The Tungsten Inert Gas (TIG) welding process was combined with a Laser-Induced Breakdown Spectroscopy (LIBS) system for the in situ measurement of chemical compositions in austenitic stainless steels. The main aim of this project was the development of a prototype for a real-time chemical composition analysis system for welding applications. In principle, the measurement of the weld pool composition allows governing the weld pool solidification behaviour by controlling the welding parameters. This control loop allows avoiding weld defects.
Chemical compositions of the weld seam is from a metallurgical point of view the most critical parameter for the occurrence of weld defects. Additionally, this new LIBS-based measurement system can be used for the monitoring and controlling of potentially dangerous emissions during the welding process in order to improve the working safety conditions. Preliminary investigations show that the chemical composition measurement of welds with LIBS is possible during and after welding.
Duplex stainless steels (DSS) are used in all industries where corrosion problems play a major role. Examples include the chemical industry, the food industry and shipping industries. DSS have a balanced phase ratio of ferrite (α) and austenite (γ). Unlike single-phase stainless steels, DSS combine the advantages of these and can therefore fit many industry requirements, such as weight saving or high mechanical strength. When these steels are welded, alloying elements can burn off and condense as thin layers on cold surface regions. This loss of chemical elements can lead to changes in the microstructure. With the help of Laser-Induced Breakdown Spectroscopy (LIBS), chemical element distributions were visualized. The results were compared with those of conventional measurement methods, such as energy dispersive X-ray analysis (EDS) and X-ray fluorescence analysis (XRF), and the results from LIBS could be validated. LIBS is suitable as a fast, straightforward measurement method for producing line scans along the weld seam and provides spatially resolved information on accumulation phenomena of burned off alloying elements. LIBS is very well suited for the detection of sub-surface elements due to the exclusively superficial ablation of the material. In addition, the measurement method has been calibrated so that quantitative statements about element concentrations can also be made.
Duplex stainless steels (DSS) are frequently used, especially in applications requiring high strength combined with high corrosion resistance in aggressive media. Examples include power plant components and maritime structures. During welding of these steels, local variations in chemical composition can occur. This results in ferritization of the material and negatively affects the mechanical properties of the components. In this work, tungsten inert gas (TIG) welding experiments were performed with DSS. Chemical composition analysis was realized in situ by using Laser Induced Breakdown Spectroscopy (LIBS). The aim of the work is to quantitatively measure the chemical composition in the weld seam of various DSS and to identify possible influences of welding parameters on the microstructure of the material. The chemical concentrations of the main alloying elements Cr, Ni, Mn on the surface of the sample during the welding process and the cooling process were measured. Mn and Ni are austenite stabilizers and their content increases during welding by using certain high alloyed filler material. Spectra were recorded every 1.3 s at a spacing of approximately 2 mm. During the cooling process the location of the measurement was not changed. The LIBS method is proofed to be suitable for the quantitative representation of the chemical compositions during the welding process.
Nichtrostende Duplexstähle (DSS) werden häufig verwendet, insbesondere bei Anwendungen, die eine hohe Festigkeit in Verbindung mit einer hohen Korrosionsbeständigkeit in aggressiven Medien erfordern. Beispiele hierfür sind Kraftwerkskomponenten und maritime Anwendungen. Beim Schweißen dieser Stähle kann es zu lokalen Schwankungen in der chemischen Zusammensetzung kommen. Dies führt zu einer Ferritisierung des Werkstoffs und beeinträchtigt die mechanischen Eigenschaften der Bauteile. In dieser Arbeit wurden Versuche zum Wolfram-Inertgas-Schweißen (WIG) mit DSS durchgeführt. Die Analyse der chemischen Zusammensetzung wurde in situ mit Hilfe der laserinduzierten Plasmaspektroskopie (LIBS) durchgeführt. Ziel der Arbeit ist es, die chemische Zusammensetzung in der Schweißnaht verschiedener DSS quantitativ zu messen und mögliche Einflüsse der Schweißparameter auf die Mikrostruktur des Werkstoffs zu ermitteln. Gemessen wurden die chemischen Konzentrationen der Hauptlegierungselemente Cr, Ni, Mn auf der Oberfläche der Probe während des Schweißprozesses und des Abkühlungsprozesses. Mn und Ni sind Austenitstabilisatoren, deren Gehalt beim Schweißen durch die Verwendung bestimmter hochlegierter Schweißzusatzwerkstoffe zunimmt. Die Spektren wurden alle 1,3 s in einem Abstand von etwa 2 mm aufgezeichnet. Während des Abkühlungsprozesses wurde der Ort der Messung nicht verändert. Die LIBS-Methode eignet sich nachweislich zur quantitativen Darstellung der chemischen Zusammensetzungen während des Schweißvorgangs.
Duplex stainless steels (DSS) are frequently used, especially in applications requiring high strength combined with high corrosion resistance in aggressive media. Examples include power plant components and maritime structures. During welding of these steels, local variations in chemical composition can occur. This results in ferritization of the material and negatively affects the mechanical properties of the components. In this work, tungsten inert gas (TIG) welding experiments were performed with DSS. Chemical composition analysis was realized in situ by using Laser Induced Breakdown Spectroscopy (LIBS). The aim of the work is to quantitatively measure the chemical composition in the weld seam of various DSS and to identify possible influences of welding parameters on the microstructure of the material. The chemical concentrations of the main alloying elements Cr, Ni, Mn on the surface of the sample during the welding process and the cooling process were measured. Mn and Ni are austenite stabilizers and their content increases during welding by using certain high alloyed filler material. Spectra were recorded every 1.3 s at a spacing of approximately 2 mm. During the cooling process the location of the measurement was not changed. The LIBS method is proofed to be suitable for the quantitative representation of the chemical compositions during the welding process.
Multiple principal element alloys encompass the well-known high entropy alloys (HEA). The alloy system represents a new class of materials consisting of at least three alloying elements, each containing 5 to 35 at.%. Thus, this alloying concept differs fundamentally from conventional materials such as steel or nickel alloys. For this purpose, the alloying elements are specifically selected, the microstructures are adjusted in a single-phase and, in some cases, multi-phase manner. In particular, conflicting goals, such as the trade-off between strength and ductility in conventional steels, are overcome. However, in the last 20 years, the focus has been on material synthesis. With the increase in available material quantities, the focus is now on processing issues such as joining and welding processes. The weldability of HEAs has received very little attention so far. The experience with dissimilar metal welds is completely lacking but is essential for the application of these materials in combination with conventional materials. The present study presents comprehensive experimental results on the weldability of an equimolar CoCrFeMnNi-HEA in cold-rolled and heat-treated condition, which was joined by tungsten inert gas welding to an austenitic steel AISI 304. The mechanical properties of the dissimilar metal welds were characterized by cross-weld tensile samples, whereas the local deformation in the weld of the different welding zones was measured by digital image correlation. In accordance with the respective initial HEA condition (cold-rolled vs. heat-treated), the local strain behavior was divergent and influenced the global mechanical properties of both DMW types. Nonetheless, the experiments provided proof in principle of the weldability for dissimilar joints of the CoCrFeMnNi-HEA welded to conventional materials like austenitic stainless steels ensuring a corresponding capability for mechanical loading. This allows further considerations on the application of these innovative materials.
The high corrosion resistance and good mechanical properties of duplex stainless steel (DSS) are due to its special chemical composition, which is a balanced phase ratio of ferrite (α) and austenite (γ). Many industrial applications require the integration of DSS components. For this, tungsten inert gas welding (TIG) is an excellent choice, as it allows an automated operation with high reproducibility. However, when the weld pool solidifies, critical ratios of α- and γ- phases can occur, which leads to solidification cracking, increased susceptibility to corrosion, and a decrease in ductility and critical strength. Previous studies have shown that these defects can be caused by the accumulation of manganese and chromium in the heat affected zone (HAZ), and this accumulation can be detected using LIBS.
Unlike conventional LIBS analyses, which requires reference samples to generate a calibration curve, calibration-free LIBS (CF-LIBS) can determine the chemical composition solely from the emission spectrum of the plasma. Numerous publications show that CF-LIBS is a fast and efficient analytical method for quantitative analysis of metal samples.
We present the results of in situ CF-LIBS analysis during TIG DSS welding. Using a new approach, it is possible to quantitatively determine the chemical composition of the weld metal directly in the welding process. The results of the CF-LIBS analysis are compared with the results of the calibration-based PLS analysis and reasonable agreement is found. Thus, the CF-LIBS method offers the significant advantage of quickly measuring in situ the concentrations of the main alloying elements that prevent the formation of welding defects, without the tedious calibration procedure.
Duplex steels are high-alloyed, stainless steels. They offer some physical advantages over other stainless steels due to the balanced phase ratio of austenite and ferrite. During welding processes, when welding fumes and vaporized material condensates, different chemical elements can accumulate on the surface of the solidified weld. Then, the formation of a protective chromium oxide layer is no longer guaranteed and pitting corrosion can occur at these places. Previous work has shown that the accumulation of manganese and chromium on the surface of the heat-affected zone of the welded high-grade steel 304L can be measured by LIBS.
We present the results of the optimization of LIBS parameters for precise thickness measurements of such thin films and for depth profile measurements Therefore, we used galvanically coated copper samples with known film thicknesses. The Concentration of manganese is reduced in the weld metal. This has a high impact on the metallografic structure of the material.
size limitations and high production costs of L-PBF make it competitive for smaller, highly complex components, while the less complex elements of an assembly are manufactured conventionally. This leads to scenarios that use L-PBF only where it’s beneficial, and it require an integration and joining to form the final product. For example, L-PBF combustion swirlers are welded onto cast parts to produce combustion systems for stationary gas turbines. Today, the welding process requires complex welding fixtures and tack welds to ensure the correct alignment and positioning of the parts for repeatable weld results. In this paper, L-PBF and milled weld preparations are presented as a way to simplify the Tungsten inert gas (TIG) welding of rotationally symmetrical geometries using integrated features for alignment and fixation. Pipe specimens with the proposed designs are manufactured in Inconel 625 using L-PBF and milling. The pipe assembly is tested and TIG welding is performed for validation. 3D scans of the pipes before and after welding are evaluated, and the weld quality is examined via metallography and computed tomography (CT) scans. All welds produced in this study passed the highest evaluation group B according to DIN 5817. Thanks to good component alignment, safe handling, and a stable welding process, the developed designs eliminate the need for part-specific fixtures, simplify the process chain, and increase the process reliability. The results are applicable to a wide range of components with similar requirements.
Influence of Surface Preparation on Cracking Phenomena in TIG-Welded High and Medium Entropy Alloys
(2022)
Multi-element systems with defined entropy (HEA—high entropy alloy or MEA—medium entropy alloy) are rather new material concepts that are becoming increasingly important in materials research and development. Some HEA systems show significantly improved properties or combinations of properties, e.g., the overcoming of the trade-off between high strength and ductility. Thus, the synthesis, the resulting microstructures, and properties of HEA have been primarily investigated so far. In addition, processing is crucial to achieve a transfer of potential HEA/MEA materials to real applications, e.g., highly stressed components. Since fusion welding is the most important joining process for metals, it is of vital importance to investigate the weldability of these materials. However, this has rarely been the subject of research to date. For that reason, in this work, the weldability depending on the surface preparation of a CoCrFeMnNi HEA and a CoCrNi MEA for TIG welding is investigated. The fusion welding of longer plates is described here for the first time for the CoCrNi alloy. The welds of both materials showed distinct formation of cracks in the heat affected Zone (HAZ). Optical and scanning electron microscopy analysis clearly confirmed an intergranular fracture topography. However, based on the results, the crack mechanism cannot be conclusively identified as either a liquid metal embrittlement (LME) or hot cracking-like liquid film separation.