Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2020 (15) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (10)
- Beitrag zu einem Tagungsband (4)
- Vortrag (1)
Schlagworte
- Microstructure (4)
- Laser beam welding (3)
- Hybrid laser-arc welding (2)
- Laserstrahlschweißen (2)
- Matching ferritic welding electrode (2)
- Mechanical mismatching (2)
- Mechanical properties (2)
- 9%Ni steel (1)
- Additive Manufacturing (1)
- Austenitic welding electrode (1)
- Circumferential weld (1)
- Cryogenic steel (1)
- Defokussierung (1)
- Duplex (1)
- Elektromagnetische Schmelzbadunterstützung (1)
- End crater (1)
- Endkrater (1)
- Equivalent heat source (1)
- Filler material distribution (1)
- Hardness (1)
- High-strength low-alloy steel (1)
- Hybrid laser arc welding (1)
- Kaltzähe Stähle (1)
- Keyhole mode welding (1)
- LMD (1)
- Lamé curves approximation (1)
- Laser Metal Deposition; Laser Beam Welding; Duplex; Stainless Steel (1)
- Laser hybrid welding (1)
- Laser metal deposition (LMD) (1)
- Laser-Hybridschweißen (1)
- Laser-Pulver-Auftragschweißen (1)
- Laser-Pulver-Auftragschweißen; Laserstrahlschweißen, Duplex, Pufferschichten (1)
- Laserhybridschweißen (1)
- MWIR (1)
- Mechanical-technological properties (1)
- Metal (1)
- Modellierung (1)
- NIR (1)
- Ni-based austenitic welding electrode (1)
- Numerical modeling (1)
- Numerical simulation (1)
- Partial penetration welding (1)
- Penetration depth (1)
- Pipeline steel of grade X120 (1)
- Preheating (1)
- Process monitoring (1)
- Pufferschichten (1)
- Rundnaht (1)
- SMAW (1)
- SWIR (1)
- Ship building (1)
- Single-pass welding (1)
- Solidification cracking (1)
- Thermal cycles (1)
- Thermography (1)
- Thick-walled steel (1)
- Toughness (1)
- V-notch impact toughness (1)
- Weld root (1)
- Welding thermal cycle (1)
- Überlappbereich (1)
Organisationseinheit der BAM
- 9.3 Schweißtechnische Fertigungsverfahren (15) (entfernen)
Eingeladener Vortrag
- nein (1)
Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone.
Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness. A better combination of These mechanical properties is ensured by applying a post weld heat treatment.
Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone.
Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness.Abetter combination of These mechanical properties is ensured by applying a post weld heat treatment.
Bislang kommt das Laserstrahlschweißen bzw. Laserhybridschweißen hauptsächlich bei Dickblechen mit einer Wandstärke von bis zu 15 mm zum Einsatz. Für Anwendungen über 20 mm war dieses Verfahren aufgrund einiger Herausforderungen bisher nur bedingt realisierbar. Eine von der Bundesanstalt für Materialforschung und -prüfung (BAM) entwickelte elektromagnetische Schmelzbadunterstützung ermöglicht nun ein einlagiges Schweißen von bis zu 30 mm Wandstärke.
Additive manufacturing offers a range of novel applications. However, the manufacturing process is complex and the production of almost defect-free parts with high reliability and durability is still a challenge. Thermography is a valuable tool for process surveillance, especially in metal additive manufacturing processes. The high process temperatures allow one to use cameras usually operating in the visible spectral range. Here, we compare the results of measurements during the manufacturing process of a commercial laser metal deposition setup using a mid wavelength infrared camera with those from a short wavelength infrared camera and those from a visual spectrum high-speed camera with band pass filter in the near infrared range.
The study deals with the application of the high-power hybrid-laser arc welding process on up to 15 mm thick pipe segments with the intention to avoid end crater imperfections during closing of the circumferential welds, where the pipes were turned during welding in 1G- and 2Gpositions.
Different techniques such as laser power ramp-down, abrupt switch-off of the laser power and change of the magnification of the laser spot diameter and defocusing of the laser beam relative to the workpiece were tested to remove the laser energy from the process. It could be shown that a high defocusing of the optic system above 40 mm with a resulting beam diameter > 2.9 mm in a short overlap length of approx.
20 mm leads to the formation of a cup-shaped weld seam, which is preferred for avoidance of cracks and pores in the end crater. A laser optics with motor-driven lens system was used for the welding experiments to defocuse the laser beam without changing the position of the arc.
Notch impact toughness of laser beam welded thick sheets of cryogenic nickel alloyed steel X8Ni9
(2020)
The paper deals with the investigations of the impact toughness of laser beam welded 14.5 mm thick sheets made of cryogenic steel X8Ni9 as a function of preheating. This 9% nickel alloyed steel is widely used in the liquefied natural gas (LNG) industry. An application of highly efficient welding processes such as high-power laser beam welding (LBW) in LNG sector requires an understanding of the interactions between the LBW process parameters and weld properties, in particular the impact toughness. The results show that the original fine-grained martensitic microstructure of the base metal (BM) is significantly changed by melting and crystallization during the LBW, what can lead to a decrease in the impact toughness of the weld metal (WM) below the required level. An optimal preheating temperature range leads to the favorable thermal welding cycle and is of remarkable importance for maintaining the notch impact toughness of laser beam welded joints of these thick steel sheets. A parameter window was identified in which V-notch impact toughness comparable to that of the BM at -196 °C was achieved.
In diesem Beitrag werden Ergebnisse der Untersuchungen eines Verfahrens zum fehlerfreien Laserstrahl Hybridschweißen von geschlossenen Rundnähten vorgestellt. Das Verfahren zielt auf die Vermeidung von Schweißimperfektionen im Überlappbereich einer laserstrahlhybridgeschweißten Rundnaht. Eine Strategie der Prozessführung beim Schließen der Rundnaht wurde entwickelt, mit der ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG Schweißprozess realisiert. Experimentelle Untersuchungen wurden an 12 mm bis 15 mm dicken Rohrabschnitten durchgeführt. Der Einfluss von Prozessparametern wie der Laserleistungsrampe und Rampenzeit, der Veränderung des Abbildungsmaßstabes und der Defokussierung des Laserstrahls auf die Erstarrungsbedingungen am Ende der Rundnaht wurde untersucht, um eine optimale Strategie zum Herausführen der Prozessenergie zu finden. Im Rahmen der experimentellen Untersuchungen konnte gezeigt werden, dass eine Defokussierung des Laserstrahls im Bereich zwischen 60 mm und 100 mm über einen kurzen Auslaufbereich der Naht von ca. 15 mm zu einer deutlich besseren Nahtausbildung im Überlappbereich führte. Es konnte eine günstige kelchförmige Schweißnahtform ohne eine Tendenz zur Rissbildung erzielt werden. Die Laseroptik mit motorisch angesteuertem Linsensystem ermöglichte dabei eine Vergrößerung des Laserstrahldurchmessers ohne eine Veränderung der Position des MSG-Lichtbogens relativ zur Bauteiloberfläche.
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.
High power laser beam welding has been already introduced in ship building industry since last two decades and is characterized by higher performance as conventional arc welding technologies through its higher welding speed, penetration depth and therefore higher productivity. Moreover, high quality weld joints are achievable thanks to a stronger automatization degree and better repeatability of the process. A further advantage of the laser beam welding is a manufacturing of parts with very low distortion according to much lower heat input, so that rework amount can be reduced significantly. Nevertheless, there are still some unresolved problems limiting the range of application of the technology in part manufacturing within ship building industry, restricted by development and application of new materials or new design of ship vessels.
The present contribution deals with some novel aspects of laser beam welding technology allowing to widen this range significantly. One of the possibilities is to increase the weld seam thickness for single pass laser or laser-hybrid welding is to apply contactless EM-support system based on generation of the Lorentz force counteracting the liquid metal drop out. Also, application of laser-hybrid welding technology for welding novel materials like cold resistant steel X8Ni9 used for construction of LNG tanks brings technological and design advantages comparing to conventional welding technologies by using of a similar alloyed filler wire instead of expensive Ni-based filler material. Finally, it is shown how the application of computational techniques can be used to helps to improve the quality of laser welded joints and avoid the critical weld failure by optimization of the welding process parameters.
Duplexstähle finden in vielen industriellen Bereichen Anwendung, dies ist nicht zuletzt ihren hervorragenden Eigenschaften, wie einer guten Korrosionsbeständigkeit, einer guten Duktilität bei trotzdem hoher Festigkeit, zuzuschreiben. Diese Eigenschaften werden jedoch durch das Schweißen, vor allem das Laserstrahlschweißen, beeinträchtigt, da die hohen Abkühlraten zu erhöhten Ferritanteilen im Schweißgut führen. Mit Hilfe eines zweistufigen Prozesses, bei dem die Kanten der Fügepartner vor dem Schweißen mit nickelhaltigem Pulver beschichtet werden, soll dieses Problem für dickwandige Bleche gelöst werden.
In diesem Zusammenhang wurden verschiedene Prozessparameter für den Laser-Pulver-Auftragschweiß-Prozess untersucht sowie die defektfreie Schweißung dieser beschichteten Kanten mit unterschiedlichen Prozessgasen.