Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
Dokumenttyp
Sprache
- Englisch (59)
- Deutsch (24)
- Russisch (2)
- Italienisch (1)
- Mehrsprachig (1)
Referierte Publikation
- nein (87) (entfernen)
Schlagworte
- Laser beam welding (21)
- Solidification cracking (13)
- Hybrid laser arc welding (7)
- Laserstrahlschweißen (6)
- Additive manufacturing (5)
- Hot cracking test (5)
- Laser metal deposition (5)
- Critical strain (4)
- Elektromagnetische Schmelzbadunterstützung (4)
- Laser Metal Deposition (4)
- Laser welding (4)
- Laserhybridschweißen (4)
- Numerical simulation (4)
- Stainless Steel (4)
- Thick-walled steel (4)
- 316L (3)
- Additive Manufacturing (3)
- Electromagnetic weld pool support (3)
- Hybrid Laser Arc Welding (3)
- Hybrid laser-arc welding (3)
- Laser-Pulver-Auftragschweißen (3)
- Mechanical properties (3)
- Ti-6Al-4V (3)
- Weld pool shape (3)
- Additive Fertigung (2)
- CTW-Test (2)
- Charpy impact toughness (2)
- Cryogenic steel (2)
- Defokussierung (2)
- Edge effects (2)
- Endkrater (2)
- Ferromagnetischer Stahl (2)
- Heißrissresistenz (2)
- High power laser beam welding (2)
- Hot cracking (2)
- Hybrid welding (2)
- Inconel 718 (2)
- Laser beam Welding (2)
- Laser hybrid welding (2)
- Laser-Hybridschweißen (2)
- Local critical strain (2)
- Material transport (2)
- Melt pool dinamics (2)
- Microstructure (2)
- Optical flow (2)
- Partial penetration (2)
- Pipe manufacturing (2)
- Pipeline (2)
- Rundnaht (2)
- Single pass welding (2)
- Temperature behavior (2)
- Thermography (2)
- Weld defects (2)
- Weldability (2)
- laser welding (2)
- Überlappbereich (2)
- 3DDruck (1)
- 9%Ni steel, (1)
- Additiv (1)
- Aluminium (1)
- Analytical model (1)
- As-shielded arc welding (1)
- Aufbaustrategie (1)
- Austenitic stainless steels (1)
- Austenitische Stähle (1)
- Build - up Strategy (1)
- Bulging (1)
- Bulging effect (1)
- CFD-model (1)
- CO2 lasers (1)
- CTW test (1)
- Circumferential weld (1)
- Combined laser manufacturing (1)
- Contact element (1)
- Conventional Ni-based austenitic welding electrode (1)
- Corrosion (1)
- Critical strain rate (1)
- Cryogenic Steel (1)
- DIC technique (1)
- Dickblech (1)
- Different welding position (1)
- Digitale Bildkorrelationstechnik (1)
- Direct Laser Metal Deposition (1)
- Duplex (1)
- Duplex AISI 2205 (1)
- Duplex stainless steel (1)
- Duplex stainless steels (1)
- Duplex steels (1)
- Electromagnetic Weld Pool Support (1)
- Electromagnetic backing (1)
- Electromagnetic weld pool support system (1)
- Elektromagnetische Badstütze (1)
- Elektromagnetische Schmelzbadsicherung (1)
- Elektromagnetische Schmelzbadstütze (1)
- Element transport (1)
- End crater (1)
- Externally loaded test (1)
- FE-model (1)
- FEA (1)
- FEM (1)
- Ferritic welding electrode (1)
- Festigkeit (1)
- Filler material distribution (1)
- Fine-grained Steel (1)
- Flow pattern (1)
- Full Penetration (1)
- Gap bridgeability (1)
- Gas shielded arc welding (1)
- Hardness (1)
- Heißriss (1)
- Heißrissanfälligkeit (1)
- High power laser keyhole welding (1)
- High strength steel (1)
- High-power fibre laser (1)
- Hochfester Stahl (1)
- Hochleistungsschweißen (1)
- Hot crack (1)
- Hybrid-laser-arc welding (1)
- Hydrostatic and arc pressure exceed the Laplace pressure (1)
- In situ strain (1)
- Kaltzähe Stähle (1)
- Keyhole mode laser beam welding (1)
- Laser Beam Welding (1)
- Laser Metal Deposition (LMD) (1)
- Laser Metal Deposition; Laser Beam Welding; Duplex; Stainless Steel (1)
- Laser metal deposition (LMD) (1)
- Laser metal fusion (1)
- Laser-Pulver-Auftragschweißen (LPA) (1)
- Laser-Pulver-Auftragschweißen; Laserstrahlschweißen, Duplex, Pufferschichten (1)
- Laser-beam welding, (1)
- Laser-hybrid welding (1)
- Laserpulverauftragschweißen (1)
- Laserstrahl-(Hybrid)schweißen (1)
- Laserstrahl-MSG-Hybridschweißen (1)
- Liquid Metal Embrittlement (1)
- Lokale Effekte (1)
- Longitudinal weld (1)
- Low Temperature Toughness (1)
- Lötrissigkeit (1)
- MSG-Schweißen (1)
- Macro Processing (Joining, Welding) (1)
- Magnetic bath support (1)
- Magnetohydrodynamics (1)
- Magnettechnik (1)
- Manganese (1)
- Mechanical Properties (1)
- Misalignment of edges (1)
- Modellierung (1)
- Modified spray arc (1)
- Multi - physical modeling (1)
- Nickel (1)
- Nickel-based superalloy (1)
- Novel metrology (1)
- Novel optical measurement (1)
- Novel optical metrology (1)
- Numerical modelling (1)
- Numerical process simulation (1)
- Optical measurement (1)
- Optical measurement technique (1)
- Optical measurment technique (1)
- Optische Emissionsspektroskopie (OES) (1)
- Pendelstrategie (1)
- Penetration depth (1)
- Pipeline steel X120 (1)
- Plasma-cut samples (1)
- Preheating (1)
- ProMoAM (1)
- Process chain (1)
- Pufferschichten (1)
- Rissanfälligkeit (1)
- Rissbildung (1)
- SEP-1220-3 (1)
- SMAW (1)
- Schallemissionsanalyse (SEA) (1)
- Schweißeignung (1)
- Schweißen von kaltzähen Stählen (1)
- Schweißunregelmäßigkeiten (1)
- Self-restraint test (1)
- Shielding gases (1)
- Ship building (1)
- Single-pass welding (1)
- Solidification behaviour (1)
- Solidification craking (1)
- Spiralstrategie (1)
- Stainless steel (1)
- Strain measurement (1)
- Strain rate (1)
- Superelliptic Lamé curves (1)
- Temperaturentwicklung (1)
- Tensile strength (1)
- Thermal cycles (1)
- Thermo-fluid flow (1)
- Thermographie (1)
- Thick Materials (1)
- Thick plate welding (1)
- Thick plates (1)
- Thick-plate welding (1)
- Thick-walled Structures (1)
- Ti - 6Al - 4V (1)
- Turbine blade (1)
- Turbine industry (1)
- Untersuchung laserstrahlgeschweißter Verbindungen (1)
- V-notch impact toughness (1)
- Vakuum (1)
- Weld imperfections (1)
- Weld pool (1)
- Weld pool geometry (1)
- Weld pool shape approximation (1)
- Welding thermal cycle (1)
- Werkstofffragen (1)
- Werkstoffranking (1)
- Widerstandspressschweißen (1)
- Widerstandspunktschweißen (1)
- Windkraftanlagen (1)
- X8Ni9 (1)
- YAG lasers (1)
- cryogenic steel (1)
- hardness (1)
- hochfeste Stähle (1)
- laser hybrid welding (1)
- local effects (1)
- microstructure (1)
- tensile strength (1)
- thermal cycles (1)
- thick plate welding (1)
- vacuum (1)
- Ökonomische und ökologische Vorteile (1)
Organisationseinheit der BAM
- 9 Komponentensicherheit (57)
- 9.3 Schweißtechnische Fertigungsverfahren (55)
- 8 Zerstörungsfreie Prüfung (2)
- 8.0 Abteilungsleitung und andere (2)
- 9.0 Abteilungsleitung und andere (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.9 Chemische und optische Sensorik (1)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (1)
Eingeladener Vortrag
- nein (11)
The weld quality and the possible defect formation are directly determined by the weld pool shape and the thermo-fluid dynamics therein. In this paper, an untypical weld pool profile, i.e., elongated at its top and bottom but narrowed at the middle, is found experimentally and numerically in the wire feed laser beam welding. The detrimental influence of the weld pool narrowing on the element transport is analyzed and discussed. A magnetohydrodynamic technique is utilized to suppress the narrowing, aiming at a more homogenous element distribution. It is found that a low-temperature region is formed in the middle of the weld pool due to the interaction of the two dominant circulations from the top and bottom regions. The weld pool is significantly narrowed due to the untypical growth of the mushy zone in the low-temperature region, which results in a direct blocking effect on the downward flow and the premature solidification in the middle region. The Lorentz force produced by a transverse oscillating magnetic field shows the potential to change the flow pattern into a single-circulation type and the low-temperature-gradient region is mitigated.
Therefore, the downward transfer channel is widened, and its premature solidification is prevented. The numerical results are well validated by experimental measurements of metal/glass observation and X-ray fluorescence element mapping.
The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high-speed camera, and two thermal imaging cameras is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs above 10 mm penetration depth. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root.
New developments in nickel-based superalloys and production methods, such as the use of additive manufacturing (AM), can result in innovative designs for turbines. It is crucial to understand how the material behaves during the AM process to advance industrial use of these techniques. An analytical model based on reaction-diffusion formalism is developed to better explain the solidification behavior of the material during laser metal deposition (LMD). The well-known Scheil-Gulliver theory has some drawbacks, such as the assumption of equilibrium at the solid-liquid interface, which is addressed by this method. The solidified fractions under the Scheil model and the pure equilibrium model are calculated using CALPHAD simulations. Differential scanning calorimeter is used to measure the heat flow during the solid-liquid phase transformation, the result of which is further converted to solidified fractions. The analytical model is compared with all the other models for validation.
Solidification cracking is still a serious problem in laser beam welding, especially in the welding of thick-walled plates. The influence of weld pool geometry on solidification cracking in partial penetration welding of thick plates is investigated within scope of this study. Therefore, a specific experimental setup of steel and quartz glass in butt configuration and on the side with high-speed camera were used to record the weld pool shape. In addition, the influence of laser inclination angle on the weld pool geometry and on solidification crack formation was investigated. The results show a bulge in the weld pool root, which is separated from an upper region by a necking region. This leads to a case where there are three different longitudinal region lengths with different solidification zones. This temporal sequence of solidification strongly promotes the formation of solidification cracks in the weld root.
Diese Arbeit zeigt erstmals die Anwendung einer elektromagnetischen Schmelzbadsicherung beim einlagigen MSG-Schweißen von dickwandigen Stählen. Die innovativen Entwicklungen im Bereich des Lichtbogenschweißverfahrens ermöglichen eine Erhöhung der Abschmelzleistung, um die Einschweißtiefe zu steigern. Somit kann die Lagenanzahl reduziert und die Produktivität gesteigert werden. Allerdings besteht insbesondere beim einlagigen Schweißen von dickwandigen Bauteilen in PA-Position ein erhöhtes Risiko für das gravitationsbedingte Austropfen der Schmelze an der Wurzel. Zur Verhinderung werden Badsicherungen eingesetzt, die mechanisch angebracht und nach dem Schweißen entfernt werden müssen, was zeit- und kostenintensiv ist.
Die im Rahmen dieser Studie eingesetzte elektromagnetische Schmelzbadsicherung wirkt dem gravitationsbedingten Austropfen der Schmelze entgegen und kompensiert den hydrostatischen Druck. Sie wirkt kontaktlos, was im Gegensatz zu herkömmlichen Badsicherungen vorteilhaft ist, so dass auf eine zeit- und kostenintensive Nachbearbeitung der Schweißnahtwurzel verzichtet werden kann. Das auf extern angelegten oszillierenden Magnetfeldern beruhende Verfahren wird dabei unterhalb des zu schweißenden Bauteils positioniert. Die Magnetfeldlinien sind quer zur Schweißrichtung ausgerichtet, sodass längs zur Schweißrichtung Wirbelströme im Werkstück und eine stets nach oben gerichtete Lorentzkraft generiert werden. Mit Hilfe der elektromagnetischen Badsicherung konnten beim einlagigen MSG-Schweißen von bis zu 10 mm dicken Blechen die Tropfenbildung vermieden werden. Die innovative Technologie ermöglicht es, dickwandige Bauteile einlagig zu schweißen und reduziert die Nachbearbeitungszeiten und -kosten deutlich.
Laserstrahlhybridschweissen von Türmen für Windkraftanlagen Ökonomische und ökologische Vorteile
(2022)
Das Laserstrahlhybridschweißen ist beim Schweißen von Türmen für Windkraftanlagen eine Alternative zum Unterpulverschweißen von Dickblechen in Mehrlagentechnik und bietet hier ökonomische und ökologische Vorteile. Der industrielle Einsatz des Verfahrens ist jedoch durch prozessspezifische Herausforderungen eingeschränkt. Die im Beitrag beschriebene kontaktlose elektromagnetische Badstütze dient zur Erweiterung des Verfahrenspotenzials im Dickblechbereich >15 mm.
With additive manufacturing in the powder bed, the component size is limited by the installation space. Joint welding of additively manufactured parts offers a possibility to remove this size limitation. However, due to the specific stress and microstructure state in the additively built material, it is unclear to what extent existing evaluation rules of joint welding are also suitable for welds on additive components. This is investigated using laser beam welding of additively manufactured pipe joints. The welds are evaluated by means of visual inspection, metallographic examinations as well as computed tomography. The types of defects found are comparable to conventional components. This is an indicator that existing evaluation regulations also map the possible defects occurring for weld seams on additive components.
Die technischen Entwicklungen in der Lasertechnologie in den letzten Jahrzehnten haben eine neue Generation von Hochleistungslasersystemen im Leistungsbereich bis zu 100 kW auf den Markt gebracht. Dennoch ist die industrielle Anwendung des Hochleistungslaserstrahlschweißens auf bis zu 15 mm dicke Bleche beschränkt. Mögliche Ursachen der Einschränkungen des Verfahrens sind z.B. die Sensibilität des Verfahrens auf Fertigungstoleranzen wie Spalt und Kantenversatz, die erhöhte Tropfenbildung bei höheren Blechdicken und eine inhomogene Verteilung des Zusatzwerkstoffes beim Laserhybridschweißen. In dieser Studie wird ein auf extern angelegte Magnetfelder basierte elektromagnetische Schmelzbadstütze eingesetzt, um die Grenzen des Verfahrens zu erweitern und die Herausforderungen zu minimieren. Der wesentliche Vorteil der elektromagnetischen Schmelzbadstütze ist, dass sie berührungslos arbeitet. Mit Hilfe der elektromagnetischen Schmelzbadstütze konnten bei 20 mm dicken Proben aus S355J2 die Tropfenbildung an der Wurzel vermieden werden. Zudem wurde der Einfluss der Kantenqualität auf die Schweißnahtqualität untersucht, wobei verschiedene Schneidverfahren zur Kantenvorbereitung eingesetzt wurden, wie z.B. Plasma-, Brenn- oder Laserschneiden. Es konnte gezeigt werden, dass auch bei schlechteren Kantenvorbereitung im Gegensatz zu gefrästen Bauteilen die Werkstoffe einlagig mittels Laserhybridschweißen bei einer hohen Schweißnahtqualität gefügt werden konnten. Bei plasmageschnittenen Proben wurden zudem eine Spaltüberbrückbarkeit bzw. Kantenversatz von bis zu 2 mm sicher überbrückt. Des Weiteren war es mit Hilfe der externen Magnetfelder möglich, die Durchmischung des Zusatzwerkstoffes über die gesamte Schweißnahttiefe deutlich zu homogenisieren.
The study deals with the influence of the heat input and the resulting cooling times on the microstructure and Charpy impact toughness of single-pass laser hybrid welded 20-mm thick high-strength steel S690QL. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured in-situ using a pyrometer and an optical fibre in three different depths of the seam where Charpy impact test specimens were also later taken. Thereby, three different heat inputs from 1.3 kJ/mm to 2 kJ/mm were investigated. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required impact toughness of 38 J/cm2 could be reached in dependance on applied heat input, especially at the heat input of 1.6 kJ/mm.
Laser metal deposition (LMD) as an additive manufacturing technique became increasingly important in recent years and thus the demand for component safety. This is the reason, for the need for reliable in-situ defect detection techniques. For laser beam weld seams an optical measurement technique based on an optical flow algorithm was successfully used to define the critical straining conditions that lead to hot cracking. This algorithm was adapted for bead-on-plate weld seams on LMD deposited layers of IN718 alloy while performing external strain on the specimen in an externally loaded hot cacking test facility. The resulting transversal hot cracks along the weld seam were localized via X-Ray inspection and the type of cracking confirmed by Scanning Electron Microscopy (SEM). The strain distribution was measured in the vicinity of the solidification front and correlated to the detected hot cracks. Based on the results this technique could be adopted for LMD experiments.
Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength and good ductility it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. In this study different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition are investigated. Afterwards laser tracks are welded, and the temperature cycles measured. The ferrite content of the tracks are analyzed by feritscope, metallographic analysis and Electron Backscatter Diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where firstly the edges of the weld partners are coated with the powder mixture by LMD and secondly those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy dispersive X-ray spectroscopy and Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material.
This paper presents investigation results of a process for defect-free hybrid laser arc welding (HLAW) of closed circumferential welds. The process aims to avoid weld imperfections in the overlap area of a HLAW circumferential weld. A process control strategy for closing the circumferential weld was developed to achieve a defect-free overlap region by controlling the solidification conditions at the end of the weld. The controlled heat flow is achieved by adjusting the parameters of both welding processes involved, the laser beam as well as gas metal arc welding (GMAW) process. Experimental investigations were carried out on 12 mm to 15 mm thick tube sections. The influence of process parameters such as the laser ramp time, the change in magnification scale and the defocusing of the laser beam on the solidifi-cation conditions at the end of the circumferential weld was investigated to find an optimum strategy for ramping out the process energy. Within the framework of the experimental studies, it was demonstrated that defocusing the laser beam in the range between 60 mm and 100 mm over a short run-out area of the weld of approximately 15 mm led to a significantly better weld formation in the overlap area. A favourable cup-shaped weld shape could be achieved without a tendency to crack. The laser optics with a motor-driven lens system made it possible to increase the laser beam diameter without changing the position of the GMAW arc relative to the component surface.
The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a wall thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a high-speed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a greater influence on the melt pool dynamics and the mixing of the elements of the filler wire. The high-speed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets
Vor allem in den letzten Jahren ist das Interesse der Industrie an der additiven Fertigung deutlich gestiegen. Die Vorteile dieser Verfahren sind zahlreich und ermöglichen eine ressourcenschonende, kundenorientierte Fertigung von Bauteilen, welche zur stetigen Entwicklung neue Anwendungsbereiche und Werkstoffe führen. Aufgrund der steigenden Anwendungsfälle, nimmt auch der Wunsch nach Betriebssicherheit unabhängig von anschließenden kostenintensiven zerstörenden und zerstörungsfreien Prüfverfahren zu. Zu diesem Zweck werden im Rahmen des von der BAM durchgeführten Themenfeldprojektes „Prozessmonitoring in Additive Manufacturing“ verschiedenste Verfahren auf ihre Tauglichkeit für den in-situ Einsatz bei der Prozessüberwachung in der additiven Fertigung untersucht. Hier werden drei dieser in-situ Verfahren, die Thermografie, die optische Emissionsspektroskopie und die Schallmissionsanalyse für den Einsatz beim Laser-Pulver-Auftragschweißen betrachtet.
The study deals with the influence of the heat input on the thermal cycles and Charpy impact toughness for hybrid laser-arc welding of 25 mm thick structural steel S355J2 using a 20-kW high-power laser in combination with an electromagnetic weld pool support. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured using a pyrometer in combination with an optical fibre in three different locations near to fusion lines corresponding to different heights of the seam. Also, Charpy impact specimens were taken from different parts of the weld joint corresponding to the different heights. The influence of the heat input was investigated for 1.8 kJ mm-1 and 3.2 kJ mm-1. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required values could be reached in dependance on applied heat input.
One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds.
In this study, steel-glass experiments were conducted to observe the melt pool geometry using a high-speed camera. The high-speed recordings and optical flow analysis show that two main flows take place in form of vortices. The lower vortex drives the melt backwards from the front keyhole wall and thus causes an extension of the melt pool, which is called bulging. This bulging promotes solidification cracking by forming a closed area filled with melt and the accumulation of impurities in the final solidification phase, resulting in low-melting phases which are under tensile stress at the end of solidification.
The use of the oscillating magnetic field as a backing support for the welding of thick components is already known. The influence of the magnetic field and the induced Lorentz forces in the melt on the melt pool geometry and the fluid flows is not yet fully investigated. The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser hybrid welding process. An AC magnet was positioned under the specimen to create an electromagnetic force directed upwards to oppose dropping. To visualise the flow characteristics of the melt, several experiments were carried out using a technique specifically designed for this purpose with mild steel made of S355J2 with a wall thickness of 20 mm and a quartz glass in a butt configuration. A high-speed camera was used to monitor the geometry of the melt pool through the glass. The influence of the magnetic field orientation to the welding direction and the oscillation frequency on the molten pool was investigated for the case of the metal-glass configuration and for laser hybrid welding. The high-speed recordings were analysed with the Optical Flow Algorithm to characterise the flow within the melt pool. The element distribution over the whole seam thickness was evaluated by X-ray fluorescence (XRF). The high-speed analysis showed that in the melt pool two vortices are formed, one in the upper part and the other in the lower part. In the region where the two vortices come together, a narrow region (necking region) forms in the melt pool. The evaluation of the high-speed recordings shows that the depth of the region where the two vortices meet is strongly influenced by the oscillation frequency. Additionally, the oscillation frequency demonstrated a greater influence on the melt pool dynamics and the mixing of the elements of the filler wire.
One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds.
Because of its excellent corrosion resistance, high tensile strength and
high ductility, duplex stainless steel 2205 offers many areas of application. Though laser beam welding accompanied by high cooling rates, duplex steels tend to perform higher ferrite contents in weld metal as the base metal, which leads to a reduction of ductility and corrosion resistance of the weld joint. To overcome this problem, a solution, based on buttering the plate edges by laser metal deposition (LMD) with material containing higher Ni concentrations prior to laser welding was suggested.
In this context different process parameters for LMD and different mixtures of duplex and nickel powder, were investigated. In a second step the possibility of welding those edges defect free while achieving balanced austenite-ferrite ratio was verified with metallographic analysis, Electron Backscatter Diffraction (EBSD) and impact testing according to Charpy. The improved corrosion resistance was observed with ASTM G48 standard test method.
Laserstrahlschweißen additiv gefertigter Bauteile: Einsetzbarkeit bestehender Bewertungsvorschriften
(2021)
Bei der additiven Fertigung im Pulverbett ist die Bauteilgröße durch den Bauraum begrenzt. Das Verbindungsschweißen additiv gefertigter Teile bietet eine Möglichkeit diese Größenbegrenzung aufzuheben. Aufgrund des spezifischen Spannungs- und Gefügezustands im additiv aufgebauten Teil ist jedoch unklar, inwiefern bestehende Bewertungsvorschriften des Verbindungsschweißens auch für Schweißnähte an additiv gefertigten Bauteilen geeignet sind. Dies wird anhand des Laserstrahlschweißens additiv gefertigter Rohrverbindungen untersucht. Die Schweißnähte werden mittels visueller Prüfung, metallografischer Untersuchungen sowie Computertomografie ausgewertet. Die festgestellten Fehlerarten sind vergleichbar zu konventionellen Bauteilen. Dies ist ein Indikator dafür, dass bestehende Bewertungsvorschriften die möglichen auftretenden Defekte auch für Schweißnähte an additiven Bauteilen abbilden.
In diesem Beitrag werden Ergebnisse der Untersuchungen eines Verfahrens zum fehlerfreien Laserstrahl-MSG-Hybridschweißen von geschlossenen Rundnähten vorgestellt. Das Verfahren zielt auf die Vermeidung von Schweißnahtunregelmäßigkeiten im Überlappbereich einer hybridgeschweißten Rundnaht. Eine Strategie der Prozessführung beim Schließen der Rundnaht wurde entwickelt, mit der ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl sowie dem Metallschutzgas (MSG)-Schweißprozess, realisiert. Experimentelle Untersuchungen wurden an 12 bis 15 mm dicken Rohrabschnitten durchgeführt. Der Einfluss von Prozessparametern wie der Veränderung des Abbildungsmaßstabs und der Defokussierung des Laserstrahls auf die Erstarrungsbedingungen am Ende der Rundnaht wurde untersucht, um eine optimale Strategie zum Herausführen der Prozessenergie zu finden.
Im Rahmen der experimentellen Untersuchungen konnte gezeigt werden, dass eine Defokussierung des Laserstrahls im Bereich zwischen 60 mm und 100 mm über einen kurzen Auslaufbereich der Naht von etwa 15 mm zu einer deutlich besseren Nahtausbildung im Überlappbereich führt. Es konnte eine günstige kelchförmige Schweißnaht ohne eine Tendenz zur Rissbildung erzielt werden. Die Laseroptik mit motorisch angesteuertem Linsensystem ermöglichte dabei eine Vergrößerung des Laserstrahldurchmessers ohne eine Veränderung der Position des MSG-Lichtbogens relativ zur Bauteiloberfläche.
Bislang kommt das Laserstrahlschweißen bzw. Laserhybridschweißen hauptsächlich bei Dickblechen mit einer Wandstärke von bis zu 15 mm zum Einsatz. Für Anwendungen über 20 mm war dieses Verfahren aufgrund einiger Herausforderungen bisher nur bedingt realisierbar. Eine von der Bundesanstalt für Materialforschung und -prüfung (BAM) entwickelte elektromagnetische Schmelzbadunterstützung ermöglicht nun ein einlagiges Schweißen von bis zu 30 mm Wandstärke.
The study deals with the application of the high-power hybrid-laser arc welding process on up to 15 mm thick pipe segments with the intention to avoid end crater imperfections during closing of the circumferential welds, where the pipes were turned during welding in 1G- and 2Gpositions.
Different techniques such as laser power ramp-down, abrupt switch-off of the laser power and change of the magnification of the laser spot diameter and defocusing of the laser beam relative to the workpiece were tested to remove the laser energy from the process. It could be shown that a high defocusing of the optic system above 40 mm with a resulting beam diameter > 2.9 mm in a short overlap length of approx.
20 mm leads to the formation of a cup-shaped weld seam, which is preferred for avoidance of cracks and pores in the end crater. A laser optics with motor-driven lens system was used for the welding experiments to defocuse the laser beam without changing the position of the arc.
Notch impact toughness of laser beam welded thick sheets of cryogenic nickel alloyed steel X8Ni9
(2020)
The paper deals with the investigations of the impact toughness of laser beam welded 14.5 mm thick sheets made of cryogenic steel X8Ni9 as a function of preheating. This 9% nickel alloyed steel is widely used in the liquefied natural gas (LNG) industry. An application of highly efficient welding processes such as high-power laser beam welding (LBW) in LNG sector requires an understanding of the interactions between the LBW process parameters and weld properties, in particular the impact toughness. The results show that the original fine-grained martensitic microstructure of the base metal (BM) is significantly changed by melting and crystallization during the LBW, what can lead to a decrease in the impact toughness of the weld metal (WM) below the required level. An optimal preheating temperature range leads to the favorable thermal welding cycle and is of remarkable importance for maintaining the notch impact toughness of laser beam welded joints of these thick steel sheets. A parameter window was identified in which V-notch impact toughness comparable to that of the BM at -196 °C was achieved.
In diesem Beitrag werden Ergebnisse der Untersuchungen eines Verfahrens zum fehlerfreien Laserstrahl Hybridschweißen von geschlossenen Rundnähten vorgestellt. Das Verfahren zielt auf die Vermeidung von Schweißimperfektionen im Überlappbereich einer laserstrahlhybridgeschweißten Rundnaht. Eine Strategie der Prozessführung beim Schließen der Rundnaht wurde entwickelt, mit der ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG Schweißprozess realisiert. Experimentelle Untersuchungen wurden an 12 mm bis 15 mm dicken Rohrabschnitten durchgeführt. Der Einfluss von Prozessparametern wie der Laserleistungsrampe und Rampenzeit, der Veränderung des Abbildungsmaßstabes und der Defokussierung des Laserstrahls auf die Erstarrungsbedingungen am Ende der Rundnaht wurde untersucht, um eine optimale Strategie zum Herausführen der Prozessenergie zu finden. Im Rahmen der experimentellen Untersuchungen konnte gezeigt werden, dass eine Defokussierung des Laserstrahls im Bereich zwischen 60 mm und 100 mm über einen kurzen Auslaufbereich der Naht von ca. 15 mm zu einer deutlich besseren Nahtausbildung im Überlappbereich führte. Es konnte eine günstige kelchförmige Schweißnahtform ohne eine Tendenz zur Rissbildung erzielt werden. Die Laseroptik mit motorisch angesteuertem Linsensystem ermöglichte dabei eine Vergrößerung des Laserstrahldurchmessers ohne eine Veränderung der Position des MSG-Lichtbogens relativ zur Bauteiloberfläche.
Additive Fertigungsverfahren gewinnen aufgrund der schnellen, flexiblen und kosten-günstigen Fertigung von Bauteilen zunehmend an Bedeutung. Das Laserpulverauf-tragschweißen (LPA) wurde anfangs hauptsächlich als Beschichtungsverfahren ein-gesetzt. Diese Technologie bewerkstelligt aber auch das Reparieren von verschlisse-nen Bauteilen, sodass diese zeitsparend und ressourcenschonend erneuert werden können. Die hohe Aufbaurate, die flexible Pulverzusammensetzung sowie die hohe Endkonturnähe ermöglichen heutzutage die Entwicklung und additive Fertigung von neuen Materialien, wie zum Beispiel Nickel-Titan-Formgedächtnislegierungen.
A self-restraint hot cracking test (free edge test) was used in combination with a novel optical measurement technique to determine the critical straining conditions for solidification cracking for the stainless steel grade 1.4828 (AISI 309). The Lucas-Kanade algorithm for the optical flow (OF) calculation was implemented to obtain the full-field displacement and then the full-field strain.
The use of external laser illumination with appropriate filters allows to obtain good image quality with good contrast. The critical straining conditions required for solidification cracking can be obtained by means the proposed technique in the immediate vicinity of the solidification front. A very good repeatability was demonstrated for the used measurement technique. The critical straining conditions for solidification cracking for the tested steel und under this welding conditions has been detected
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.
High power laser beam welding has been already introduced in ship building industry since last two decades and is characterized by higher performance as conventional arc welding technologies through its higher welding speed, penetration depth and therefore higher productivity. Moreover, high quality weld joints are achievable thanks to a stronger automatization degree and better repeatability of the process. A further advantage of the laser beam welding is a manufacturing of parts with very low distortion according to much lower heat input, so that rework amount can be reduced significantly. Nevertheless, there are still some unresolved problems limiting the range of application of the technology in part manufacturing within ship building industry, restricted by development and application of new materials or new design of ship vessels.
The present contribution deals with some novel aspects of laser beam welding technology allowing to widen this range significantly. One of the possibilities is to increase the weld seam thickness for single pass laser or laser-hybrid welding is to apply contactless EM-support system based on generation of the Lorentz force counteracting the liquid metal drop out. Also, application of laser-hybrid welding technology for welding novel materials like cold resistant steel X8Ni9 used for construction of LNG tanks brings technological and design advantages comparing to conventional welding technologies by using of a similar alloyed filler wire instead of expensive Ni-based filler material. Finally, it is shown how the application of computational techniques can be used to helps to improve the quality of laser welded joints and avoid the critical weld failure by optimization of the welding process parameters.
Duplexstähle finden in vielen industriellen Bereichen Anwendung, dies ist nicht zuletzt ihren hervorragenden Eigenschaften, wie einer guten Korrosionsbeständigkeit, einer guten Duktilität bei trotzdem hoher Festigkeit, zuzuschreiben. Diese Eigenschaften werden jedoch durch das Schweißen, vor allem das Laserstrahlschweißen, beeinträchtigt, da die hohen Abkühlraten zu erhöhten Ferritanteilen im Schweißgut führen. Mit Hilfe eines zweistufigen Prozesses, bei dem die Kanten der Fügepartner vor dem Schweißen mit nickelhaltigem Pulver beschichtet werden, soll dieses Problem für dickwandige Bleche gelöst werden.
In diesem Zusammenhang wurden verschiedene Prozessparameter für den Laser-Pulver-Auftragschweiß-Prozess untersucht sowie die defektfreie Schweißung dieser beschichteten Kanten mit unterschiedlichen Prozessgasen.
Duplexstähle finden aufgrund ihrer Eigenschaften, wie der guten Korrosionsbeständigkeit, einer hohen Festigkeit bei gleichzeitig guter Duktilität häufig industrielle Anwendung. Durch die hohen Abkühlraten beim Laserstrahlschweißen weisen Schweißnähte jedoch anstelle eines ausgeglichenen Duplexgefüges einen deutlich erhöhten Ferritanteil, im Vergleich zum Basiswerkstoff, auf. Dies führt zu einer verringerten Duktilität sowie Korrosionsbeständigkeit. Um dieses Problem zu lösen, wurde ein Prozess entwickelt, der auf einer Kantenbeschichtung mit nickelhaltigem Zusatzmaterial der zu fügenden Bleche mittels Laser-Pulver-Auftragschweißen (LPA) basiert.
Die resultierenden Schweißnähte wurden zerstörend anhand von Schliffbildern, EDX-Aufnahmen, Härtemessungen und Kerbschlagbiegeversuchen geprüft.
Because of its excellent corrosion resistance, high tensile strength and high ductility, duplex stainless steel 2205 offers many areas of application. Though laser beam welding accompanied by high cooling rates, duplex steels tend to perform higher ferrite contents in weld metal as the base metal, which leads to a reduction of ductility and corrosion resistance of the weld joint. To overcome this problem, a solution, based on buttering the plate edges by laser metal deposition (LMD) with material containing higher Ni concentrations prior to laser welding was suggested.
In this context different process parameters for LMD process were investigated. In a second step the possibility of welding those edges defect free while achieving balanced austenite-ferrite ratio was verified with metallographic analysis, Electron Backscatter Diffraction (EBSD) and impact testing according to Charpy.
A novel approach for the reconstruction of an equivalent volumetric heat source from a known weld pool shape is proposed. It is based on previously obtained weld pool geometries from a steady-state thermo-fluid dynamics simulation. Hereby the weld pool dimensions are obtained under consideration of the most crucial physical phenomena, such as phase transformations, thermo-capillary convection, natural convection and temperature-dependent material properties. The algorithm provides a time and calibration efficient way for the reproduction of the weld pool shape by local Lamé curves. By adjusting their parameters, the identification of the finite elements located within the weld pool is enabled. The heat input due to the equivalent heat source is assured by replacing the detected nodes’ temperature by the melting temperature.
The model offers variable parameters making it flexible and adaptable for a wide range of workpiece thicknesses and materials and allows for the investigation of transient thermal effects, e.g. the cooling stage of the workpiece. The calculation times remain acceptably short especially when compared to a fully coupled process simulation. The computational results are in good agreement with performed complete-penetration laser beam welding experiments.
With global increases in clean energy demand, the natural gas is gaining in importance. Pipelines are the safest and most cost-effective way of transporting natural gas. Due to high transport volume and resulting high operation pressure, the demand for ultra-high strength steel grades such as X120 is very strong. As a result of the fact that these steels are produced by thermo-mechanical controlled processing, the welding process must be selected accordingly. Based on investigations, a high heat input such as by submerged arc welding process leads to softening in the weld metal and loss of strength whereas pure laser beam welding results in high cooling rates and deteriorate toughness of the weld metal. The objective of this research is to investigate the influence of heat input to mechanical properties of hybrid laser-arc welded pipeline steels of grade X120. Test specimens with a thickness of 20 mm could be welded without preheating in a single-pass with different welding velocities to observe the largest possible parameter window of the heat input. The achieved V-notch impact energy for hybrid laser-arc welded samples was 144±37 J at a testing temperature of -40 °C. With a tensile strength of 930±4 MPa the requirements of API 5L was achieved. To prevent gravity drop-outs at the slow welding speeds, an electromagnetic weld pool support system was used, which works contactless and is based on generating Lorentz forces. It was therefore possible to control the cooling rate in order to meet the requirements of the mechanical properties. By adapting the electromagnetic weld pool support to the laser and laser hybrid welding process, the application potential of these technologies for industrial implementation can be drastically increased.
Vermeidung von Schweißimperfektionen im Überlappbereich bei laserstrahlhybridgeschweißten Rundnähten
(2019)
Die Laserstrahl-Hybrid-Schweißtechnologie erweist sich in der schweißtechnischen Fertigung immer mehr als innovative Alternative gegenüber anderen Schweißverfahren. Obwohl das Laserstrahl-Hybridschweißverfahren viele wirtschaftliche Vorteile gegenüber herkömmlichen Schweißverfahren aufweist, wie z.B. große Einschweißtiefe und dadurch eine reduzierte Anzahl von Schweißlagen, geringe thermische Belastung des Grundwerkstoffes aufgrund reduziertem Wärmeeintrag, konnte das Schweißverfahren überwiegend für das Schweißen von Längsnähten demonstriert werden. Eine Vielzahl von Schweißaufgaben, z.B. beim Schweißen von Segmenten von Windkraftanlagen oder dem Orbitalschweißen beim Verlegen von Großrohrleitungen sieht vor, dass die zu schweißenden Bauteile mit einer Rundnaht zusammengefügt werden. Die schweißtechnische Herausforderung ist hier, dass beim Schließen einer Rundnaht mit der Entstehung eines fehlerbehafteten Überlappbereiches zu rechnen ist. Ein zentrales Problem im Überlappbereich einer laserstrahl- sowie laserhybridgeschweißten Rundnaht ist die Bildung von Imperfektionen wie Poren, Rissen sowie die Bildung eines Endkraters, welcher als geometrische Kerbe wirkt. Bisher liegen keine universellen Lösungen zur fehlerfreien Ausführung von geschlossenen Rundnähten beim Laserstrahl-Hybridschweißen vor. Diese Studie befasst sich mit der Entwicklung eines Verfahrens, mit dem die Entstehung von o.g. Schweißimperfektionen vermieden wird. Die Strategie der Prozessführung beim Schließen der Rundnaht sieht hervor, dass ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht werden kann. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG-Schweißprozess realisiert.
Im Rahmen dieser Arbeit wurde eine Serie von Schweißversuchen an 9,5 mm dicken Rohabschnitten aus hochfestem Pipelinestahl X100Q mit Variation der Prozessparameter wie der Laserleistung, der Defokussierung des Laserstrahls sowie der Endkraterfüllzeit im Überlappbereich der Rundnaht durchgeführt. Nachfolgend werden die erzielten Ergebnisse dargestellt und diskutiert.
Results of experimental investigations of the relationship between laser-hybrid welding process parameters, type of the filler metal and the mechanical properties of the welds made from 9% nickel cryogenic steel X8Ni9 are discussed. The results contribute to the development and conversion in the industrial practice a new laser beam-based welding technology for the automated manufacturing of LNG tanks. The remarkable heterogeneity in the chemical composition of the weld metal as well as an insufficient impact toughness could be indicated by using austenitic filler wire. The most promising results were achieved by applying 11%Ni filler wire, which is similar to the base material. A correlation between impact toughness and wire feeding speed could be shown. The highest impact toughness was 134 J at -196°C. The laser-hybrid welds passed the tensile test. The failure stress of 720 MPa with a fracture location in the base metal was achieved for all samples tested.
Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support
(2019)
Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
The presented study deals with the performing and mechanical testing of single pass hybrid laser-arc welds (HLAW) on 25 mm thick plates made of steel grade S355J2. One of the challenges have to be solved at full penetration HLAW of thick plates is the drop formation occurring due to the disbalances of the forces acting in the keyhole and on the melt pool surface. Such irregularities mostly limit the use of high-power laser beam welding or HLAW of thick-walled constructions. To overcome this problem, an innovative concept of melt pool support based on generating Lorentz forces in the weld pool is used in this work. This method allows to perform high quality welds without sagging even for welding of 25 mm thick plates in flat position at a welding speed of 0.9 m min-1. For the obtain of full penetrated welds a laser beam power of 19 kW was needed. A high V-impact energy of up to 160 J could be achieved at the test temperature of 0 °C. Even at the most critical part in the weld root an impact energy of 60 J in average could be reached. The tensile strength of the weld reaches that of the base material. An introduce of the HLAW process with electromagnetic support of the melt pool in the industrial practice is an efficient alternative to the time- and cost-intensive arc-based multi-layer welding techniques which are established nowadays for joining of thick-walled constructions.
In this study, the influence of the welding speed and the arc power on the solidification crack formation for partial penetration laser hybrid welded Thick-Walled plates were investigated. Experimentally, a linear correlation between the welding velocity and the crack number was observed. That is by reducing the welding velocity the crack number was reduced.
The reduced welding velocity showed a strong impact on stress, as the model demonstrated a very lower stress amount in comparison to the reference case. The reduction of the welding speed could be a helpful technique to reduce the hot cracking. The wire feed speed showed a very slight influence on the crack formation. That can be returned to the large distance between the critical region for cracking and the arc region.
The shape of the parts, created by the technology of direct laser metal deposition (DLMD), is influenced by various parameters, for example, the power and diameter of the laser source spot. The contribution of energy from the laser affects the temperature distribution in the formed layers. The changing temperature in the working area entails a Change in the geometry of the layers and affects the stability of the process. In this paper, experiments on the measurement of temperature cycles in the DLMD process with different directions of the filling track are carried out. An infrared camera was used to measure thermal cycles. The calibration of the acquired data (i.e. correspondence table between the intensity of thermal radiation of the material and the absolute temperature) was done with help of two-color pyrometer ex situ and in situ measurements. The experiments are carried out on two materials 316L and Inconel 718. The effect of the maximum temperature on the layer height is shown, and thermal cycles in the formation of layers for different filling strategies are presented.
Laserhybridschweißen von dickwandigen Stählen mit elektromagnetischer Schmelzbadunterstützung
(2019)
Die steigenden Anforderungen in Hinsicht auf Sicherheitsfaktoren von gefügten Bauteilen führen zu einer Zunahme der zu schweißenden Bauteildicken. Das Laserstrahl-Lichtbogen-Hybridschweißverfahren – verbreitet im industriellen Einsatz vor allem im Schiffs- und Windkraftanlagenbau – ermöglicht das einlagige Fügen von dickwandigen Strukturen. Eine Herausforderung stellt das Schweißen von dickwandigen Bauteilen mit reduzierter Geschwindigkeit in Wannenlage (PA-Position) da. Sie ist aufgrund des erhöhten hydrostatischen Druckes und die daraus resultierenden Tropfenbildung an der Wurzelseite bedingt realisierbar. Die im Rahmen dieser Studie eingesetzte elektromagnetische Schmelzbadunterstützung wirkt dem gravitationsbedingten Austropfen der Schmelze entgegen und kompensiert den hydrostatischen Druck. Dabei werden unterhalb der Schweißzone mit Hilfe eines extern angelegten oszillierenden Magnetfeldes Wirbelströme im Werkstück induziert, die eine nach oben gerichtete Lorentzkraft erzeugt. Die Lorentzkraft wirkt dem hydrostatischen Druck entgegen und stellt einen sicheren Schweißprozess ohne Tropfenbildung dar. Mit dem Hybridschweißverfahren mithilfe der elektromagnetischen Schmelzbadunterstützung gelingt es mit einem 20-kW Faserlaser bis zu 30 mm dicke Bleche in einer Lage zu schweißen. Bei 25 mm dicken einlagig geschweißten Platten aus S355 konnte ein Spalt bis 1 mm und ein Kantenversatz bis zu 2 mm sicher überbrückt werden. Die Reduzierung der Schweißgeschwindigkeit hat eine Verringerung der notwendigen Laserleistung zur Folge und begünstigt außerdem die mechanisch-technologischen Eigenschaften, infolge der reduzierten Abkühlgeschwindigkeit. Durch die geringe Martensitbildung führt dies zu einer Verbesserung der Kerbschlagzähigkeit.
The shape of the weld pool in laser beam welding plays a major role to understand the dynamics of the melt and its solidification behavior. The aim of the present work was its experimental and numerical investigation. To visualize the geometry of the melt pool in the longitudinal section a butt joint configuration of 15 mm thick structural steel and transparent quartz glass was used. The weld pool shape was recorded by means of a high-speed video camera and two thermal imaging MWIR and VIS cameras. The observations show that the dimensions of the weld pool vary depending on the depth. The regions close to the surface form a teardrop shaped weld pool. A bulge-region and its temporal evolution were observed approximately in the middle of the depth of the weld pool. Additionally, a transient numerical simulation was performed until reaching a steady state to obtain the weld pool shape and to understand the formation mechanism of the observed bulging phenomena. A fixed keyhole with an experimentally obtained shape was used to represent the full-penetration laser beam welding process. The model considers the local temperature field, the effects of phase transition, thermo-capillary convection, natural convection and temperature-dependent material properties up to evaporation temperature. It was found that the Marangoni convection and the movement of the laser heat source are the dominant factors for the formation of the bulging-region. Good correlation between the numerically calculated and the experimentally observed weld bead shapes and the time-temperature curves on the upper and bottom surface were found.
The laser hybrid welding process offers many advantages regarding deep penetration, increased welding velocity and with the help of the supplied filler wire an improved bridgeability to gap and misalignment tolerances. High power laser systems with a power of approx. 30 kW are already available on the market. Nevertheless, multi-layer technology with an arc process is still used for welding of plates from a thickness from 20 mm. A potential cause is the process instability with increasing laser power. It is inevitable that gravity drop-out due to the high hydrostatic pressure at increasing wall thickness especially at welding in flat position and with a low welding speed. The surface tension decreases with increasing root width resulting from low welding velocities. To prevent such inadmissible defects of the seam a use of weld pool support is required. Usual weld pool support systems such as ceramic or powder supports require a mechanical detachment which is time-consuming. The electromagnetic weld pool support system described in this work shows an alternative weld pool support which works contactless. It is based on generating Lorentz forces in the weld pool due to oscillating magnetic field and induced eddy currents. This innovative technology offers single pass welds up to 28 mm in flat position and reduced welding velocity with a laser power of just 19 kW. It also leads to improved mechanical-technological properties of the seams because of the slow cooling rate. With usage of an electromagnetic weld pool support the limitation of the hybrid laser arc welding process in the thick sheet metal will be extend.
The hybrid laser arc welding (HLAW) process provides many advantages such as improved gap bridgeability, deep penetration and misalignment of edges, that is why the process is used increasingly in industrial applications e.g. shipbuilding, power plant industry and line-pipe manufacturing. The obvious encountered problem for single pass welding in flat position is the gravity drop-out at low welding velocities. With the usage of an electromagnetic weld pool support system, which is based on generating Lorentz forces within the weld pool, wide seams followed by reduced welding velocities could be achieved in this study leading to the realization of a gap bridgeability up to 1 mm, misalignment of edges up to 2 mm and a single pass weld up to 28 mm thickness with a 20-kW fibre laser. These developments expand the boundaries of the HLAW process for different industrial applications. As a result, less accurate preparation of the edges would be sufficient, which saves time for manufacturing.
The present research work encloses results of experimental investigations of the interaction between welding process parameters for laser-beam and hybrid-laser-arc as well as type of the filler metal and the achievable mechanical properties of the weld joints on steel grade X8Ni9+QT640 for cryogenic service containing 9% nickel. The results obtained contribute to the development and conversion in the industrial practice a new laser beam-based welding technology for the automated manufacturing of facilities for the liquefaction, storage and the transport of natural gases (LNG facilities). The results show, that the martensitic microstructure of the laser weld metal including low amount of retained austenite not exceeding 3.5% leads to the relatively low V-notch impact energy. The remarkable heterogeneity in the chemical composition of the weld metal through the weld thickness could be recognized in the case of hybrid-laser-arc welding with ERNiCrMo-3 austenitic filler metal, what also led to insufficient impact toughness of the weld metall. The most promising results could be achieved by using 11%Ni filler wire, which is similar to the base metal and provides a homogeneous microstructure with uniform distribution of Ni through the weld seam. It is remarkable, that a correlation between Charpy impact toughness and wire feeding speed and respectively process heat input exists. The highest toughness values were 134±58 J at -196C. The both laser as well as laser-hybrid welds passed the tensile test. The failure stress of 720±3 MPa with a fracture location in the base material was achieved for all samples tested.
The present research work aims at clarification of the effect of the welding electrode type on the mechanical properties of SMA welded joints of 9%Ni steel plates. Properties of produced SMA welded joints were evaluated using different non-destructive and destructive investigation methods. In comparison with the conventionally used Ni-based welding electrode ENiCrMo-3 (AWS A5.11), an experimentally produced non-conventional ferritic welding electrode with 11%Ni (ENi11-Company specification) has resulted in a better combination of the mechanical properties of SMA welded joints of this steel type for critical cryogenic applications. Besides, a positive economic impact for the experimentally produced non-conventional ferritic welding electrode, due to its lower cost, could be another attractive aspect.
In this study, a three-dimensional CFD-simulation model was developed to simulate the fluid flow in the weld pool. The CFD-model showed a bulging region in the middle of the depth, which is separated from the top surface and bottom surface by two narrowing regions. It can be concluded that the interaction of the movement of the laser source with the Marangoni vortex leads to a teardrop shape at the upper and bottom surface of the workpiece. Additionally, it shows that the bulging in the weld is a result of the backflows on the upper and lower sides due to the thermo-capillary-driven flows. The weld pool shape was used as a heat source in a two-dimensional thermomechanical model, which allows a highly accurate transformation of the weld pool dimensions obtained from the CFD model. This developed technique allows the consideration of physical aspects, which cannot be considered when using traditional heat sources. The mechanical model has shown that the chronological order of the solidification of the weld has a significant influence on the nature and distribution of the stresses in the weld. High tensile stress has been observed in the bulging region, i.e. in the susceptible region for solidification cracking, when compared to the other narrowing regions, which show compressive stress.
This paper represents the results for proposed optical flow method based on the Lucas-Kanade (LK) algorithm applied to two different problems. The following observations can be made:
- The estimated strain and displacement for conducted tensile test are generally very close to those measured with conventional DIC-technique.
- The LK technique allows measurement of strain or displacement without special selection of a region of interest.
Using a novel optical measurement technique together with the optical flow algorithm, a twodimensional deformation analysis during welding was conducted. This technique is the first to provide a measurement of the full strain field locally in the immediate vicinity of the solidification front. Additionally, the described procedure of the optical measurement allows the real material-dependent values of critical strain characterizing the transition to hot cracking during laser welding processes to be determined.
The weldability of materials is still for many years a highly contentious issue, particularly regarding the causes of the hot crack formation. Because of the process-related temperature and emissions, direct measurement for the arising strain in the close vicinity of the welding process is challenged. therefore, the externally loaded hot cracking testes remain for decades the only way to determine the critical straining conditions for solidification cracking. In this study, a novel optical two-dimensional in situ observation technique has been developed to analyse the strain evaluation during the welding process in the moment of crack formation. Additionally, the Controlled Tensile Weldability test (CTW test) was used to generate the hot crack under different global straining conditions. To record the welding process and the moment of the solidification crack initiation a CMOS camera was used which inserted coaxially into the optical path of the welding laser. As illumination source a diode laser with wave length 808 nm was employed to illuminate the welding region. An interference filter was placed on the camera lens, allowing only the illumination wavelength to pass through and reflecting all other wavelengths, so that the melt pool and the re-solidifying metal could be visualized in a single image. in order to obtain good temporal resolution, the frame rate of the camera was set to 1100 frame per second in. The contrast in images obtained using this unique setup allows to apply the optical flow technique based on Lucas-Kanade (LK) algorithm to follow the pixels in each image sequence and then to calculate the displacement field. The strain was calculated based on the estimated displacement. Using this technique, the local strains and strain rates under different global straining condition has been determined and analysed. The results shown Dependency between the external strain rate and the critical local strain and strain rate has been observed. That is to say, the critical local strain and strain rate are increased with an increase of the strain rate. Moreover, the described procedure of the optical measurement allows to determine the real martial dependent values of critical strain and strain rate characterizing transition to the hot cracking during laser welding processes.The experiments as well as the measurement has been performed on the stainless steel 316L (1.4404)