Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2020 (22) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (19)
- Beitrag zu einem Tagungsband (2)
- Vortrag (1)
Sprache
- Englisch (22) (entfernen)
Schlagworte
- Laser beam welding (8)
- Mechanical properties (4)
- Microstructure (4)
- Additive manufacturing (3)
- Cryogenic steel (2)
- Element transport (2)
- Hybrid laser-arc welding (2)
- Laser metal deposition (2)
- Matching ferritic welding electrode (2)
- Mechanical mismatching (2)
- Numerical modelling (2)
- Numerical simulation (2)
- Welding thermal cycle (2)
- 9%Ni steel (1)
- Additive Manufacturing (1)
- Advanced high-strength steels (1)
- Artificial neural network (1)
- Austenitic welding electrode (1)
- Bulge effect (1)
- Circumferential weld (1)
- Clustering (1)
- Computer vision (1)
- Crack (1)
- DED (1)
- Deep learning (1)
- Deep penetration (1)
- Die-casted aluminum (1)
- Dimensional accuracy (1)
- Directed Energy Deposition (1)
- Directed energy deposition (1)
- Electromagnetic supported degassing (1)
- Electron beam welding (1)
- End crater (1)
- Equivalent heat source (1)
- Filler material distribution (1)
- Filler wire (1)
- Finite Element Method (1)
- Hardness (1)
- Heat Treatment (1)
- Heat input (1)
- Heat treatment (1)
- High strength steels (1)
- High-strength low-alloy steel (1)
- Hold time (1)
- Hot crack (1)
- Hot cracking (1)
- Inconel 718 (1)
- Instumented indentation test (1)
- Keyhole mode welding (1)
- LMD (1)
- Lamé curves approximation (1)
- Laser (1)
- Laser Metal Deposition; Laser Beam Welding; Duplex; Stainless Steel (1)
- Laser hybrid welding (1)
- Laser metal deposition (LMD) (1)
- Liquid metal embrittlement (1)
- Low feed rates (1)
- Magnetohydrodynamics (1)
- Mathematical modeling (1)
- Mechanical-technological properties (1)
- Molten pool dynamics (1)
- Ni-based austenitic welding electrode (1)
- Ni-based superalloy (1)
- Numerical Simulation (1)
- Numerical modeling (1)
- Partial penetration welding (1)
- Path planning (1)
- Penetration depth (1)
- Pipeline steel of grade X120 (1)
- Porosity (1)
- Preheating (1)
- Resistance spot welding (1)
- SMAW (1)
- Seam geometry (1)
- Simulation (1)
- Single-pass welding (1)
- Solidification (1)
- Solidification cracking (1)
- Steady-state weld pool (1)
- Thermal cycles (1)
- Thick-walled steel (1)
- Toughness (1)
- V-notch impact toughness (1)
- Weld end crater (1)
- Weld root (1)
- Welding simulation (1)
Organisationseinheit der BAM
- 9.3 Schweißtechnische Fertigungsverfahren (22) (entfernen)
Eingeladener Vortrag
- nein (1)
Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone.
Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness. A better combination of These mechanical properties is ensured by applying a post weld heat treatment.
Ni-based superalloys are well established in various industrial applications, because of their excellentmechanical properties and corrosion resistance at high temperatures. Despite the high development stage anda common industrial use of these alloys, hot cracking remains a major challenge limiting the weldability ofthe materials. As commonly known, the hot cracking susceptibility during welding increases with the amountof precipitation phases. Hence, a large amount of highstrength Ni-Alloys is rated as non-weldable. A newapproach based on electron beam welding at low feed rates shows great potential for reducing the hotcracking tendency of precipitation-hardened alloys. However, geometry and properties of the weld seamdiffer significantly in comparison to the common process range for practical uses. The aim of this study is toinvestigate the influence of welding parameters on the seam geometry at low feed rates between 1 mm/s and10 mm/s. For this purpose, 25 bead on plate welds on a 12 mm thick sheet made of Inconel 718 are carriedout. First, the relevant parameters are identified by performing a screening. Then the effects discovered arefurther studied by using a central composite design. The results show a significant difference between theanalyzed weld seam geometry in comparison to the well-known appearance of electron beam welded seams.
Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone.
Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness.Abetter combination of These mechanical properties is ensured by applying a post weld heat treatment.
Notch impact toughness of laser beam welded thick sheets of cryogenic nickel alloyed steel X8Ni9
(2020)
This research work deals with the investigations of the impact toughness of laser beam welded 14.5 mm thick sheets made of cryogenic steel X8Ni9 as a function of preheating. This 9% nickel alloyed steel is widely used in the liquefied natural gas (LNG) industry. An application of highly efficient welding processes such as high-power laser beam welding (LBW) in LNG sector requires an understanding of the interactions between the LBW process parameters and weld properties, in particular the impact toughness. The results show that the original fine-grained martensitic microstructure of the base metal (BM) is significantly changed by melting and crystallization during the LBW, what can lead to a decrease in the impact toughness of the weld metal (WM) below the required level. An optimal preheating temperature range leads to the favorable thermal welding cycle and is of remarkable importance for maintaining the notch impact toughness of laser beam welded joints of these thick steel sheets. A parameter window was identified in which V-notch impact toughness comparable to that of the BM at -196 °C was achieved.
The transport phenomena in the wire feed laser beam welding are investigated numerically. A three-dimensional transient heat transfer and fluid flow model coupled with free surface tracing and element transport is developed. A ray-tracing method with local grid refinement algorithm is used to calculate the multiple reflections and Fresnel absorption on the keyhole wall. The filler material flows backward along the lateral side of the weld pool, and subsequently flows forward along the longitudinal plane. The occurrence of the bulging phenomenon may further prevent the downward transfer of the additional elements to the root of the weld pool.
The study deals with the application of the high-power hybrid-laser arc welding process on up to 15 mm thick pipe segments with the intention to avoid end crater imperfections during closing of the circumferential welds, where the pipes were turned during welding in 1G- and 2Gpositions.
Different techniques such as laser power ramp-down, abrupt switch-off of the laser power and change of the magnification of the laser spot diameter and defocusing of the laser beam relative to the workpiece were tested to remove the laser energy from the process. It could be shown that a high defocusing of the optic system above 40 mm with a resulting beam diameter > 2.9 mm in a short overlap length of approx.
20 mm leads to the formation of a cup-shaped weld seam, which is preferred for avoidance of cracks and pores in the end crater. A laser optics with motor-driven lens system was used for the welding experiments to defocuse the laser beam without changing the position of the arc.
Notch impact toughness of laser beam welded thick sheets of cryogenic nickel alloyed steel X8Ni9
(2020)
The paper deals with the investigations of the impact toughness of laser beam welded 14.5 mm thick sheets made of cryogenic steel X8Ni9 as a function of preheating. This 9% nickel alloyed steel is widely used in the liquefied natural gas (LNG) industry. An application of highly efficient welding processes such as high-power laser beam welding (LBW) in LNG sector requires an understanding of the interactions between the LBW process parameters and weld properties, in particular the impact toughness. The results show that the original fine-grained martensitic microstructure of the base metal (BM) is significantly changed by melting and crystallization during the LBW, what can lead to a decrease in the impact toughness of the weld metal (WM) below the required level. An optimal preheating temperature range leads to the favorable thermal welding cycle and is of remarkable importance for maintaining the notch impact toughness of laser beam welded joints of these thick steel sheets. A parameter window was identified in which V-notch impact toughness comparable to that of the BM at -196 °C was achieved.
Directed energy deposition is a metal additive manufacturing process that builds parts by joining material in a layer-by-layer fashion on a substrate. Those parts are exposed to rapid thermo-cycles which cause steep stress gradients and the layer-upon-layer manufacturing fosters an anisotropic microstructure, therefore stress relief heat treatment is necessary. The numerical simulation can be used to find suitable parameters for the heat treatment and to reduce the necessary efforts to perform an effective stress relieving. Suitable validation Experiments are necessary to verify the results of the numerical simulation.
In this paper, a 3D coupled thermo-mechanical model is used to simulate the heat treatment of an additive manufactured component to investigate the application of a C-ring geometry for the distortion-based validation of the numerical simulation.
Therefore, the C-ring samples were 3D scanned using a structured light 3D scanner to quantify the distortion after each process step.
Directed energy deposition additive manufactured parts have steep stress gradients and an anisotropic microstructure caused by the rapid thermo-cycles and the layer-upon-layer manufacturing, hence heat treatment can be used to reduce the residual stresses and to restore the microstructure. The numerical simulation is a suitable tool to determine the parameters of the heat treatment process and to reduce the necessary application efforts. The heat treatment simulation calculates the distortion and residual stresses during the process. Validation experiments are necessary to verify the simulation results. This paper presents a 3D coupled thermo-mechanical model of the heat treatment of additive components. A distortion-based validation is conducted to verify the simulation results, using a C-ring shaped specimen geometry. Therefore, the C-ring samples were 3D scanned using a structured light 3D scanner to compare the distortion of the samples with different post-processing histories.
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.