185 cracks were initiated in a soda-lime-silica glass by Vickers indentation and grown under controlled dry nitrogen atmosphere. Direct observation of subcritical crack growth (SCCG) upon indentation was performed using a video camera with an image acquisition rate of 3 ms. The results show that the validity of K(c) relations used to determine the indentation fracture toughness from a single imprint is questionable. It seems that correlation of crack length to stress intensity necessitate the use of statistical significant data of multiple crack events.
Um das Risswachstum in Gläsern zu untersuchen, sind in einer Glovebox 185 Risse ausgehen von Vickers-Eindrücken in Kalk-Natron-Glas initiiert und gewachsen. Die direkte Beobachtung des unterkritischen Risswachstums erfolgte mit einer Hochgeschwindigkeitskamera. Die Ergebnisse zeigen, dass die statistische Auswertung vieler radialer Risse von multiplen Rissevents notwendig ist, um eine Korrelation zum Spannungsintensitätsfaktor ziehen zu können.