Mechanism of porosity growth during homogenisation in single crystal nickel-based superalloys
(2013)
Several mechanisms for porosity growth in single crystal nickel-based superalloys during homogenisation heat treatment have been proposed in the literature. They were carefully checked using different experimental methods, namely quantitative light microscopy, scanning electron microscopy, transmission electron microscopy, X-ray diffraction and density measurements. It is shown that the main mechanism is the Kirkendall–Frenkel effect, i.e. generation of voids due to uncompensated efflux of Al atoms from dissolving γ/γ′-eutectic areas. The Al diffusion is supported by the afflux of vacancies from surrounding γ-matrix which results in porosity growth. This conclusion is confirmed by the estimation of the vacancy afflux towards the dissolving eutectic.