Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2019 (221) (entfernen)
Dokumenttyp
Sprache
- Englisch (217)
- Deutsch (3)
- Mehrsprachig (1)
Referierte Publikation
- ja (221) (entfernen)
Schlagworte
- Quantum yield (9)
- Corrosion (7)
- Fluorescence (7)
- Lifetime (6)
- Mechanochemistry (6)
- Photoluminescence (6)
- Additive manufacturing (5)
- Cyclization (5)
- Lanthanide (5)
- Laser beam welding (5)
Organisationseinheit der BAM
- 6 Materialchemie (71)
- 5 Werkstofftechnik (44)
- 9 Komponentensicherheit (40)
- 1 Analytische Chemie; Referenzmaterialien (35)
- 8 Zerstörungsfreie Prüfung (30)
- 6.3 Strukturanalytik (28)
- 7 Bauwerkssicherheit (25)
- 1.2 Biophotonik (24)
- 6.6 Physik und chemische Analytik der Polymere (21)
- 9.3 Schweißtechnische Fertigungsverfahren (19)
Automotive engine lubricants
(2019)
In 2003, ASTM Manual 37, Fuels and Lubricants Handbook: Technology, Properties, Performance and Testing, featured a chapter discussing automotive lubricants, including engine oils, automatic transmission fluids, manual transmission fluids, gear lubricants, and greases. This chapter, by Schwartz, Tung, and McMillan, surveyed all of these classes of lubricants, up to its publication in 2003.
More recently, the period between 2003 and 2010 has been addressed as part of a book copublished by ASTM and SAE International (coeditors Simon Tung and George Totten), where Fox surveyed the development of engine oil specifications that emerged during those years.
This chapter surveys the evolution of engine oil design and testing since 2002 and concludes with insights into future directions offered by recent tribological research. Our objective is to provide a reader new to the field with an understanding of the following:
- Engine oil composition and formulation
- North American engine oil specification development, and an outline of emergent European specifications
- How emergent specifications and legislative requirements are linked to the introduction of new engine hardware
- How tribological innovation can contribute to future enhancements in engine efficiency
In parallel, we will provide several tables comparing groups of contemporaneous specifications.
Carbidic Austempered Ductile Iron (CADI) microstructures containing eutectic carbides can be produced by the addition of carbide stabilizing elements, such as chromium. Carbides formed from the addition of Cr are eutectic of M3C type. The presence of such hard phases can enhance the abrasion wear resistance of ductile iron. A new CADI can be produced by the addition of Nb. Niobium carbide particles are formed in the beginning of solidification and remain stable once they are insoluble in solid iron matrix. The dry sand abrasive wear resistance of ductile irons alloyed with 1.0, 1.8, and 2.4 wt% Nb were tested in both “as-cast” and “heat treated” conditions using standard ASTM G65. Results were compared to abrasive wear data obtained on ductile iron alloyed with 1 wt% Cr, CADI (1 wt% Cr), and the basic composition of iron without carbide stabilizing elements. In the “ascast” condition, the addition of Nb did not lead to a reduction in wear, while CADI with Nb is a promising substitute for CADI with Cr addition, because both materials showed very similar values of abrasion resistance.
Micro-ploughing and micro-cutting mechanisms were observed on the worn surfaces of ductile irons. Abrasive wear resistance of these alloys was correlated with the volume fraction of carbides.
Eu2+ is used to replace toxic Pb2+ in metal halide perovskite nanocrystals (NCs). The synthesis implies injection of cesium oleate into a solution of europium (II) bromide at an experimentally determined optimum temperature of 130 ○C and a reaction time of 60 s. Structural analysis indicates the formation of spherical CsEuBr3 nanoparticles with a mean size of 43 ± 7 nm. Using EuI2 instead of EuBr2 leads to the formation of 18-nm CsI nanoparticles, while EuCl2 does not show any reaction with cesium oleate forming 80-nm EuCl2 nanoparticles.
The obtained CsEuBr3 NCs exhibit bright blue emission at 413 nm (FWHM 30 nm) with a room temperature photoluminescence quantum yield of 39%. The emission originates from the Laporte-allowed 4f7–4f65d1 transition of Eu2+ and shows a PL decay time of 263 ns.
The long-term stability of the optical properties is observed, making inorganic lead-free CsEuBr3 NCs promising deep blue emitters for optoelectronics.
Singlet oxygen can severely damage biological tissue, which is exploited in photodynamic therapy (PDT). In PDT, the effective range is limited by the distribution of the photosensitizer (PS) and the illuminated area. However, no distinction is made between healthy and pathological tissue, which can cause undesired damage. This encouraged us to exploit the more acidic pH of cancerous tissue and design pH-controllable singlet oxygen-generating boron-dipyrromethene (BODIPY) dyes. A pH sensitivity of the dyes is achieved by the introduction of an electronically decoupled, photoinduced electron transfer (PET)-capable subunit in meso-position of the BODIPY core. To favor triplet-state formation as required for singlet Oxygen generation, iodine substituents were introduced at the chromophore core. The resulting pH-controlled singlet oxygen-generating dyes with pKa values in the physiological range were subsequently assessed regarding their potential as pH-controlled PS for PDT.
Using HeLa cells, we could successfully demonstrate markedly different pH-dependent cytotoxicities upon illumination.
The hydration process of Portland cement in a cementitious system is crucial for development of the high-quality cementbased construction material. Complementary experiments of Xray diffraction analysis (XRD), scanning electron microscopy (SEM) and time-resolved laser fluorescence spectroscopy (TRLFS) using europium (Eu(III)) as an optical probe are used to analyse the hydration process of two cement systems in the absence and presence of different organic admixtures.
We Show that different analysed admixtures and the used sulphate carriers in each cement system have a significant influence on the hydration process, namely on the time-dependence in the formation of different hydrate phases of cement. Moreover, the effect of a particular admixture is related to the type of sulphate carrier used.
The quantitative information on the amounts of the crystalline cement paste components is accessible via XRD analysis. Distinctly different morphologies of ettringite and calcium-silicate-hydrates (C-S-H) determined by SEM allow visual conclusions about formation of these phases at particular ageing times. The TRLFS data provides information about the admixture influence on the course of the silicate reaction. The dip in the dependence of the luminescence decay times on the hydration time indicates the change in the structure of C-S-H in the early hydration period. Complementary information from XRD, SEM and TRLFS provides detailed information on distinct periods of the cement hydration process.
Due to the stochastic nature of crack nucleation by Vickers indentation, a statistical analysis of propagation rates of 185 radial cracks was performed. Crack growth was observed directly using a video camera with high Image acquisition rate. It is found that propagation rates are controlled by the environmental reactions at the crack-tip shortly after their initiation (< 1 s). Calibration of the stress intensity KI showed that the residual stress factor χ and the exponent n of the equation KI==χPc−n (with P==load and c==crack length) are broadly distributed among the 185 analyzed cracks, ranging from 10−16 to 104 and from 0.1 to 5, respectively. For the most frequent crack, the equation KI==0.052Pc−1.47 holds. The results show that correlations of indentation-induced crack length to stress intensity necessitate the use of statistical significant data that are calibrated by the environmental reactions at the crack-tip.
Hydrogen gas diffusivity of fourteen glasses of the Na2O-Al2O3-SiO2 system are studied along the joins quartzalbite-jadeite-nepheline (Qz-Ab-Jd-Np, fully polymerized) and albite-sodium disilicate (Ab-Ds, depolymerized).
Density measurements show that ionic porosity decreases from 54.4% (Qz) to 51.5% (Np) and from 52.4% (Ab) to 50.2% (Ds). Hydrogen diffusivity D follows similar trends but at another scale. D at 523 K decreases from 4×10−12 to 3×10−14m2 s−1 (Qz-Np) and from 4×10−13 to 3×10−15m2 s−1 (Ab-Ds). Charge compensating Na+ acting as a filling agent in fully polymerized network structures leads to up to one order of Magnitude higher diffusivities as depolymerized glass structures of the same SiO2 content where Na+ takes the role of a
modifier ion. Temperature dependence of the diffusivity indicates that both the activation energy involved with the moving H2 molecule as well as the accessible volume in the structure contribute to this compositional trend.
Roaldite – Fe4N – has been identified in the São Julião de Moreira iron meteorite using electron backscatter diffraction (EBSD) and simultaneously acquired energy-dispersive x-ray spectroscopy (EDS). Mean-periodic-number images derived from raw EBSD patterns confirm this phase by an even higher spatial resolution compared to EDS.
Roaldite appears in the form of systematically and repetitively aligned plates. Despite the locally heavy plastic deformation, it is shown that the origin of the oriented precipitation of roaldite is linked to the orientation of the kamacite matrix. Roaldite can be considered to be precipitated from kamacite using an inverse Kurdjumov-Sachs (K-S) or Nishiyama-Wassermann (N-W) orientation relationship. A more accurate discrimination is impossible due to the accumulated shock deformation, which blurs the local reference orientation of kamacite. The habit plane of roaldite is found to be {112}R, which is most likely parallel to {120}K of kamacite. Some of the roaldite plates contain two orientation variants which repeatedly alternate. Their misorientation angle is about 12°.
A concept for the growth of silica shells with a thickness of 5–250 nm onto oleate-coated NaYF4:Yb3+/Er3+ upconversion nanoparticles (UCNP) is presented. The concept enables the precise adjustment of shell thicknesses for the preparation of thick-shelled nanoparticles for applications in plasmonics and sensing. First, an initial 5–11 nm thick shell is grown onto the UCNPs in a reverse microemulsion. This is followed by a stepwise growth of these particles without a purification step, where in each step equal volumes of tetraethyl orthosilicate and ammonia water are added, while the volumes of cyclohexane and the surfactant Igepal® CO-520 are increased so that the ammonia water and surfactant concentrations remain constant. Hence, the number of micelles stays constant, and their size is increased to accommodate the growing core–shell particles. Consequently, the formation of core-free silica particles is suppressed. When the negative zeta potential of the particles, which continuously decreased during the stepwise growth, falls below −40 mV, the particles can be dispersed in an ammoniacal ethanol solution and grown further by the continuous addition of tetraethyl orthosilicate to a diameter larger than 500 nm. Due to the high colloidal stability, a coalescence of the particles can be suppressed, and single-core particles are obtained. This strategy can be easily transferred to other nanomaterials for the design of plasmonic nanoconstructs and sensor systems.
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding Parameters on the formation of end crater defects such as pores, cracks, root excess weld metal and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp-down causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques.
A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of between 8 mm and 10 mm and then transferred on the 10 mm thick pipe sections made of high-strength pipeline steel API5L-X100Q.
For the vast majority of ellipsometric measurements, the application of planar substrates is mandatory and requires a proper sample alignment prior to the measurement. Here, the authors present a generalized approach of how to extract the isotropic ellipsometric sample parameters from an imaging Mueller-matrix measurement even if the sample is significantly misaligned. They validate the method by layer-thickness calculations based on imaging Mueller-matrix measurements of flat crystalline silicon samples that were misaligned on purpose. Furthermore, they also exploit this method’s capabilities to perform spatially resolved layer-thickness measurements of a single-layer indium-tin-oxide coating on a fused-silica microlens without the need of realignment or repositioning of the sample during the measurement.
Among the various welding technologies, resistance spot welding (RSW) and laser beam welding (LBW) play a significant role as joining methods for the automobile industry. The application of RSW and LBW for the automotive body alters the microstructure in the welded areas. It is necessary to identify the mechanical properties of the welded material to be able to make a reliable statement about the material behavior and the strength of welded components. This study develops a method by which to determine the mechanical properties for the weldment of RSW and LBW for two dual phase (DP) steels, DP600 and DP1000, which are commonly used for the automotive bodies. The mechanical properties of the resistance spot weldment were obtained by performing tensile tests on the notched tensile specimen to cause an elongation of the notched and welded area in order to investigate its properties. In order to determine the mechanical properties of the laser beam weldment, indentation tests were performed on the welded material to calculate its force-penetration depth-curve. Inverse numerical simulation was used to simulate the indentation tests to determine and verify the parameters of a nonlinear isotropic material model for the weldment of LBW. Furthermore, using this method, the parameters for the material model of RSW were verified. The material parameters and microstructure of the weldment of RSW and LBW are compared and discussed. The results show that the novel method introduced in this work is a valid approach to determine the mechanical properties of welded high-strength steel structures. In addition, it can be seen that LBW and RSW lead to a reduction in ductility and an increase in the amount of yield and tensile strength of both DP600 and DP1000.
The efficient and sensitive detection of pathogenic microorganisms in aqueous environments, such as water used in medical applications, drinking water, and cooling water of industrial plants, requires simple and fast methods suitable for multiplexed detection such as flow cytometry (FCM) with optically encoded carrier beads. For this purpose, we combine fluorescent Cd-free Ag−In−S ternary quantum dots (t-QDs) with fluorescence Lifetimes (LTs) of several hundred nanoseconds and superparamagnetic Fe3O4 nanoparticles (SPIONs) with mesoporous CaCO3 microbeads to a magneto-fluorescent bead platform that can be surface-functionalized with bioligands, such as antibodies. This inorganic bead platform enables immuno-magnetic separation, target enrichment, and target quantification with optical readout. The beads can be detected with steady-state and time-resolved fluorescence microscopy and flow cytometry (FCM). Moreover, they are suited for readout by time gated emission. In the following, the preparation of these magneto-fluorescent CaCO3 beads, their spectroscopic and analytic characterization, and their conjugation with bacteria-specific antibodies are presented as well as proof-of-concept measurements with Legionella pneumophila including cell cultivation and plating experiments for bacteria quantification. Additionally, the possibility to discriminate between the long-lived emission of the LT-encoded capture and carrier CaCO3 beads and the short-lived Emission of the dye-stained bacteria with time-resolved fluorescence techniques and single wavelength excitation is demonstrated.
A thorough characterization of starting materials is the precondition for further research, especially for cement, which contains various phases and presents quite a complex material for fundamental scientific investigation. In the paper at hand, the characterization data of the reference cement CEM I 42.5 R used within the priority program 2005 of the German Research Foundation (DFG SPP 2005) are presented from the aspects of chemical and mineralogical compositions as well as physical and chemical properties. The data were collected based on tests conducted by nine research groups involved in this cooperative program. For all data received, the mean values and the corresponding errors were calculated. The results shall be used for the ongoing research within the priority program.
An effective method for evaluating the fatigue strength of thick unidirectional composite laminates of wing spar caps has been presented here. A typical width-tapered bending specimen has been developed for a four-point loading set up. Static and fatigue loading was performed at a load ratio R = -1. The complex stress state has been investigated numerically by finite element analysis. Finally, the concept is proven experimentally on specimens made of pultruded fibre rods.
The fatigue behavior of the continuously tapered width by water Jet cutting has been compared to discrete tapering via rod-drop. The new method enables a screening of material fatigue behavior caused by normal and shear loading.
Der 60 °C-Betonversuch ist eine in Deutschland und international verbreitete Methode um die Empfindlichkeit von Gesteinskörnungen und Betonen hinsichtlich einer Alkali-Kieselsäure Reaktion (AKR) zu prüfen. Dieser Beitrag stellt eine neuentwickelte automatisierte Variante der Prüfmethode in einem Minireaktor vor. Dabei werden die Dehnungen von Betonprismen nicht, wie beim konventionellen Test manuell, sondern automatisch in entsprechend ausgerüsteten Prüfbehältern gemessen. Neben einer Reduzierung des Messaufwands bringt die automatisierte Prüfung im Minireaktor weitere Vorteile. Die Dehnungssignale werden, anders als bei der konventionellen Messung, quasi-kontinuierlich aufgezeichnet und bilden das Expansionsverhalten der Prismen detailliert ab. Außerdem bleiben Unterbrechungen der AKR-provozierenden Lagerung aus, die bei der konventionellen Prüfung notwendig sind. Im Beitrag werden die automatisierte und konventionelle Prüfung anhand der Dehnungen von Prismen zweier Gesteinskörnungen verglichen. In Übereinstimmung mit vorhergehenden Untersuchungen sind im Minireaktor gemessene Dehnungen systematisch kleiner als manuell gemessene. Als mögliche Ursache werden Unterschiede im Auslaugverhalten experimentell untersucht. Zur Überprüfung der Einstufung der zwei Gesteinskörnungen erfolgen außerdem Referenzprüfungen in der Nebelkammerlagerung bei 40 °C.
In summary, we report a highly modular solid TTA-UC system comprising of a crystalline, thermally stable PCN222(Pd) MOF with CA-coated MOF channels and with a DPA annihilator embedded in a solution-like environment in the MOF channels. This solid material displays blue upconverted delayed emission with a luminescence lifetime of 373 us, a threshold value of 329 mW*cm-2 and a triplet–triplet energy transfer efficiency of 82%. This optical application adds another facet to the versatile chemistry of PCN-222 MOFs. The design concept is also applicable to other TTA-UC pairs and enables tuning of the UCL color, for example, by replacing DPA with other dyes as exemplarily shown for 2,5,8,11-tetra-tert-butyl-perylene, that yields UCL at 450 nm. Current work aims to reduce the oxygen sensitivity and to increase the retention of the trapped annihilators in organic environments, for example, by tuning the chain length of the carboxylic acid and by coating the MOF surface. In addition, the TTA-UC efficiency will be further enhanced by reducing the reabsorption of the UC emission caused by Pd(TCPP) and by optimizing the sensitizer/annihilator interface.
Friction stir welding (FSW) of high-melting temperature alloys, such as steel and Inconel, requires tooling that can survive under the applied loads at the elevated temperatures. Tungsten-Rhenium (W-Re) alloys are a suitable candidate for this application; however, the costs typically associated with achieving the required densities and grain structure for the tooling are high due to the lengthy traditional processing required. Further costs are incurred in machining the starting bar stock to the final FSW tooling configuration. An alternate processing method is used in this study to shorten the fabrication time using direct current sintering which rapidly consolidates the starting powders at lower temperatures than used in traditional powder metallurgy. Although this process enables retention of the fine grain size, the sintering time is too short to form the desired single, solid phase. Therefore, the specimens were subjected to a post-consolidation heat treatment to fully solutionize the W matrix. Once the desired density and solid solution phase was verified in coupons, the final processing parameters were used to consolidate a net shape tool for FSW.
Ferritic spheroidal graphite cast iron (SGI) materials have a remarkable technical poten-tial and economic impact in modern industry. These features are closely related to the question of how the cast materials can be produced without structural defects and graphite degenerations such as for example chunky graphite. Although the chunky graphite degeneration superficially seems to be well known, its metallurgical background is still controversially discussed, appropriate field-tested non-destructive tools for its quantification in castings are lacking and the knowledge on its impact on material properties is fairly limited. Addressing this status, the article is providing a current overview on the subject. Existing theories on formation and growth mechanisms of chunky graphite are briefly reviewed. Furthermore, from a metallurgical point of view, causes for the appearance of chunky graphite as well as preventive measures are concisely summarized. Particular attention is paid to the morphology of chunky graphite and how it can be characterized by destructive and non-destructive techniques. Special emphasis was laid on providing a comprehensive overview on the impact of chunky graphite on strength, ductility, fatigue limit, fatigue crack growth rate as well as fracture tough-ness of ferritic SGI materials based on experimental data. Moreover, conclusions for the assessment of castings affected by chunky graphite are drawn.
Nanoporous media exhibit structures significantly smaller than the wavelengths of visible light and can thus act as photonic metamaterials. Their optical functionality is not determined by the properties of the base materials, but rather by tailored, multiscale structures, in terms of precise pore shape, geometry, and orientation. Embedding liquid crystals in pore space provides additional opportunities to control light–matter interactions at the single-pore, meta-atomic scale. Here, we present temperature-dependent 3D reciprocal space mapping using synchrotron-based X-ray diffraction in combination with high-Resolution birefringence experiments on disk-like mesogens (HAT6) imbibed in self-ordered arrays of parallel cylindrical pores 17 to 160 nm across in monolithic anodic aluminium oxide (AAO). In agreement with Monte Carlo computer simulations we observe a remarkably rich self-assembly behaviour, unknown from the bulk state. It encompasses transitions between the isotropic liquid state and discotic stacking in linear columns as well as circular concentric ring formation perpendicular and parallel to the pore axis. These textural transitions underpin an optical birefringence functionality, tuneable in magnitude and in sign from positive to negative via pore size, pore surface-grafting and temperature. Our study demonstrates that the advent of large-scale, self-organised nanoporosity in monolithic solids along with confinement-controllable phase behaviour of liquid-crystalline matter at the single-pore scale provides a reliable and accessible tool to design materials with adjustable optical anisotropy, and thus offers versatile pathways to finetune polarisation-dependent light propagation speeds in materials. Such a tailorability is at the core of the emerging field of transformative optics, allowing, e.g., adjustable light absorbers and extremely thin metalenses.
Molecular mobility of cyanophenyl alkylbenzoates (CPnBs) (n = 2, 3, 7 – number of carbon atoms in the alkyl chain) in the bulk and in composites with aerosil A380 is investigated by broadband dielectric spectroscopy, while thermal analysis and infrared spectroscopy were applied to characterise the molecular species. The work completes preliminary results obtained for the members with n = 4 … 6. An interaction by hydrogen bonding, between aerosil surface – OH groups and – CN or ester groups of the CPnB molecules takes place. It slows down the relaxation process as observed for related composites in comparison to the pure materials. The existence of two types of bonding might be the reason that Vogel temperature for the relaxation process in the surface layer does not show the odd-even effect. Temperature dependence of the relaxation rates for composites
shows a crossover behaviour from a high to a low temperature regime. Moreover, the temperature dependence of the dielectric strength is unusual. As the loading degree is similar, comparison of the dielectric, spectroscopic and thermal data obtained here and with the results obtained for the composites with n = 4 … 6 can be directly done. Increasing the number of the members of the homologous series confirms and hardens the preliminary conclusions.
Chemically modified bioactive glasses based on ICIE16 were prepared with the melt-quenching method using water as a quenching medium. The sinterability of these bioactive glasses was investigated and is discussed in this article. The sintering experiments were conducted with different sintering temperatures, sintering times and heating rates. Those parameters are crucial for dense glass with an amorphous structure. The particle size (d50) of the starting glass powder was determined at 88 μm and kept constant. The pre-pressed glass pellets were cold-isostatically pressed at 300 MPa to a green density of around 63 %. Density development, phase identification, shrinkage behavior and the microstructure were investigated to determine the sinterability of the developed glasses. The glass powders were sintered at different temperatures inside the processing window while crystallization was monitored. The results have shown that the sinterability of the developed glasses strongly dependsonthe proposed chemical additions. The highest density reached was 96 %, which belongs to BP1 glass with sintering conditions of 20 K/min heating rate for 60 min at 750 °C.
Organic and inorganic nanoparticles (NPs) are increasingly used as drug carriers, fluorescent sensors, and multimodal labels in the life and material sciences. These applications require knowledge of the chemical nature, total number of surface groups, and the number of groups accessible for subsequent coupling of e.g., antifouling ligands, targeting bioligands, or sensor molecules. To establish the concept of catch-and-release assays, cleavable probes were rationally designed from a quantitatively cleavable disulfide moiety and the optically detectable reporter 2-thiopyridone (2-TP). For quantifying surface groups on nanomaterials, first, a set of monodisperse carboxy-and amino-functionalized, 100 nm-sized polymer and silica NPs with different surface group densities was synthesized. Subsequently, the accessible functional groups (FGs) were quantified via optical spectroscopy of the cleaved off reporter after its release in solution. Method validation was done with inductively coupled plasma optical emission spectroscopy (ICP-OES) utilizing the sulfur atom of the cleavable probe. This comparison underlined the reliability and versatility of our probes, which can be used for surface group quantification on all types of transparent, scattering, absorbing and/or fluorescent particles. The correlation between the total and accessible number of FGs quantified by conductometric titration, qNMR, and with our cleavable probes, together with the comparison to results of conjugation studies with differently sized biomolecules reveal the potential of catch-and-release reporters for surface analysis. Our findings also underline the importance of quantifying particularly the accessible amount of FGs for many applications of NPs in the life sciences.
The influence of size effects on the thermoelectric properties of thin platinum films is investigated and compared to the bulk. Structural properties, like the film thickness and the grain size, are varied. We correlate the electron mean free path with the temperature dependence of the electrical conductivity and the absolute Seebeck coefficient SPt of platinum. A measurement platform was developed as a standardized method to determine SPt and show that SPt,film is reduced compared to SPt,bulk. Boundary and surface scattering reduce the thermodiffusion and the phonon drag contribution to SPt,film by nearly the same factor. We discuss in detail on behalf of a model, which describes the temperature dependence of the absolute Seebeck coefficient, the influence of size effects of electron-phonon and phonon-phonon interaction on SPt.
Advanced high strength steels are usually coated by a zinc layer for an increased resistance against corrosion. During the resistance spot welding of zinc coated steel grades, liquid metal embrittlement (LME)mayoccur. As a result, cracking inside and around the spot weld indentation is observable. The extent of LME cracks is influenced by a variety of different factors. In this study, the impact of the used electrode geometry is investigated over a stepwise varied weld time.
A spot welding finite element simulation is used to analyse and explain the observed effects. Results show significant differences especially for highly increased weld times. Based on identical overall dimensions, electrode geometries with a larger working plane allow for longer weld times, while still preventing LME within the investigated material and maintaining accessibility.
The laser implantation–named technique aims to address the tribological problems frequently seen on tool surfaces during hot stamping. It is based on the creation of elevated dome- or ring-shaped hard structures on the surface of tool steels by a localized dispersing of hard particles. Therefore, a combination of the two distinct approaches that are normally used in surface Technology for optimizing friction and wear, i.e., surface texturing and surface material optimization, are realized in one processing step. In experimental studies, a localized dispersing of TiB2 particles in the surface layer of the hot work tool steel X38CrMoV5-3 was considered and compared with punctual laser–remelted textures. The structures (micro-) hardness was measured at top- and cross-sections. With the aid of a scanning electron microscope, energy dispersive X-ray spectroscopy and X-ray diffraction the interaction between the hard particles and the substrate material were studied. From the results, an optimal parameter range was identified for laser implantation. To the investigation’s end, the implant geometry was measured by optical microscopy and White light microscopy. Furthermore, a mathematic model was introduced, which allows a prediction of the implant geometry as a response to the laser parameters. It was shown that the implantation of TiB2 particles leads to a significant hardness increase up to 1600 HV1 due to the dispersion of initial particles and an in situ precipitation of new titanium-rich phases. It was possible to create defect-free dome- and ring-shaped microstructures on the surfaces. It was also shown that the implants geometry highly depends on the applied laser parameters. The applied central composite design shows a good agreement with the experimental results.
In this paper, the influence of the bulk temperature (BT) of Polycarbonate (PC) on the occurrence and growth of Laser-induced Periodic Surface Structures (LIPSS) is studied. Ultrashort UV laser pulses with various laser peak fluence levels F_0 and various numbers of overscans (N_OS) were applied on the surface of pre-heated Polycarbonate at different bulk temperatures. Increased BT leads to a stronger absorption of laser energy by the Polycarbonate. For N_OS < 1000 High Spatial Frequency LIPSS (HSFL), Low Spatial Frequency LIPSS perpendicular (LSFL-I) and parallel (LSFL-II) to the laser polarization were only observed on the rim of the ablated tracks on the surface but not in the center of the tracks. For N_OS ≥ 1000 , it was found that when pre-heating the polymer to a BT close its glass transition temperature (T_g), the laser fluence to achieve similar LIPSS as when processed at room temperature decreases by a factor of two. LSFL types I and II were obtained on PC at a BT close to T_g and their periods and amplitudes were similar to typical values found in the literature. To the best of the author’s knowledge, it is the first time both LSFL types developed simultaneously and consistently on the same sample under equal laser processing parameters. The evolution of LIPSS from HSFL, over LSFL-II to LSFL I, is described, depending on laser peak fluence levels, number of pulses processing the spot and bulk temperature.
Additively manufactured test specimens made of polyamide 12 (PA 12) by Laser Sintering as well as of acrylonitrile butadiene styrene (ABS) by Fused Layer Modelling, were characterised with active thermography directly after manufacturing and after artificial weathering. For this, two different excitation methods (flash and pulse heating) were used and compared, regarding their suitability for the detection of constructed and imprinted defects inside the test specimens. To increase the quality of the thermograms, data processing methods like thermal signal reconstruction (TSR) and Fourier Transformation after TSR were applied. To further investigate the long-term stability of the additively manufactured test specimens towards environmental stress, like UV radiation, heat, humidity, water contact and frost with active thermography, an artificial weathering test over 2000 hours (~3 months) was applied to the specimens. The monitoring of the changes in the optical properties of the weathered plastics was supplemented by spectral reflectance and UV/VIS spectroscopy.
In the present work it was shown that the tribologcal profiles of special model oxides under dry unidirectional sliding have shown, that sub-oxides have a contribution to the tribological behavior of carbides and cermets, when they are tribo-oxidatively formed, because their tribological profiles as monolithic materials are homologous in part or totally, or compete with hardmetals or cermets, depending from the operating conditions regarded.
A high-pressure neutron diffraction study was conducted on polycrystalline samples of the two known polymorphs of 2,4,6-trinitrotoluene [monoclinic (m) and orthorhombic (o) TNT] under hydrostatic conditions. Isothermal equations of state were obtained for both polymorphic forms. Neither polymorph was observed to undergo a phase transition in the pressure region 0–5 GPa, with both polymorphs displaying smooth compression behavior across the pressure range. This differs somewhat from previous X-ray diffraction and Raman spectroscopy investigations in which discontinuities were observed in the P–V curves and spectral changes were reported at ∼2 GPa. The high-pressure response of these materials is supported by dispersion-corrected density functional theory calculations which, while overestimating the experimental bulk moduli, give excellent agreement with the observed smooth compression response of both phases.
The authors describe and interpret curvature-related changes to the ellipsometric readout. As model system for a concave curvature, a set of three spherical microscopic indents in silicon (100) of different sizes was prepared by instrumented indentation testing using a spherical indenter. For reference, these samples were characterized by AFM to reveal the topography of each structure. The concavelike indents were analyzed by Mueller-Matrix imaging ellipsometry to extract lateral intensity images of 12 elements of the Mueller-Matrix. As a result of the detailed analysis of the image elements m22, m23, and m14, it was possible to correlate intensity changes and symmetry properties to depolarization and cross polarization induced by the edge threshold and the curved surface of the indent.
Large-pore ordered mesoporous silica (OMS) COK-12, analogous to the well-known SBA-15, but synthesized in a more environmentally friendly way and exhibiting a shorter plate-like structure, was grafted with different amounts of graphene oxide (GO) for the first time in an inexpensive and rapid process, that was successfully upscaled. Samples were examined with nitrogen sorption analysis, SAXS, Raman spectroscopy, XPS, and zeta potential analysis. Adsorption experiments with the cationic dye methylene blue (MB) were conducted on the grafted materials and on pure COK-12, taking into account the influence of initial dye concentration (30–600 mg L-1), adsorbent dosage (0.2–14 g L-1), contact time (0.3–300 min), solution pH (4 10), and influence of salts and temperature (0–1 M NaCl, 80 C) to simulate industrial dye effluent. The adsorption process was found to be represented best by the Langmuir isotherm model, i.e., adsorption is a monolayer process. The calculated maximum Adsorption capacities were found to be 20.2 and 197.5 mg g-1 at dosages of 5 and 0.5 g L-1 for pure COK-12 and COK-12 grafted with 50 wt% GO, respectively, at pH 5.65 and MB concentration of 100 mg L-1.
Adsorption kinetics were found to follow the pseudo-second order model, i.e., chemisorption is the rate controlling step. The adsorption performances could be well preserved at simulated dye effluent.
Desorption was found to be most effective with hydrochloric acid. The COK-12 grafted with GO presented in this work shows superior adsorption properties in comparison to other grafted OMS materials. In addition, grafting with GO remarkably improved the stability of COK-12 in aqueous solution.
First phosphorus AB2 monomer for flame-retardant hyperbranched polyphosphoesters: AB2vs. A2 + B3
(2019)
Branched polymers are an important class of polymers with a high number of terminal groups, lower viscosity compared to their linear analogs and higher miscibility, which makes them especially interesting for flame retardant applications, where the flame retardants (FR) are blended with another polymer matrix. Hyperbranched polyphosphoesters (hbPPEs) are gaining more and more interest in the field of flame retardancy, as low molar mass FRs often have the disadvantage of blooming out or leaching, which is not desired in consumer products. Here, we present the first phosphorus-based AB2 monomer for the synthesis of hbPPEs and assess its flame-retardant performance in an epoxy resin compared to a hbPPE synthesized by an A2 + B3 approach. The hbPPE synthesized from an AB2 monomer exhibited a slightly higher performance compared to a similar hbPPE, which was prepared by A2 + B3 polyaddition, probably due to its higher phosphorus content.
Molecular MRI is a promising in-vivo modality to detect and quantify morphological and molecular vessel-wall changes in atherosclerosis. The combination of different molecular biomarkers may improve the risk stratification of patients. This study aimed to investigate the feasibility of simultaneous visualization and quantification of plaque-burden and inflammatory activity by dual-probe molecular
MRI in a mouse-model of progressive atherosclerosis and in response-to-therapy. Homozygous apolipoprotein E knockout mice (ApoE−/−) were fed a high-fat-diet (HFD) for up to four-months prior to MRI of the brachiocephalic-artery. To assess response-to-therapy, a statin was administered for the same duration. MR imaging was performed before and after administration of an elastin-specific gadolinium-based and a macrophage-specific iron-oxide-based probe. Following in-vivo MRI, samples were analyzed using histology, immunohistochemistry, inductively-coupled-mass-spectrometry and laser-inductively-coupled-mass-spectrometry. In atherosclerotic-plaques, intraplaque expression
of elastic-fibers and inflammatory activity were not directly linked. While the elastin-specific probe demonstrated the highest accumulation in advanced atherosclerotic-plaques after four-months of HFD, the iron-oxide-based probe showed highest accumulation in early atherosclerotic-plaques after two months of HFD. In-vivo measurements for the elastin and iron-oxide-probe were in good agreement
with ex-vivo histopathology (Elastica-van-Giesson stain: y = 298.2 + 5.8, R2 = 0.83, p < 0.05; Perls‘ Prussian-blue-stain: y = 834.1 + 0.67, R2 = 0.88, p < 0.05). Contrast-to-noise-ratio (CNR) measurements of the elastin probe were in good agreement with ICP-MS (y = 0.11x-11.3, R² = 0.73, p < 0.05). Late stage atherosclerotic-plaques displayed the strongest increase in both CNR and gadolinium concentration (p < 0.05). The gadolinium probe did not affect the visualization of the iron-oxide-probe and vice versa. This study demonstrates the feasibility of simultaneous assessment of plaque-burden.
This study demonstrates the potential of the concurrent assessment of inflammatory activity and ECM degradation by dual-probe molecular MRI in an experimental mouse model of AAA. Based on the combined information from both molecular probes the rupture of AAAs could reliably be predicted, with higher accuracy compared with each probe alone. The combined in vivo quantification of these biomarkers in 1 imaging session may be useful to improve the in vivo characterization of AAAs.
Two kinds of cyclic poly(D- and L-lactide)s were synthesized, namely CI labeled samples mainly consisting of even-numbered cycles with low dispersity and CII, CIII or CIV-labeled ones consisting of equal amounts of even and odd-numbered cycles with high dispersity and igher molecular weights (Mw up to 300 000). Furthermore, linear poly L-lactide)s were prepared by initiation with ethanol and in both series the molecular weight was varied. The formation of stereocomplexes from cyclic poly(D-lactide)s and all kinds of poly L-lactide)s was performed in dichloromethane/toluene mixtures. The stereocomplexes crystallized from the reaction mixture were characterized in the virgin state and after annealing at 205 °C.
Stereocomplexes free of stereohomopolymers with crystallinities up to 80% were obtained from all experiments in yields ranging from 60 to 80%. Despite the high annealing temperature (maintained for 1 h), little transesterification was observed and the crystallinity slightly increased.
Wild bees are important pollinators for agricultural crops and solitary species such as Osmia bicornis are particularly suitable for pollination management. Wild bees share floral resources with managed honey bees and may be exposed to emerging infectious diseases. Although studies have explored the prevalence of pathogens in solitary wild bee species, data regarding the impact of pathogens on solitary bee health are lacking.
We carried out experiments examining whether the solitary bee species O. bicornis is susceptible to infection with the emerging pathogen The results obtained indicate that N. ceranae may be able to infect O. bicornis but its impact on host fitness is negligible: survival rates did not differ between Control and inoculated bees, although male survival was marginally lower after infection. To explore the possible field-relevance of our findings, we collected wild bees near an infected and a non-infected hive and showed that N. ceranae was shared between managed and wild bees, although only the in presence of infected honey bees.
The findings of the present study show that O. bicornis is susceptible to pathogen spillover and could act as a potential reservoir host for N. ceranae in pollinator networks. Additional studies on this species incorporating sublethal effects, multiple infections and other interacting stressors are warranted.
An investigation of the two-component phase diagram of the CaNaPO4- CaKPO4system performed using various analysis techniques is reported. The continuous solid solution series of α-CaMPO4 existing above 700 °C undergoes eutectoid decomposition during cooling to β-CaMPO4-based solid solutions enriched with Na and K, and to an intermediate nonstoichiometric compound with an ideal composition of CaK0.6Na0.4PO4. All three compounds exhibit significant volumetric effects associated with first-order phase transitions, with positive volume changes under cooling for the intermediate compound. Increased K content in ceramics based on CaKyNa1-yPO4 compositions enhances the strength properties of those ceramics, including their fracture toughness, which is associated with increased density. Increased K content also has a smaller effect of inducing phase transformations accompanied by strong volume changes.
The crystallization behavior of sodium ion conductive Na2MnP2O7 glass was examined to clarify the crystallization mechanism. The formation of thermodynamically metastable phase, layered Na2MnP2O7, at the surface of the glass occurred. Heat treatment at 430 °C for 3 h lead to surface crystals of Na2MnP2O7 oriented with the (101) direction perpendicular to the sample surface. As the heat treatment temperature increased, the glass-ceramic samples deformed, and the presence numerous micro bubbles due to dissolved water was detected.
A seamless pipe made of AISI 321 stainless steel represented a part of a transportation Pipeline system for hydrogen-containing hot gas in a hydrocarbon cracking unit. After a service period of approximately 21 months, a segment of such pipe demonstrated the cracks, causing leakage and respective fire. For clarification of a failure root cause, various metallurgical investigations combined with numerical simulations have been applied. The results revealed that the rupture of seamless pipe was evidently influenced by hydrogen assisted cracking (HAC). An increased susceptibility of the alloy to HAC had to be attributed to its sensitive microstructure which was related to the occurrence of slip bands with a high quantity in austenite grains, particularly in the specific region underneath the outer wall surface. In addition, the intensity of restraint resulting from the T-joint weld configuration caused respectively higher triaxial stresses in the confined area on the outer wall surface where the crack started. The numerical simulations of hydrogen diffusion revealed that a uniform hydrogen concentration profile over the pipe wall thickness was reached when the service period was more than 20 months. This duration agreed well to the timeto-failure of the actual component. Considering additionally that the final stage of rupture by overload was preceded by severe HAC, as confirmed by the respective intergranular fracture topography.
Based on the three-phase model of semi-crystalline polymers, we determined all phase fractions of the NiAl-LDH/PLLA nanocomposites in dependence on the concentration of the nanofiller. Moreover, the rigid amorphous fraction (RAF) was separated into the RAFcrystal and the RAFfiller unbiasedly. A detailed comparison to the related nanocomposite system MgAl-LDH/PLLA was made considering that Mg and Ni have different atomic weights. As a first result is was found that NiAl-LDH/PLLA displays a higher crystallization rate compared to MgAl-LDH/PLLA, which is related to the different morphologies of the two nanocomposite systems. For both systems RAFcrystal increases with increasing concentration of the nanofiller. This means in the case of the nanocomposite not each crystal produces the same amount of RAF, as often assumed. Also, RAFfiller increases with the concentration for both systems but in a different way. This is discussed considering again the different morphologies of both nanocomposites.
The miraculously preserved 2000-year-old Dead Sea Scrolls, ancient texts of invaluable historical significance, were discovered in the mid-20th century in the caves of the Judean desert. The texts were mainly written on parchment and exhibit vast diversity in their states of preservation. One particular scroll, the 8-m-long Temple Scroll is especially notable because of its exceptional thinness and bright ivory color. The parchment has a layered structure, consisting of a collagenous base material and an atypical inorganic overlayer. We analyzed the chemistry of the inorganic layer using x-ray and Raman spectroscopies and discovered a variety of evaporitic sulfate salts. This points toward a unique ancient production technology in which the parchment was modified through the addition of the inorganic layer as a writing surface. Furthermore, understanding the properties of these minerals is particularly critical for the development of suitable conservation methods for the preservation of these invaluable historical documents.
Aircraft main landing gear (MLG) components are commonly manufactured from low-alloyed, martensitic, ultra-high strength steels (UHSS) that have to be coated for corrosion protection, representing an expensive and environmentally harmful production step. To avoid already partly banned corrosion protection plating, the new high-alloyed UHSS, Ferrium S53 (UNS S10500), has been designed to replace lowalloyed legacy materials and has been subjected to a limited field test over five years. As with the legacy alloys, UNS S10500 has a fully hardened martensitic microstructure known to be susceptible to hydrogen assisted cracking, per se. Containing about 10 wt% Cr, steels such as S10500 are at the lower limit for corrosion resistant alloys. Similar to super-martensitic stainless steels used in the oil and gas industry, a common failure sequence in marine environments represents pitting and subsequent hydrogen assisted stress corrosion cracking (HASCC). For addressing such phenomena quantitively, as required for respective lifetime assessments of MLG components and systems, the tolerance of such materials dependent on the absorbed hydrogen concentration must be evaluated quantitatively. However, there is a lack of such valuable materials data, as well as of the fractographic behavior dependent on the hydrogen concentration that might be absorbed during HASCC. To provide an improved understanding of the hydrogen dependent mechanical and fractographic behavior, samples of the legacy AISI 4340 and the new S10500 MLG steels have electrochemically been hydrogen-saturated and subjected to tensile testing. In contrast to a previous study, this contribution for the first time focuses on materials that have been salvaged from real service used landing gear components. In this study, it has been demonstrated that the service-applied S10500 steel has not only a higher strength, but also an improved ductility in comparison to the legacy AISI 4340 steel after similar service durations that provides a higher tolerance against hydrogen concentrations that might be absorbed during potential pitting and HASCC in marine environments. In addition, it has been found that the absorbed hydrogen concentration significantly affects the fracture behavior. Interestingly, hardening of the hydrogen charged low-alloyed AISI 4340 steel changes the fracture topography from trans- toward intergranular, while hardening of the S10500 steel turned the fracture topography from inter- to transgranular at respectively high hydrogen concentrations.
Nonclassical crystallization typically occurs via the attachment of individual nanoparticles. Intuitively, materials synthesized via this route should exhibit pronounced surface roughness and porosity as a hallmark of the formation process via particle accretion. Here, we demonstrate that nonclassical mineralization of calcium carbonate allows synthesis of ultra-smooth and dense surfaces with unprece-dented root-mean-square roughness of 0.285 nm, simply by con-trolling the hydration state of the nanosized building blocks using Mg doping. High fidelity coating of corrugated substrates can even be achieved. Nonclassical crystallization can thus lead to space-filling inorganic solid-state materials transgressing the implicit porosity commonly expected for particle-driven self-organization processes.
Mechanochemically synthesized metal–organic Framework material HKUST-1 in combination with acrylonitrile butadiene styrene polymer was used to form a polymer metal–organic framework composite material by a simple extruder.
This composite filament was used for 3D printing. Xray diffraction measurements were used to prove the homogeneous distribution of the metal–organic framework in the polymer on a centimeter scale, whereas X-ray Absorption Edge Tomography using a synchrotron radiation source was able to evaluate the 3D distribution of the metal–organic framework material both in the filament and the resultant printed sample with a resolution of a few lm. Our very first data indicate that, apart from a few clusters having significantly higher Cu concentration, HKUST-1 is distributed homogeneously down to the 100 lm length scale in both polymer bulk materials in the form of clusters with a size of a few lm. Absorption Edge Tomography in combination with data fusion also allows for the calculation of the metal–organic framework amount located on the external polymer surface.
In Vivo Biotransformations of Indium Phosphide Quantum Dots Revealed by X‑Ray Microspectroscopy
(2019)
Many attempts have been made to synthesize cadmium-free quantum dots
(QDs), using nontoxic materials, while preserving their unique optical properties. Despite impressive advances, gaps in knowledge of their intracellular fate, persistence, and excretion from the targeted cell or organism still exist, precluding clinical applications. In this study, we used a simple model organism (Hydra vulgaris) presenting a tissue grade of organization to determine the biodistribution of indium phosphide (InP)-based QDs by X-ray fluorescence imaging. By complementing elemental imaging with In L-edge X-ray absorption near edge structure, unique information on in situ chemical speciation was obtained. Unexpectedly, spectral profiles indicated the appearance of In−O species within the first hour post-treatment, suggesting a fast degradation of the InP QD core in vivo, induced mainly by carboxylate groups. Moreover, no significant difference in the behavior of bare core QDs and QDs capped with an inorganic Zn(Se,S) gradient shell was observed. The results paralleled those achieved by treating animals with an equivalent dose of indium salts, confirming the preferred bonding type of In3+ ions in Hydra tissues. In conclusion, by focusing on the chemical identity of indium along a 48 h long journey of QDs in Hydra, we describe a fast degradation process, in the absence of evident toxicity. These data pave the way to new paradigms to be considered in the biocompatibility assessment of QD-based biomedical applications, with greater emphasis on the dynamics of in vivo biotransformations, and suggest strategies to drive the design of future applied materials for nanotechnology-based diagnosis and therapeutics.
With the goal to improve their photostability, InP-based QDs are passivated with three types of inorganic shells, namely (i) a gradient ZnSexS1−x shell, (ii) an additional ZnS shell on top of the gradient shell with two different thicknesses (core/shell/shell, CSS), (iii) an alumina coating on top of ZnS. All three systems have photoluminescence Quantum yields (PLQY) > 50%and similar PL decay times (64–67 ns). To assess their photostability they are incorporated into a transparent poly (methyl methacrylate) (PMMA) matrix and exposed to continuous irradiation with simulated sunlight in a climate chamber. The alumina coated core/shell system exhibits the highest stability in terms of PLQY Retention as well as the lowest shift of the PL maximum and lowest increase of the PL linewidth, followed by the CSS QDs and finally the gradient shell system. By means of XPS studies we identify the degradation of the ZnS outer layer and concomitant xidation of the emissive InZnP core as the main origins of degradation in the gradient structure. These modifications do not occur in the case of the alumina-capped sample, which exhibits excellent chemical stability. The gradient shell and CSS systems could be transferred to the aqueous phase using surface ligand exchange with penicillamine. Cytotoxicity studies on human primary keratinocytes revealed that exposure for 24 h to 6.25–100 nM of QDs did not affect cell viability. However, a trend toward reduced cell proliferation is observed for higher concentrations of gradient shell and CSS QDs with a thin ZnS shell, while CSS QDs with a thicker ZnS shell do not exhibit any impact.