Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2019 (976) (entfernen)
Dokumenttyp
- Vortrag (443)
- Zeitschriftenartikel (257)
- Posterpräsentation (116)
- Beitrag zu einem Tagungsband (104)
- Sonstiges (18)
- Forschungsbericht (10)
- Buchkapitel (9)
- Dissertation (6)
- Monografie (3)
- Zeitschriftenheft (Herausgeberschaft für das komplette Heft) (3)
Sprache
- Englisch (731)
- Deutsch (235)
- Mehrsprachig (8)
- Russisch (1)
- Spanisch (1)
Schlagworte
- Additive Manufacturing (47)
- Corrosion (45)
- Korrosion (33)
- Additive manufacturing (29)
- Additive Fertigung (20)
- Microstructure (17)
- Nanoparticles (17)
- Fluorescence (16)
- Computed tomography (15)
- Mechanochemistry (14)
Organisationseinheit der BAM
- 6 Materialchemie (229)
- 9 Komponentensicherheit (215)
- 7 Bauwerkssicherheit (164)
- 8 Zerstörungsfreie Prüfung (163)
- 5 Werkstofftechnik (161)
- 9.3 Schweißtechnische Fertigungsverfahren (118)
- 7.6 Korrosion und Korrosionsschutz (96)
- 8.5 Röntgenbildgebung (84)
- 6.6 Physik und chemische Analytik der Polymere (70)
- 1 Analytische Chemie; Referenzmaterialien (68)
- 9.4 Integrität von Schweißverbindungen (63)
- 4 Material und Umwelt (55)
- 6.3 Strukturanalytik (55)
- 5.1 Mikrostruktur Design und Degradation (51)
- 8.0 Abteilungsleitung und andere (51)
- 1.2 Biophotonik (44)
- 2 Prozess- und Anlagensicherheit (43)
- 6.1 Oberflächen- und Dünnschichtanalyse (40)
- 6.2 Material- und Oberflächentechnologien (40)
- 3 Gefahrgutumschließungen; Energiespeicher (39)
- 5.4 Multimateriale Fertigungsprozesse (35)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (32)
- 6.7 Materialsynthese und Design (29)
- 5.2 Metallische Hochtemperaturwerkstoffe (28)
- 5.6 Glas (27)
- 9.5 Tribologie und Verschleißschutz (24)
- 5.3 Polymere Verbundwerkstoffe (23)
- 7.1 Baustoffe (23)
- 8.4 Akustische und elektromagnetische Verfahren (21)
- 4.5 Kunst- und Kulturgutanalyse (19)
- 6.5 Synthese und Streuverfahren nanostrukturierter Materialien (18)
- 4.1 Biologische Materialschädigung und Referenzorganismen (16)
- 9.0 Abteilungsleitung und andere (16)
- 4.2 Material-Mikrobiom Wechselwirkungen (15)
- 2.1 Sicherheit von Energieträgern (12)
- 3.2 Gefahrguttanks und Unfallmechanik (12)
- 7.4 Baustofftechnologie (12)
- 9.2 Versuchsanlagen und Prüftechnik (12)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (10)
- 1.5 Proteinanalytik (9)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (9)
- 5.5 Materialmodellierung (9)
- 2.0 Abteilungsleitung und andere (8)
- 8.6 Faseroptische Sensorik (8)
- 2.2 Prozesssimulation (7)
- 2.5 Konformitätsbewertung Explosivstoffe/Pyrotechnik (7)
- 3.0 Abteilungsleitung und andere (7)
- 3.4 Sicherheit von Lagerbehältern (7)
- 2.4 Prüfung und Bewertung von Explosivstoffen/Pyrotechnik (6)
- 5.0 Abteilungsleitung und andere (6)
- 1.4 Prozessanalytik (5)
- 3.3 Sicherheit von Transportbehältern (5)
- 1.1 Anorganische Spurenanalytik (4)
- 1.9 Chemische und optische Sensorik (4)
- 4.3 Schadstofftransfer und Umwelttechnologien (4)
- 6.0 Abteilungsleitung und andere (4)
- 9.6 Additive Fertigung metallischer Komponenten (4)
- 2.3 Einstufung von Gefahrstoffen und -gütern (3)
- 4.0 Abteilungsleitung und andere (3)
- 7.0 Abteilungsleitung und andere (3)
- S Qualitätsinfrastruktur (3)
- 7.2 Ingenieurbau (2)
- S.2 Digitalisierung der Qualitätsinfrastruktur (2)
- Z Zentrale Dienstleistungen (2)
- Z.1 Organisation, Controlling (2)
- 1.0 Abteilungsleitung und andere (1)
- 1.7 Organische Spuren- und Lebensmittelanalytik (1)
- 1.8 Umweltanalytik (1)
- 8.2 Zerstörungsfreie Prüfmethoden für das Bauwesen (1)
- P Präsident (1)
- P.0 Präsident und andere (1)
- S.0 Abteilungsleitung und andere (1)
Eingeladener Vortrag
- nein (443)
Defects as a root cause of fatigue failure of metallic components. II: Non-metallic inclusions
(2019)
This second part of the review on defects as root cause of fatigue failure comprises the origin, the nature and the effects of non-metallic inclusions. Topics addressed are the different kinds of inclusions formed during the manufacturing process, various types of mis-match causing local stresses and, as a consequence, fatigue crack initiation, and effects of characteristics such as size, morphology, localization, spatial distribution and orientation of the defects on the fatigue behavior. Methods for inclusion counting and sizing are discussed along with statistical aspects necessary to be considered when evaluating structural components.
Aktuell werden Prozessmonitoringsysteme in der additiven Fertigung (AM) zur Überwachung der Energiequelle, des Bauraums, des Schmelzbades und der Bauteilgeometrie zumindest im metallbasierten AM schon kommerziell angeboten. Weitere Verfahren aus den Bereichen der Optik, Spektroskopie und zerstörungsfreien Prüfung werden in der Literatur als geeignet für die in-situ Anwendung bezeichnet, es finden sich aber nur wenige Berichte über konkrete Umsetzungen in die Praxis.
Die Bundesanstalt für Materialforschung und -prüfung hat ein neues Projekt gestartet, dessen Ziel die Entwicklung von Verfahren des Prozessmonitorings zur in-situ Bewertung der Qualität additiv gefertigter Bauteile in AM-Prozessen mit Laser- bzw. Lichtbogenquellen ist. Verschiedene Verfahren der zerstörungsfreien Prüfung, wie Thermografie, optische Tomografie, optische Emissionsspektroskopie, Wirbelstromprüfung und Laminografie werden in verschiedenen AM-Prozessen zum Einsatz gebracht und die Ergebnisse fusioniert. Die evaluierten Ergebnisse werden mit Referenzverfahren wie Computertomografie und Ultraschall-Tauchtechnik verglichen. Ziel ist eine deutliche Reduzierung aufwändiger und zeitintensiver, zerstörender oder zerstörungsfreier Prüfungen nach der Fertigung des Bauteiles und zugleich eine Verringerung von Ausschussproduktion.
Hier wird das Projekt als Ganzes vorgestellt und der Fokus auf verschiedene Methoden der Temperaturmessung mit Hilfe der Thermografie gelegt. Anforderungen an die Messtechnik für verschiedene AM-Systeme werden diskutiert und erste experimentelle Ergebnisse werden präsentiert.
The fast and accurate detection of disease-related biomarkers and potentially harmful analytes in different matrices is one of the main challenges in the life sciences. In order to achieve high signal-to-background ratios with frequently used photoluminescence techniques, luminescent reporters are required that are either excitable in the first diagnostic window or reveal luminescence lifetimes exceeding that of autofluorescent matrix components. Here, we demonstrate a reporter concept relying on broad band emissive ternary quantum dots (QDs) with luminescence lifetimes of a few hundred nanoseconds utilized for prolongating the lifetimes of organic or inorganic emitters with lifetimes in the order of a very few 10 ns or less through fluorescence resonant energy transfer. Using spectrally resolved and time-resolved measurements of the system optical response we demonstrate the potential of lifetime multiplexing with such systems exemplarily for AgInS2/ZnS and CdSe/ZnS QDs.
Additive Fertigung hat in den letzten Jahren aufgrund der hohen Flexibilität stark an Bedeutung gewonnen. Insbesondere in der Luft- und Raumfahrttechnik werden hohe Anforderungen an die Qualitätskontrolle additiv gefertigter Bauteile gestellt. Teile die mit dem selektiven Laserschmelzen (SLM) hergestellt werden, bilden schon währen des Fertigungsprozesses Poren oder Risse aus. Aus diesem Grund ist die zerstörungsfreie Prüfung jedes Bauteils notwendig. Erste Versuche haben gezeigt, dass die ex-situ Wirbelstromprüfung von SLM-Bauteilen mit hochauflösenden MR Sonden möglich ist und dass Fehler im Bereich von einiger µm detektiert werden können. In dem Vortrag wird eine automatisierte in-situ Wirbelstromprüfung von SLM-Bauteilen vorgestellt. Für die Prüfung wird eine Vielzahl hochauflösender MR Sensoren verwendet, um die benötige hohe Ortsauflösung bei gleichzeitig kurzer Prüfzeit zu erreichen. Zusätzlich werden klassische Methoden der Signalverarbeitung verwendet, um die Kosten und die Komplexität des Systems trotz hoher Prüffrequenz zu minimieren. Das vorgestellte System kann in der Zukunft helfen automatisiert Prüfberichte zu generieren, den SLM-Prozess zu kontrollieren oder automatisiert Fehlstellen auszuheilen.
Subsurface residual stresses (RS) were investigated in Ti-6Al-4V cuboid samples by means of X-ray synchrotron diffraction. The samples were manufactured by laser powder bed fusion (LPBF) applying different processing parameters, not commonly considered in open literature, in order to assess their influence on RS state. While investigating the effect of process parameters used for the calculation of volumetric energy density (such as laser velocity, laser power and hatch distance), we observed that an increase of energy density led to a decrease of RS, although not to the same extent for every parameter variation. Additionally, the effect of support structure, sample roughness and LPBF machine effects potentially coming from Ar flow were studied. We observed no influence of support structure on subsurface RS while the orientation with respect to Ar flow showed to have an impact on RS.We conclude recommending monitoring such parameters to improve part reliability and reproducibility.
T92 steel was oxidized at 650 °C for 1000 h in dry and wet oxyfuel gases. The microstructure of inner oxide layer was investigated using scanning transmission electron microscopy and energy dispersive spectroscopy on thin lamellas of oxide cross-sections. The oxides were composed of fine equiaxed grains and separated into Fe-rich and Cr-rich regions. Fe-rich regions were wustite and iron sulphide while Cr-rich regions consisted of Fe-Cr spinel with different stoichiometries. Precipitates of (W,Mo)-rich oxides were formed within the oxide scale and beneath the oxide/alloy interface. Often iron sulphide and (W,Mo)-rich oxide were surrounded by Cr-rich spinel.
Wepresent here a systematic analysis of the influence of Tm3+ Doping concentrations (xTm) on the excitation power (P)-dependent upconversion luminescence and -performance of hexagonal-Phase NaYF4: 20% Yb3+, xTm%Tm3+ upconversion nanoparticles (UCNPs) for xTm of 0.2, 0.5, 0.8, 1.2, and 2.0, respectively. Our results reveal the influence of these differentTm3+ doping concentrations with respect to optimized upconversion quantum yield (ΦUC) values of the variousTm3+ upconversion emission bands, with the highestΦUC values of theTm3+ emission bands above 700 nmresulting for different xTm values as theTm3+ emission bands below 700 nm. This underlines the potential ofTm3+ dopant concentration for colour tuning. Special emphasis was dedicated to the spectroscopic parameters that can be linked to the (de)population pathways of the variousTm3+ energy levels, like the P- and xTm-dependent slope factors and the intensity ratios of selected emission bands. The evaluation of all parameters indicates that not only energy transfer upconversion-, but also crossrelaxation processes between neighbouringTm3+ ions play a vital role in the (de)population of the excited energy levels of Yb3+, Tm3+ codoped nanocrystals.
We present a series of results that demonstrate that the broadband photoluminescence (PL) of aqueous glutathione-capped Ag−In−S (AIS) nanocrystals (NCs) is an inherent property of each NC, rather than a collective characteristic of an NC ensemble. By analyzing parameters affecting the PL features such as the postsynthesis annealing and the deposition of a passivating ZnS shell, we found no correlation between the spectral width of the PL band of AIS (AIS/ZnS) NCs and the density of the lattice defects. Analysis of the PL spectra of a series of size-selected AIS/ZnS NCs revealed that the PL width of fractionated NCs does not depend on the NC size and size distribution. The PL measurements in a broad temperature window from 320 to 10 K demonstrated that the PL width does not decrease with decreasing temperature as expected for an emission arising from thermally activated detrapping processes. Also, we show that the model of the self-trapped exciton can be versatilely applied to reconstruct the PL spectra of different AIS NCs and can account for the effects typically attributed to variations in defect state energy. Measurements of the PL properties of single AIS/ZnS NCs highlighted the broadband nature of the emission of individual NCs. The presented results show that the broadband PL of ternary NCs most probably does not originate from lattice defects but involves the NC lattice as a whole, and, therefore, by tailoring the NC structure, PL efficiencies as high as those reported for binary cadmium or lead chalcogenide NCs can be potentially reached.
Elastomers are usually reinforced by large amount of fillers like carbon black (CB) or silica in order to improve various mechanical properties, such as Young’s modulus, hardness, tear resistance, abrasion resistance, and gas barrier properties. In recent years, such improvements were also obtained by using nanoparticles at significantly lower filler loadings. Graphene is a twodimensional (2D) sheet of a thickness in the atomic scale, composed of a honeycomb structure of sp2 carbon atoms. Besides significant mechanical reinforcement, graphene harbors the potential to be used as a multifunctional filler, as it can also increase the conductivity and weathering stability of elastomer matrices. Ultraviolet (UV) irradiation and oxidative agents can lead to the degradation of elastomers due to a multistep photooxidative process, including the formation of radicals. Carbon-based fillers have an influence on these reactions, as they can absorb UV radiation and act as radical scavengers.
This chapter summarizes the results of our larger project on multilayer graphene (MLG)/elastomer nanocomposites, previously published, which present a comprehensive case study of MLG as a multifunctional nanofiller in elastomer/graphene nanocomposites. Different elastomeric matrices are compared in order to demonstrate the outstanding impact of MLG as a general benefit. The dependency of this effect on concentration is discussed in detail. Taking into account the key role of dispersion, different mixing procedures are compared, evaluating a facile implementation of graphene nanocomposites into conventional rubber processing. Finally, the most probable commercial uses of MLG nanofillers in combination with conventional CB are studied. The nanocomposites were prepared in the kg scale in order to obtain enough specimens to investigate various properties of the uncured and vulcanized rubbers at the highest quality level, including rheology, curing, morphology, several mechanical properties, abrasion, conductivity, gas permeation, burning behavior, and weathering stability. The structure property relationships are asserted and questioned, for example, by investigating the radical scavenging ability or aspect ratio of the MLG. This chapter illustrates the state of the art of graphene/rubber nanocomposites targeted for commercial mass applications.
The quality of components made by laser beam melting (LBM) additive manufacturing is naturally influenced by the quality of the powder bed. A packing density <1 and porosity inside the powder particles lead to intrinsic voids in the powder bed. Since the packing density is determined by the particle size and shape distribution, the determination of these properties is of significant interest to assess the printing process. In this work, the size and shape distribution, the amount of the particle’s intrinsic porosity, as well as the packing density of micrometric powder used for LBM, have been investigated by means of synchrotron X-ray computed tomography (CT). Two different powder batches were investigated: Ti–6Al–4V produced by plasma atomization and stainless steel 316L produced by gas atomization. Plasma atomization particles were observed to be more spherical in terms of the mean anisotropy compared to particles produced by gas atomization. The two kinds of particles were comparable in size according to the equivalent diameter. The packing density was lower (i.e., the powder bed contained more voids in between particles) for the Ti–6Al–4V particles. The comparison of the tomographic results with laser diffraction, as another particle size measurement technique, proved to be in agreement.
Faser-Kunststoff-Verbunde (FKV) werden zunehmend in der Luft- und Raumfahrt, der Automobil- und Windenergieindustrie eingesetzt. Die hier entwickelten Bauteile sind oft nicht nur multiaxialen mechanischen Belastungen, sondern auch hohen klimatischen Beanspruchungen ausgesetzt. Einsatztemperaturen zwischen -60°C und 100°C bei 10-90% relativer Feuchte sind keine Seltenheit, in der Raumfahrt sind die thermischen Belastungen noch extremer. Die Auswirkungen einer Wechselwirkung extremer klimatischer Beanspruchungen mit multiaxialen mechanischen Belastungen wurden bisher kaum betrachtet. Das Ziel des Projektes ist die Untersuchung des Ermüdungsverhaltens der Faser-Kunststoff-Verbunde in Abhängigkeit von multiaxialer mechanischer Belastung, Temperatur und Feuchte. Dazu werden umfangreiche experimentelle Untersuchungen an Flach- und Rohrproben sowie numerische und analytische Berechnungen durchgeführt.
Im Rahmen des Seminarvortrags wird eine mikromechanische Modellierung der thermischen Eigenspannungen innerhalb des FKV vorgestellt, welche anhand eines Finite-Elemente-Modells validiert wird. Zur Bestimmung einer Schädigungsgrenze werden verschiedene Energieansätze diskutiert, welche anschließend mit den experimentell erhaltenen Ergebnissen im Temperaturbereich zwischen -60 °C und 70 °C verglichen werden. Dabei wird gezeigt, dass mithilfe der mikromechanischen Formulierung eine temperaturunabhängige Masterschädigungslinie für quasistatisch belastete Probekörper abgeleitet werden kann. Des Weiteren können Elastizitäten und Festigkeiten in Abhängigkeit der Temperatur mit den mikromechanischen Mischungsregeln bestimmt werden. So kann der experimentelle Aufwand beim Nachweis thermomechanisch belasteter Strukturen reduziert werden. Ein ähnlicher Ansatz wird für schwingende Ermüdungsbelastung bei verschiedenen Umgebungstemperaturen diskutiert und experimentell überprüft.
Editorial
(2019)
Dear Readers, a new year started for all of us (as I write these lines, possibly it was already some time ago when these lines are finally available) and this is the time for the so-called New Year’s resolutions. Setting goals and changing our behavior as well in a private as in a professional context.
For Scientists the resolutions may comprise tasks like finalizing a longago started publication, picking up the loose ends of an application for funding or just bringing the running projects in a greater structure.
Knowledge of the compressional and thermal behaviour of metals and alloys is of a high fundamental and applied value. In this work, we studied the behaviour of Ir, Rh, and their fcc-structured alloys, Ir0.42Rh0.58 and Ir0.26Os0.05Pt0.31Rh0.23Ru0.15, up to 70 GPa using the diamond anvil cell technique with synchrotron X-ray diffraction. We found that all these materials are structurally stable upon room-temperature hydrostatic compression in the whole pressure interval, as well as upon heating to 2273 K both at ambient and high pressure. Rh, Ir0.42Rh0.58 and Ir0.26Os0.05Pt0.31Rh0.23Ru0.15 were investigated under static compression for the first time. According to our data, the compressibility of Ir, Rh, fcc–Ir0.42Rh0.58, and fcc Ir0.26Os0.05Pt0.31Rh0.23Ru0.15, can be described with the 3rd order Birch-Murnaghan equation of state with the following parameters: V0 = 14.14(6) Å3·atom−1, B0 = 341(10) GPa, and B0' = 4.7(3); V0 = 13.73(7) Å3·atom−1, B0 = 301(9) GPa, and B0' = 3.1(2); V0 = 13.90(8) Å3·atom−1, B0 = 317(17) GPa, and B0' = 6.0(5); V0 = 14.16(9) Å3·atom−1, B0 = 300(22) GPa, B0' = 6(1), where V0 is the unit cell volume, B0 and B0' – are the bulk modulus and its pressure derivative.
Active thermography is a well suited non-destructive testing method for the challenging inspection of wind rotor blades. Since the GFRP structures are up to some centimetres thick, long pulse heating is required to provide an appropriate energy input into the structure. So far, no best practice exists to guarantee a reliable detection of deep-lying flaws. In this work, a step wedge specimen having a maximum thickness of 34mm is systematically investigated by experiment and well-matched simulations to assess the influence of the experimental parameters, like the absorbed energy, on thermal contrasts. Finally, a scheme to conduct full-scale test of a wind rotor blade in less than three hours is proposed.
Absorption edge tomography is a method which exploits the sudden change of the attenuation coefficient, when the photon energy crosses the absorption edge of an element. The beamline BAM line at BESSY II, which is operated by the Federal Institute for Materials Research and Testing, can provide a monochromatized beam in a photon energy range from 5 keV up to 80 keV with a bandwidth of 2%. Together with the microtomography setup, this enables differential tomography sensitive to any element with N >= 24 (Cr) by using an appropriate K- or L-edge in this range. Here, a polymer filament embedding metal organic framework (MOF) was prepared and used for 3D printing. Absorption edge tomography at the copper K edge was employed to perform a non-destructive 3D characterization of the microstructure of the embedded MOF. Data fusion was then used to determine the size distribution of the embedded MOF.
Absorption edge tomography is a method which exploits the sudden change of the attenuation coefficient, when the photon energy crosses the absorption edge of an element. The beamline BAM line at BESSY II, which is operated by the Federal Institute for Materials Research and Testing, can provide a monochromatized beam in a photon energy range from 5 keV up to 80 keV with a bandwidth of 2%. Together with the microtomography setup, this enables differential tomography sensitive to any element with N >= 24 (Cr) by using an appropriate K- or L-edge in this range. Here, a polymer filament embedding metal organic framework (MOF) was prepared and used for 3D printing. Absorption edge tomography at the copper K edge was employed to perform a non-destructive 3D characterization of the microstructure of the embedded MOF. Data fusion was then used to determine the size distribution of the embedded MOF.
Due to their excellent creep resistance and good oxidation resistance, 9–12% Cr ferritic–martensitic stainless steels are widely used as high temperature construction materials in power plants. However, the mutual combination of different loadings (e.g., creep and fatigue), due to a “flexible” operation of power plants, may seriously reduce the lifetimes of the respective components. In the present study, low cycle fatigue (LCF) and relaxation fatigue (RF) tests performed on grade P92 helped to understand the behavior of ferritic–martensitic steels under a combined loading. The softening and lifetime behavior strongly depend on the temperature and total strain range. Especially at small strain amplitudes, the lifetime is seriously reduced when adding a hold time which indicates the importance of considering technically relevant small strains.