Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2020 (4) (entfernen)
Dokumenttyp
- Posterpräsentation (4) (entfernen)
Sprache
- Englisch (4) (entfernen)
Referierte Publikation
- nein (4)
Schlagworte
- Additive manufacturing (1)
- Computed tomography (1)
- Crystal structure (1)
- Curing Monitoring (1)
- Degradation (1)
- Extrusion (1)
- Far-infrared spectroscopy (1)
- LPBF (1)
- Laser Powder Bed Fusion (1)
- MID IR Spectroscopy (1)
- Microstructure-property relations (1)
- Neutron diffraction (1)
- Pore orientation (1)
- Preferred orientation (1)
- Residual stress (1)
- Thermography (1)
- X-ray diffraction (1)
- X-ray refraction (1)
Organisationseinheit der BAM
- 8.0 Abteilungsleitung und andere (4) (entfernen)
Rapid cooling rates and steep temperature gradients are characteristic of additively manufactured parts and important factors for the residual stress formation. This study examined the influence of heat accumulation on the distribution of residual stress in two prisms produced by Laser Powder Bed Fusion (LPBF) of austenitic stainless steel 316L. The layers of the prisms were exposed using two different border fill scan strategies: one scanned from the centre to the perimeter and the other from the perimeter to the centre. The goal was to reveal the effect of different heat inputs on samples featuring the same solidification shrinkage. Residual stress was characterised in one plane perpendicular to the building direction at the mid height using Neutron and Lab X-ray diffraction. Thermography data obtained during the build process were analysed in order to correlate the cooling rates and apparent surface temperatures with the residual stress results. Optical microscopy and micro computed tomography were used to correlate defect populations with the residual stress distribution. The two scanning strategies led to residual stress distributions that were typical for additively manufactured components: compressive stresses in the bulk and tensile stresses at the surface. However, due to the different heat accumulation, the maximum residual stress levels differed. We concluded that solidification shrinkage plays a major role in determining the shape of the residual stress distribution, while the temperature gradient mechanism appears to determine the magnitude of peak residual stresses.
Novel Technique for On-Line Monitoring of the Curing Process of Fiber Reinforced Polymer Composites
(2020)
A specially designed experimental set up has been integrated into a commercially available FT IR Spectrometer for ATR experiments on Epoxy Systems. Representative data of far infrared spectra measured during the curing process at different temperatures of an epoxy system will be presented in dependency of the curing situation. The experiments and the selected set up are discussed to demonstrate its potential for future monitoring and ageing control applications during a manufacturing process of polymer composites.
Porous ceramic diesel particulate filters (DPFs) are extruded products that possess macroscopic anisotropic mechanical and thermal properties. This anisotropy is caused by both morphologic features (mostly the orientation of porosity) and crystallographic texture. We systematically studied those two aspects in a cordierite and two aluminum titanate (AT) ceramic materials of different porosity using mercury porosimetry, gas adsorption, electron microscopy, X-ray diffraction, and X-ray refraction radiography. We found that a lower porosity in AT content implies a larger isotropy of both the crystal texture and the porous space orientation. We also found that, analogous to cordierite, AT crystallites do align with their axis of negative thermal expansion along the extrusion direction. However, unlike what found for cordierite, the aluminium titanate crystallite form is such that a more pronounced (0 0 2) texture along the extrusion direction implies porosity aligned perpendicular to it.
THz and mid IR spectroscopy of high-molecular PE (HMW) and ultra high-molecular PE (UHMW) reveals modifications of the molecular structure. Characteristic absorption bands are changed if the two materials are exposed by γ-Co60 radiation up to 600 kGy and subsequently stored at an annealing temperature of 398 K until for 729 days. UHMW-PE and HMW-PE behave differently during the ageing process because of their molecular weight and inherent structure distinctions. The spectroscopic data offer characteristic absorption bands, which have been used to describe the complete ageing process in more detail. For instance, the integral absorption in the B1u THz-region can be used to describe quantitatively the reduction of crystallinity. The formation of trans vinylene unsaturation and the decay of vinyl during ageing can be observed in detail in the mid IR range.