Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Dokumenttyp
- Vortrag (145) (entfernen)
Sprache
- Englisch (145) (entfernen)
Referierte Publikation
- nein (145)
Schlagworte
- Corrosion (41)
- Geothermal (14)
- Stainless steel (8)
- CCUS (7)
- Cement (7)
- Copper (7)
- Durability (7)
- Crevice corrosion (6)
- Polyaniline (6)
- Steel (6)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (145) (entfernen)
Eingeladener Vortrag
- nein (144)
Nowadays, various polymeric materials are used in E&E applications with sufficient flame retardance by adding rather different flame retardants. It doesn’t matter whether cables are used outdoor or are installed indoor as building products, the weathering exposures such as UV radiation, humidity and variation in temperature occur and influence the flame-retardant property. Recently, the lifetime of the flame retardance itself becomes an increasingly important factor. In this work, several devices were used to perform accelerated artificial ageing simulating different environment exposures.
The comprehensive and global understanding of the durability of flame retardance in dependence on the weathering or ageing conditions is still a matter of discussion. Therefore, the weathering resistance of various halogen-free fire-retarded polymers was investigated in this work. Polymeric systems with different kinds of fire retardants were chosen, including various fire retardant mechanisms. Ethylene Vinyl Acetate (EVA) blends with high amounts of inorganic flame retardant such as aluminum hydroxide (ATH), boehmite and synergists, which mainly dilutes the polymer resin work as heat sink and cooling agent, and enhance residue formation was examined. Thermoplastic Polyurethane (TPU) was modified with melamine cyanurate (MC), which mainly acts by changed melt flow and dripping behavior as well as fuel dilution. Additionally, aluminum diethylphosphinate and boehmite are induced as assistant flame retardant. Furthermore, glass fiber reinforced Polyamide 66 (PA) was investigated containing different kinds of aluminum diethylphosphinate based flame retardant mixtures, which acts by flame inhibition and additional char formation.
The degradation of the surface was analyzed after the different weathering conditions. Most of the specimens exhibited an intensive material degradation at the top surface accompanied by a distinct discoloration, e.g. getting darker or showing yellowing. The weathering of the EVA samples lead to numerous cracks (already) after 4000 h. The corresponding changes in the chemical structure was investigated by ATR FT-IR for all materials.
The flammability was investigated by cone calorimeter, UL-94 burning chamber, and oxygen index (LOI) using plate and bar specimens. The flame retardance of most of the materials studied degrades only slightly or were rather stable for the investigated exposure times. Interestingly, also some opposite results were found. EVA modified by different inorganic flame retardants such as ATH achieved higher LOI after exposing in the humidity chamber and the accelerated oxidation under water in the autoclaves. It is suggested that the particle size of ATH and boehmite plays an important role, when these flame retardants agglomerate at the surface during accelerated weathering.
Both materials, EVA and TPU, were also investigated as cable jackets. While EVA modified with inorganic flame retardants exhibits low-smoke and non-dripping fire behavior, TPU flame-retarded with MC yields cables with pronounced melt-dripping. Cone calorimeter tests were carried out using cable rafts of the size of 100 mm * 100 mm as well as our self-made cable module test, which simulates the vertical full-scale test of a bundle of cables at the bench-scale. Both methods were used to investigate the weathering resistance of the flame retardance in cables. The results of the cable module test for the flame-retarded EVA cables were only slightly affected even when a long time hydrothermal ageing was carried out. This is because of inorganic residue which just delays the fire growth but does not extinguish. However, for the flame-retarded TPU cable jackets, the cable module test exhibited an accelerated fire spread and a melt-dripping behavior which was promoted by weathering exposure.
Water Migration in One-Side Heated Concrete: 4D In-Situ CT Monitoring of the Moisture-Clog-Effect
(2018)
In order to study damage in concrete exposed to fire, a series of continuous X-ray computed tomography (CT) measurements were performed on a concrete sample heated, in-situ, on one side. The water migration relative to time and 3D space and, in particular, the dynamic condensation and vaporization of water droplets in the pores was quantified. This approach shows significant potential for further investigation of fire-related concrete damage.
Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. Here, by means of inelastic neutron scattering, the vibrational density of states (VDOS) and the molecular mobility were investigated for PIM-1, the prototypical polymer with intrinsic microporosity. The results are compared to data measured for a more conventional high-performance polyimide used in gas separation membranes (Matrimid).
The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. In comparison to the Boson peak of Matrimid, that of PIM-1 is shifted to lower frequencies. This shift is discussed considering the microporous, sponge-like structure of PIM-1 as providing a higher compressibility at the molecular scale than for conventional polymers.
Elastic fixed window scans were measured on a neutron backscattering spectrometer to have an overview about the molecular dynamics at a time scale of ca. 1 ns. The temperature dependence of the estimated mean squared displacement shows a step-like increase in the temperature range from 100 K to 250 K indicating the onset of some molecular mobility. The nature of this motional process was analyzed in detail by quasielastic neutron scattering where the data are discussed with regard to both the q- and the temperature dependence.
Utilisation of alkali-sensitive aggregates for concrete pavements by internal hydrophobisation
(2021)
In order to avoid the increased ASR damage to concrete pavements in the German motorway network in the future, the ARS 04/2013 introduced mandatory suitability tests to exclude alkali-sensitive aggregates in new construction measures. This resulted in a significant reduction of suitable aggregates. Against this background, borderline alkali-sensitive aggregates are to be made usable by adding an internal water repellent agent during concrete casting. The ASR avoidance strategy is based on the significant reduction of the penetration of water and de-icing salt solution into the concrete pavement. Laboratory tests show that, with a suitable active ingredient, the ASR damage process can be significantly reduced with internal hydrophobisation. The disadvantage is that this is associated with a deterioration of the mechanical properties and the resistance to freeze-thaw with de-icing salt. The aim of the ongoing research is to reduce these disadvantages through targeted modification of the hydrophobising agent and air-entraining agent.
Explosive spalling is caused by, among others, the thermohydraulic spalling mechanism. During this process, vaporization, dehydration, moisture-transport and condensation processes interact. As a result, a drying and dehydration zone as well as a saturated zone, known as a moisture clog, are observed inside the unilaterally-heated concrete. The presented research is focused on the experimental investigation of the underlying thermohydraulic processes.
To investigate these, a test methodology based on X-ray computed tomography (CT) and nuclear magnetic resonance (NMR) was developed. Thereby, the X-ray CT scans are carried out simultaneously during the application of a defined unilateral-heating regime on a specially-constructed specimen. This miniaturized specimen, equipped with a double-layer casing, reproduces the condition within a planar, unilaterally-heated building component.
A preliminary test methodology and the first experimental results were presented at the 5th International Workshop on Concrete Spalling in Borås, Sweden (2017). The contribution for the upcoming workshop presents an improved version of this test methodology and new results for a high-performance concrete (HPC) mixture exposed to temperatures up to 500 °C. Regarding the CT measurements, a higher time-resolution of 15 min was achieved and a quantification of the moisture changes was implemented. Due to an increase in signal quality of the NMR measurements, a pore-size specific moisture distribution can now be resolved. This allows to conclude about the moisture reconfiguration between small gel pores and larger interhydrate pores. Additionally, the NMR measurement are no longer limited to first 2.5 cm below the heated surface but a one-dimensional moisture distribution can now be estimated over the whole 10 cm long specimen.
The presented results demonstrate that the combination of X-ray CT and NMR measurements enables to image and quantify the thermally-induced moisture transport and reconfiguration from small gel pores up to macro pores. This provides important insights into the thermohydraulic damage mechanism and leads to a better understanding of spalling avoidance strategies, like the addition of polypropylene fibres.
The collaborative project “Impacts of impurities in CO2 streams captured from different emitters in a regional cluster on transport, injection and storage (CLUSTER)” aimed to set up recommendations on how to define “reasonable minimum composition thresholds” that CO2 streams should meet when accessing CO2 transport pipeline networks. Within CLUSTER, we investigated potential impacts of CO2 streams with different and temporally variable compositions and mass flow rates along the whole CCS chain. Investigations included, amongst others, impacts on: Corrosion of pipeline steel, pipeline network design and related transport costs, alteration of well bore cements, pressure evelopment and rock integrity, geochemical reactions, and petrophysical and geomechanical rock properties.
All investigations are based on a generic CCS chain scenario. In this scenario, CO2 streams are captured from a spatial cluster of eleven emitters and collected in a regional pipeline network. Emitters comprise seven fossil fuel-fired power plants equipped with different capture technologies, two cement plants, one refinery and one integrated iron and steel plant. In total, 19.78 Mio t CO2 (including impurities) are captured in the emitter cluster annually. The combined CO2 stream is transported in a trunk line with a length of 400 km (100 km of these offshore) and is injected into five generic storage structures. The storage reservoirs are saline aquifers of the Buntsandstein.
The investigations revealed beneficial and deteriorating impacts of different impurities and combinations thereof. Overall, no fundamental technical obstacles for transporting, injecting and storing CO2 streams of the modelled variable compositions and mass flow rates were observed. Based on the results, the CLUSTER project team recommends not to define “minimum composition thresholds” for CO2 streams as strict threshold values for eachindividual impurity in the stream. Instead, CO2 stream compositions and variabilities for specific CCS projects should be constrained with regard to a set of parameters including i) the overall CO2 content, ii) maximum contents of relevant impurities or elements, iii) acceptable variability of CO2 stream composition, and iv)impurity combinations to be avoided.
Concrete has a long history in the construction industry and is currently one of the most widely used building materials. Especially precast concrete elements are frequently utilized in construction projects for standardized applications, increasing the quality of the composite material, as well as reducing the required building time. Despite the accumulated knowledge, continuous research and development in this field is essential due to the complexity of the composite combined with the ever-growing number of applications and requirements. Especially in view of global climate change, design aspects as CO2 emissions and resource efficiency require new mix designs and optimization strategies. A result of the material’s high complexity and heterogeneity on multiple scales is that utilizing the full potential with changing demands is highly challenging, even for the established industry. We propose a framework based on an ontology, which automatically combines experimental data with numerical simulations. This not only simplifies experimental knowledge transfer, but allows the model calibration and the resulting simulation predictions to be reproducible and interpretable. This research shows a way towards a more performance oriented material design. Within this talk we present our workflow for an automated simulation of a precast element, demonstrating the interaction of the ontology and the finite element simulation. We show the automatic calibration of our early-age concrete model [1, 2], to improve the prediction of the optimal time for the removal of the form work.
The aim of the project LeBeDigital is to present opportunities of digitalization for concrete applications and show a way towards a performance oriented material design.
Due to the high complexity of the manufacturing process of concrete and the range of parameters affecting the effective composite properties, a global optimization is challenging.
Currently, most optimization is only carried out on a narrow scope related to the respective players, e.g. a mix optimization for a target strength, or a design optimization for minimum weight, using a given mix. To enable a path toward a full global optimization
requires a reproducible chain of data, accessible for all contributors.
We propose a framework based on an ontology, which automatically combines experimental data with numerical simulations. This not only simplifies experimental knowledge transfer, but allows the model calibration and the resulting simulation predictions to be
reproducible and interpretable. In addition to an optimized set of parameters, this setup allows to study the quality and uncertainty of the data and models, as well as giving information about optimal experiments to improve the data set.
We will present the proposed optimization workflow, using the example of a precast concrete element. The contribution will focus on the workflow and challenges of an interoperable FEM formulation.
Polymers of intrinsic microporosity (PIMs) have recently emerged as novel materials for a broad range of high-performance applications from gas separation to electronic devices. The very rigid, contorted polymer chains show only limited molecular mobility and therefore pack inefficiently giving rise to intrinsic microporosity with pore sizes generally smaller than 1 nm resulting in BET surface areas larger than 700 m2/g. Using conventional thermal analysis techniques, no glass transition temperature (Tg) of PIMs could be unambiguously detected up to now. Employing fast scanning calorimetry (FSC) based on a one chip sensor, decoupling the time scales responsible for the glass transition and the thermal decomposition is a reliable strategy to overcome this limitation. The FSC device is capable to heat and cool a small sample (ng-range) with ultrafast rates of several ten thousand K/s. Evidence of a glass transition is obtained for a series of PIMs with different chain rigidities. Local small-scale fluctuations are held responsible for the glass transition of highly rigid PIMs rather than segmental motions as in conventional polymers.
According to the results of the experiments carried out, the following points can be concluded:
1. Exposure tests showed that specimens with the addition of SiO2 particles and polyaniline particles exhibit better corrosion resistance than specimens with the addition of only polyaniline particles or binder only.
2. Open circuit potential measurements showed that in the beginning of the experiments, both coatings had an open circuit potential 100 mV higher than carbon steel. Within one day of immersion, the potential of carbon steel increased significantly, indicating the formation of oxide layer. After extended exposure the carbon steel potential sat between PS1 (which had higher potential) and PS2 (which had a lower potential) and all three were in the range –600 mV to –500 mV vs Ag/AgCl.
3. Both coatings PS-1 and PS-2 were degraded with increasing exposure time, shown by the decrease of absolute impedance value at low frequency range after 2, 4, and 6 days exposure.
4. Potentiodynamic test was performed after 3 hours and 6 days exposure, and it was shown that the coating in the initial stage exhibited more passive behavior than the specimens exposed for 6 days.
The adaption of the set-up for gas permeability measurements for ultra-high performance concrete
(2022)
In the framework of this project, a steam pressure vessel was to be developed from ultra-high perfor-mance concrete (UHPC) to withstand process temperatures of 200 °C and the respective steam pressure of 15,5 bar. To guarantee the long-term water vapour tightness of the system, the permeability of two UHPC mixtures were tested after long-term cyclic autoclaving. As UPHC shows a high density and therefore low permeability, measurements after the RILEM-Recommendation (TC 116-PCD) reached their detection limit. Therefore, the measurement set-up was adapted to measure the permeability of highly dense UHPC more reliably and quickly. This adaption includes measurements in a higher pres-sure range, the change of sample size thickness and the usage of Ar as a medium compared with the RILEM Recommendation. Additionally, the system was equipped with two pressure sensors and Ar-flowmeters to guarantee a continuous record of the experimental parameters. The new system was tested and evaluated by comparing measurements with the RILEM recommended system. Preliminary results show that the adapted system is capable to provide efficient and reliable results of concrete with low permeability.
With increasing focus on industrialized processing, investigating, understanding, and modelling the structural build-up of cementitious materials becomes more important. The structural build-up governs the key property of fresh printable materials -- buildability -- and it influences the mechanical properties after the deposition. The structural build-up rate can be adjusted by optimization of the mixture composition and the use of concrete admixtures. Additionally, it is known, that the environmental conditions, i.e. humidity and temperature have a significant impact on the kinetic of cement hydration and the resulting hardened properties, such as shrinkage, cracking resistance etc. In this study, small amplitude oscillatory shear (SAOS) tests are applied to examine the structural build-up rate of cement paste subject to different temperatures under controlled humidity. The results indicate significant influences of the ambient temperature on the intensity of the re-flocculation (Rthix) rate, while the structuration rate (Athix) is almost not affected. A bi-linear thixotropy model extended by temperature dependent parameters coupled with a linear viscoelastic material model is proposed to simulate the mechanical behaviour considering the structural build-up during the SAOS test.
For extrusion-based 3D concrete printing, the early age mechanical behavior is influenced by various time dependent phenomena: structural build-up, plasticity as well as viscosity. The structural build-up is governing the stability and early-age strength development of the fresh printable cementitious materials and with that influencing the printability, buildability, and open time of the printing process. Generally, it is influenced by a number of factors, i.e. composition of the printable material, printing regime, and ambient conditions (temperature, humidity, etc.). There are several approaches to model the structural build-up of cementitious materials. All models are based on a time-dependent internal structural parameter describing the flocculation state, which is assumed to be zero after mixing and increases with time. The approaches differ in the definition of the time dependency (linear, exponential, bi-linear). Usually, the parameters are defined for a specific material composition without considering the influence of ambient conditions.
In this contribution, the bi-linear structural build-up model [Kruger et al., Construction and Building Materials 224, 2019] is extended by the temperature influence. Temperature changes will occur in real life printing processes due to changing ambient conditions (summer, winter, day, night) as well as the printing process (pressure changes etc.) and have a significant impact on the structural build-up process: an increase of the temperature leads to a faster dissolution of cement phases, accelerates hydration and boosts the Brownian motion. For that reason, the model parameters are simulated as temperature dependent using an Arrhenius function. Furthermore, the proposed extended model is calibrated based on measurement data using Bayesian inference. A very good agreement of the predicted model data with the measured control data was reached. Additionally, the structural build-up model is integrated into a viscoelastic and elastoplastic mechanical model, simulating the whole mechanical behavior during layer deposition.
Main message: Sustainability, or in other words, exploiting environmental conservation for the economic welfare and prosperity for all, would revolutionise the plastics industry were it to become predominant practice as a linear, fossil-fuel–based economy is switched to a carbon circular economy. Food for though is given by dint of a critical overview of the current trends in sustainable flame-retardant polymeric materials.
Introduction:
Transforming the plastics industry into a carbon circular economy over the next 30 years requires an immediate revolution entailing the development of cutting-edge materials and the planning of future industrial production plants. Hence, the innovative field of flame-retardant polymeric materials should lend its strength to drive this challenge. Visionary solutions are proposed to inspire us, while the implementation of economically feasible concepts can take us forward into the future.
Experimental The synthesis, processing, polymer analysis, thermal analysis, and investigation of fire behaviour from our own research are performed according to the state of the art, mostly in accordance with the pertinent ISO standards. Indeed, some of our equipment is part of the accredited lab; for the other methods we fulfil equivalent quality standards in terms of maintenance, calibration, participation in round robins, etc. Work steps such as the synthesis or preparation of new materials are usually outsourced or done with partners that have the relevant core competence. The talk also presents examples from other groups whose experimental is described in the corresponding scientific papers.
Results and Discussion An overview of current trends towards producing sustainable, flame-retardant polymeric materials is presented, using examples from the literature and by sketching our own projects performed in recent years. The examples are structured along a common theme leading from the use of old and new natural materials with some intrinsic flame retardancy, via flame-retardant biopolymers and biocomposites, to using renewable sources for flame retardants with the objective of exploiting natural sources available as industrial waste streams. Natural flame retardants and adjuvants are highlighted, although the status of most may be assessed as merely motivating our vision. Nevertheless, there are natural material streams finding their way into polymer mass production as fillers, adjuvants, polymers, or renewable educt sources. Natural substances originating from industrial waste streams open the door to sustainable solutions, because they are often available at low cost and avoid competition for land with farming or virgin forests. Aside from this main topic, remarks will address the recycling of flame-retarded polymeric materials; vitrimers are mentioned as a potential material for recyclable thermosets. At the end of the day, only convincing property profiles will prevail both for exploiting renewable sources and circular design, including cost effectiveness, sufficient availability, consistent quality, processibility, mechanical properties, and flame retardancy. However, sustainability must not be merely tolerated as an additional demand, but should instead be recognized as a solution, because sustainability aspires to ensure our economic welfare now and in the future.
Acknowledgement:
The examples shown from own project were supported by funding grants: BMBF WTZ: 01DN16040, DFG Scha 730/19-1, VW-Stiftung: Experiment No: 97437, DFG Scha 730/20-1, BMBF KMU Innovativ 031B1289B.
Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids
(2019)
The susceptibility of AISI 304 stainless steel to crevice corrosion on the effect of contact with electrochemically active fluids was investigated using exposure and stepwise potentiostatic polarisation. Crevice materials made up of 304 SS and Polyether ether ketone (PEEK) forming two kinds of crevices including 304 SS-to-PEEK and 304 SS-to-304 SS were tested.
Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids
(2019)
The susceptibility of AISI 304 stainless steel to crevice corrosion on the effect of contact with electrochemically active fluids was investigated using exposure and stepwise potentiostatic polarisation. Crevice materials made up of 304 SS and Polyether ether ketone (PEEK) forming two kinds of crevices including 304 SS-to-PEEK and 304 SS-to-304 SS were tested.
This study explores the acceleration of material design in the concrete industry, focusing on improving carbonation resistance, a key factor in the durability of concrete structures. Traditional tests for carbonation resistance are lengthy, but with the construction industry aiming for sustainable production, finding a balance between carbonation resistance and CO2 footprint is crucial. Our research employs two innovative methods: 1. Applying the Sequential Learning App for Materials Discovery (SLAMD), an AI materials design framework, to an extensive dataset of real-world concrete compositions to selectively test materials that meet market demands: maximum durability, optimal eco-durability, and the best cost-durability trade-off. 2. Investigating 1H Nuclear Magnetic Resonance (NMR) relaxometry as a quick alternative for characterizing carbonation behavior, as it saves time compared to traditional tests and assesses the complete material's pore space. Specific NMR features are then integrated into the material design model, with the model's performance compared against traditional approaches. The results of our study are compelling, demonstrating that materials can be precisely tailored to meet specific requirements with minimal data points. This marks a significant stride in the concrete industry, indicating that NMR-based, low-fidelity surrogate characterizations, combined with a focused, data-driven design approach, can substantially accelerate the development of durable, sustainable concrete mixtures.
Study of Polyaniline/Silicon Dioxide based Coating on Carbon Steel in Artificial Geothermal Brine
(2021)
By using the available resources in Indonesia, such as silicon dioxide and marine coating base, the PANI/SiO2 modified alkyd coating was able to protect carbon steel in a deaerated artificial geothermal water. The screening of coatings shows that the modification by adding individual pigment was not sufficient to protect carbon steel even during a short-term exposure, indicated by the discoloration after only seven days of exposure. Electrochemical tests indicated that there was no significant change in the Ecorr between the coated and uncoated carbon steel at room temperature. At 150 °C, the coated carbon steel has a lower potential than that of carbon steel, indicating that the coating is protecting carbon steel cathodically or slowing down the corrosion reaction. Finally, a long-term exposure test confirmed that the PANI/SiO2 modified coating successfully protects the carbon steel in the Sibayak artificial geothermal water up to 150 °C for 6 months.
A few layer/multilayer graphene (MLG) with a specific surface area of BET ≥ 250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution or latex premixing of master batches followed by conventional two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of ca. 35, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR).[1-5] 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM).[6-8] The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development.
Thermoplastic starch polymer blends as biodegradable materials are well known and used mainly as packaging material. In order to exploit new application fields for these materials, additional properties such as flame retardancy or increased mechanical strength are required. This work focuses on the flammability and fire behavior of a thermoplastic starch/polyester blend reinforced with natural fibers derived from Mexican industry processes wastes, such as keratin fibers from the tannery industry or coconut fibers[1]. Different fiber contents as well as combinations of varying contents of aluminum trihydroxide, expandable graphite or ammonium polyphosphate were tested in LOI, UL94, cone calorimeter and TG-FTIR in order to investigate and assess the concentration dependence of the fibers and flame retardants as well as synergistic effects between both components. In combination with ammonium polyphosphate, the coconut fibers induce a synergistic effect by reinforcing the char residue and creating a more stable heat barrier during forced flaming combustion in the cone calorimeter. Synergism is also observed in the oxygen test. The recycling of otherwise wasted material is a true challenge in material development, thus this work is a first step in the direction of sustainable and biodegradable materials.
In Europe biodiesel gained from rapeseeds are considered as an alternative to common fossil fuels due to its environmental performance and its independence from import of raw materials. Biodiesel is also suitable to serve as blending component to heating oil. In that case, it must be considered that changes of fuel composition might cause material degradation.
The objective of this research was to investigate the resistance of metallic materials exposed to heating oil, heating oil blend B20 with 20 % biodiesel and pure biodiesel. Furthermore, the resistance of metals to eight-year aged B10 and six-year aged pure biodiesel was evaluated. Ageing of biodiesel forms acids and water which might propagate metal corrosion. The investigated metals (aluminium, unalloyed steel, austenitic CrNi-steel, copper, die cast zinc and brass) are commonly used for components in middle distillate facilities.
According to DIN 50905-4 the immersed metals were exposed in a climate chamber at 50°C for 4 weeks. The metallic materials were evaluated as resistant if the annual corrosion rate due to uniform corrosion remained under 0.1 mm/year and no localized corrosion in the form of pitting occurred.
The corrosion rates of the exposed materials stayed far below the limit of 0.1 mm/year for all tested fuels. An exception was die cast zinc ZP0410 in eight-year aged B10; a corrosion rate up to 0.3 mm/year due to uniform corrosion was measured. In no case localized corrosion occurred. Copper and brass caused discolouration of biodiesel from yellow to green.
In conclusion, the tested metallic materials were resistant in heating oil, heating oil blend B20 and pure biodiesel at 50 °C. Even the metals exposed to six-year aged biodiesel and eight-year aged B10 showed no uniform or localized corrosion; except for zinc, which was not resistant in eight-year aged B10.
Additive manufacturing (AM) has revolutionized the manufacturing industry, offering a new paradigm to produce complex geometries and parts with customized properties. Among the different AM techniques, the wire arc additive manufacturing (WAAM) process has gained significant attention due to its high deposition rate and low equipment cost. However, the process is characterized by a complex thermal history, dynamic metallurgy, and mechanical behaviour that make it challenging to simulate it in real-time for online process control and optimization.
In this context, a reduced order model (ROM) using the proper generalized decomposition (PGD) method is proposed as a powerful tool to overcome the limitations of conventional numerical methods and enable the real-time simulation of the temperature field of WAAM processes. Though, the simulation of a moving heat source leads to a hardly separable parametric problem, which is handled by applying a novel mapping approach. Using this procedure, it is possible to create a simple separated representation of the model, also allowing to simulate multiple layers.
In this contribution, a PGD model is derived for the WAAM procedure simulating the temperature field. A good agreement with a standard finite element method is shown. The reduced model is further used in a stochastic model parameter estimation using Bayesian inference, speeding up calibrations and ultimately leading to a calibrated real-time simulation.
Additive manufacturing (AM) has revolutionized the manufacturing industry, offering a new paradigm to produce complex geometries and parts with customized properties. Among the different AM techniques, the wire arc additive manufacturing (WAAM) process has gained significant attention due to its high deposition rate and low equipment cost. However, the process is characterized by a complex thermal history making it challenging to simulate it in real-time for online process control and optimization.
In this context, a reduced order model (ROM) using the proper generalized decomposition (PGD) method [1] is proposed as a powerful tool to overcome the limitations of conventional numerical methods and enable the real-time simulation of the temperature field of WAAM processes. These simulations use a moving heat source leading to a hardly separable parametric problem, which is handled by applying a novel mapping approach [2]. This procedure makes it possible to create a simple separated representation of the model, which allows to simulate multiple layers.
In this contribution, a PGD model is derived for the temperature field simulation of the WAAM process. A good agreement with a standard finite element method is shown. The reduced model is further used in a stochastic model parameter estimation using Bayesian inference, speeding up calibrations and ultimately leading to a calibrated real-time simulation.
Numerical simulations are essential in predicting the behavior of systems in many engineering fields and industrial sectors. The development of accurate virtual representations of actual physical products or processes (also known as digital twins) allows huge savings in cost and resources. In fact, digital twins would allow reducing the number of real, physical prototypes, tests, and experiments, thus also increasing the sustainability of production processes and products’ lifetime. Standard numerical methods fail in providing real time simulations, especially for complex processes such as additive manufacturing applications.
This work aims to use a reduced order model for efficient wire arc additive manufacturing simulations, calibrations and real-time process control. Model reduction, e.g. the proper generalized decomposition [1,2] method, is a popular concept to decrease the computational effort. A new mapping approach [3] was applied to simulate a moving heat source with the proper generalized decomposition. Using this procedure even complex models can be simulated in real-time. The physical model is later on calibrated with the use of a stochastic model updating process and the reduced order model, leading to an optimized real-time simulation.
In this contribution, a proper generalized decomposition model for a bead-on-plate wire arc additive manufacturing is presented. It is also coupled with a stochastic model updating process identifying the heat source characteristics as well as the boundary conditions of the transient thermal problem, whereas the heat source shape is simulated using a Goldak heat source
Basic oxygen furnace slag (BOFS) is a by-product of steelmaking of which about 10.4 Mt are produced annually in the EU. BOFS is mostly used in road construction, earthwork and hydraulic engineering. However, in this use, the iron bound in BOFS is lost and the opportunity to produce higher value products from BOFS is forgone.
In recent decades, many researchers have investigated the production of both Portland cement clinker and crude iron from BOFS via a thermochemical reductive treatment. The reductive treatment of liquid BOFS causes a reduction of iron oxides to metallic iron, which separates from the mineral phase due to its higher density and can be recovered. An advantage of this process is that simultaneously the chemical composition of the reduced BOFS is adapted to that of Portland cement clinker and the hydraulic reactive mineral alite (Ca3SiO5) is formed.
In this study, German BOFS was reduced in a small-scale electric arc furnace and a low-iron mineral product rich in alite was produced. Despite a chemical and mineralogical composition similar to that of Portland cement clinker, the reduced BOFS produced less heat of hydration, and its reaction was delayed compared to Portland cement. However, adding gypsum accelerated the hydration rate of the reduced BOFS.
Further research to improve the hydraulic properties of the reduced BOFS is essential. If successful, the production of a hydraulic material and crude iron from BOFS could have economic and ecological benefits for both the cement and steel industry.
Steelmaking slag is a by-product of steel production of which 4.5 Mt were produced in 2020 in Germany alone. It is mainly used in road construction, earthwork and hydraulic engineering. A smaller part is returned to the metallurgical circle, used as fertilizer or landfilled.
With this use, iron oxides still contained in steelmaking slag are lost. In addition, the possibility of producing higher-grade products from steelmaking slag is foregone. In recent decades, many researchers have investigated the production of Portland cement clinker and crude iron from basic oxygen furnace slags (BOFS) via a reductive treatment. Carbothermal treatment of liquid BOFS causes a reduction of iron oxides to metallic iron, which separates from the mineral phase due to its higher density. Simultaneously, the chemical composition of the reduced slag is adapted to that of the Portland cement clinker.
In this study, German BOFS was reduced in a small-scale electric arc furnace using petrol coke as a reducing agent. The resulting low-iron mineral product had a similar chemical composition to Portland cement clinker and was rich in the tricalcium silicate solid solution alite (Ca3SiO5). Based on its chemical and mineralogical composition, similar to that of Portland cement clinker, the reduced BOFS has the potential to react comparably. In our study, the reduced BOFS produced less heat of hydration compared to OPC and its hydraulic reaction was delayed. However, adding gypsum has been shown to accelerate the hydration rate of the reduced BOFS compared to that known from the calcium silicates of Portland cement clinker.
Further research to improve the hydraulic properties of the reduced slag is essential. If successful, producing a hydraulic binder and crude iron from BOFS could have economic and ecological benefits for both the cement and steel industry.
High performance polymers of intrinsic microporosity (PIMs) have emerged as novel materials with broad applications from gas separation to electronic devices. Sufficiently rigid, even contorted polymer chains show only limited molecular mobility, therefore undergo inefficient packing and give rise to intrinsic microporosity with pore size generally smaller than 1 nm and BET surface areas larger than 700 m2/g. Further performance optimization and long-term stability of devices incorporating PIMs rely on our understanding of structure-processing-property relationships and physical aging, in which glass transition plays a key role. Up to now no glass transition temperature (Tg) of PIMs could be detected with conventional thermal analysis techniques before degradation. Decoupling the time scales responsible for the glass transition and the thermal decomposition is a reliable strategy to overcome this. This was achieved by employing fast scanning calorimetry (FSC) based on a chip sensor, which is capable to heat and cool a small sample (ng-range) with ultrafast rates of several ten thousand K/s. FSC provides definitive evidence of glass transition of a series of PIMs with a special consideration on the chain rigidity. The determined glass transition temperature of these PIMs follows the order of the rigidity of their backbone structures. FSC provides the first clear-cut experimental evidence of the glass transition of PIM-EA-TB with a Tg of 663 K, PIM-1 of 644 K and PIM-DMDPH-TB of 630 K at a heating rate of 1Χ104 K/s. Local fluctuations are featured in glass transition of highly rigid PIMs. As conformational changes are prevented by the backbone rigidity, the glass transition must rather be assigned to local small scale fluctuations.
Al2O3 coatings are often used as protective layers on steels against electrochemical and high-temperature corrosion because they are chemically inert and stable at elevated temperatures. This study presents preliminary work on the possibilities of using Al2O3 sol-gel coatings for corrosion protection of martensitic stainless steels in geothermal environments. Al2O3 sol-gel coatings were applied on UNS S42000, which is known to be susceptible to uniform and localized corrosion. The coated steel specimens were then tested in two types of artificial geothermal water, which simulate the geothermal fluids found in Sibayak (SBY), Indonesia, and North German Basin (NGB), Germany, respectively. SBY has pH 4 and 1.5 g/L of chloride ions, whereas NGB has a pH of 6 and 166 g/L of chloride ions. All experiments were carried out in autoclaves at 150 °C and 1 MPa under the deaerated condition. Evaluations were performed by investigating the surface profiles of both uncoated and coated steels before and after the corrosion test using a Laser Scanning Microscope (LSM) and Scanning Electron Microscope (SEM). Finally, Electrochemical Impedance Spectroscopy (EIS) was performed to compare the corrosion resistance of Al2O3 coated steels in SBY and NGB solutions. It was observed from the corrosion test that Al2O3 coatings are more suitable for use in the geothermal water with a higher pH.
Nickel-free, nitrogen alloyed austenitic stainless-steels, with about 19 wt.-% Mn and 0,8 wt. % N, are an interesting alternative to classic CrNi austenitic stainless steels due to their superior mechanical properties (Rm > 900 MPa, A5 > 50 %, Av > 350 J) in the solution annealed condition. The formation of chromium-rich nitrides during suboptimal heat treatment, processing or application leads to an inhomogeneous distribution of alloying elements in the microstructure, which reduces the corrosion resistance. Consequently, an accurate knowledge of the sensitization behavior is indispensable for the use of nickel-free, high-nitrogen austenitic stainless steels. The relationship between artificial aging, phase formation and corrosion resistance was investigated on the alloys X8CrMnN18-19 (1.3815) and X8CrMnMoN18-19-2 (1.4456), both alloyed with 0,8 wt.-% Nitrogen, in the present work. The microstructural evolution was studied by LM and SEM while the corrosion resistance was characterized with the electrochemical potentiodynamic reactivation (EPR) and the KorroPad indicator-test. Both alloys showed increased corrosion susceptibility within critical aging parameters. Finally, a sensitization diagram was described successfully for both alloys showing the positive effect of molybdenum.
Basic oxygen furnace slag (BOFS) is a by-product of the steelmaking process, of which about 10.4 Mt are produced annually in the European Union. Besides its predominant use in road construction, earthwork, and hydraulic engineering, it is also possible to use BOFS as a source material for Portland cement clinker.
The main difference in the chemical composition of BOFS from the chemical composition of Portland cement clinker is its high content of iron oxides (7-50 wt.%). In recent decades, many researchers have investigated the production of both Portland cement clinker and crude iron from BOFS via thermochemical reductive treatment. Carbothermal treatment of liquid BOFS causes reduction of iron oxides to metallic iron, which separates from the mineral phase due to its higher density.
In this study, German BOFS was reduced in a small-scale electric arc furnace using petrol coke as reducing agent. The produced low-iron mineral product was chemically similar to Portland cement clinker and contained the most important Portland cement mineral alite (Ca3SiO5) as main component. Besides alite, the mineral product contained other Portland cement clinker constituents such as belite (β-Ca2SiO4) and tricalcium aluminate (Ca3Al2O6).
The production of Portland cement clinker and crude iron from BOFS has economic and ecological benefits for both the cement and steel industry. Cement clinker from reduced BOFS may be used as a substitute for cement clinker from conventional cement production, thereby CO2 emissions will be reduced. The steel industry benefits from a high-value application for its by-products that avoids cost expensive landfilling and may even bring economic advantages. However, reductive treatment requires high temperatures and, for economic reasons, has to be carried out immediately after casting of the liquid BOFS, which is a logistical challenge for most steel plants. A cost-benefit analysis is therefore essential.
Ground Granulated Blast-Furnace Slag (GGBFS), a by-product of the iron-making process, has gained significant attention as a supplementary cementitious material and has become increasingly popular in recent years due to its remarkable properties. GGBFS can significantly reduce the environmental impact of cement production when it comes to building concrete structures. GGBFS can either be blended with ordinary Portland cement (OPC) (up to a 90% replacement), or it can be used in the production of alkali-activated materials (AAMs). However, a comprehensive understanding of the pore solution composition is necessary for understanding various aspects of cementitious materials and their durability, including corrosion behavior, passivation of steel, and resistance to deteriorative processes. In the present work, the pore solutions of seven different GGBFS-containing cements (alkali-activated slag, alkali-activated slag/fly ash blends, a hybrid alkaline cement, CEM III/C, and CEM III/B) were extracted and analysed by inductively coupled plasma-optical emission spectroscopy, ion chromatography, pH, redox potential, and conductivity measurements. For comparison, a Portland cement pore solution was analysed similarly. The Concentrations of reduced sulfur were noteworthy in all GGBFS-containing cements, particularly in alkali-activated cements, where concentrations were notably higher compared to standard cements. The redox potentials of the pore solutions were primarily dictated by the concentrations of reduced sulfur, although other factors may contribute. Additionally, sulfur species in the pore solutions had an impact on pH, electrical conductivity, and other properties pertinent to the corrosion of reinforcements.
Geothermal brine is a complex system containing a wide variety of dissolved salts resulting from the condition s in a geothermal well. These fluids lead to corrosion in pipes and other parts of geothermal system construction and necessitate intense research efforts in finding new suitable materials. Carbon steel is susceptible to corrosion in geothermal brine especially when it is exposed to a high temperature and high-pressure medium, which is considered to be an aggressive environment. An artificial geothermal water, bas ed on a brine composition found in Indonesia, was used to investigate the performance of high alloyed materials. The electrolyte has pH 4 and contains 1,500 mg/l Cl-, 20 mg/l SO4 2-, 15 mg/l HCO3 -, 200 mg/l Ca 2+, 250 mg/l K+, and 600 mg/l Na+. In order to protect the bare material in geothermal application, it is necessary to either use high alloyed material s or coatings. In this research, a coating system consisting of polyaniline and silicon dioxide was investigated regarding its behavior to protect carbon steel. In detail, the effect of SiO2 and polyaniline (PANi) addition was evaluated by exposure and electrochemical tests for 7 days, i.e. electrochemical impedance spectroscopy (EIS) and open circuit potential (OCP) at room temperature and 150 °C with 1 MPa pressure.
PE-HD as a polymeric fuel storage tank material: Photooxidation, fuel sorption and long-term storage
(2018)
High-density polyethylene (PE-HD) is a commodity thermoplastic polymer which is typically used for packing of dangerous goods. Its good resistance against photooxidation, fuels, chemicals and other environmental factors in addition to low production costs makes PE-HD attractive for fuel storage applications. Typical engine fuels stored in polymer tanks are petrol, diesel and biodiesel that receives increasing attention as proper alternative to fossil fuels. One of the major problems with biodiesel is its susceptibility to oxidize due to its chemical composition of unsaturated fatty acids which also can cause polymer degradation.
The aim of this study is to investigate the influence of different environmental factors, UV radiation and commonly stored fuels, on the mechanical, physical and chemical properties of two types of PE-HD polymers (stabilized and non-stabilized). The influence on the mechanical properties was tested by Charpy and tensile tests, chemical and physical properties were evaluated by Fourier-transform infrared spectroscopy (FTIR) and by dynamical mechanical analysis (DMA) tests. Samples were characterized after varying exposure time of UV radiation and after fully and partially immersion in biodiesel. In addition, similar experiments were conducted using diesel for comparison.
Carbon Capture and Storage (CCS) is identified as an excellent technology to reach the target of CO2 reduction. However, the safety issue and cost-effectiveness hinder the future of CCS. For the reliability and safety issues of injection wells, the corrosion resistance of the materials used needs to be determined.
In this study, representative low-cost materials including carbon steel 1.8977 and low alloyed steel 1.7225 were investigated in simulated pore water at 333 K and under CO2 saturation condition to represent the worst-case scenario: CO2 diffusion and aquifer fluid penetration. These simulated pore waters were made from relevant cement powder to mimic the realistic casing-cement interface. Electrochemical studies were carried out using the pore water made of cement powder dissolved in water in comparison with those dissolved in synthetic aquifer fluid, to reveal the effect of cement as well as formation water on the steel performance. Two commercially available types of cement were investigated: Dyckerhoff Variodur® and Wollastonite. Variodur® is a cement containing high performance binder with ultra-fine blast furnace slag which can be used to produce high acid resistance concrete. On the other hand, Wollastonite is an emerging natural material mainly made of CaSiO3 which can be hardened by converting to CaCO3 during CO2 injection.
The results showed the pH-reducing effect of CO2 on the simulated pore water/aquifer (from more than 10 to less than 5) leading to the active corrosion process that happened on both 1.8977 and 1.7225. Electrochemical characterization showed negative free corrosion potential and polarisation curves without passive behaviors. The tested coupons suffered from pitting corrosion, which was confirmed by surface analysis. Interestingly, basing on the pit depth measurements from the tested coupons and the hardness of cement powder, it is suggested that Variodur® performed better than Wollastonite in both aspects. The electrochemical data was compared to that resulted from exposure tests to give a recommendation on material selection for bore-hole construction.
Emanating from developing flame retarded biocomposites, we have proposed renewable natural fibers (including keratin) taken from industrial waste as an authentic sustainable approach. More recently, we have investigated non-vegan flame retardant approaches. This paper loves to give you an insight into our ongoing projects on biogenic industrial wastes like leather, bone meal, and insects. Materials were characterized multi-methodically, flame retardant modes of action quantified, decomposition mechanism proposed, and synergisms explained. Considering the large quantities of leather waste (LW) in industrial-scale production, we underline LW as multifunctional bio-adjuvants. LW enhances the flame retardancy of poly(ethylene-vinyl acetate) (EVA) containing phosphorus flame retardants (P-FR). Products/by-products of the invertebrate and vertebrate farming, respectively, are promising bio-based adjuvants in flame retarded bio-epoxy thermosets. While the addition of bone meal yields the formation of an inorganic shield, protein-based powders from insects provide an intumescent behavior. In combination with a P-FR superior charring and self-extinguishing are obtained.
Acknowledgement: In part of this work was supported by the Volkswagen Foundation grant “Experiment!” No. 97437.
Nuclear magnetic resonance (NMR) with focus on 1H protons is increasingly applied for non-destructive testing applications. Besides mobile NMR, laboratory devices such as the NMR core-analyzing tomograph are used. As their magnetic field is more homogeneous, they enable measurements with higher signal-to-noise ratios (SNR), but with limited sample sizes. The tomograph presented here (8.9 MHz) was constructed for a maximum sample diameter of 70 mm and length of up to 1 m. The resolution, the echo time (min. 50 µs), the SNR and the measurement type can be adjusted by means of exchangable coils. The tomograph enables measurements along the complete sensitive length, slice-selective and even 2- or 3-dimensional measurements. A movable sample lifting system thereby allows a precise positioning of the sample.
For centuries, churches, secular buildings and museums have been furnished with valuable works of art. Many works of art are UV- and light-sensitive. It is well known that especially UV radiation causes damage and discoloration in paintings, textiles, plastics, wood and other materials. In particular, the wavelengths between 280 and 410 nm cause color changes, embrittlement or destruction of e.g. plastics over time. Therefore, strongly UV-absorbing glasses are advantageous for architecture and are necessary for the protection of cultural assets. As restorers in all disciplines become more and more aware, the demands placed on buildings and their furnishings in terms of climate are becoming increasingly detailed and precise. The aim in each case is to preserve the valuable artwork.
For some years now, the industry has been offering the protection of cultural objects by installing special UV-protective glasses. Currently, UV protection for church buildings is realized by laminated safety glass equipped with appropriate UV-protective plastic films. Technically, this always means a second pane of glass in front of the windows, which is installed outside the building. This creates climatic gaps that are difficult to control and deterioration due to ageing effects can be expected. At the same time, this protective glazing is not invisible and has a considerable aesthetic influence on the interior and exterior appearance of the building. Meanwhile, the preservation of historical monuments accepts such aesthetic cuts on buildings in order to protect the artwork in the interior from UV light. To this day, however, the long-term durability of UV protection provided by inserted plastic films is still controversial.
To date the only available alternative on the market is a mouth-blown UV protection glass which uses a so-called overlay to provide UV protection. This shows that UV protection can also be achieved by glasses without plastic films thus realizing an exclusive inorganic protection which normally is more stable than a polymeric one. So far there are not enough studies to prove long-term durability.
The aim of this project is to provide existing glazing or new glazing to be created with a highly transparent layer that ensures this UV-protective filter function below 400 nm. The glass coating is to be applied to the glass over a large area and fired into the surface like a classic ceramic enamel paint with the same technics. In addition, it should be long-term durable in its function. It means, that the glass has to be fused at temperatures below 630 °C during the firing process, its chemical durability has to be high, its coefficient of thermal expansion has to be as close as the one of the substrate (usually float glass) and the glass has to absorb the UV-radiation within a thin thickness (thinner as 100 µm).
In this project, the long-term durability of commercial UV-protective glasses is examined. New low melting glasses containing UV-absorbing ions are being developed. Their UV-absorption as a thin layer is analyzed as well as their chemical durability and their thermal properties.
We are grateful to BMWI for the financial support in the frame of the Central Innovation Programme for SMEs (ZIM).
The presentation shows systematic investigations to describe the corrosion and corrosion product formation processes of pure zinc under the climatic conditions currently prevailing in the Federal Republic of Germany. The investigations in their entirety aim at questioning current and establishing new ways of looking at the formation of corrosion products of pure zinc under atmospheric corrosion conditions. Thus, they make a significant contribution in understanding corrosion protection by zinc and zinc coatings. In particular, the focus is placed on the initial stage of the corrosion product formation. A systematic investigation of this time range, which is characterized by very reactive corrosion products, is only made possible by using gel-type electrolytes. The short periods of time at the beginning of weathering is now measurable and their influence on the formation of corrosion products and the kinetics of layer formation describable. By combining the new electrochemical approach with gravimetric, microscopic and analytical methods, new insights could be gained both on a methodic and scientific level.
The presentation shows systematic investigations to describe the corrosion and corrosion product formation processes of pure zinc under the climatic conditions currently prevailing in the Federal Republic of Germany. The investigations in their entirety aim at questioning current and establishing new ways of looking at the formation of corrosion products of pure zinc under atmospheric corrosion conditions. Thus, they make a significant contribution in understanding corrosion protection by zinc and zinc coatings. In particular, the focus is placed on the initial stage of the corrosion product formation. A systematic investigation of this time range, which is characterized by very reactive corrosion products, is only made possible by using gel-type electrolytes. The short periods of time at the beginning of weathering is now measurable and their influence on the formation of corrosion products and the kinetics of layer formation describable. By combining the new electrochemical approach with gravimetric, microscopic and analytical methods, new insights could be gained both on a methodic and scientific level.
The presentation shows systematic investigations to describe the corrosion and corrosion product formation processes of pure zinc under the climatic conditions currently prevailing in the Federal Republic of Germany. The investigations in their entirety aim at questioning current and establishing new ways of looking at the formation of corrosion products of pure zinc under atmospheric corrosion conditions. Thus, they make a significant contribution in understanding corrosion protection by zinc and zinc coatings. In particular, the focus is placed on the initial stage of the corrosion product formation. A systematic investigation of this time range, which is characterized by very reactive corrosion products, is only made possible by using gel-type electrolytes. The short periods of time at the beginning of weathering is now measurable and their influence on the formation of corrosion products and the kinetics of layer formation describable. By combining the new electrochemical approach with gravimetric, microscopic and analytical methods, new insights could be gained both on a methodic and scientific level.
2D layered nanoparticles enable a distinct reduction of filler loadings in rubber compounds combined with a boost in performance due to their high surface to volume ratio. They often enable unique property profiles providing a great potential as effective fillers in rubber, especially by enhancing mechanical and barrier properties.
As the best possible incorporation into the elastomer matrix is crucial for the efficiency of the nanofiller, dispersing and exfoliation of the nanoparticles without formation of agglomerates usually constitutes an outstanding challenge - especially when using conventional processing methods. Laboratory-scale approaches for highly dispersed nanocomposites sometimes solve this problem, but these are often too energy and time consuming and provide no scale up possibility for real applications. Therefore, a latex premixing process was established to produce highly filled masterbatches, enabling the processing with conventional techniques.
The presence of nanoparticles greatly impacts the behavior of elastomeric compounds, besides affecting the properties of the final product also the processing is influenced (rheology, crosslinking).
In this study, nanocomposites of natural rubber and multilayer graphene (MLG) were prepared via a latex masterbatch route. Different strategies for masterbatch premixing are compared (stirring vs. ultrasonication, coagulation vs. drying). Dispersion and exfoliation of MLG were determined by transmission electron microscopy. The reinforcing effect of MLG affects the viscosity while the dispersed graphene layers may also act as diffusion barrier/absorbent for the crosslinking agents. In contrast to that, MLG forms physical crosslinks in the final product. Swelling measurements and differential scanning calorimetry allow a differentiation between chemical and physical network links. Different technical properties of the nanocomposites were measured with respect to mechanical and application relevant behavior.
Multiscale modeling of heterogeneous structures based on a localized model order reduction approach
(2023)
Many of today’s problems in engineering demand reliable and accurate prediction of failure mechanisms of mechanical structures. Thus, it is necessary to take into account the heterogeneous structure on the smaller scale, to capture the underlying physical phenomena. However, this poses a great challenge to the numerical solution since the computational cost is significantly increased by resolving the smaller scale in the model. Moreover, in applications where scale separation as the basis of classical homogenization schemes does not hold, the influence of the smaller scale on the larger scale has to be modelled directly. This work aims to develop an efficient concurrent methodology to model heterogeneous structures combining the variational multiscale method (VMM) [1] and model order reduction techniques (e. g. [2]). First, the influence of the smaller scale on the larger scale can be taken into account following the additive split of the displacement field as in the VMM. Here, also a decomposition of the global domain into subdomains, each containing a fine grid discretization of the smaller scale, is introduced. Second, local reduced approximation spaces for the smaller scale solution are constructed by exploring possible solutions for each subdomain based on the concept of oversampling [3]. The associated transfer operator is approximated by random sampling [4]. Herein, we propose to incorporate the actual physical behaviour of the structure of interest in the training data by drawing random samples from a multivariate normal distribution with the solution of a reduced global problem as mean. The local reduced spaces are designed such that local contributions of each subdomain can be coupled in a conforming way. Thus, the resulting global system is sparse and reduced in size compared to the direct numerical simulation, leading to a faster solution of the problem.
Elastomers, such as hydrogenated acrylonitrile-butadiene rubber (HNBR) are usually mechanically reinforced with high loadings of carbon black (CB) to achieve the properties demanded; high amounts of mineral flame retardants are used to fulfill fire safety requirements. These high filler loadings sometimes cause deterioration of the physical properties of the material. In this study, multilayer graphene (MLG), a nanoparticle made of only 10 graphene sheets, is applied in low loadings (3 phr) to reduce the total amount of filler or boost performance.1,2,3 In former studies nanofiller achieved increased flame retardancy at very low lowdings.4,5,6 The dispersion of the nanofiller is essential for the properties of the nanocomposites.7 The nanocomposites were prepared via master batch by an ultrasonically assisted solution mixing and subsequent conventional two-roll milling.
SEM and TEM micrographs and rheological measurements revealed that the MLG nanoparticles were well dispersed in the HNBR matrix. In the HNBR nanocomposites, 3 phr MLG replaced 15 phr CB, 3 phr ATH or 15 phr CB + 3 phr ATH and achieved large consistent improvement in curing, rheological and mechanical properties of the HNBR. The nanocomposites with partial replaced CB reduced the filler loading up to 60% without any deterioration of the properties. The HNBR/MLG nanocomposites achieved an even higher Young’s modulus, hardness and thermal conductivity. MLG achieved advanced flame retardancy by improving the protection layer. The layer is created during the burning phase and acted as an afterglow suppressor. This study proposed the combination of ATH with MLG as a promising approach to reduce the amount of filler, in addition to improving the mechanical properties and fire performance of HNBR rubbers.
A few layer/multilayer graphene (MLG) with a specific surface area of BET=250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution mixing of master batches followed by two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of 34, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR). 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability, the latter shown by the reduction in heat release rate in the cone calorimeter. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM). The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development.
Polymeric membranes represent a cost- and energy-efficient solution for gas separation. Recently Polymers of Intrinsic Microporosity (PIMs) have been in a great interest because of their outstanding BET surface area larger than 700m2/g and pore size smaller than 1 nm. PIMs are a promising candidate in gas separation with high permeability and appealing selectivity due to their inefficient packing derived from a combination of ladder-like rigid segments with sites of contortion. However, it is recognized this class of polymers suffer from decrease in performance with time due to physical aging. The initial microporous structures approach a denser state via local chain rearrangements, leading to a dramatic reduction in permeability. As chain packing during film casting and physical aging are the key factors determine the performance in separation applications, characterization of the molecular mobility in these materials has been proved to provide valuable information. In recent research on PIM-1 the archetypal PIM, a molecular relaxation process with high activation energy together with a significant conductivity in the glassy state has been found and explained with the formation of local intermolecular agglomerates due to interaction of π-electrons in aromatic moieties of the polymer backbone. In this work, the dielectric behavior of the polymeric films and their response upon heating (aging) were measured by isothermal frequency scans during different heating/cooling cycles in a broad temperature range down to 133K for the first time. Multiple dielectric processes following Arrhenius behavior were observed. Local fluctuations, Maxwell-Wagner-Sillars (MWS) polarization and structural relaxations were discussed correlating to structural-properties of PIM-1. Up to now, no other work has studied the role of porosity and thermal history of PIM-1 film in dielectric processes. The goal is by eliminating thermal history and considering storing conditions provide better understanding on aging and plasticizing in high free volume glassy polymer PIM-1.
Especially now in times of the energy revolution, the demand for energy-efficient separation processes promotes the advancement of new high-performance materials for use as highly selective separation membranes. Polymers with intrinsic microporosity (PIMs) are of high interest in the field of gas separation membranes. Currently the application of PIMs for membrane technology is still restrained by their strong tendency to physical aging involving a significant loss of their good gas separation properties. Physical aging phenomenon is related to the molecular mobility of PIMs which was investigated by broadband dielectric spectroscopy (BDS) previously [1]. In this work, covalent phosphinine-based framework (Eto-CPSF) was used as a nanofiller (0-10 wt %) in a PIM-1 matrix to potentially enhance the gas transport properties and prevent physical aging. Since molecular mobility is a fundamental parameter determining gas transport as well as physical aging in such a material, our study includes dielectric investigations by BDS of pure PIM-1 and PIM-1/Eto-CPSF mixed matrix membranes to establish a correlation between molecular mobility and gas transport properties. In addition, gas permeability was determined by the time-lag method (0-10 bar pressure) at 35 °C for N2, O2, CH4 and CO2 for all MMMs.
The dielectric behavior of the polymeric films and their response upon heating were measured by isothermal frequency scans during different heating/cooling cycles in a broad temperature range up to 250 °C. Multiple dielectric processes following Arrhenius behavior were observed. Local fluctuations, Maxwell-Wagner-Sillars (MWS) polarization and structural relaxations were discussed correlating to structural-properties of PIM-1. As main result for MMMs, the permeability of PIM-1 for CH4 and CO2 gases were increased significantly with only 5 wt% of nanofiller within the polymer matrix. However, this is not observed for Eto-CPSF concentrations higher than ca. 7 wt% probably due to a microphase separated morphology of the nanocomposite system. Furthermore, the permselectivity of membranes for pair gases O2/N2 and CO2/N2 show enhancement up to a concentration of about 7 wt% Eto-CPSF filler.
The global demand for concrete is growing, and with it, its carbon footprint. Current literature proposes biochar, a product of pyrolysis, as a possible car-bon sink to reduce the carbon footprint of concrete. This work investigates the microstructure of Portland cement pastes with 0%, 5%, and 25% of the cement replaced with wood biochar, since this should influence its macro-scopic mechanical properties. MIP, gas sorption, NMR, and µ-CT were used to analyze the pore space of the three materials. The combination of these methods, each with different resolution, enables a multi-scale investigation of biochar impact on the microstructure of cement pastes. NMR confirmed that biochar can absorb moisture and, thus, reduces the effective water-to-cement ratio. MIP and gas sorption results show 0% and 5% volume re-placement have similar gel pore structure. The results from µ-CT investiga-tions suggest that biochar may reduce the formation of larger pores. The in-clusion of non-reactive porous particles such as biochar increase the porosity of the material and should act as a weakness in terms of mechanical proper-ties. Overall, this study highlights the need to carefully tailor replacement rates to control the impact of biochar on the microstructure concrete mixtures and sees a strong need for further studies on mechanical properties.
The aim of the work presented was the evaluation of corrosion resistance
of various materials in geothermal Waters as a base to create a catalogue of suitable materials for applications in (not only) German geothermal power plants.
Users shall be enabled to have a basis for designing such facilities. High alloyed corrosion resistant alloys are suitable and do not cause copper or lead deposition. They shall be chosen for future design of the piping system, either in massive or in cladded form, if crevices formation with non-metallic materials can be prevented!
By exposure and electrochemical tests in the laboratory the Cu-effect on corrosion behavior of carbon steel, high-alloyed steels and Ti-alloy can be assessed.
Critical materials specific properties were determined by static exposure and electrochemical tests in an artificial geothermal water with high salinity and low pH, containing Cu. Conclusions were drawn using characteristic potential values.
It could be shown that significant Cu-deposition and -precipitation only occurred in combination with carbon steel. High-alloyed materials (S31603, S31653, S31700, S31703, S31803 and N08904) prevent the disturbing Cu-agglomeration. Therefore, they are suitable to be chosen for future design of the piping system, either in massive or in cladded form, if formation of crevices with non-metallic materials can be excluded.
From the interactions and pitting corrosion point of view, R50400 seems to be most favorable.
Lessons learned from long-term corrosion investigations and –monitoring in saline thermal waters
(2018)
Investigations of corrosion processes in geothermal well in Groß Schönebeck showed
Most tested materials (apart of carbon steel) proved to be corrosion resistant within the installations.
- Stability of coatings cannot be guaranteed.
- Main risk: Electrochemical corrosion of carbon steel casing with dissolved Cu resulting in clogging the reservoir
The corrosion prevention strategy requires use of higher alloyed casing materials depending on resistance parameters, availability and economic feasibility.
Fugenfüllsysteme für Fahrbahnbeläge unter höchsten Beanspruchungen bestimmen in zunehmenden Maße die sichere Verfügbarkeit des Autobahnnetzes. Die aktuellen europäischen technischen Regelungen zu deren Verwendbarkeit folgen noch einem spezifikatorischen Ansatz auf empirischen Grundlagen. Es hat sich gezeigt, dass ein solcher Ansatz den Dauerhaftigkeits- und Nutzungsanforderungen nicht mehr entsprechen kann. Der Autor plädiert in seinem Vortrag für einen Paradigmenwechsel hin zu einem funktionsanalytischen Bewertungsansatz. Es werden Vorschläge für eine versuchstechnische Lösung des Problems und die damit verbundenen Chancen für Optimierung und Innovation aufgezeigt.
Since 2016 ISO Technical Committee (TC) 265 is working on standardization the whole CCS-process chain. Around 30 countries are working together to provide international guidelines. As ISO 27913 was the first standard finished within these activities it is already in the stage of first revision.
The objective of ISO 27913 is “to provide specific requirements and recommendations on certain aspects of safe and reliable design, construction and operation of pipelines intended for the large-scale transportation of CO2 that are not already covered in existing pipeline standards such as ISO 13623, ASME B31.8, EN 1594, AS 2885 or other standards. Existing pipeline standards cover many of the issues related to the design and construction of CO2 pipelines; however, there are some CO2 specific issues that are not adequately covered in these standards. The purpose of this document is to cover these issues consistently. Hence, this document is not a standalone standard, but is written to be a supplement to other existing pipeline standards for natural gas or liquids for both onshore and offshore pipelines.”
This contribution shall provide information on the content, the current stage of the revision process, encourage to contribute to this standard and make listeners aware to consider the influence of ISO standard on documents currently in draft.
Ultra high performance concrete (UHPC) is characterised by its high compressive strength of more than 150 MPa and its high durability. Due to thermal treatment at 90°C a strength comparable to the 28-days-strength can be achieved immediately after the treatment and in some cases can be even further increased up to 30 %. The explanations for the increase in strength are the accelerated hydration of the clinker minerals and the intensified pozzolanic reaction contributing to a denser microstructure and hence, a high performance in compressive strength.
Former research shows that thermal treatment can lead to inhomogeneities in form of a visible zonation within the cross-section. The width of the margin increases with shorter pre-storage time before the thermal treatment and with omitting protective measures against desiccation during the treatment. Specimens exhibiting a zonation typically show a lower compressive strength compared to the undisturbed reference whereas changes in chemistry, mineral content and microstructure were not reported in detail.
In this study the zonation of thermally treated UHPC is investigated with respect to its chemistry, mineral composition and microstructure to allow predictions on durability and strength development. Measurements show a change in pore sizes, minerals phase composition and element distribution leading to the visible zonation and weaker bending tensile strength compared to the reference.
In this paper, we demonstrate the value of 1H NMR
relaxometry for studying the hydration of clinker-reduced, more
climate-friendly cementitious binders. The results were obtained
on typical CEM I cements and samples containing two different
reactive agricultural ashes as well as non-reactive biochars as
supplementary cementitious materials. The findings prove that
time-resolved NMR measurements provide valuable additional
information when combined with classical heat flow calorimetry.
To prevent future alkali-aggregate reaction (AAR) damage, which has occurred frequently in the German highway network in recent years, a new regulation has been drafted. This regulation severely limits the use of alkali-sensitive aggregates by requiring that their suitability be verified by certified inspectors using newly developed AAR concrete tests that involve the external supply of alkali. This has led to a significant limitation in the number of aggregates usable for concrete pavements. A novel AAR avoidance strategy is now being pursued, which aims to enable the use of borderline alkali-sensitive aggregates through the application of an internal water-repellent treatment. The addition of water repellents during concrete production should significantly reduce the ingress of water and external de-icing salts into the concrete pavement, thus reducing the potential for AAR damage.
This paper presents the results of laboratory tests to assess the suitability of this new AAR prevention strategy. Representative, highly AAR-susceptible road paving concrete made with an alkali-sensitive greywacke and various water repellents were used as the basis for these experiments. The tests for concrete suitability included determining the conventional fresh and hardened concrete properties as well as concrete prism tests with external alkaline supply. Building on these results, laser-induced breakdown spectroscopy (LIBS) analyses of de-icing-salt intrusion as well as microscopic examinations for verification of the AAR characteristics were carried out.
The results of the AAR concrete tests with external alkaline supply support the conclusion that, when hydrophobic agents containing a suitable active ingredient are used, the AAR damage process in road paving concrete can be sufficiently prevented.
If the amount of sulfate within the mix design for concrete is not balanced, ettringite formation which first controls solidification continues while the concrete is hardening. Ettringite forms by reaction of sulfate contained in the cement or in some admixture with calcium aluminate (C3A) as cement component. The “late primary
ettringite formation” promotes an increase in volume within the hardened concrete leading to cracks. To analyze the effect of substituting part of ordinary Portland cement (OPC) by a treated brown coal fly ash mortar bars were tested according to ASTM C452. This test method was originally developed to extrapolate from the internal to external sulfate attack and is based on the idea that by testing a concrete mixture containing sulfate the process of deterioration is accelerated because it does not have to diffuse into the concrete before reaction first. In addition to the samples prescribed in ASTM C452 further samples in the size of the German SVA procedure were tested also designed for accessing the external sulfate resistance. The results show that while the replacement of 25 % of cement by brown coal fly ash leads to length changes around the limit defined by ASTM, the substitution of 50 % cement exceeded the limit by a multiple. The progress of expansion is the very similar for the two geometries tested. In-situ XRD measurements confirmed that while for pastes made of OPC the formation of ettringite is completed after 20 hours, this is not true for the mixtures containing the brown coal fly ash.
In a different study the effect of hydrothermal treatment on the phase composition of ultra-high-performance concrete was analyzed. The results show that the sulfate and aluminate resulting from the decomposition of ettringite are bound into new phases. If this binding is permanent this might allow the larger use of sulfate bearing raw
materials.
Integrated Coating System for Corrosion Protection of Carbon Steel in Artificial Geothermal Brine
(2022)
Corrosive geothermal brines are a major challenge to geothermal power-plants. For cost reasons, plant designers prefer to use carbon and low alloyed steels, which are susceptible to uniform and localized corrosion when exposed to geothermal brines having acidic and saline properties. To solve such problem, coatings or inhibitors would be a protective solution as an alternative to the use of high alloyed materials.
This study investigated a coating system consisting of polyaniline/silicon dioxide based on resources locally available in Indonesia. Protection against corrosion of carbon steel was shown by long-term (28 day) exposure and electrochemical tests of coated carbon steels, performed in an artificial acidic and saline geothermal brine, comparable to the conditions encountered at a site in Indonesia.
Therefore, an integrated coating system is proposed for corrosion protection, combining the electrochemical functionality of polyaniline and the physical advantages of silica.
The first documentation of fuel biodeterioration dates back to the late 19th century. However, extensive studies concerning the microbial fuel contamination started in 1980’s. Polymeric fuel storage tanks containing diesel and biodiesel provide environmental conditions for microbial growth. Several studies demonstrated that bacteria, which were found in contaminated fuel systems, can use fuels as macronutrient; but such bacteria can also cause microbiologically influenced corrosion and fouling.
The aim of this study is to investigate the initial attachment behavior of bacteria, isolated from a diesel contamination, on neat and photooxidized high-density polyethylene (PE-HD). Two common PE-HD’s, less- and biodiesel-stabilized, were radiated to UV light representing a tank exposed to sunlight. The effect of photooxidiation on PE-HD’s surface were characterized chemically by Fourier-transform infrared spectroscopy (FTIR). The attached bacteria Pseudomonas aeruginosa and Bacillus subtilis on the polymer surface were evaluated by fluorescence microscopy and colony-forming unit tests (CFU).
The presence of polycarboxylate ether (PCE) based superplasticizers (SPs) has an enormous influence on the early hydration of cement. Therefore, the talk presents first experimental results about the influence of a delayed addition time of PCE SPs on the hydration of cement and tricalcium aluminate (C3A) pastes, investigated by isothermal heat flow calorimetry and in-situ XRD.
The state of fresh concrete is predominantly determined by the rheological properties of the cement paste. In order to control performance spectra and requirements of novel concretes and to better understand macroscopic phenomena, comprehensive knowledge of the material behavior of fresh cement suspensions as well as of the complex relationships of mechanisms at the nano and micro scale are necessary. This work focuses on micro and nano rheology of suspensions of cementitious model systems and the influence of polycarboxylate-based admixtures on the rheology. The phenomena are driven by multiple parameters such as adsorption and particle interactions. Hence, the first part examines the interaction between polycarboxylate ether (PCE) and synthesized clinker phases and hydration products as model systems with regard to early hydration products.
The presence of polycarboxylate ether (PCE) based superplasticizers (SPs) has enormous influence on the early hydration of cement. C3A as the most reactive phase of Portland cement plays a significant role in early hydration reactions and affects the rheological performance. Therefore, this talk presents experimental results about the influence of delayed addition of PCEs on the Hydration of alite and C3A-gypsum pastes investigated by isothermal heat flow calorimetry. Complementary in-situ XRD was carried out on C3S and C3A-gypsum pastes to analyze hydration and phase changes related to the addition of PCE. Cement pastes with a delayed addition of PCE showed less retardation compared to simultaneous addition. The alteration caused by PCE is much more pronounced for C3A-gypsum mixes. With a delayed addition of SP, the hydration of C3A is less retarded or even accelerated. It is obvious that there is less retardation the later the addition of SP. Furthermore, the PCE alter the hydration of C3A when added delayed and exhibit changes in kinetics and Hydration rates. XRD results showed that more C3A is dissolved in the presence of PCE. Also, the gypsum depletion occurs earlier in the presence of PCE and even faster with delayed addition. Without PCE AFm starts to form just after the gypsum depletion. However, in the presence of PCE AFm already starts to form at the beginning of the hydration. Due to the faster gypsum depletion in the presence of PCE, also the transformation from ettringite into AFm begins earlier, but takes longer as without SP.
Influence of Precipitating Brine Components on Materials Selection for Geothermal Applications
(2021)
By exposure and electrochemical tests in the laboratory the Cu- and Pb-effect on corrosion behavior and performance of carbon steel and a corrosion resistant alloy could be assessed. Critical material specific properties were determined by static exposure and electrochemical tests in artificial geothermal water with high salinity and low pH, containing Cu/Pb.
It could be shown that significant Cu- resp. Pb-deposition and precipitation only occurred in combination with carbon steel. Corrosion resistant alloys (e. g. Cr- and Ni-dominated stainless steels) prevent the disturbing Cu-agglomeration resp. Pb-deposition. Therefore, they are suitable to be chosen for future design of geothermal piping system, either in massive or in cladded form. Regarding corrosion, formation of crevices with non-metallic materials shall be avoided.
So, in addition to its already known limited corrosion resistance, carbon steel shall not be used when copper or lead species are content of the geothermal brine. Otherwise precipitation and/or deposition of metallic copper resp. lead must be expected, increasing the susceptibility of clogging the piping system.
From the interactions and pitting corrosion point of view, corrosion resistant alloys (preferably Ni-rich) seem to be most favorable when selecting materials for applications in such geothermal brines.
Significant Cu-deposition and precipitation only occurred in combination with carbon steel. High-alloyed materials prevent the disturbing Cu-agglomeration. Pb-deposition and precipitation only occurred in combination with carbon steel. No negative Pb-effect could be observed in combination with high-alloyed steels. High alloyed corrosion resistant alloys are suitable and shall be chosen for future design of the piping system, either in massive or in cladded form, to prevent unwanted interactions with brine components.
Significant Cu-deposition and ‑precipitation only occurred in combination with carbon steel. High-alloyed materials prevent the disturbing Cu-agglomeration. Pb-deposition and ‑precipitation only occurred in combination with carbon steel. No negative Pb-effect could be observed in combination with high-alloyed steels. High alloyed corrosion resistant alloys are suitable and shall be chosen for future design of the piping system, either in massive or in cladded form, if formation of crevices with non-metallic materials can be excluded!
Polymers with intrinsic microporosity are promising candidates for the active separation layer in green gas separation membranes and as active materials for electronic applicatons. Here, by means of inelastic neutron scattering, the vibrational density of states (VDOS) and the molecular mobility were investigated for PIM-1, the prototypical polymer with intrinsic microporosity. The results are compared to data measured for a more conventional high-performance polyimide used in gas separation membranes (Matrimid).
The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. In comparison to the Boson peak of Matrimid, that of PIM-1 is shifted to lower frequencies. This shift is discussed considering the microporous, sponge-like structure of PIM-1 as providing a higher compressibility at the molecular scale than for conventional polymers.
Elastic fixed window scans were measured on a neutron backscattering spectrometer to have an overview about the molecular dynamics at a time scale of ca. 1 ns. The temperature dependence of the estimated mean squared displacement shows a step-like increase in the temperature range from 100 K to 250 K indicating the onset of some molecular mobility. The nature of this motional process was analysed in detail by quasielastic neutron scattering combining Time-of-Flight and backscattering where the data are discussed with regard to both the q- and the temperature dependence.
Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. These polymers are characterized by a high permeability and reasonable permselectivity. The latter point is somehow surprising because for microporous systems a more Knudson-like diffusion is expected then a size dependent temperature activated sieving process. It was argued in the framework of a random gate model that molecular fluctuations on a time scale from ps to ns are responsible for the permselectivity.
Here series of polymers of intrinsic microporosity (PIMs) as well as microporous polynorbornenes with bulky Si side groups and a rigid backbone are considered. The polymers have different microporosity characterized by high BET surface area values.
First inelastic time-of-flight neutron scattering measurements were carried out to investigate the low frequency density of state (VDOS). The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. It was found that the frequency of the maximum position of the Boson peak correlates with the BET surface area value.
Secondly elastic scans as well as quasielastic neutron scattering measurements by a combination of neutron time-of-flight and backscattering have been out. A low temperature relaxation process was found for both polymers. This process was assigned to the methyl group rotation. It was analysed in terms of a jump diffusion in a three-fold potential. The analysis of the dependence of the elastic incoherent structure factor on the scattering vector yields the number of methyl groups which might be immobilized.
The neutron scattering experiments were accompanied by fast scanning calorimetry and broadband dielectric investigations as well as atomistic molecular dynamic simulations.
Impact of acid condensation on wetting and corrosion behavior of CO2 transport-pipeline steel
(2018)
Es ist allgemein akzeptiert, das Korrosion in CO2-Transport-Pipelines vernach¬lässigbar ist, solange der Wassergehalt des CO2-Stroms deutlich unter der maximal löslichen Menge liegt. Bisher gibt es keinen allgemeinen Konsens darüber, welcher maximale Wassergehalt in zu transportierendem CO2 zugelassen werden sollte. Bei einem Druck von 100 bar und im Temperaturbereich von 277 K bis 298 K beträgt die Löslichkeit von Wasser in CO2 ca. 1.900 bis 3.200 ppmv, aber die Korrosionsrate von Stählen steigt schon ab einem Wassergehalt von 500 ppmv deutlich an. Bei Anwesenheit von Begleitstoffen wie SO2, NO2 und O2, können sich HNO3, H2SO3 und H2SO4 bilden. Menge und Zusammensetzung von kondensierter Säure sind von der Gaszusammensetzung abhängig, und der Korrosionsmechanismus und die Korrosionsform sind vom Kondensationsverhalten abhängig.
Elektrochemische Messungen zur hygienischen Bewertung additiv gefertigter Bauteile werden diskutiert. Die Bewertung und Details des Werkstoffs werden beschrieben, Anwendungsbeispiele gezeigt.
Basic oxygen furnace slags (BOFS) are a by-product of steel production. In 2016, 10.4 Mt of BOFS were produced in the European Union (EU). The main part of BOFS is used in road construction, earthwork and hydraulic engineering. A smaller part is returned to the metallurgical circle, used as fertilizer or landfilled. However, it is also possible to produce higher value products from BOFS. For example, many researchers have investigated the possibility of producing Portland cement clinker and crude iron from BOFS by a carbothermal post-treatment.
In this study, German BOFS was reduced in a small-scale electric arc furnace using petrol coke as reducing agent. The carbothermal treatment reduces the iron oxides in the BOFS to metallic iron, which accumulates at the bottom of the furnace by density separation. In addition to metallic iron, the process generates a mineral product rich in the tricalcium silicate solid solution alite. As the main constituent of Portland cement clinker, the hydraulic reactive mineral alite is of high economic importance.
In previous studies, the hydraulic reactivity of the mineral product was investigated by testing the compressive strength of blends with 70 wt.% ordinary Portland cement (OPC). Recent investigations focused on the hydraulic properties of the pure mineral product from the reduced BOFS. The heat of hydration of the mineral product was measured by isothermal calorimetry and compared with the heat of hydration of a synthetic low-iron slag and OPC. In addition, the formation of hydration products was investigated with differential scanning calorimetry (DSC) and x-ray diffraction analysis (XRD) on freeze-dried samples after defined curing times. The results of the calorimetric measurements indicate that the mineral product produced less heat of hydration and its reaction was delayed compared to the synthetic low-iron slag and OPC. Hydration products such as portlandite and calcium silicate hydrates (C-S-H) formed later and in lower amounts.
The production of a hydraulic material from BOFS by reductive treatment is of great interest to both the cement and steel industries. The substitution of cement clinker in OPC with a hydraulic material such as reduced BOFS leads to a reduction in greenhouse gas emissions from cement production. The steel industry benefits from an application for its by-products that avoids cost expensive landfilling and may even bring economic advantages. Furthermore, it may be possible to return the recovered crude iron to production.
For the construction of hot water storage tanks, ultra high performance concrete proofed to be a suitable building material to ensure water tightness. Common storage tanks build with concrete are designed to endure temperatures up to 90 °C. To increase the energy efficiency however, modern tanks need to withstand temperatures above 100 °C. With increasing temperature and correlating water vapor pressures, the cement must meet new requirements. Thermodynamic modelling is a promising tool for predicting the phase stabilities of minerals in the cement within these temperature and pressure ranges (T/P). Thus, mixture designs can be investigated and optimized with regard to the expected mineral phases in selected T/P-ranges. Additionally, predictions of the long-term material behavior can be derived from thermodynamic data and subsequently the experimental effort can be reduced notably. On the other hand, validation of predictions is needed. The base for the thermodynamic model is a thermodynamic equilibrium and thus, the experimental data for validation should approach the presumed conditions of the equilibrium. This study investigates variable experimental conditions for the hydration of Portland cement at 100 °C to reach a sufficiently progressed development of the phase composition. In case of Portland cement, the highest degree of hydration achievable within a reasonable time span is the most significant parameter. Therefore, Portland cement pastes with w/c ratios from 0.4 to 0.6 and dwell times up to three weeks were examined with powder X-ray diffraction to identify mineral phase changes. At 100 °C and high humidity, Portland cement paste shows the expected mineral phases like portlandite, katoite, and remaining clinker phases. The cement pastes with high water content and long dwell time seem to have the highest degree of hydration, even though the AFm phases stabilize with increasing w/c ratio. A dwell time of two weeks and a w/c ratio of 0.5 was found to provide the mineral composition with the highest degree of hydration including the major phase transitions.
Zinc materials are of high importance in the field of corrosion protection. For example, almost half of the annual production of zinc is used as anti-corrosive layer for steel components, particularly under atmospheric conditions. The corrosion protection is frequently ascribed to zinc carbonate species with low solubility which form on the metal surface under atmospheric conditions. Due to the technological importance and wide use of zinc materials, its corrosion behavior and the formation of reaction products has been intensively investigated over decades.
Assuming atmospheric corrosion conditions, an initial native passive film of few nanometers thickness forms spontaneously. It consists of zinc oxide and hydroxide, transforming into various species in dependence of the surrounding atmospheric conditions.
This study focusses on the investigation of corrosion product layers on massive titanium-zinc sheets, formed during short- and mid-term exposure experiments by Fourier-transformed infrared spectroscopy. This method enables the investigation of extremely thin native passive films which form during the initial hours of exposure. Furthermore, aged surface layers are analyzed which were formed by transformation of initial passive layers over the time of several weeks. The spectroscopic investigations are complemented by scanning electron microscopy (SEM/EDX) in order to obtain information on the chemical composition and morphology of the corrosion products. The combination of both methods offers a comprehensive view on the processes occurring in the early stages of zinc corrosion.
Concrete has a long history in the construction industry and is currently one of the most widely used building materials. Unfortunately, the concrete industry has a significant impact on the environment by contributing to about 9% of the total anthropogenic greenhouse gas (GHG) emissions. Concrete is a highly complex composite material. However, the main source of concrete's GHG emissions is the cement. This leads to two main strategies when trying to reduce the environmental impact. The first is to reduce the cement within the concrete mix. This can be done by substituting it using additives or increasing the amount of aggregates. Usually this will lead to decreased material properties, like compressive strength or stiffness. The second option is to reduce the amount of required concrete by optimizing the topology of the structure. However, this might require higher compressive strength. In addition, there are other properties like to workability which need to be considered. All in all, this leads to a highly complex optimization problem, which requires the estimation of effective concrete properties, based on the mixture as input to a predictive simulation.
We present an automated workflow framework which combines experimental data with simulations, calibrates the simulation and performs the desired optimization. This workflow includes classical FE models, design guidelines based on model codes, as well as data driven methods. The chosen example is a beam, for which the concrete mixture is optimized to reduce GHG emissions. The first step is an estimation of material parameters, based on experimental data. This includes measures of stochastic distribution, allowing the quantification of the quality of the estimated parameters. The second step is the optimization. It takes into account constraints like the loading capacity after 28 days, the maximum allowed temperature during cement hydration and the maximum time till demoulding. The applied models include a Mori-Tanaka-based homogenization method to estimate effective concrete parameters, an FE simulation including the evolution of the concrete compressive strength and stiffness, the temperature field, displacements, and stress. This research shows a way towards a more performance-oriented material design.
A series of field exposure tests according to ISO 9223 up to 9226 was carried out at different locations to determine the corrosivity and the corrosion progress of different test sites throughout northern and eastern Germany. Standard test specimens of steel, zinc, copper and aluminium were exposed to rural, city and marine atmosphere at test sites of the Bundesanstalt für Materialforschung und -prüfung (BAM). Test sites at city atmosphere comprised exposure on a rooftop, next to a highly frequented road and directly at a motorway. Exposure under marine conditions was carried out at Heligoland in the North Sea. The specimens were stored under sheltered and unsheltered conditions on each test site, respectively. Corrosion rates after the first year of field exposure were determined and used for the classification of the atmospheres and the test sites regarding the corrosivity category.
Results after the first year of exposure were presented at the EUROCORR 2018 in Cracow. The current presentation will present an update of results of the systematic study after five years of exposure. The corrosion progress and the mass loss of the standard metals steel, zinc, copper and aluminium will be presented and discussed with respect to the atmospheric conditions and the time of wetness at the test sites. In addition, the difference between sheltered and unsheltered conditions will be discussed.
Fatigue induced degradation in pavement concrete and its effect on the alkali-silica-reaction
(2018)
In recent years the German motorway network has seen an increase in the occurrence of damage to concrete road surfaces that can be attributed to the alkali-silica reaction (ASR). In view of the often drastically reduced service life of road surfaces due to ASR, research activity in this field has notably increased. Alongside preventative measures in concrete technology i.e. the usage of low-alkali cements, the main research focus up to now has been on the development of performance-oriented testing procedures for ASR prevention. The effects of mechanicallyinduced damage resulting from cyclic traffic and climatic loading have previously not been taken into consideration.
The assessment of the myriad degradation and transport processes necessary for an understanding of these effects requires close interaction between experiments and corresponding multi-scale models. This contribution is focused on the experiments utilizing innovative testing techniques. The research is founded on a series of fatigue tests performed on large-scale beams with simultaneous tracking of the degradation process using non-destructive evaluation methods. Subsequently, smaller test specimens were extracted from the predamaged beams for further experiments. These experiments included investigation of the influence of fatigue-induced cracks on moisture and alkali transport. Subsequent storage of the small-scale test specimens, with and without cyclic pre-damage, in an ASR-conducive environment then provided initial findings on the influence of fatigue-induced degradation on the ASR.
The results show that the degradation process can be well observed with the test Setup developed for the fatigue experiments. Further, a small but noticeable increase of mass Transport due to fatigue-induced degradation was measured, which correspondingly indicated an increased ASR damage potential.
This work examined the factors that influence the droplet corrosion of CO2 pipeline steels caused by oxyfuel flue gases in dense phase CO2 at 278 K, simulating the underground transport conditions. The wetting properties were studied by contact angle measurement, revealing pH and time dependency on the reactive wetting behaviors of carbon steel X70. Exposure tests with CO2 saturated water droplet on steel surface showed that the impurities (220 ppmv SO2 and 6700 ppmv O2) diffused into the droplet and then reacted with metal surfaces in dense phase condition, forming the corrosion products. The corrosion rate was confirmed strongly depending on the droplet volume as well as the SO2 concentration. Condensation experiments carried out on freshly polished coupons in CO2 with 200 ppmv H2O, 220 ppmv SO2 and 6700 ppmv O2, showed that the formation and aggregation of droplets is time and temperature dependent. At 278 K, condensation happened stronger and the corrosion products, mainly consisted of dense hydrated FeSO3/FeSO4. While at 288 K, more fluffy corrosion products consisting of iron oxide/hydroxide and hydrated FeSO3/FeSO4 were found. Further exposure tests on carbon steel coupons with different surface roughness did not reveal the difference in weight loss/gain and therefore the corrosion rate.
The worldwide spread of windfarms brings new challenges, especially for concrete structures as a part of towers, connecting joints and foundations of wind turbines. High-cyclic loadings in such structures lead to a high relevance of the subject of fatigue. A proper assessment of the fatigue strength of concrete demands therefore a basis of reliable experimental data and the development of standardized testing methods. This article presents first results of an ongoing research program of BAM (Bundesanstalt für Materialforschung und -prüfung) which is a part of a joint project (WinConFat) funded by the German Federal Ministry for Economic Affairs and Energy. The subproject investigates the effects of size and slenderness of the specimens on the fatigue behaviour of high strength concrete at different stress levels. Not only the fatigue strength, but also the fatigue process itself is monitored by means of several measurement methods. Strain measurements are used to calculate the load dependent elastic modulus in the fatigue hysteresis as indicators for fatigue development. Furthermore, the application of non-destructive methods like acoustic emission analysis and ultrasonic measurement in laboratory tests gives a deeper insight into damage processes under cyclic loading. The results shall be used to improve design rules for concrete members under fatigue load and to develop or improve non-destructive techniques for in-service structural health monitoring.
In recent years, the use of simulation-based digital twins for monitoring and assessment of complex mechanical systems has greatly expanded. Their potential to increase the information obtained from limited data makes them an invaluable tool for a broad range of real-world applications. Nonetheless, there usually exists a discrepancy between the predicted response and the measurements of the system once built. One of the main contributors to this difference in addition to miscalibrated model parameters is the model error. Quantifying this socalled model bias (as well as proper values for the model parameters) is critical for the reliable performance of digital twins. Model bias identification is ultimately an inverse problem where information from measurements is used to update the original model. Bayesian formulations can tackle this task. Including the model bias as a parameter to be inferred enables the use of a Bayesian framework to obtain a probability distribution that represents the uncertainty between the measurements and the model. Simultaneously, this procedure can be combined with a classic parameter updating scheme to account for the trainable parameters in the original model. This study evaluates the effectiveness of different model bias identification approaches based on Bayesian inference methods. This includes more classical approaches such as direct parameter estimation using MCMC in a Bayesian setup, as well as more recent proposals such as stat- FEM or orthogonal Gaussian Processes. Their potential use in digital twins, generalization capabilities, and computational cost is extensively analyzed.
Evaluation of corrosion resistance of metallic materials is essential to assure safe and reliable operation of geothermal sites. One need to be aware that corrosion is not a material's but a system property, determined by medium, material and construction aspects. Various corrosion types have to be evaluated. Conditions in laboratory shall reflect on-site reality. Depending on brine composition and temperature suitability of metallic materials can be ranked. Most important outcome of the research is that highly saline geothermal brines require high alloyed materials, for safe long-term operation.
Slow crack growth (SCG) under the influence of external fluid media, usually termed environmental stress cracking (ESC), is still one of the most frequent origins of severe damage and failure of polymeric materials. For polyethylene (PE) this is relevant for mass products, like bottles for consumer products, but also for high-performance materials for pipes or industrial packaging, including containers for chemicals and other dangerous goods. Especially for high-density polyethylene (PE-HD) the susceptibility to SGC and ESC is depending on the complex interplay between molecular weight and architecture and the resulting semicrystalline morphology, especially the formation of tie-molecules.
A reliable assessment of the resistance against this damage phenomenon is essential for demanding as well as safety-critical applications and has to take into account suitable testing methodologies and conditions in combination with environmental media reflecting the properties representative for typical fillings and relevant components causing ESC. In this context a better understanding of different influencing factors, such as sorption, swelling or surface activity is necessary together with a detailed characterization of different stages of crack propagation and underlying mechanisms. Therefor well-established testing methods, such as the Full Notch Creep Test (FNCT), were complemented by detailed fracture surface analysis using e.g. LSM and SEM in combination with a time-dependent optical monitoring of the progressing crack growth.
For the crack growth also the ratio of fibrillated craze zone to crack opening is important for the deeper understanding of crack propagation and related material parameters which can be additionally addressed by X-ray computed tomography.
Carbon Capture and Storage (CCS) is identified as an excellent technology to reach the target of CO2 reduction. However, the safety issue and cost effectiveness hinder the future of CCS. For the reliability and safety issues of injection wells the corrosion resistance of the materials used needs to be determined.
In this study, representative low cost materials including carbon steel 1.8977 and low alloyed steel 1.7225 were embedded in cement to mimic the realistic casing-cement interface. Electrochemical studies were carried out using these metal-cement specimens in comparison with those made of metal only in CO2 saturated synthetic aquifer fluid, at 333 K, to reveal the effect of cement on the steel performance. The results showed the protective effect of cement on the performance of pipeline metals during polarisation process. However, the corrosion current density was high in all cases, with and without cement, indicating that the corrosion resistance of these materials is low. This conclusion was supported by the surface analysis of the polarized specimens, which revealed both homogenous and pitting corrosions. Furthermore, to reveal the possible protective performance of FeCO3, the pipeline steels were pre-carbonated and then tested in the same condition as freshly polished specimens.
It is well known that cement manufacture, including CaCO3 calcination and clinker formation, is associated with substantial energy consumption and significant greenhouse gas emissions. Alkali-activated binders (AAB) and concretes made from them can significantly contribute to reducing CO2 emissions caused by the construction industry. However, to what extent and for how long concretes made from AAB can protect the steel in reinforced concrete components from corrosion is still unclear. Unlike PC-based binders, AABs are made by reacting alkaline solutions with solid precursors such as fly ash and ground granulated blast furnace slag (GGBFS). Therefore, steel reinforcement corrosion mechanisms in AAMs differ from PC-based binders. The present study aims to evaluate the corrosion behavior of steel rebar in alkali-activated materials (AAMs) synthetic pore solution with different chemical concentrations representing different GGBFS and Flay Ash based binders by performing electrochemical tests to measure the corrosion rate and corrosion potential of steel rebar. This information can be used to improve the design of AAMs in order to ensure a longer service life for these materials.
Electrochemical deposition of polyaniline on carbon steel for corrosion study in geothermal solution
(2018)
Polyaniline has been widely developed for many applications, e.g., sensor, supercapacitor component, electrochromic devices, and anticorrosion pigments [1]. Although the addition of polyaniline pigment in organic coatings has been an alternative for corrosion protection in industrial application, the protection mechanism is still not fully understood [2]. Herein in this study, as a part of the development of polyaniline/silicon dioxide coating for geothermal application, polyaniline has been deposited electrochemically on carbon steel surface and tested in geothermal solution to study the contribution of polyaniline in the corrosion protection of a polyaniline-based composite in the geothermal system. The electrochemical deposition was carried out by immersing carbon steel in 0.1 M oxalic acid and 0.05 M aniline, with the polarization potential of -0.6 – 1.5 V vs. Ag/AgCl, and a scan rate of 10 mV/s. To observe the surface/interface reaction between the electrolyte and electrode surface during the electrochemical polymerization, electrochemical impedance spectroscopy (EIS) measurement was applied after each cycle. For corrosion study in the geothermal application, this experiment used an artificial geothermal solution with the composition of 1,500 mg/l Cl-, 20 mg/l SO42-, 15 mg/l HCO3-, 200 mg/l Ca2+, 250 mg/l K+, and 600 mg/l Na+, and pH 4 to simulate a geothermal brine found in Sibayak, Indonesia. Electrochemical measurements were performed by monitoring the open circuit potential over seven days, with the interruption of EIS every 22 hours. The experiments were performed at room temperature and 150 °C (1 MPa) in a free oxygen environment. Polyaniline coated carbon steel is more durable in a room temperature environment compared to 150 °C, which could be caused by the iron oxalate dissolution at elevated temperature. This degradation was further proven by the impedance spectra, which showed a reduction of approximately ten times for specimens measured at 150 °C as compared to the specimens measured at room temperature.
The electrochemical behavior of UNS N08031 was investigated as a function of electrode potential in Green-Death solution at 40 °C. The UNS N08031 surface is in a stable passive state during cyclic potentiodynamic polarization without an initiation and/or propagation of localized corrosion. In potentiostatic polarization of UNS N08031 for 3600 s, passive current density increases with an increase in the passivation potential from 0.7 to 1.0 VSSE (silver/silver chloride reference electrode in saturated potassium chloride) Electrochemical impedance spectroscopy (EIS) and Mott-Schottky (M-S) analysis showed that a more defective n-type semiconductive passive film forms as the potential increases. X-ray photoelectron spectroscopy (XPS) revealed that passive film consists of mainly chromium and minor iron and nickel oxides. The mechanism of the defective passive film formation is discussed. The increase of the applied potential is considered to be a reason for the change in passive film stability.
While today, engineers can choose from a wide range of rheology modifying admixtures, in some parts of the world, these are difficult to access, due to their complex processing. However, alternatives can be bio-based polymers such as polysaccharides from various sources. These are easily accessible all over the world, do not demand for complicated processing, and typically they are more sustainable than many established materials, which are crude oil-based.
The paper presents the effects of acacia gum, cassava starch and the gum of triumfetta pendrata A. Rich on the rheological performance of cementitious systems. It is shown that acacia gum can be as efficient as polycarboxylate based superplasticisers, cassava starch can reduce the yield stress slightly with little effect on the plastic viscosity, and the gum of triumfetta pendrata A. Rich increases the thixotropy of cement pastes with plasticizing polymers significantly.
While alkali-activated binders offer certain advantages over traditional Portland cement binders, particu¬larly in terms of resistance against chemical attacks and potentially environmental footprint, their degra¬dation mechanisms remain incompletely understood at present, specifically carbonation. Thus, this study investigates the impact of natural and accelerated carbonation (1% and 4% CO2) on three different compositions of alkali-activated concretes: 100% calcined clay (C100) binder, 100% ground blast furnace slag (S100) binder, and a 40% calcined clay and 60% blast furnace slag blend (C40S60). C100 concretes exhibit faster carbonation kinetics, with five times greater natural carbonation depths than S100. This difference diminishes under accelerated carbonation, showing a 1.5 times difference for 1% CO2 and complete carbonation for 4% CO2 at 90 days. The results thus confirm that accelerated carbonation testing of low-Ca alkali-activated concretes yields results that are not representative of natural carbonation. The C40S60 sample demonstrates a carbonation profile similar to a CEM I concrete, i.e., a high carbonation resistance. Microstructure analysis indicates the formation of three polymorphs of calcium carbonate for S100 (calcite, vaterite, and aragonite), with a higher CO2 concentration favouring aragonite over vaterite. C100 exhibits no calcium carbonates; instead, sodium carbonates form, including trona for 4% CO2 and natrite for both accelerated tests. C40S60 shows calcium and sodium carbonates, although to a lesser extent, containing predominantly calcite and minor signals of natrite. Suitable compositions, like C40S60, prove as effective during natural or accelerated carbonation tests as conventional Portland cement concrete.
In this work, the focus was set on the corrosion process of condensate as drops on the surface of carbon steels (X52, X70), martensitic steel UNS S41500, and superaustenite UNS 08031 in CO2 atmosphere with impurities at 278 K (to simulate the transportation condition in a buried pipeline). Exposure tests were performed at both normal pressure and high pressure where CO2 is supercritical or in dense phase. The drop, 1 ‑ 10 µL in volume, was prepared by dropping CO2 saturated ultra-pure water onto the surface of steel coupons in a one-liter-autoclave. The CO2 gas stream, simulating the oxyfuel flue gas with varying concentration of impurities (SO2 and O2), was then pumped into the autoclave to observe the condensation and corrosion impacts of impurities. Comparable exposure tests were carried out with the same gas mixture and the same volume of water as vapor to observe the drop formation and the corrosion process that follows. The wettability and stability of drops on the surface of steel coupons in CO2 supercritical/dense phase environment was evaluated additionally by contact angle measurement.