This article is devoted to the study of the bulging effect in deep penetration laser beam welding. The numerical results of the investigations are based upon experimental results from previous studies to reveal the relationship between the bulging effect and the hot cracking formation, as well as the mixing of alloying elements in the weld pool. The widening of the molten pool in its center area can be observed in full penetration as well as in partial penetration welds on 8 mm and 12 mm thick structural steel plates, respectively. The weld pool shape is extracted from the simulations to evaluate the extent of the necking of the solidification line as well as the bulging phenomena and its influence on the hot cracking phenomena. Relying on an earlier numerical study utilizing a fixed keyhole, simulation models considering a dynamic keyhole are developed thereto. Additionally, the mixing behavior of alloying elements during partial penetration is investigated. The link between the bulge and the studied phenomena is found to be significant.
Components distort during directed energy deposition (DED) additive manufacturing (AM) due to the repeated localised heating. Changing the geometry in such a way that distortion causes it to assume the desired shape – a technique called distortion-compensation – is a promising method to reach geometrically accurate parts. Transient numerical simulation can be used to generate the compensated geometries and severely reduce the amount of necessary experimental trials. This publication demonstrates the simulation-based generation of a distortioncompensated DED build for an industrial-scale component. A transient thermo-mechanical approach is extended for large parts and the accuracy is demonstrated against 3d-scans. The calculated distortions are inverted to derive the compensated geometry and the distortions after a single compensation iteration are reduced by over 65%.
Distortions in Additive Manufacturing (AM) Laser Metal Deposition (LMD) occur in the newly-built component due to rapid heating and solidification and can lead to shape deviations and cracking. This paper presents a novel approach to quantify the distortions experimentally and to use the results in numerical simulation validation. Digital Image Correlation (DIC) is applied together with optical filters to measure in-situ distortions directly on a wall geometry produced with LMD. The wall shows cyclic Expansion and shrinking with the edges bending inward and the top of the sample exhibiting a slight u-shape as residual distortions. Subsequently, a structural Finite Element Analysis (FEA) of the experiment is established, calibrated against experimental temperature profiles and used to predict the in-situ distortions of the sample. A comparison of the experimental and numerical results reveals a good agreement in length direction of the sample and quantitative deviations in height direction, which are attributed to the material model used. The suitability of the novel experimental approach for measurements on an AM sample is shown and the potential for the validated numerical model as a predictive tool to reduce trial-and-error and improve part quality is evaluated.