Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (170) (entfernen)
Sprache
- Englisch (143)
- Deutsch (20)
- Russisch (5)
- Italienisch (1)
- Mehrsprachig (1)
Schlagworte
- Laser beam welding (42)
- Additive manufacturing (14)
- Laser metal deposition (14)
- Microstructure (11)
- Laser welding (9)
- Mechanical properties (9)
- Solidification cracking (9)
- Resistance spot welding (7)
- Hybrid laser-arc welding (6)
- Numerical simulation (6)
Organisationseinheit der BAM
- 9 Komponentensicherheit (139)
- 9.3 Schweißtechnische Fertigungsverfahren (137)
- 5 Werkstofftechnik (2)
- 5.2 Metallische Hochtemperaturwerkstoffe (2)
- 5.5 Materialmodellierung (1)
- 7 Bauwerkssicherheit (1)
- 7.7 Modellierung und Simulation (1)
- 9.0 Abteilungsleitung und andere (1)
- 9.6 Additive Fertigung metallischer Komponenten (1)
The paper presents the experimental results into the development of a multi-channel system for monitoring and quality assurance of the multi-wire submerged arc welding (SAW) process for the manufacture of large diameter pipes. Process signals such as welding current, arc voltage and the acoustic signal emitted from the weld zone are recorded and processed to provide information on the stability of the welding process. It was shown by the experiments that the acoustic pattern of the SAW process in a frequency range between 30 Hz and 2.5 kHz contains the most diagnostic information. The on-line quality assessment of the weld seam produced is carried out in combination with methods of artificial intelligence (AI). From the results obtained, it can be concluded that the use of the latest concepts in welding and automation technology, combined with the high potential of AI, can achieve a new level of quality assurance in pipe manufacturing.
In this contribution, we present a physically motivated heat source model for the numerical modeling of laser beam welding processes. Since the calibration of existing heat source models, such as the conic or Goldak model, is difficult, the representation of the heat source using so-called Lamé curves has been established, relying on prior Computational Fluid Dynamics (CFD) simulations.
Lamé curves, which describe the melting isotherm, are used in a subsequent finite-element (FE) simulation to define a moving Dirichlet boundary condition, which prescribes a constant temperature in the melt pool. As an alternative to this approach, we developed a physically motivated heat source model, which prescribes the heat input as a body load directly. The new model also relies on prior CFD simulations to identify the melting isotherm. We demonstrate numerical results of the new heat source model on boundary-value problems from the field of laser beam welding and compare it with the prior CFD simulation and the results of the Lamé curve model and experimental data.
A fundamental study of physical mechanisms of wineglass-shaped fusion zone profile in laser melting
(2024)
The fusion zone geometry in laser melting processes e.g., laser welding and laser-based additive manufacturing, of metallic materials has commonly a wineglass-shaped profile which is critical to the grain orientation and stress distribution. Hereby, we adopt for the first time a decoupling work through a combination of multi-physics modelling and experiments to reveal the fundamental mechanisms of this special morphology. Two physicsbased easy-to-use metal vapour models are proposed to consider the vapour’s momentum and thermal effects separately. It is found that the direct laser energy absorption and Marangoni shear stress which are widely hypothesised to dominate the wineglass-shape formation show only a minor influence. The additional heating from the metallic vapour plume rather than its momentum impact contributes predominantly to the enlarging of the molten pool top region, resulting directly in the formation of the wineglass-shaped fusion zone. The generality of the plume heating effect is also validated in two types of materials (steel and Al) in a wide range of parameters.
Despite the advances in hardware and software techniques, standard numerical methods fail in providing real-time simulations, especially for complex processes such as additive manufacturing applications. A real-time simulation enables process control through the combination of process monitoring and automated feedback, which increases the flexibility and quality of a process. Typically, before producing a whole additive manufacturing structure, a simplified experiment in the form of a beadon-plate experiment is performed to get a first insight into the process and to set parameters suitably. In this work, a reduced order model for the transient thermal problem of the bead-on-plate weld simulation is developed, allowing an efficient model calibration and control of the process. The proposed approach applies the proper generalized decomposition (PGD) method, a popular model order reduction technique, to decrease the computational effort of each model evaluation required multiple times in parameter estimation, control, and optimization. The welding torch is modeled by a moving heat source, which leads to difficulties separating space and time, a key ingredient in PGD simulations. A novel approach for separating space and time is applied and extended to 3D problems allowing the derivation of an efficient separated representation of the temperature.
The results are verified against a standard finite element model showing excellent agreement. The reduced order model is also leveraged in a Bayesian model parameter estimation setup, speeding up calibrations and ultimately leading to an optimized real-time simulation approach for welding experiment using synthetic as well as real measurement data.
It is proposed to model the experimentally observed weld pool boundary with superellipses (Lamé curves) and to find the unknown parameters of the curves using optimization methods. It has been shown experimentally that during laser welding of austenitic stainless steel with a thickness of 2 mm at a speed of 20 mm/s, the rear weld pool part has a shape close to triangular which can be accurately approximated by a superellipse. Analytical dependences of the trajectory and growth rate of the crystal and its cross-sectional area on the geometry of the rear weld pool part are obtained.
A method of solving the thermo-fluid dynamics problem is presented, enabling the prediction of the shape and dimensions of the weld pool during keyhole laser welding of thick plates. It is shown that the rear weld pool boundary can be satisfactorily approximated by a set of superellipses (Lamé curves). The presence of a convex rear weld pool boundary in the mid-plane has been observed experimentally and reproduced numerically. It was shown that in this zone the concentration of liquating impurities increases and the local solidification temperature decreases, contributing to the susceptibility to hot cracking.
Numerical and experimental assessment of liquid metal embrittlement in externally loaded spot welds
(2024)
Zinc-based surface coatings are widely applied with high-strength steels in automotive industry. Some of these base materials show an increased brittle cracking risk during loading. It is necessary to examine electrogalvanized and uncoated samples of a high strength steel susceptible to liquid metal embrittlement during spot welding with applied external load. Therefore, a newly developed tensile test method with a simultaneously applied spot weld is conducted. A fully coupled 3D electrical, thermal, metallurgical and mechanical finite element model depicting the resistant spot welding process combined with the tensile test conducted is mandatory to correct geometric influences of the sample geometry and provides insights into the sample’s time dependent local loading. With increasing external loads, the morphology of the brittle cracks formed is affected more than the crack depth. The validated finite element model applies newly developed damage indicators to predict and explain the liquid metal embrittlement cracking onset and development as well as even ductile failure.
Beim Unterpulverschweißen sind die Prozessgeräusche ein Indikator für eine gute Fügequalität. Diese Beurteilung kann i.d.R. nur von einer erfahrenen Fachkraft durchgeführt werden. Eine kürzlich entwickelte künstliche Intelligenz kann automatisch das akustische Prozesssignal anhand vortrainierter Merkmale klassifizieren und die Fügequalität anhand des Geräuschs beurteilen. Der Algorithmus, einmal richtig trainiert, kann den Prüfaufwand beim Unterpulverschweißen deutlich reduzieren.
Abstract
In the post-processing of large maritime components, a considerable amount of waste in the form of milling and grinding chips is produced. At the same time, additive manufacturing technologies have shown great potential in producing high-volume parts for maritime applications, allowing novel design approaches and short lead times. In this context, this study presents a sustainable approach to recycle and use aluminium bronze waste material, generated during post-processing of large cast ship propellers, as feedstock for laser-powder directed energy deposition. The recycling technology used to produce powder batches is inductive re-melting in combination with ultrasonic atomization. The derived metal powders are characterized using digital image analysis, powder flowability tests, scanning electron microscopy as well as energy dispersive X-ray spectroscopy. Compared to conventional metal powders produced by gas atomization, the recycled material shows excellent sphericity and a powder size distribution with a higher content of finer and coarser particles. Metallographic sections of deposited additively produced specimens show an increased hardness and reduced ductility, but also competitive densities and higher yield and ultimate tensile strength compared to cast material. The process chain shows high potential for the maritime sector to enable circular and sustainable manufacturing.
The effect of the oscillating metal vapor plume on the keyhole and molten pool behavior during the laser beam welding of AlMg3 aluminum alloys is investigated by experimental and numerical methods. The real-time height of the metal vapor plume is measured by high-speed camera observation. The obtained experimental results are used to evaluate the additional heating source and laser beam attenuation caused by the scattering and absorption based on the Beer–Lambert theory. Furthermore, the dynamic behavior of the metal vapor plume is incorporated into a 3D transient heat transfer and fluid flow model, coupled with the ray tracing method, for the laser beam welding of the AlMg3 alloy. It is found that additional heating resulting from the scattered and absorbed laser beam energy by the metal vapor plume significantly expands the shape of the molten pool on the top region. Moreover, the oscillating metal vapor plume caused the fluctuation of the high-temperature region in the molten pool. The probability of keyhole collapse at the bottom increases 17% due to the oscillating laser power induced by the laser beam attenuation. The internal interplay between the metal vapor plume, molten pool shape, and keyhole collapse is obtained. The developed model has been validated by experiments, which shows a good agreement.