For reliability and safety issues of injection wells, corrosion resistance of materials used needs to be determined. Herein, representative low-cost materials, including carbon steel X70/1.8977 and low alloyed steel 1.7225, were embedded in mortar to mimic the realistic casing-mortar interface. Two types of cement were investigated: (1) Dyckerhoff Variodur commercial Portland cement, representing a highly acidic resistant cement and (2) Wollastonite, which can react with CO2 and become stable under a CO2 stream due to the carbonation process. Exposure tests were performed under 10 MPa and at 333 K in artificial aquifer fluid for up to 20 weeks, revealing crevice corrosion and uniform corrosion instead of expected pitting corrosion. To clarify the role of cement, simulated pore water was made by dispersing cement powder in aquifer fluid and used as a solution to expose steels. Surface analysis, accompanied by element mapping on exposed specimens and their crosssections, was carried out to trace the chloride intrusion and corrosion process that followed.
CO2 streams captured from power stations or industrial plants may contain impurities that impact the consecutive steps of the CO2 capture and storage (CCS) chain. As the basis for an optimization of CO2 purity over the whole CCS chain, impacts of different impurities were investigated at key steps including studies on (i) corrosion of metallic materials in CO2 streams and brine, (ii) fluid and interfacial properties as a function of pressure, temperature and CO2 stream composition and their implications for CO2 transport, injection and geological storage, (iii) costs of different pipeline design options, (iv) geochemical alterations at typical reservoir conditions and their implications for geomechanical rock properties. Major findings are synthesized for two exemplary single source-single sink CCS chain scenarios involving CO2 stream compositions typical for pre-combustion capture and oxyfuel combustion. Recommendations for material selection for compression, transport and injection were derived for various CO2 stream compositions. To reliably control corrosion, a limitation of water contents to 50 ppmv is recommended for pipeline transportation of all CO2 streams. At geological storage conditions, the presence of either O2, NOx or SO2 only weakly affected fluid-mineral/rock interactions that still impacted geomechanical rock properties.