The life time of mechanical components in high temperature applications is basically determined by their workings. Corrosion determines the loss of material corresponding to the loss of the effective load-bearing section and consequently increasing stress levels. To improve the material selection for such applications a numerical life prediction corrosion model for different alloys and environments is needed. Based on the ferritic alloys FeCr and FeCrCo a first quantitative model is to be developed. For this purpose, the alloys are aged at 600°C, 650°C and 700°C in synthetic air under normal pressure for between 10 and 240 hours. The first objective is to establish a quantitative relationship between the oxidation rate as a function of composition and microstructure of the alloys. The influence of the inner interface as an essential parameter for transport by diffusion on the oxidation kinetics is discussed in this presentation.
Chromia forming high alloyed ferritic-austenitic steels are being used as boiler tube materials in biomass and coal-biomass co-fired power plants. Despite thermodynamic and kinetic boundary conditions, microstructural features such as grain orientation, grain sizes or surface deformation contribute to the oxidation resistance and formation of protective chromium-rich oxide layers. This study elucidates the impact of microstructure such as the grain size and number of carbide precipitates on high temperature oxidation at 650°C in 0.5% SO2 atmosphere. Cold-rolled Fe-16Cr-0.2C material was heat-treated to obtain two additional microstructures. After exposure to hot and reactive gases for 10 h < t < 1000 h layer thicknesses and microstructure of oxide scales are observed by scanning electron microscopy and Energy-dispersive X-ray spectroscopy. The two heat treated alloys showed reasonable oxidation resistance after 1000 h of exposure. The oxidation rate was substantially higher for the alloy with a duplex matrix after heat treatment compared to the fine-grained material.
The fundamental impact of sulfur and water on corrosion rates and potential failure of the exposed material is well known. However, the access to the related corrosion mechanism causing material degradation is often a problem to solve. This study investigates the effect of SO2 and water vapor in the initial stages of corrosion of an Fe9Cr0.5Mn model alloy at 650 °C in situ. The analysis was carried out under laboratory conditions using energy-dispersive X-ray diffraction (EDXRD).
Oxidation of a Fe-13Cr alloy under water vapor at 600 °C produced a zone of nano-sized precipitation underneath the outside scale formed by iron oxides and Fe‒Cr spinel. The majority of the spinel layer shows a mixed orientation relationship to the ferritic matrix {100}α || {100}sp & <011>α || <001>sp. However, also the discovered precipitated particles are characterized by the same crystallographic orientation relationship to the respective ferritic parent grain. The habit of the precipitates is best described by a lath morphology with their main axis parallel to <100> of ferrite.
Energy dispersive X-ray spectroscopy (EDX) and electron backscatter diffraction (EBSD) in an scanning electron microscope (SEM) have been applied to characterize the oxide layer in the micrometer scale. The clearly smaller precipitates were subsequently investigated by transmission electron microscopy (TEM). Specimens have been prepared by focused ion-beam (FIB) milling at an area previously characterized by EBSD. They cover the ferritic base material, but mainly the precipitation zone and the Fe‒Cr spinel layer. Energy filtered selected area diffraction (SAD) in the conventional (C)TEM and high-angle annular darkfield (HAADF) imaging in the scanning (S)TEM mode were employed in the characterization of the specimens.
Commercial grade-1 titanium samples (Ti, 99.5% purity) were treated using three alternative methods, i.e., fs-laser processing in air, thermal heat treatment in an oven, or anodization in an electrochemical bath, all resulting in the formation of differently conditioned superficial oxide layers. The laser processing was carried out by a Ti:sapphire laser (pulse duration 30 fs, central wavelength 790 nm, pulse repetition rate 1 kHz) in a regime of generating laser-induced periodic surface structures (LIPSS). The experimental conditions (laser fluence, spatial spot overlap) were optimized in a sample-scanning geometry for the processing of several square-millimetres large surface areas covered homogeneously by these nanostructures. The thermal processing in the oven was done at two different temperatures, while the electrochemical anodization was performed at room temperature, aiming to generate different polymorphs of titanium oxide at similar oxide layer thickness. The irradiated surface regions were characterized by optical and scanning electron microscopy, and micro Raman spectroscopy. The tribological performance of the differently treated titanium surfaces was characterized in the regime of mixed friction by reciprocating sliding tests against a sphere of hardened steel in un-additivated paraffin oil and fully formulated engine oil as lubricants. The specific tribological performance of the differently treated surfaces is discussed on the basis of possible physical and chemical mechanisms.
Mechanical characterization of high-density polyethylene in contact with diesel and biodiesel fuels
(2016)
Renewable resources become more and more relevant to maintain energy demands for an increasing global population. Biosynthetic fuels like biodiesel might replace conventional petrochemical fuels, such as diesel. However, more research is needed to characterize the interaction between the different fuels and polymeric materials widely used in the fuel infrastructure as well as for automotive parts. Especially changes in the structural properties and mechanical behavior of the polyethylene (PE-HD) have to be addressed.
The presented work comprises the direct interaction of high density polyethylene (PE-HD) with diesel and biodiesel, resulting in swelling and plasticization. Also long-term degradation phenomena will be discussed.
The chosen PE-HD types are typical thermoplastic resins for container and storage tank applications. The impact of diesel and biodiesel in PE-HD is investigated by changes in the mechanical properties with emphasis on the Charpy impact strength. Furthermore, structural and dynamic influences on the polymeric material induced by diesel and biodiesel are proven in Dynamic Mechanical Analysis (DMA). Both methods, Charpy impact strength and DMA, reveal softening effects due to the migration of diesel and biodiesel into the amorphous regions of PE-HD.
Since biodiesel is more prone to oxidative degradation compared to diesel, the fuel/air/polymer-interaction is studied for partly immersed tensile test specimens. Main focus of the evaluation is the co-oxidation. Here, the accelerated deterioration of PE caused by the sorption of the facile oxidation of biodiesel into the solid polymer might be a major degradation mechanism in this context.