Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2019 (27) (entfernen)
Dokumenttyp
- Vortrag (27)
Referierte Publikation
- nein (27)
Schlagworte
- MIC (8)
- Corrosion (7)
- Methanogens (6)
- Archaeometry (4)
- Ink (4)
- Coptic (3)
- Manuscripts (3)
- Arabic Recipes (2)
- Archaea (2)
- Cultural heritage (2)
- Environmental Simulation (2)
- HI-Tension (2)
- Inks (2)
- Material science (2)
- Microbiologically influenced corrosion (2)
- Nanomaterialien (2)
- Non destructive analytical techniques (2)
- Sulfate reducing bacteria (2)
- 3D inspection (1)
- Additive Fertigung (1)
- Additive Manufacturing (AM) (1)
- Additive manufacturing (1)
- Advanced Materials (1)
- Aerosol measurements (1)
- Arabic recipes (1)
- Black Ink (1)
- Bundesoberbehörden (1)
- Codicology (1)
- Corrosion product (1)
- Corrosion products (1)
- DIN EN 16516 (1)
- DIN EN 717-1 (1)
- Emissionsprüfkammer (1)
- Environmental simulation (1)
- Flow-system (1)
- Formaldehyd (1)
- Forschungsstrategie (1)
- Fume (1)
- Gesteinskorrosion (1)
- Glass scanning (1)
- In situ (1)
- Ink terminology (1)
- Interdisciplinary (1)
- Kraftstoffabbau (1)
- Kraftstoffbehälter (1)
- Laser Powder Bed Fusion (L-PBF) (1)
- Leather (1)
- Metal reducing bacteria (1)
- Metallkorrosion (1)
- Metalls (1)
- Microbial (1)
- NDT (1)
- Nano (1)
- Nanorods (1)
- Nanotechnologie (1)
- Neuartige Materialien (1)
- Optische Tomografie (1)
- Papyrus (1)
- Parchment (1)
- Particle gas emission (1)
- Plume (1)
- Process monitoring (1)
- Prozessmonitoring (1)
- Restoration and conservation (1)
- SRB (1)
- Spatter (1)
- Stained glass (1)
- Structured light scanning (1)
- Tanning (1)
- Thermografie (1)
- X-ray spectroscopic techniques (1)
- XANES (1)
Organisationseinheit der BAM
- 4 Material und Umwelt (27) (entfernen)
Eingeladener Vortrag
- nein (27) (entfernen)
The Interdisciplinary Alchemist: Reproduction and Study of Black Inks from the Islamicate World
(2019)
The identification of the materials constituting an artefact is the basis of any correct conservation project, for this reason (among others) in the last 50 years analytical techniques have been applied to the study of manuscripts. Unfortunately, the scientific investigation of Arabic books is still uncommon, focusing mainly on single case studies, often producing unclear results, especially for black inks. This lack of knowledge prompted a recent research in which black ink recipes have been collected from written Arabic sources on bookmaking, their feasibility has been assessed, and finally some of them have been reproduced. These samples were artificially aged and analysed through an array of analytical techniques, mostly non-invasive and non-destructive, in order to build a database of Arabic inks and their ingredients and also to verify the detection limits of the portable equipment employed. In this talk I will present some instances of how this approach can help textual criticism, for example in evaluating variants and determining the competence of authors and compilers. At the same time the research highlights how much this scientific work depends on textual studies, especially concerning the identification of ingredients. Moreover, I will focus on some of the problematics I faced both during the textual interpretation and the actual reproduction of the recipes and how they influenced the results of the scientific analyses. In particular I’ll look into the role played by the degree of purity of the components and the function (real and perceived) of some of the ingredients.
Die gemeinsame Forschungsstrategie der Bundesoberbehörden zur Nanotechnologie wurde 2016 veröffentlicht. Die darin enthaltenen Aufgaben wurden von den Bundesoberbehörden vielfältig bearbeitet. Diese Präsentation gibt einen Überblick über die Projekte, die von der BAM bis 2019 bearbeitet wurden/werden und sich in den Rahmen der Forschungsstrategie einordnen.
Das Prozessmonitoring stellt einen wichtigen Baustein für eine Qualitätssicherung additiv gefertigter Bauteile dar, insbesondere bei kleinen Losgrößen. Der Vortrag zeigt einen Überblick aktueller Entwicklungen der BAM im Bereich des Prozessmonitorings für das Laserstrahlschmelzen (laser powder bed fusion) metallischer Werkstoffe. Durch Vergleich mit der Referenzmethode Computertomografie wird am Beispiel der thermografischen Verfahren gezeigt, wie relevante Defekte in Bauteilen detektiert werden können und Einsatzpotenziale sowie Limitierungen aufgezeigt.
The project ProMoAM is presented. The goal of the project is to evaluate which NDT techniques or combination of techniques is suited for in-situ quality assurance in additive manufacturing of metals. To this end, also 3d-data fusion and visualization techniques are applied. Additional ex-situ NDT-techniques are used as references for defect detection and quantification. Feasability studies for NDT-techniques that are presently not applicable for in-situ use are performed as well.
The presentation gives a brief overview of the whole project and the different involved NDT-techniques.
Neuartige Materialien, die bekannte (Werk-)Stoffe mit neuen Funktionalitäten ausstatten, spielen eine zunehmend wichtige Rolle im Bereich der Materialforschung und -prüfung. Das Spektrum neuartiger Materialien reicht von der gezielten Oberflächenfunktionalisierung und -strukturierung makroskopischer Materialien, dünnen Beschichtungen bis hin zu mikro- und nanoskaligen Kompositmaterialien und funktionalen Materialien an der Schnittstelle zur Biologie, Biotechnologie, nachhaltige Energiespeicherung und Sensorik. Dabei bieten neuartige Materialien die Chance, Werkstoffe und Produkte mit erweiterter oder verbesserter Funktionalität zu erhalten und Sicherheit bereits im Designprozess zu berücksichtigen. Durch dieses breite Anwendungsspektrum und die Herausforderungen, die solche Materialien für die Sicherheit in Chemie und Technik mit sich bringen, sind diese in allen Themenfeldern der BAM repräsentiert (Material, Analytical Sciences, Energie, Infrastruktur und Umwelt).
Die Aufgaben der BAM erstrecken sich dabei von der Herstellung von Referenzmaterialien für Industrie, Forschung und Regulation, über die Erstellung von standardisierten Referenzverfahren für nachhaltige Messungen im Umwelt- und Lebenswissenschaftsbereich bis hin zur Bereitstellung von belastbaren und zitierbaren Referenzdaten. Durch die genaue Charakterisierung neuartiger Materialien können potentiell problematische Substanzen identifiziert und deren Risiken besser abgeschätzt werden. In diesem Beitrag werden einige aktuelle Beispiele aus diesen Bereichen vorgestellt.
Parchment
(2019)
This lecture will present history of parchment based on written sources and chemical examination of antique, medieval and modern parchment.
Our studies of the Dead Sea Scrolls writing surfaces show that they can be divided roughly into three groups: leather, parchments of a light tint, and those of various shades of brown. The latter ones are invariably tanned, whereas the middle group is characterized by the presence of various inorganic salts. Some of the pale parchments, among them the Temple Scroll (11Q19), are remarkably similar to medieval European parchment. Therefore we have formulated the working theory that in the Judaea of the Hellenistic period two different parchment-making traditions existed side by side: an ‘eastern’ one (represented by the tanned parchments of Qumran, closely resembling Aramaic documents from the fifth century BC, and a ‘western’ one (represented by the untanned/lightly tanned ones similar to early Christian Greek parchments).
This division has found support during our studies of the Geniza fragments, in which Babylonian and Palestinian traditions seem to follow the “eastern” and “western” technologies, respectively.
The lecture traces the origins of paper, the manufacture and the spread from China to the Middle East and Europe.
Though technological progress considerably affected each step of the manufacture of paper, the essence of the invention remains unchanged until today. The process of manufacturing handmade paper can be divided into a number of steps:
- choosing the raw material (e.g. cellulose from wood, cotton, rags)
- beating and grinding the fibres into small pieces
- producing a liquid pulp of the desired texture
- treating the pulp with various additives
- filling the pulp suspension into a paper mould
- draining the water
- pressing and drying to get the actual sheet
- various post-production treatments
We will see how the manufacturing process is reflected in the properties of the paper and its degradation. A special attention will be paid to the instrumental analysis for identification of the paper types. Also watermark play an important role in the studies of the manuscripts. A short overview will be offered at the ends of the lecture.
Laser Powder Bed Fusion (L-PBF) is a promising additive manufacturing (AM) technology for metal part production especially for complex and lightweight structures or functional designs. In L PBF processes several by-products including welding plume and its condensates, spatter and ejected powder are generated during laser exposure. Investigations of micro- and nano-sized by-products have received little attention in literature. This study focuses on the analysis of particle emissions in L PBF of 316L stainless steel using a scattered light aerosol spectrometer and a fast mobility particle sizer spectrometer during the process which allows for in-situ analysis of particle sizes in the range of 6 nm to 100 µm. A distinct correlation of emission signals to part position can be revealed. In addition, a significant influence of laser scanning vector directions on emission signals is presented. Furthermore, differing powder layer thicknesses can be recognised by deviations in emission signals.
Microbially influenced corrosion (MIC) of iron is usually attributed to sulfate-reducing microorganisms (SRM) which act upon the metal by the reactiveness of hydrogen sulfide, and by withdrawal of the available electrons in electrical contact with the metal. Methanogenic archaea can also cause MIC by directly withdrawing electrons from the iron surface for methanogenesis. However, the mechanistic details and kinetics of the overall process are poorly understood. Precipitation of siderite, a by-product of methanogenesis, (4Fe + 5HCO3 + 5H+ 4FeCO3 + CH4 + 3H2O) can lead to an insulating layer on the metal surface and lower the corrosion rate. Still, the extent of FeCO3 precipitation may be significantly influenced by environmental conditions such as pH and advective processes.
Microbiologically influenced corrosion (MIC) of iron is usually attributed to sulfate-reducing microorganisms (SRM) in offshore industries, such as the oil and gas pipelines, due to the high concentrations of sulfate in the seawater. SRM act upon the metal by the reactiveness of hydrogen sulfide (HS-), and by withdrawal of the available electrons (Fe --> Fe2+ + 2e-; E° = -0.47 V) in electrical contact with the metal (EMIC). However, methanogenic archaea can also cause MIC. Because they do not produce HS-, withdrawal of electrons may be their main corrosive mechanism; however, mechanistic details and kinetics of the overall process are poorly understood.
To investigate the corrosion potential of methanogens, we studied the EMIC methanogenic strains isolated from marine sediments (Methanobacterium-affiliated strain IM1) and crude oil tanks (Methanococcus maripaludis Mic1c10), in an in-house developed flow-through cell to simulate a fluctuating environment. A co-culture of M. maripaludis and D. alaskensis was also established to study the effect of syntrophic growth on metal corrosion that may occur in industrial pipelines. Results indicate that the rates of iron corrosion due to coupled methanogenesis (up to 0.4 mm/yr) are higher to that caused by the marine SRM Desulfovibrio alaskensis (0.15 mm/yr). Surface analyses of the metal showed severe pitting with high methane production. Genomic analysis of the EMIC methanogen M. maripaludis Mic1c10 will provide an insight on the mechanisms of MIC. Such knowledge and deeper understanding also from an electrokinetic point of view may not only provide further models in microbial electrophysiology, but also contribute to mitigation strategies in MIC
Microbiologically influenced corrosion (MIC) of iron is usually attributed to sulfate-reducing microorganisms (SRM) in offshore industries, such as the oil and gas pipelines, due to the high concentrations of sulfate in the seawater. SRM act upon the metal by the reactiveness of hydrogen sulfide (HS-), and by withdrawal of the available electrons (Fe --> Fe2+ + 2e-; E° = -0.47 V) in electrical contact with the metal (EMIC). However, methanogenic archaea can also cause MIC. Because they do not produce HS-, withdrawal of electrons may be their main corrosive mechanism; however, mechanistic details and kinetics of the overall process are poorly understood.
To investigate the corrosion potential of methanogens, we studied the EMIC methanogenic strains isolated from marine sediments (Methanobacterium-affiliated strain IM1) and crude oil tanks (Methanococcus maripaludis Mic1c10), in an in-house developed flow-through cell to simulate a fluctuating environment. A co-culture of M. maripaludis and D. alaskensis was also established to study the effect of syntrophic growth on metal corrosion that may occur in industrial pipelines. Results indicate that the rates of iron corrosion due to coupled methanogenesis (up to 0.4 mm/yr) are higher to that caused by the marine SRM Desulfovibrio alaskensis (0.15 mm/yr). Surface analyses of the metal showed severe pitting with high methane production. Genomic analysis of the EMIC methanogen M. maripaludis Mic1c10 will provide an insight on the mechanisms of MIC. Such knowledge and deeper understanding also from an electrokinetic point of view may not only provide further models in microbial electrophysiology, but also contribute to mitigation strategies in MIC
Microbiologically influenced corrosion (MIC) of iron is usually attributed to sulfate-reducing microorganisms (SRM) in oil and gas facilities. SRM act upon the metal by the re-activeness of hydrogen sulfide (HS-), and by withdrawal of the available electrons in electrical contact with the metal (EMIC). Methanogenic archaea (MA) can also cause MIC (Mi-MIC). Several MAs were identified to be corrosive by using elemental iron as the sole electron donor for methanogenesis, including Methanobacterium-affliated IM1 and Methanococcus maripaludis Mic1c10. Currently, low corrosion rates were reported for MA, possibly due to the formation of siderite (4Fe + 5HCO3- + 5H+ ® 4FeCO3 + CH4 + 3H2O). Since MA do not produce HS-, withdrawal of electrons may be their main corrosive mechanism; however, mechanistic details and kinetics of the overall process are poorly understood.
To investigate the corrosion potential of MA, we studied the EMIC methanogenic strains (IM1 and Mic1c10) individually or part of a syntrophic co-culture with SRM. Corrosion studies were conducted using an in-house developed flow-through system to simulate fluctuating environmental conditions. Results indicate that the rates of iron corrosion by MA (up to 0.4 mm/yr) are higher to that caused by the marine SRM Desulfovibrio alaskensis (0.15 mm/yr) and the co-culture (0.1 mm/yr). Scanning electron microscopy (SEM) images of the metal incubated with MA showed severe pitting corrosion. Genomic analysis of the EMIC MA was conducted to provide an insight on the possible cellular mechanisms that could be involved. Furthermore, low concentrations of MA-targeting biocides will be applied to EMIC MA in static and flow conditions to gain insights for possible mitigation strategies. Such knowledge and deeper understanding also from an electrokinetic point of view may not only provide further models in microbial electrophysiology, but also contribute to mitigation strategies in MIC.
Microbiologically influenced corrosion (MIC) of iron is usually attributed to sulfate-reducing microorganisms (SRM) in offshore industries, such as the oil and gas pipelines, due to the high concentrations of sulfate in the seawater. SRM act upon the metal by the reactiveness of hydrogen sulfide (HS-), and by withdrawal of the available electrons (Fe --> Fe2+ + 2e-; E° = -0.47 V) in electrical contact with the metal (EMIC). However, methanogenic archaea can also cause MIC. Because they do not produce HS-, withdrawal of electrons may be their main corrosive mechanism; however, mechanistic details and kinetics of the overall process are poorly understood.
To investigate the corrosion potential of methanogens, we studied the EMIC methanogenic strains isolated from marine sediments (Methanobacterium-affiliated strain IM1) and crude oil tanks (Methanococcus maripaludis Mic1c10), in an in-house developed flow-through cell to simulate a fluctuating environment. A co-culture of M. maripaludis and D. alaskensis was also established to study the effect of syntrophic growth on metal corrosion that may occur in industrial pipelines. Results indicate that the rates of iron corrosion due to coupled methanogenesis (up to 0.4 mm/yr) are higher to that caused by the marine SRM Desulfovibrio alaskensis (0.15 mm/yr). Surface analyses of the metal showed severe pitting with high methane production. Genomic analysis of the EMIC methanogen M. maripaludis Mic1c10 will provide an insight on the mechanisms of MIC. Such knowledge and deeper understanding also from an electrokinetic point of view may not only provide further models in microbial electrophysiology, but also contribute to mitigation strategies in MIC.
Microbiologically influenced corrosion (MIC) of iron is usually attributed to sulfate-reducing microorganisms (SRM) in offshore industries, such as the oil and gas pipelines, due to the high concentrations of sulfate in the seawater. SRM act upon the metal by the reactiveness of hydrogen sulfide (HS-), and by withdrawal of the available electrons (Fe --> Fe2+ + 2e-; E° = -0.47 V) in electrical contact with the metal (EMIC). However, methanogenic archaea can also cause MIC. Because they do not produce HS-, withdrawal of electrons may be their main corrosive mechanism; however, mechanistic details and kinetics of the overall process are poorly understood.
To investigate the corrosion potential of methanogens, we studied the EMIC methanogenic strains isolated from marine sediments (Methanobacterium-affiliated strain IM1) and crude oil tanks (Methanococcus maripaludis Mic1c10), in an in-house developed flow-through cell to simulate a fluctuating environment. A co-culture of M. maripaludis and D. alaskensis was also established to study the effect of syntrophic growth on metal corrosion that may occur in industrial pipelines. Results indicate that the rates of iron corrosion due to coupled methanogenesis (up to 0.4 mm/yr) are higher to that caused by the marine SRM Desulfovibrio alaskensis (0.15 mm/yr). Surface analyses of the metal showed severe pitting with high methane production. Genomic analysis of the EMIC methanogen M. maripaludis Mic1c10 will provide an insight on the mechanisms of MIC. Such knowledge and deeper understanding also from an electrokinetic point of view may not only provide further models in microbial electrophysiology, but also contribute to mitigation strategies in MIC.zeige weniger
Inks and pigments
(2019)
The writing materials used in various cultures and epochs can be divided into two groups. The first comprises materials that write themselves, producing script by rubbing their own material off onto the writing surface. It includes charcoal, graphite, chalk, raddle, and metal styluses. Depending on the material and consistency, these are cut or pressed to make styluses and then used for writing.
The second group comprises all coloring liquids that are applied to the writing surface with a quill, pen, or printing block. It includes inks made from dye solutions (for example, tannin inks) and those made from pigment dispersions (for example, sepia, soot, and bister inks). The latter are sometimes also rubbed as pastes into letters incised into the writing surface, where they increase visual contrast.
Due to the variety of recipes and the natural origin of raw materials, there is a wide range of different components and impurities in writing materials.
Soluble inks (Tinten)
Soluble inks are based mainly on dyes forming a water solution. Colored inks were manufactured with different plant or insect dyes (e.g. Brazil wood, kermes). To stabilize the volatile material, the dyes were mixed with a mordant (e.g., alum).
Brown plant inks – best-known as blackthorn or Theophilus’ inks – are usually produced from the blackthorn bark and wine. In the early European Middle Ages, inks of this kind were widely used in the production of manuscripts in monasteries. Usually, they are light brown, so sometimes small amounts of iron sulfate were added, which led to what was called an “imperfect” iron gall ink. The difference between “classic” iron gall ink and such imperfect ink is therefore not clear: the distinction is not possible, especially with the naked eye.
Dispersion inks (Tuschen)
According to its generic recipe, one of the oldest black writing materials is produced by mixing soot with a binder dissolved in a small amount of water. Thus, along with soot, binders such as gum arabic (ancient Egypt) or animal glue (China) are among the main components of soot inks. From Pliny’s detailed account of the manufacture of various soot-based inks, we learn that, despite its seeming simplicity, producing pure soot of high quality was not an easy task in Antiquity. Therefore, we expect to find various detectable additives that might be indicative of the time and place of production. One such carbon ink requires the addition of copper sulfate . The experimental discovery of this ink in 1990 led to a misleading expression “metal ink” that is sometimes found in the literature.
Colored dispersion inks based on pigments such as orpiment, cinnabar, or azurite have been known since Antiquity. Natural or artificially produced minerals are finely ground and dispersed in a binding medium. As in soot inks, water-soluble binders such as gum arabic or egg white were used.
Iron gall ink (Eisengallustinten)
Iron gall inks are a borderline case between these two groups. They are produced from four basic ingredients: galls, vitriol as the main source of iron, gum arabic as a binding media, and an aqueous medium such as wine, beer, or vinegar. By mixing gallic acid with iron sulfate, a water-soluble ferrous gallate complex is formed; this product belongs to the type “soluble inks”. Due to its solubility, the ink penetrates the writing support’s surface, making it difficult to erase. Exposure to oxygen leads to the formation of insoluble black ferric gallate pigment, i.e., “dispersion ink”.
Natural vitriol consists of a varying mixture of metal sulfates. Since for ink making it was obtained from different mines and by various techniques, inks contain many other metals, like copper, aluminum, zinc, and manganese, in addition to the iron sulfate. These metals do not contribute to color formation in the ink solution, but possibly change the chemical properties of the inks.
Ink recipes from the islamic era: Texts, manuscripts, ink reproductions and scientific analyses
(2019)
Ink recipes can often be found in Arabic manuscripts. They may be included in treatises of diverse subjects – from handbooks for secretaries or calligraphers to books on arts and crafts, to alchemical and astrological essays. Recipes can also appear, with or without relation to the main text in the manuscript, in the form of lists or collections or even added in empty spaces as single entries. Why were these recipes written down? Were they used by the many professionals dealing with inks in their every-day work? Or were they part of the literary genre of adab with little or no practical application? To answer these questions a research project was set up: ink recipes have been collected from written Arabic sources, their feasibility has been assessed and some of them have been reproduced. These samples were artificially aged and analysed through an array of analytical techniques, most non-invasive and non-destructive, and the results compared to the data obtained by the application of the same analyses on concrete manuscripts. The codicological characteristics of the manuscripts have also been studied. My aim in this talk is to show how such an interdisciplinary approach could be beneficial for the study of material culture.
Papyrus was in use in the Islamic world until the 11th century and few ink recipes collected from treatises about the art of the books are dedicated to this support. But papyrus was also burnt in order to obtain soot used as an ingredient for a particular type of ink (midād al-qarāṭīs). In this talk I will give an overview of the recipes – in particular those by ar-Rāzī –, their context and transmission in order to evaluate this double nature of papyrus, which is considered at the same time a writing support and a material to be recycled. Moreover, I will discuss what kinds of ink are most likely to be found, according to these literary sources, on Arabic manuscripts and documents written on papyrus and compare them to the typologies mentioned for paper and parchment. These results are the premises of a research project starting at the beginning of 2019, in which a number of dated fragments from several European institutions will be analysed with non-destructive techniques in order to establish a profile of the main writing media used in the early centuries of the Islamic Era.
Die von der BAM eingekauften Holzwerkstoffplatten (Verlegespanplatten, OSB, Multiplexplatten) verschiedener Hersteller zeigten teilweise hohe Formaldehyd-emissionen unter den Prüfbedingungen nach EN 16516, eine Spanplatte hielt den Grenzwert von 0,1 ppm selbst bei Prüfung nach DIN EN 717-1 nicht ein, dürfte also in Deutschland gar nicht in den Verkauf gelangen.
Holzwerkstoffe, die unter den Prüfbedingungen der DIN EN 717-1 die Formaldehydklasse E1 einhalten, können insbesondere bei großflächigem Einsatz im Innenraum zu Überschreitungen des Richtwertes für die Innenraumluft führen. Zusätzlich zur Anpassung des Luftwechsels ist auch der Parameter Beladung bei einer Überarbeitung der Norm anzupassen. In der DIN EN 16516 werden produktspezifische (am Einsatz der Produkte orientierte) Beladungsfaktoren vorgegeben. Für den Einsatz von Holzwerkstoffplatten ergäben sich Beladungen von 0,4 (Boden oder Decke), 1,0 (Wände), 1,4 (Wände plus Boden oder Decke) und 1,8 m²/m³ (Wände, Boden und Decke). Um die realen Bedingungen in modernen Gebäuden abzubilden, ist deshalb eine Beladung von 1,8 m²/m³ für die Prüfkammermessung erforderlich. Hierbei ist darauf hinzuweisen, dass für die Beladung im Referenzraum Möbel nicht berücksichtigt wurden.
Damit soll sichergestellt werden, dass die Einhaltung des Schutzniveaus bei realen Innenraumbedingungen auch unter den Randbedingungen eines niedrigen Luftwechsels sowie bei sommerlichen Bedingungen und heutigem Lüftungsverhalten der Menschen soweit wie möglich gewährleistet ist.
Fifty shades of black: Typologies and terminology of black inks in the light of new discoveries
(2019)
The identification of the materials constituting an artefact is the basis of any correct conservation project. For this reason (among others) in the last 50 years analytical techniques have been applied to the study of manuscripts. Unfortunately, the scientific investigation of Arabic books is still uncommon, focusing mainly on single case studies of illuminated manuscripts where the black media used to write the text is largely overlooked. This lack of knowledge prompted a recent research in which black ink recipes have been collected from written Arabic sources, their feasibility has been assessed, and some of them have been reproduced. These samples were artificially aged and analysed through an array of analytical techniques, mostly non-invasive and non-destructive, in order to build a database of Arabic inks and their ingredients and to verify the detection limits of the equipment employed. Finally, the results were compared to the data collected from historical manuscripts.
In this talk I will focus on the ink typologies and the terminology (ancient and modern) used to describe them. In particular I will highlight how even the modern classification fails to capture the variety encountered in both recipes and manuscripts, particularly in the light of recent discoveries. I will address especially the terminological and conceptual issues of mixed inks – in the form of carbon inks and tannins, of carbon and iron gall inks, and of carbon and metallic salts –, iron gall inks made without vitriol and iron gall inks made with sources of tannins different from gall nuts.
Microbiologically induced corrosion due to bacterial biofilms causes several problems in industrial systems, technical applications and in medicine. Prior to the formation of a biofilm on a substrate, planktonic cells attach on the surface. Hence, the properties of the surface play a key role in biofilm formation and are of great importance for the development of strategies to prevent bacterial attachment and biofilm formation.
This project aims at clarifying to which extent surface micro-/nanostructuring and chemical functionalization affects bacterial attachment and whether a synergistic combination of the two can be used to control bacterial adhesion. To answer these questions, model surfaces with regular patterns of 5-10 micrometers in size have been prepared, which provide distinct zones differing in terms of their chemistry or nano-roughness. This was achieved by micro contact printing of self-assembled monolayers with different functional groups and deposition of patterned ZnO nanorod arrays for studying the effect of surface chemistry and morphology, respectively. Typical contrasts studied were combinations of positively/negatively charged, hydrophobic/hydrophilic or flat/rough.
The attachment behavior of bacteria on tailored surfaces were studied in a flow chamber as a function of time. The strain Pseudomonas fluorescens SBW25 was chosen as a model organism. DNA-intercalating dyes such as Syto9 have a high affinity to adsorb on ZnO nanorods. To overcome this limitation a genetic modification was performed by introducing a gene which expresses a green fluorescent protein in P. fluorescens SBW25 enabling the quantitative evaluation of the flow chamber studies by means of fluorescence microscopy. Further analysis of the attachment behavior was performed by means of scanning electron microscopy.
The presentation will summarize the results of our systematic study on the role of individual parameters on bacterial attachment and highlight synergistic combinations, showing an inhibition or enhancing effect. As the investigations with model substrates enable a precise control of the surface parameters, this approach can be applied to different microorganisms and material systems to achieve a correlative description of bacterial adhesion on solid surfaces.
The initial focus of this research was on the development of a general workflow for the documentation and monitoring of historical stained glass windows using structured light scanning.
Therefore windows from different churches, time periods and with different corrosion and damage phenomena were scanned before and after conservation measures.