Roaldite – Fe4N – has been identified in the São Julião de Moreira iron meteorite using electron backscatter diffraction (EBSD) and simultaneously acquired energy-dispersive x-ray spectroscopy (EDS). Mean-periodic-number images derived from raw EBSD patterns confirm this phase by an even higher spatial resolution compared to EDS.
Roaldite appears in the form of systematically and repetitively aligned plates. Despite the locally heavy plastic deformation, it is shown that the origin of the oriented precipitation of roaldite is linked to the orientation of the kamacite matrix. Roaldite can be considered to be precipitated from kamacite using an inverse Kurdjumov-Sachs (K-S) or Nishiyama-Wassermann (N-W) orientation relationship. A more accurate discrimination is impossible due to the accumulated shock deformation, which blurs the local reference orientation of kamacite. The habit plane of roaldite is found to be {112}R, which is most likely parallel to {120}K of kamacite. Some of the roaldite plates contain two orientation variants which repeatedly alternate. Their misorientation angle is about 12°.
Electron backscatter diffraction (EBSD) and scanning electron microscopy were combined to study the effect of residual defect density on corrosion initiation in aluminium alloy AA2024-T3. EBSD was used to determine the level of misorientation (MO), from pixel to pixel, within individual grains. The MO can be determined with respect to either the average orientation angle of the grain or with respect to the average orientation angle of the surrounding pixels (in this instance, a matrix of 7×7 surrounding pixels has been applied). Herein, the MO, determined using the surrounding pixels, was used as the means for the assessing the level of defect density within a grain. It was found that there was a noteworthy, but not definitive, correlation of MO with corrosion initiation after 1 min exposure to 0.1 M NaCl solution. Additionally, the S and θ-phase particles were also identified using EBSD, displaying a range of MO and therefore defect density.