Due to the rapid thermal cycles involved in additive manufacturing of metals, high internal stresses and peculiar microstructures occur, which influence the parts mechanical properties. To systematically examine their formation, in-process measurements of the temperature are needed. Since the part emissivity is strongly inhomogeneous and rapidly changing in the process, the applicability of thermography for the determination of thermodynamic temperatures is limited. Measuring the thermal radiation in different wavelengths simultaneously, temperature and emissivity can be separated. Here, we present results of a preliminary study using multispectral thermography to obtain real temperatures and emissivities in directed energy deposition (DED) processes.
Rapid localized heating and cooling during additive manufacturing using laser deposition method (LMD) lead to loss of dimensional accuracy as well as cracking of built parts. Finite-Element welding simulations allow prediction of geometrical deviations and accumulated residual stresses as well as their optimization before conducting experiments. Due to the great length of stacked welds, calculation times for fully transient thermomechanical simulations are currently long, the calculation stability suffers from the high number of contact bodies in the model and the modelling effort is high, as the geometries need to be sliced and positioned layer-wise.
In this contribution, an integrated modelling approach is demonstrated for a thin-walled LMD component made from 30 layers of 1.4404 (316L) stainless steel: Instead of the layer-by-layer modelling strategy commonly found in the literature, the whole component mesh is kept in one piece and the fully transient, layer-by-layer material deposition is implemented via element sets. In contrast to prior simulations, nonlinear contact between the layers does not have to be considered, significantly decreasing calculation times. The calculated distortions are compared to recently published, in-situ digital image correlation (DIC) measurements as well as numerical simulations conducted with the established layer-wise modelling strategy to judge result quality. Finally, the improvement in calculation time and ease-of-use is compared between both modelling approaches and conclusions regarding future usage for industrial-scale components are drawn.
Funktional gradierte Materialien auf Basis von Stellite und Stahl im Laserpulver-Auftragschweißen
(2022)
Das Hinzufügen von Stellite auf Stahl ist eine typische Vorgehensweise um Bauteile gegen Verschleiß und Korrosion zu schützen. Der Sprung in den Materialeigenschaften kann jedoch zu Rissen und somit zum Versagen der Beschichtung führen. Um die Lebensdauer von Beschichtungen zu erhöhen wird daher ein gradierter Übergang mit verschiedenen Materialpaarungen untersucht.
Um Bauteile vor Verschleiß und Korrosion zu schützen werden Beschichtungen aus resistenteren Materialien aufgetragen. Hierzu zählen unter anderen die Legierungen auf Cobalt-Chrom Basis. Der diskrete Materialsprung ist jedoch unter thermischen und mechanischen Belastungen häufig Ursache für das Versagen der Beschichtung. In dieser Arbeit werden daher Materialgradierungen von verschiedenen Stahllegierungen zu einer Cobalt-Chrom Basislegierung untersucht. Die Ergebnissen werden dafür auch mit Resultaten zu vorangegangenen Untersuchungen verglichen. Kern der Arbeit bilden geätzte Schliffbilder der Materialpaarungen und Auswertungen mittels Farbeindringprüfung sowie die metallografische Bestimmung der Porosität. Ziel der Arbeit ist ein defektfreier Aufbau der funktional gradierten Materialpaarungen.
Durch pulverbasiertes Directed-Energy Deposition lassen sich Gradierungen fertigen, um diskrete Materialübergänge zu vermeiden und die Lebensdauer von Hartschichten zu erhöhen. Die Kombination aus Stahl als Basiswerkstoff und einer verschleiß- und korrosionsbeständigen Co-Cr Legierung verspricht durch Vermeiden von Spannungskonzentrationen das Verhindern von Abplatzungen und Rissen in der Schutzschicht. Um die Qualität des gefertigten Bauteils zu beurteilen, liegen für solche Funktional Gradierten Materialien (FGM) wenig Erkenntnisse vor. Daher wird im Rahmen dieser Studie eine Methodik erarbeitet, um die relative Dichte eines Funktional Gradierten Materials auf Stahl und Co-Cr Basis mittels Maschinendaten zu bestimmen. Anschließend wird unter Einsatz eines künstlichen neuronalen Netzes anhand von Sensordaten die relative Dichte vorhergesagt. Das trainierte Netz erreicht eine Vorhersagegenauigkeiten von 99,83%. Abschließend wird eine Anwendung anhand von einem Demonstrator gezeigt.
Additive manufacturing promises a high potential for the maritime sector. Directed Energy Deposition (DED) in particular offers the opportunity to produce large-volume maritime components like propeller hubs or blades without the need of a costly casting process. The post processing of such components usually generates a large amount of aluminum bronze grinding waste. The aim of the presented project is to develop a sustainable circular AM process chain for maritime components by recycling aluminum bronze grinding waste to be used as raw material to manufacture ship Propellers with a laser-powder DED process. In the present paper, grinding waste is investigated using a dynamic image Analysis system and compared to commercial DED powder. To be able to compare the material quality and to verify DED process parameters, semi-academic sample geometries are manufactured.
Laser Metal Deposition (LMD) as a technology for additive manufacturing allows the production of large components outside of closed working chambers. Industrial applications require a stable process as well as a constant deposition of the filler material in order to ensure uniform volume growth and reproducible mechanical properties. This paper deals with the influence of travel path strategies on temperature profile and material deposition. Meandering and spiral hatching strategies are used in the center as well as in the edge of a specimen. The temperature is measured with thermocouples attatched to the backside of the specimen. The tests are carried out on the materials S235JR and 316L. The results show a strong dependence of the maximum temperatures on the travel path strategy and the welding position on the component.
Additive manufacturing is no longer just used for the production of prototypes but already found its way into the industrial production. However, the fabrication of massive metallic parts with high geometrical complexity is still too time-consuming to be economically viable. The combination of the powder bed-based selective laser melting process (SLM), known for its geometrical freedom and accuracy, and the nozzle-based laser metal deposition process (LMD), known for its high build-up rates, has great potential to reduce the process duration. For the industrial application of the SLM-LMD hybrid process chain it is necessary to investigate the interaction of the processes and its effect on the material properties to guarantee part quality and prevent component failure. Therefore, hybrid components are manufactured and examined before and after the heat treatment regarding the microstructure and the hardness in the SLM-LMD transition zone. The experiments are conducted using the nickel-based alloy Inconel 718.
In den letzten Jahren hat vor allem die Nachfrage nach additiven Fertigungstechnologien und Reparaturverfahren für Hochfeste Werkstoffe einen starken Aufschwung erlebt. Ein Verfahren, welches sich neben der Herstellung von Beschichtungen besonders für diese Anwendungen eignet, ist das Laser-Pulver-Auftragschweißen. Es wird besonders für Reparaturen bzw. zur Herstellung von teuren Bauteilen, wie Werkzeuge oder Turbinenteilen, eingesetzt. Da diese Teile oft großen mechanischen sowie thermischen Belastungen ausgesetzt sind, ist es besonders wichtig, dass die erzeugte Struktur eine hohe Qualität aufweist. In dieser Arbeit wird die statistische Versuchsplanung genutzt, um Modelle für die Oberflächenbeschaffenheiten von Inconel 718 zu generieren. Als Grundlage dient hierbei ein zentral zusammengesetzter Versuchsplan mit großem Parameterfenster. So wird die Leistung zwischen 550 Watt und 1950 Watt, der Vorschub von 530 mm/min bis 920 mm/min, der Pulvermassenstrom von 3 g/min bis 12 g/min sowie der Spotdurchmesser von 1 mm bis 2 mm variiert. Auf diese Weise wird die Spurgeometrie beeinflusst. Darüber hinaus wird das Überlappungsverhältnis zwischen 20% bis 50% verändert. Die Auswertung der Oberflächenbeschaffenheit erfolgt mit dem auf der Fokusvariation basierendem Oberflächenmessgerät Alicona Infinite-Focus. Dieses Verfahren der 3D Mikrokoordinatenmesstechnik gewährleistet eine zuverlässige Auswertung der Spurgeometrie, der Welligkeit sowie die Messung der mittleren arithmetischen Höhe Sa zur Bestimmung der Oberflächenrauheit. Anschließend werden die generierten Modelle verifiziert. Ziel dabei ist, kostenintensive Vorversuche in Zukunft einzusparen. Darüber hinaus wird das Prozessverständnis erweitert und signifikante Einflussfaktoren identifiziert.