It is well known that cement manufacture, including CaCO3 calcination and clinker formation, is associated with substantial energy consumption and significant greenhouse gas emissions. Alkali-activated binders (AAB) and concretes made from them can significantly contribute to reducing CO2 emissions caused by the construction industry. However, to what extent and for how long concretes made from AAB can protect the steel in reinforced concrete components from corrosion is still unclear. Unlike PC-based binders, AABs are made by reacting alkaline solutions with solid precursors such as fly ash and ground granulated blast furnace slag (GGBFS). Therefore, steel reinforcement corrosion mechanisms in AAMs differ from PC-based binders. The present study aims to evaluate the corrosion behavior of steel rebar in alkali-activated materials (AAMs) synthetic pore solution with different chemical concentrations representing different GGBFS and Flay Ash based binders by performing electrochemical tests to measure the corrosion rate and corrosion potential of steel rebar. This information can be used to improve the design of AAMs in order to ensure a longer service life for these materials.
In the late 1980s, a new type of corrosion appeared in drinking water installations where galvanized steel pipes failed forming a deep groove with no corrosion at the other surfaces. The reason was discussed quite fiercely between failure analysts and material suppliers. In the end the discussion lead to the solution: inductive welded pipes of a certain sulphur content were prone to selective corrosion. The history of the arguments is discussed using old communications between Wilhelm Schwenk and Wolfgang Stichel, who later published the results in a paper unfortunately only I german.
Thus the knowledge got lost and new cases based on the same material problems are observed in application of so-called C-Steel piping systems. Failure cases are shown.
Significant Cu-deposition and precipitation only occurred in combination with carbon steel. High-alloyed materials prevent the disturbing Cu-agglomeration. Pb-deposition and precipitation only occurred in combination with carbon steel. No negative Pb-effect could be observed in combination with high-alloyed steels. High alloyed corrosion resistant alloys are suitable and shall be chosen for future design of the piping system, either in massive or in cladded form, to prevent unwanted interactions with brine components.
The screening of coatings shows that the modification by adding individual pigment was not sufficient to protect carbon steel even during a short-term exposure, indicated by the discoloration after only seven days of exposure.
Electrochemical tests indicated that the coating cathodically protects carbon steel or slows down the corrosion reaction.
A long-term exposure test confirmed that the PANI/SiO2 modified coating successfully protects the carbon steel in the Sibayak artificial geothermal water at 150 °C for 6 months.
Significant Cu-deposition and ‑precipitation only occurred in combination with carbon steel. High-alloyed materials prevent the disturbing Cu-agglomeration. Pb-deposition and ‑precipitation only occurred in combination with carbon steel. No negative Pb-effect could be observed in combination with high-alloyed steels. High alloyed corrosion resistant alloys are suitable and shall be chosen for future design of the piping system, either in massive or in cladded form, if formation of crevices with non-metallic materials can be excluded!
The presentation shows systematic investigations to describe the corrosion and corrosion product formation processes of pure zinc under the climatic conditions currently prevailing in the Federal Republic of Germany. The investigations in their entirety aim at questioning current and establishing new ways of looking at the formation of corrosion products of pure zinc under atmospheric corrosion conditions. Thus, they make a significant contribution in understanding corrosion protection by zinc and zinc coatings. In particular, the focus is placed on the initial stage of the corrosion product formation. A systematic investigation of this time range, which is characterized by very reactive corrosion products, is only made possible by using gel-type electrolytes. The short periods of time at the beginning of weathering is now measurable and their influence on the formation of corrosion products and the kinetics of layer formation describable. By combining the new electrochemical approach with gravimetric, microscopic and analytical methods, new insights could be gained both on a methodic and scientific level.
Commercially available carbon steels are suitable for compression and pipelines as long as moisture content and impurities are limited. (water 50 to 100 ppmv, SO2 and NO2 ca. 100 ppmv) Corrosion rates increase with increasing water content. (0.2 – 20 mm/a) Condensation of acids and therefore droplet formation is always possible, even at low water contents. A low SO2 content within the CO2-stream might be more important than a low water content. Cr13-steels showed a general susceptibility to shallow pitting and pitting. So, they seem to be not suitable for CCUS applications. Low alloyed steels showed better corrosion behavior (predictable uniform corrosion). For direct contact with saline aquifer fluids only high alloyed steels shall be used.
Evaluation of corrosion resistance of metallic materials is essential to assure safe and reliable operation of geothermal sites. One need to be aware that corrosion is not a material's but a system property, determined by medium, material and construction aspects. Various corrosion types have to be evaluated. Conditions in laboratory shall reflect on-site reality. Depending on brine composition and temperature suitability of metallic materials can be ranked. Most important outcome of the research is that highly saline geothermal brines require high alloyed materials, for safe long-term operation.
Integrated Coating System for Corrosion Protection of Carbon Steel in Artificial Geothermal Brine
(2022)
Corrosive geothermal brines are a major challenge to geothermal power-plants. For cost reasons, plant designers prefer to use carbon and low alloyed steels, which are susceptible to uniform and localized corrosion when exposed to geothermal brines having acidic and saline properties. To solve such problem, coatings or inhibitors would be a protective solution as an alternative to the use of high alloyed materials.
This study investigated a coating system consisting of polyaniline/silicon dioxide based on resources locally available in Indonesia. Protection against corrosion of carbon steel was shown by long-term (28 day) exposure and electrochemical tests of coated carbon steels, performed in an artificial acidic and saline geothermal brine, comparable to the conditions encountered at a site in Indonesia.
Therefore, an integrated coating system is proposed for corrosion protection, combining the electrochemical functionality of polyaniline and the physical advantages of silica.