Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2021 (5) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (4)
- Vortrag (1)
Sprache
- Englisch (5)
Schlagworte
- AFM (5) (entfernen)
Organisationseinheit der BAM
- 6 Materialchemie (3)
- 6.1 Oberflächen- und Dünnschichtanalyse (2)
- 9 Komponentensicherheit (2)
- 9.5 Tribologie und Verschleißschutz (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.6 Anorganische Referenzmaterialien (1)
- 6.2 Material- und Oberflächentechnologien (1)
- S Qualitätsinfrastruktur (1)
- S.1 Qualität im Prüfwesen (1)
Eingeladener Vortrag
- nein (1)
Effect of the Anchoring Layer and Transport Type on the Adsorption Kinetics of Lambda Carrageenan
(2021)
The kinetics of lambda carrageenan (λ-car) adsorption/desorption on/from anchoring layers under diffusion- and convection-controlled transport conditions were investigated. The eighth generation of poly(amidoamine) dendrimers and branched polyethyleneimine possessing different shapes and polydispersity indexes were used for anchoring layer formation. Dynamic light scattering, electrophoresis, streaming potential measurements, optical waveguide lightmode spectroscopy, and quartz crystal microbalance were applied to characterize the formation of mono- and bilayers. The unique combination of the employed techniques enabled detailed insights into the mechanism of the λ-car adsorption mainly controlled by electrostatic interactions. The results show that the macroion adsorption efficiency is strictly correlated with the value of the final zeta potentials of the anchoring layers, the transport type, and the initial bulk concentration of the macroions. The type of the macroion forming the anchoring layer had a minor impact on the kinetics of λ-car adsorption. Besides significance to basic science, the results presented in this paper can be used for the development of biocompatible and stable macroion multilayers of well-defined electrokinetic properties and structure.
In this paper, the accurate determination of the size and size distribution of bipyramidal anatase nanoparticles (NPs) after deposition as single particles on a silicon substrate by correlative Scanning Electron Microscopy (SEM) with Atomic Force Microscopy (AFM) analysis is described as a new measurement procedure for metrological purposes. The knowledge of the exact orientation of the NPs is a crucial step in extracting the real 3D dimensions of the particles. Two approaches are proposed to determine the geometrical orientation of individual nano‐bipyramides: (i) AFM profiling along the long bipyramid axis and (ii) stage tilting followed by SEM imaging. Furthermore, a recently developed method, Transmission Kikuchi Diffraction (TKD), which needs preparation of the crystalline NPs on electron‐transparent substrates such as TEM grids, has been tested with respect to its capability of identifying the geometrical orientation of the individual NPs. With the NPs prepared homogeneously on a TEM grid, the transmission mode in a SEM, i.e., STEM‐in‐SEM (or T‐SEM), can be also applied to extract accurate projection dimensions of the nanoparticles from the same sample area as that analysed by SEM, TKD and possibly AFM. Finally, Small Angle X‐ray Scattering (SAXS) can be used as an ensemble technique able to measure the NPs in liquid suspension and, with ab‐initio knowledge of the NP shape from the descriptive imaging techniques, to provide traceable NP size distribution and particle concentration.
It sounds like being a simple analytical task, it is definitely not. The way toward accurate measurement of the size distribution of nanoparticles (NPs) with complex shape, having a broad size polydispersity, with inhomogeneous chemistry, and with a high degree of agglomeration/aggregation is very challenging for all available analytical methods. Particularly for the NPs with complex shape, the access to the smallest dimension (as e.g. required for regulatory purposes) can be enabled only by using imaging techniques with spatial resolution at the nanoscale. Moreover, the full 3D-chacterisation of the NP shape can be provided either by advanced characterization techniques like 3D-TEM tomography or by correlative analysis, i. e. synergetic/complementary measurement of the same field-of-view of the sample with different probes. Examples of the latter type of analysis are: i) electron microscopy for the lateral dimensions and AFM for the height of the NPs, ii) SEM with STEM-in-SEM (also called T-SEM), iii) Electron Microscopy with TKD (Transmission Kikuchi Diffraction) for determination of the geometrical orientation of crystalline NPs, iv) Raman and SEM for e.g. thickness of graphen flakes, or v) Electron Microscopy for descriptive NP shape and SAXS for the NP concentration, the latter as a NP property able to be measured with higher and higher accuracy. For all these types of measurement, reference NPs are necessary for the validation of the measured size. Particularly non-spherical reference NPs are still missing. Examples of such new reference NPs as characterized by the correlative analyses enumerated above will be presented in detail in the contribution.
In the present paper, friction and mechanical properties of AFM-Scan-Induced ripple structures on films of polystyrene and poly-n-(butyl methacrylate) are investigated. Force volume measurements allow a quantitative analysis of the elastic moduli with nanometer resolution, showing a contrast in mechanical response between bundles and troughs. Additionally, analysis of the lateral cantilever deflection shows a clear correlation between friction and the sample topography. Those results support the theory of crack propagation and the formation of voids as a mechanism responsible for the formation of ripples. This paper also shows the limits of the presented measuring methods for soft, compliant, and small structures.
High spatially resolved quantitative bioimaging of CdSe/ZnS Quantum Dots uptake in two kinds of cells is investigated combining laser ablation inductively coupled plasma mass spectrometry and the spatially resolved analysis of dried pL-droplets from a solution with a known concentration of Quantum Dots. Single cells and dried pL-droplets are morphologically characterized by Atomic Force Microscopy. A number concentration of CdSe/ZnS QDs between 3.5 104 and 48 104 is estimated to be uptaken by several selected single cells, after being incubated in the presence of a QDs suspension added to a standard cell culture medium. Mono-elemental bioimaging at subcellular resolution seems to show a higher number concentration of the CdSe/ZnS QDs in the cytosol around the cell nucleus.