coupled with the applied corrosive species and the level of humidity in the CO2 stream, leading to different compositions of acidic condensates. Applying a reducing atmosphere results in very little corrosion rates, but provokes pitting corrosion. In contrast, oxidizing or mixed settings lead to a clearly increased growth of the corrosion layer, but exhibit shallow uniform corrosion. Exceptional nitric acid results in intergranular corrosion. Investigations on the specimens were carried out by optical microscopy, XRD, SEM/EDX, and AAS/IC.
Integrated Coating System for Corrosion Protection of Carbon Steel in Artificial Geothermal Brine
(2022)
Corrosive geothermal brines are a major challenge to geothermal power-plants. For cost reasons, plant designers prefer to use carbon and low alloyed steels, which are susceptible to uniform and localized corrosion when exposed to geothermal brines having acidic and saline properties. To solve such problem, coatings or inhibitors would be a protective solution as an alternative to the use of high alloyed materials.
This study investigated a coating system consisting of polyaniline/silicon dioxide based on resources locally available in Indonesia. Protection against corrosion of carbon steel was shown by long-term (28 day) exposure and electrochemical tests of coated carbon steels, performed in an artificial acidic and saline geothermal brine, comparable to the conditions encountered at a site in Indonesia.
Therefore, an integrated coating system is proposed for corrosion protection, combining the electrochemical functionality of polyaniline and the physical advantages of silica.
Influence of Precipitating Brine Components on Materials Selection for Geothermal Applications
(2021)
Since geothermal wells are a feasible energy source to replace fossil fuel supply, many technologies have been developed to take advantage of geothermal energy. Nevertheless, service conditions in geothermal facilities are in many cases extreme in terms of corrosion due to the chemical composition of hydrothermal fluids and temperatures. Therefore, materials selection based on preliminary material qualification is essential to guarantee a secure and reliable operation of the facilities. During operation of a geothermal research facility in Groß Schönebeck copper and lead effects have been found downhole. Occurring mechanisms and measures to prevent precipitation or scaling needed to be investigated as well as potential influences of such precipitates on corrosion resistance of metallic materials used for equipment.
This contribution deals with the evaluation of the corrosion behavior of carbon steel and corrosion resistant alloys in copper and/or lead containing artificial geothermal water, simulating the conditions in the Northern German Basin.
The behavior of these materials in an artificial geothermal water obtained by electrochemical measurements and exposure tests are presented. While carbon steel exhibits precipitation and deposition, higher alloyed material shows different response to such species and a higher resistance in saline geothermal water.
Basing on these results the suitability of the investigated corrosion resistant alloy is given for use in such conditions, whereas carbon steel creates difficulties due to its susceptibility to Cu- and Pb-precipitation.
Influence of Precipitating Brine Components on Materials Selection for Geothermal Applications
(2021)
By exposure and electrochemical tests in the laboratory the Cu- and Pb-effect on corrosion behavior and performance of carbon steel and a corrosion resistant alloy could be assessed. Critical material specific properties were determined by static exposure and electrochemical tests in artificial geothermal water with high salinity and low pH, containing Cu/Pb.
It could be shown that significant Cu- resp. Pb-deposition and precipitation only occurred in combination with carbon steel. Corrosion resistant alloys (e. g. Cr- and Ni-dominated stainless steels) prevent the disturbing Cu-agglomeration resp. Pb-deposition. Therefore, they are suitable to be chosen for future design of geothermal piping system, either in massive or in cladded form. Regarding corrosion, formation of crevices with non-metallic materials shall be avoided.
So, in addition to its already known limited corrosion resistance, carbon steel shall not be used when copper or lead species are content of the geothermal brine. Otherwise precipitation and/or deposition of metallic copper resp. lead must be expected, increasing the susceptibility of clogging the piping system.
From the interactions and pitting corrosion point of view, corrosion resistant alloys (preferably Ni-rich) seem to be most favorable when selecting materials for applications in such geothermal brines.
Since geothermal wells are a feasible energy source to replace fossil fuel supply, many technologies have been developed to take advantage of geothermal energy. Nevertheless, service conditions in geothermal facilities are in many cases extreme in terms of corrosion due to the chemical composition of hydrothermal fluids and temperatures. Therefore, materials selection based on preliminary material qualification is essential to guarantee a secure and reliable operation of the facilities. During operation of a geothermal research facility in Groß Schönebeck copper and lead effects have been found downhole. Occurring mechanisms and measures to prevent precipitation or scaling needed to be investigated as well as potential influences of such precipitates on corrosion resistance of metallic materials used for equipment.
This contribution deals with the evaluation of the corrosion behavior of carbon steel and corrosion resistant alloys in copper and/or lead containing artificial geothermal water, simulating the conditions in the Northern German Basin.
The behavior of these materials in an artificial geothermal water obtained by electrochemical measurements and exposure tests are presented. While carbon steel exhibits precipitation and deposition, higher alloyed material shows different response to such species and a higher resistance in saline geothermal water.
Basing on these results the suitability of the investigated corrosion resistant alloy is given for use in such conditions, whereas carbon steel creates difficulties due to its susceptibility to Cu- and Pb-precipitation.
Significant Cu-deposition and precipitation only occurred in combination with carbon steel. High-alloyed materials prevent the disturbing Cu-agglomeration. Pb-deposition and precipitation only occurred in combination with carbon steel. No negative Pb-effect could be observed in combination with high-alloyed steels. High alloyed corrosion resistant alloys are suitable and shall be chosen for future design of the piping system, either in massive or in cladded form, to prevent unwanted interactions with brine components.
Significant Cu-deposition and ‑precipitation only occurred in combination with carbon steel. High-alloyed materials prevent the disturbing Cu-agglomeration. Pb-deposition and ‑precipitation only occurred in combination with carbon steel. No negative Pb-effect could be observed in combination with high-alloyed steels. High alloyed corrosion resistant alloys are suitable and shall be chosen for future design of the piping system, either in massive or in cladded form, if formation of crevices with non-metallic materials can be excluded!
This textbook fulfills its dedication of being the “essential reference for the field, featuring protocols, analysis,fundamentals and the latest advances” of impedance spectroscopy to its readers. It really provides an insight in all facets of this powerful technique.
It should not be missed in the bookshelf of electrochemists and all other interested researchers and engineers who want to be on the current state of this technique.
Recent studies have shown that even at a very low concentration of impurities (less than 100 ppmv of SO2, NO2, O2 and H2O) the droplet formation and condensation of sulfuric and nitric acids in dense phase CO2 are possible and observable. To reveal the mechanism of droplet corrosion in dense phase CO2 at high pressure and low temperature, further studies on factors that affect wettability and resulting corrosion behaviors of transport pipeline steels are needed. In this study, effects of surface morphology were investigated by varying surface roughness of carbon steel coupons exposed to CO2 stream containing impurities to measure the wettability by contact angle and to observe the condensation as well as possible droplet corrosion that followed. Other considered factors were: pH of the droplet, temperature, droplet volume, and exposure time.