Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Dokumenttyp
- Zeitschriftenartikel (12)
- Vortrag (4)
- Forschungsdatensatz (3)
- Beitrag zu einem Tagungsband (2)
- Dissertation (2)
- Posterpräsentation (1)
Schlagworte
- Aging (24) (entfernen)
Organisationseinheit der BAM
- 5 Werkstofftechnik (11)
- 5.2 Metallische Hochtemperaturwerkstoffe (9)
- 1 Analytische Chemie; Referenzmaterialien (4)
- 1.2 Biophotonik (4)
- 3 Gefahrgutumschließungen; Energiespeicher (4)
- 6 Materialchemie (4)
- 3.4 Sicherheit von Lagerbehältern (3)
- 9 Komponentensicherheit (3)
- 5.1 Mikrostruktur Design und Degradation (2)
- 6.1 Oberflächen- und Dünnschichtanalyse (2)
Eingeladener Vortrag
- nein (4)
In the past two decades, numerous relaxation or physical aging experiments of metallic glasses have revealed signatures of intermittent atomic-scale processes. Revealed via intensity cross-correlations from coherent scattering using X-ray photon correlation spectroscopy (XPCS), the observed abrupt changes in the time-domain of atomic motion does not fit the picture of gradual slowing down of relaxation times and their origin continues to remain unclear. Using a binary Lennard-Jones model glass subjected to microsecond-long isotherms, we show here that temporally and spatially heterogeneous atomic-cluster activity at different length-scales drive the emergence of highly non-monotonous intensity cross-correlations. The simulated XPCS experiments reveal a variety of time-dependent intensity-cross correlations that, depending on both the structural evolution and the 𝑞-space sampling, give detailed insights into the possible structural origins of intermittent aging measured with XPCS.
The article covers data on the Brinell hardness of the forged precipitation-hardened aluminum alloy EN AW-2618A in the initial T61 condition (i. e. slightly underaged) and after isothermal aging for up to 25,0 0 0 h at aging temperatures between 160 °C and 350 °C. In addition, the hardness was determined on specimens after creep testing at 190 °C and various stresses. The hardness decreases with increasing ag- ing time due to the microstructural evolution of the harden- ing precipitates. The drop occurs faster the higher the aging temperature. Aging under creep load additionally accelerates the hardness decrease.
Fatigue tests were performed on the forged aluminum alloy EN AW-2618A in the T61 state. Different stress ratios (R = -1, R = 0.1) were selected to study the influence of mean stress on fatigue life. Two overaged states (10 h/230 ◦C, 1000 h/230 ◦C) were also tested to investigate the influence of overaging on fatigue life. Transmission electron microscopy (TEM) was used to characterize the precipitates (S-phase), which are mainly responsible for the strength of the alloy. A fractographic analysis was also performed to determine the failure mode. Overaging reduces the fatigue life compared to the T61 state. The longer the aging time, the lower the fatigue resistance. The reason is the decrease in (yield) strength, which correlates with the radius of the S-phase: the precipitate radius increases by a factor of approximately two for the overaged states compared to the initial state. The analysis of the fracture surfaces showed crack initiation occurs predominantly on the outer surface and is
associated with the primary phases.
The mechanical strength of wrought high-strength aluminum alloys is essentially based on precipitation hardening, possibly in combination with prior forming, e. g. by stretching. Important parameters for achieving an optimum combination of hardness, strength, ductility, toughness, and further properties such as corrosion resistance are age-hardening temperature and time.
During thermal (mechanical) treatment, nucleation and growth of precipitates takes place, leading to the desired degree of hardening. In aluminum alloys, precipitation sequences are usually passed through, i. e. a sequence of metastable precipitates is formed before the stable phase can precipitate. The optimum combination of properties is therefore based on a certain (optimum) microstructure, which can, however, change during the use of a component, since the microstructure is not stable. This happens in particular when the operating temperatures are close to the aging temperature and/or the operating times are sufficiently long. An external mechanical load may accelerate the processes. The presentation gives some examples for this.
Elastomer seals are mounted as barrier seals in lid systems of containers designed for transport and disposal of negligible heat generating radioactive waste and as auxiliary seals in spent fuel storage and transportation casks (dual purpose casks (DPC)). When the behavior of mounted seals under normal and hypothetical accident conditions of disposal and transport is to be simulated, a comprehensive knowledge of their complex mechanical properties at every state of aging is necessary. In previous works, BAM’s efforts in experimental investigations on specimen artificially aged at different temperatures and times and the implementation of the found results in finite element material models were presented. Additionally, our approaches to reproduce the aging process itself and to extrapolate the results of artificially accelerated aging to longer times were presented. Numerical simulations have shown that the behavior of the seal during mounting and one-sided pressurizing and the resulting performance values such as leakage rate strongly depend on the coefficient of friction (COF) between flange and seal. The friction coefficient, in turn, depends on the aging state of the elastomer material as several publications suggest (see below).
Dynamic COF between an exemplary ethylene propylene diene rubber (EPDM) material and a stainless steel ball were determined by using a self-designed linear oscillation tribometer. Unaged and artificially aged EPDM specimen stored for 30 days and 100 days at a temperature of 150 °C were tested. A stainless steel ball (d=10 mm) is brought in contact with the specimen’s surface und loaded by normal forces of 2.5 N, 5 N, 10 N and 20 N. During a reciprocating movement of the EPDM sheet, the horizontal force/friction force is continuously measured, and the COF can be derived.
It is well known that friction is a complex phenomenon especially in soft materials. It cannot be excluded that the measured friction force is influenced by additional force components, resulting from the ball’s grooving through the elastomer’s surface. This force depends on the penetration depth of the ball and on the resistance of the elastomer in its different states of aging. The latter results from microstructural changes i.e., chain scission and additional crosslinking that occur during aging which in turn influence the softening or hardening of the material.
A finite element (FE) ABAQUS® model was developed to reproduce the measurement process. It should help to better understand the physical mechanisms and to quantify the percentage of measured forces resulting from real friction on the one hand and forces resulting from unintended side effects that could falsify the result on the other hand. The behavior of the elastomer in its different states of aging is reproduced by a FE material model already presented in previous works of BAM.
Elastomer seals are mounted as barrier seals in lid systems of containers designed for transport and disposal of negligible heat generating radioactive waste and as auxiliary seals in spent fuel storage and transportation casks (dual purpose casks (DPC)). When the behavior of mounted seals under normal and hypothetical accident conditions of disposal and transport is to be simulated, a comprehensive knowledge of their complex mechanical properties at every state of aging is necessary. In previous works, BAM’s efforts in experimental investigations on specimen artificially aged at different temperatures and times and the implementation of the found results in finite element material models were presented. Additionally, our approaches to reproduce the aging process itself and to extrapolate the results of artificially accelerated aging to longer times were presented. Numerical simulations have shown that the behavior of the seal during mounting and one-sided pressurizing and the resulting performance values such as leakage rate strongly depend on the coefficient of friction (COF) between flange and seal. The friction coefficient, in turn, depends on the aging state of the elastomer material as several publications suggest (see below).
Dynamic COF between an exemplary ethylene propylene diene rubber (EPDM) material and a stainless steel ball were determined by using a self-designed linear oscillation tribometer. Unaged and artificially aged EPDM specimen stored for 30 days and 100 days at a temperature of 150 °C were tested. A stainless steel ball (d=10 mm) is brought in contact with the specimen’s surface und loaded by normal forces of 2.5 N, 5 N, 10 N and 20 N. During a reciprocating movement of the EPDM sheet, the horizontal force/friction force is continuously measured, and the COF can be derived.
It is well known that friction is a complex phenomenon especially in soft materials. It cannot be excluded that the measured friction force is influenced by additional force components, resulting from the ball’s grooving through the elastomer’s surface. This force depends on the penetration depth of the ball and on the resistance of the elastomer in its different states of aging. The latter results from microstructural changes i.e., chain scission and additional crosslinking that occur during aging which in turn influence the softening or hardening of the material.
A finite element (FE) ABAQUS® model was developed to reproduce the measurement process. It should help to better understand the physical mechanisms and to quantify the percentage of measured forces resulting from real friction on the one hand and forces resulting from unintended side effects that could falsify the result on the other hand. The behavior of the elastomer in its different states of aging is reproduced by a FE material model already presented in previous works of BAM.
It is common practice in the application of finite element analysis to model compression set (CS) of elastomers during aging with two different material models according to the two-network theory of Tobolsky. The theory relies on the existence of two networks. The first one represents the original network after vulcanization and is sensitive to chain scission. The second network accounts for the formation of additional crosslinking during aging. Besides the use of user subroutines to describe the two-network model, an element overlay technique is also needed as the full set of both material behaviors did not exist for assignment to a single element. This element overlay technique is valuable for research and developmental purposes but makes extension to industrial usage quite challenging. Our goal is to simulate the CS of elastomers after long-term aging in a commercial finite element software with no need for extra subroutine codes or mesh superposition.
Ethylene propylene diene (EPDM) O-rings were aged in a compressed state at 75 °C, 100 °C, 125 °C and 150 °C for up to 183 days. Investigations of the experimental test results were used to identify material models and their parameters to develop a finite element model to simulate CS. The model was implemented in the finite element software ABAQUS/Standard® with a sequential temperature-displacement coupling.
Regarding the influence of temperature, the Arrhenius equation is adopted for the time-temperature relationship. The activation energy value that is required for the simulation is firstly determined from shifting the experimental CS results with the time-temperature superposition technique and plotting the shift factors in an Arrhenius diagram. The experiments were compared with the simulation results. Afterwards different activation energies were used in the simulation and discussed. A suitable choice of the activation energy value with regard to the reference temperature and the test temperature is presented. With the chosen activation energies, the match between numerical CS values after long-term aging and the experimental results was improved.
Fluorescent semiconductor nanocrystals, also known as quantum dots (QDs), enabled many advancements in biotechnology, photovoltaics, photocatalysis, quantum computing and display devices. The high versatility of this nanomaterial is based on their unique size-tunable photoluminescence properties, which can be adjusted from the visible to the near-infrared range. In contrast to other nanomaterials, QDs made the transition from a laboratory curiosity to the utilization in commercial products, like the QLED television screen or in smartphone displays. The best investigated QDs are composed of heavy metals like cadmium or lead, which is not the best choice in terms of toxicity and environmental pollution. A more promising material is Indium Phosphide (InP), which is also currently used by Samsung, Sony and co. in the QLED displays.
In this contribution, I would like to give you a sneak peek behind the curtains of nanomaterial synthesis and show how this material is produced, how to stabilize their structural properties, and assess their toxicity in environmentally relevant conditions. Furthermore, I would like to present a synthesis method to accomplish the last open challenge in display technology of a blue luminescent LED based on QDs by introducing a new element to the InP QDs.
During the service life of structural sealant glazing (SSG) facades, the loadbearing capacity of the silicone bonds needs to be guaranteed. Laboratory Tests can assess the durability of SSG-systems based on mechanical characteristics of the bond after simultaneous exposure to both climatic and mechanical loads.
This article studies how the material characteristics of two common structural sealants are affected by laboratory and field exposure. Dynamic mechanical Analysis (DMA) confirms a reduction in the dynamic modulus of exposed Silicone samples. Results from thermogravimetric analysis, Fourier-transform infrared spectroscopy, differential scanning calorimetry, and small-angle X-ray scattering/wide-angle X-ray scattering show differences between the two sealants and indicate no/minor changes in the composition and morphology of the laboratory and field exposed sealants. Mechanical characterization methods, such as DMA, and tensile and shear testing of the structural bond, are shown to be sensitive toward the combined climatic and mechanical loadings, and are hence suitable for studying degradation mechanisms of structural sealants.
The use of inorganic lanthanide-doped upconversion nanoparticles (UCNP) in bioimaging and cellular studies requires biocompatible particles. One possible cause of UCNP toxicity is the release of potentially harmful fluoride and lanthanide ions as revealed by dilution studies in aqueous environments, particularly under high dilution conditions. To address this issue, suitable surface coatings preventing such effects in combination with fast screening methods suited for online monitoring and in situ analyses are desired.
Here we present systematic studies of differently sized β-NaYF4:Yb,Er UCNP stabilized with different surface coatings and hydrophilic ligands varying in binding strength to the particle surface in various aqueous environments at different temperatures and UCNP concentrations. The concentration of the fluoride and lanthanide ions released upon particle dissolution was quantified electrochemically with a fluoride ion-sensitive electrode and inductively coupled plasma optical emission spectrometry (ICP-OES) and monitored fluorometrically, thereby exploiting the sensitivity of the upconversion luminescence to changes in size and surface chemistry. Moreover, changes in surface chemistry were determined with X-Ray photoelectron spectroscopy (XPS). Based upon our results, we could derive optimum screening parameters for UCNP stability studies and determine conditions and coating procedures and ligands for enhancing UCNP stability in aqueous environments.
Molten salt containing systems gain in importance for sustainable energy use and production. For research and development, interactions of molten salts with potential container materials are of major interest. This article introduces preparation procedures to display an intact metal and salt microstructure and their interface using light optical microscopy and scanning electron microscopy. The exemplary material combination is the ternary salt mixture NaCl-KCl-MgCl2 and the low alloyed steel 1.4901 (T92) with a maximum service temperature of 550 °C. These are potential elements/materials for use in latent heat thermal energy storages.
Simulation of the θ′ Precipitation Process with Interfacial Anisotropy Effects in Al-Cu Alloys
(2021)
The effects of anisotropic interfacial properties and heterogeneous elasticity on the growth and ripening of plate-like θ′-phase (Al2Cu) in Al-1.69 at.% Cu alloy are studied. Multi-phase-field simulations are conducted and discussed in comparison with aging experiments. The precipitate/matrix interface is considered to be anisotropic in terms of its energy and mobility. We find that the additional incorporation of an anisotropic interfacial mobility in conjunction with the elastic anisotropy result in substantially larger aspect ratios of the precipitates closer to the experimental observations. The anisotropy of the interfacial energy shows comparably small effect on the precipitate’s aspect ratio but changes the interface’s shape at the rim. The effect of the chemo-mechanical coupling, i.e., the composition dependence of the elastic constants, is studied as well. We show that the inverse ripening phenomenon, recently evidenced for δ’ precipitates in Al-Li alloys (Park et al. Sci. Rep. 2019, 9, 3981), does not establish for the θ′ precipitates. This is because of the anisotropic stress fields built around the θ′ precipitates, stemming from the precipitate’s shape and the interaction among different variants of the θ′ precipitate, that disturb the chemo-mechanical effects. These results show that the chemo-mechanical effects on the precipitation ripening strongly depend on the degree of sphericity and elastic isotropy of the precipitate and matrix phases.
Long-time behavior of surface properties of microstructures fabricated by multiphoton lithography
(2021)
The multiphoton lithography (MPL) technique represents the future of 3D microprinting, enabling the production of complex microscale objects with high precision. Although the MPL fabrication parameters are widely evaluated and discussed, not much attention has been given to the microscopic properties of 3D objects with respect to their surface properties and time-dependent stability. These properties are of crucial importance when it comes to the safe and durable use of these structures in biomedical applications. In this work, we investigate the surface properties of the MPL-produced SZ2080 polymeric microstructures with regard to the physical aging processes during the post-production stage. The influence of aging on the polymeric microstructures was investigated by means of Atomic Force Microscopy (AFM) and X-ray Photoelectron Spectroscopy (XPS). As a result, a time-dependent change in Young’s Modulus, plastic deformation, and adhesion and their correlation to the development in chemical composition of the surface of MPL-microstructures are evaluated. The results presented here are valuable for the application of MPL-fabricated 3D objects in general, but especially in medical technology as they give detailed information of the physical and chemical time-dependent dynamic behavior of MPL-printed surfaces and thus their suitability and performance in biological systems.
We studied the dissolution behavior of β NaYF4:Yb(20%), Er(2%) UCNP of two different sizes in biologically relevant media i.e., water (neutral pH), phosphate buffered saline (PBS), and Dulbecco’s modified Eagle medium (DMEM) at different temperatures and particle concentrations. Special emphasis was dedicated to assess the influence of different surface functionalizations, particularly the potential of mesoporous and microporous silica shells of different thicknesses for UCNP stabilization and protection. Dissolution was quantified electrochemically using a fluoride ion selective electrode (ISE) and by inductively coupled plasma optical emission spectrometry (ICP OES). In addition, dissolution was monitored fluorometrically. These experiments revealed that a thick microporous silica shell drastically decreased dissolution. Our results also underline the critical influence of the chemical composition of the aqueous environment on UCNP dissolution. In DMEM, we observed the formation of a layer of adsorbed molecules on the UCNP surface that protected the UCNP from dissolution and enhanced their fluorescence. Examination of this layer by X ray photoelectron spectroscopy (XPS) and mass spectrometry (MS) suggested that mainly phenylalanine, lysine, and glucose are adsorbed from DMEM. These findings should be considered in the future for cellular toxicity studies with UCNP and other nanoparticles and the design of new biocompatible surface coatings.
We demonstrate the potential of time-resolved luminescence spectroscopy for the straightforward assessment and in situ monitoring of the stability of upconversion nanocrystals (UCNPs). Therefore, we prepared hexagonal NaYF4:Yb3+,Er3+ UCNPs with various coatings with a focus on phosphonate ligands of different valency, using different ligand exchange procedures, and studied their dissolution behaviour in phosphate-buffered saline (PBS) dispersions at 20 °C and 37 °C with various analytical methods. The amount of the released UCNPs constituting fluoride ions was quantified by potentiometry using a Fluoride ion-sensitive electrode and particle disintegration was confirmed by transmission electron microscopy studies of the differently aged UCNPs. In parallel, the luminescence features of the UCNPs were measured with special emphasis on the lifetime of the sensitizer emission to demonstrate its suitability as Screening parameter for UCNP stability and changes in particle composition. The excellent correlation between the changes in luminescence lifetime and fluoride concentration highlights the potential of our luminescence lifetime method for UCNP stability screening and thereby indirect monitoring of the release of potentially hazardous fluoride ions during uptake and dissolution in biological systems. Additionally, the developed in situ optical method was used to distinguish the dissolution dynamics of differently sized and differently coated UCNPs.
Bei der Auslegung von Druckbehältern kommen, auf Grund ihrer hohen spezifischen Festigkeit, vermehrt Faserverbundwerkstoffe zum Einsatz. Durch eine hohe Streuung von Material- und Produktionsparametern sowie unterschiedlichster Belastungsszenarien gestaltet sich jedoch Aussagen über die Lebensdauer sowie eine Festlegung sinnvoller Prüffristen als schwierig. Im Fokus der Untersuchungen steht ein Behälterdesign mit metallischem Liner und einem kohlenstofffaserverstärkten Kunststoffverbund, wobei die Lebensdauer maßgeblich durch den im Metall vorherrschenden Eigenspannungszustand bestimmt wird. Mit Hilfe einer alterungsbegleitenden Eigenspannungsanalyse werden Eigenspannungsveränderungen erfasst und in einem erarbeiteten Betriebsfestigkeitsmodell berücksichtigt. Durch eine Nachstellung verschiedener Belastungsszenarien kann gezeigt werden, dass durch die Berücksichtigung einer veränderlichen Eigenspannung die Anzahl ertragbarer Lastwechsel bis zum Versagen sowie damit verbundene Überlebenswahrscheinlichkeiten mit einer erhöhten Genauigkeit abgeschätzt werden können.
A study was made on the effect of creep loading on the precipitate radii evolution of the aluminum alloy 2618A.
The overageing process of the alloy was investigated under load at a temperature of 190 °C with stresses between 79 and 181 MPa and compared to stress free isothermal ageing. The precipitates responsible for strength were characterized using dark-field transmission electron microscopy (DFTEM). This allows the experimental Determination of radii distributions of the rod-shaped Al2CuMg precipitates and the evaluation regarding their mean precipitate radius. It was found that the mean precipitate radius enables the comparison of the different microstructural conditions of crept and uncrept samples. The mean precipitate radii of the samples experiencing creep are significantly higher than those of undeformed samples. It was shown that the acquired radii distributions are viable to determine averaged particle radii for comparison of the aged samples. A ripening process including pipe diffusion along dislocations describes the data on coarsening very well for the creep samples.
Materials subjected to high-temperature service conditions will change their microstructure with time. Associated with this aging process is a change of mechanical properties as well as a change of damage mechanisms. Within the scope of the FVV project Aging and Lifetime, Fraunhofer IWM in Freiburg and BAM in Berlin (both Germany) experimentally characterized the widespread high-temperature aluminum alloy EN AW-2618A in different overaging states. Based on the experimental findings, models for numerical lifetime assessment with the finite-element method were implemented.
Für Anwendungen, bei denen Elastomerdichtungen ihre Dichtheit über sehr lange Zeiträume (z. B. Jahrzehnte) behalten müssen, ohne dass ein Austausch praktikabel wäre, ist es nötig, die Lebensdauer solcher Dichtungen zuverlässig bestimmen zu können. Aus diesem Grund wurden Alterungsversuche an O-Ring-Dichtungen sowie Flachproben auf Basis von hydriertem Acrylnitril-Butadien-Kautschuk (HNBR), Ethylen-Propylen-Dien-Kautschuk (EPDM) und Fluorkautschuk (FKM) über bis zu zwei Jahre bei mehreren Temperaturen durchgeführt. Zur Untersuchung der auftretenden Eigenschaftsveränderungen wurden u. a. Härtemessungen, Zugversuche, dynamisch-mechanische und thermogravimetrische Analysen durchgeführt. Zur Beurteilung des Relaxations- und Rückstellverhaltens der alternden Dichtungen wurden außerdem Druckspannungsrelaxations- und Druckverformungsrestmessungen durchgeführt. Darüber hinaus wurde die Leckagerate gemessen, um ein Versagen der Dichtung zu detektieren. Durch die Untersuchung der gealterten Proben wurden sowohl die auftretenden Eigenschaftsveränderungen charakterisiert wie auch die damit zusammenhängenden Alterungsmechanismen diskutiert. Anhand der großen Datenmenge aus Ergebnissen von verschiedenen Untersuchungsmethoden, die für mehrere Alterungszeiten und -temperaturen durchgeführt wurden, sollte zusätzlich die günstigste Vorgehensweise für Lebensdauervorhersagen ermittelt werden. Dies beinhaltete auch die Bestimmung eines Lebensdauerkriteriums, das mit dem Auftreten von Leckage und damit dem Versagen der Dichtung zusammenhängt. Hinsichtlich der Eigenschaftsänderungen und Alterungsmechanismen wurde beim HNBR eine starke Versprödung aufgrund dominanter Vernetzungsreaktionen während der Alterung festgestellt. Diese resultierten auch darin, dass die Sauerstoffpermeabilität abnahm, so dass der Sauerstofftransport ins Innere der Probe (hauptsächlich bei den dickeren O-Ringen) behindert wurde. Dies führte dazu, dass diffusionsbegrenzte Oxidationseffekte (DLO-Effekte) auftraten, d. h. dass das Probeninnere weniger stark alterte als oberflächennahe Bereiche. Während der Alterung von EPDM traten sowohl Kettenspaltungen wie auch Vernetzungsreaktionen auf, was sich vor allem in einer Verschlechterung der Zugeigenschaften und einer Abnahme der Druckkraft sowie in einem steigenden Druckverformungsrest äußerte. Bei sehr stark gealterten Proben dominierten ebenfalls Vernetzungsreaktionen, was sich auch in deutlichen DLO-Effekten äußerte. Aufgrund seiner ausgeprägten Oxidations- und Hochtemperaturbeständigkeit wies FKM vergleichsweise geringe Degradationserscheinungen auf. Nur mit Druckspannungsrelaxation und Druckverformungsrest waren nennenswerte Änderungen ersichtlich. Messungen der statischen Leckagerate ergaben, dass die O-Ringe erst bei sehr weit fortgeschrittener Degradation undicht wurden und bis zu diesem Zeitpunkt kein allmählicher Anstieg der Leckagerate beobachtet werden konnte. Aus diesem Grund wurden Leckagemessungen mit einem modifizierten Versuchsaufbau durchgeführt, bei dem die Dichtung während der Messung leicht entlastet wird. Da dieser Test eine dynamische Rückstellung der Dichtung erfordert und damit höhere Ansprüche an die Dichtung stellt, wurde am geprüften EPDM-O-Ring ein früheres Versagen beobachtet. Der entsprechende Alterungszeitpunkt wurde als Versagenszeitpunkt definiert. Dieser wurde anhand der Daten verschiedener Messmethoden mit dem Degradationszustand korreliert und entspricht beispielsweise einem Druckverformungsrest von 80 %. Auf der Grundlage dieses Kriteriums konnten Lebensdauern mittels Zeit-Temperatur-Verschiebung bestimmt werden. Im Rahmen dieser Arbeit wurden zahlreiche Erkenntnisse darüber gewonnen, worauf bei beschleunigten Alterungsversuchen und Lebensdauerprognosen von O-Ringen zu achten ist und welche Fehlerquellen vermieden werden sollten. Dies wird zusammen mit Empfehlungen für eine bestmögliche Versuchsdurchführung ausführlich diskutiert.
HNBR, EPDM and FKM O-rings were aged uncompressed and compressed at 75 °C, 100 °C, 125 °C and 150 °C for up to 1 year. HNBR exhibited the strongest ageing effects with high increases of hardness and glass transition temperature. Furthermore, heterogeneous ageing caused by diffusion-limited oxidation effects had a significant influence for HNBR at ageing temperatures of 125 °C and 150 °C. EPDM showed similar property changes as HNBR, but less pronounced. FKM displayed only minor ageing effects. O-rings aged in compression exhibited considerable compression set (CS). CS data was used for a time-temperature shift and resulting master curve construction. Leakage rate measurements showed that O-rings can remain leak tight under static conditions even if material properties have already deteriorated strongly.