Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Dokumenttyp
- Zeitschriftenartikel (9) (entfernen)
Sprache
- Englisch (9) (entfernen)
Referierte Publikation
- nein (9) (entfernen)
Schlagworte
- In situ measurement (4)
- LIBS (3)
- Welding (3)
- Duplex stainless steel (2)
- TIG welding (2)
- Acicular ferrite (1)
- Austenite (1)
- Austenitic stainless steels (1)
- Charpy toughness (1)
- Chemical composition (1)
Organisationseinheit der BAM
In situ chemical analysis of duplex stainless steel weld by laser induced breakdown spectroscopy
(2024)
The high corrosion resistance and good mechanical properties of duplex stainless steel (DSS) are due to its special chemical composition, which is a balanced phase ratio of ferrite (α) and austenite (γ). Many industrial applications require the integration of DSS components. For this, Gas tungsten arc welding (GTAW) is an excellent choice, as it allows an automated operation with high reproducibility. However, when the weld pool solidifies, critical ratios of α- and γ- phases can occur, which lead to solidification cracking, increased susceptibility to corrosion, and a decrease in ductility and critical strength. Previous studies have shown that these defects can be caused by the accumulation of manganese and chromium in the heat affected zone (HAZ), requiring ongoing monitoring of this accumulation. A suitable method for such monitoring is laser-induced breakdown spectroscopy (LIBS), which can be used in two operating modes: calibration using standard reference samples and calibration-free. Unlike conventional quantitative LIBS measurements, which require reference samples to generate a calibration curve, calibration-free LIBS (CF-LIBS) allows chemical compositions to be determined solely from the emission spectrum of the plasma. Numerous publications show that CF-LIBS is a fast and efficient analytical method for the quantitative analysis of metal samples. In this work, CF-LIBS is applied to spectra obtained during GTAW DSS welding and the result is compared with those obtained by PLS analysis. A good correlation was found between both types of analysis, demonstrating the suitability of the CF-LIBS method for this application. The CF-LIBS method has a significant advantage over conventional LIBS due to the rapid in situ measurement of concentrations of major alloying elements without calibration procedure. This, combined with fast feedback and appropriate adjustment of welding parameters, helps prevent welding defects.
Duplex stainless steels (DSS) are frequently used, especially in applications requiring high strength combined with high corrosion resistance in aggressive media. Examples include power plant components and maritime structures. During welding of these steels, local variations in chemical composition can occur. This results in ferritization of the material and negatively affects the mechanical properties of the components. In this work, tungsten inert gas (TIG) welding experiments were performed with DSS. Chemical composition analysis was realized in situ by using Laser Induced Breakdown Spectroscopy (LIBS). The aim of the work is to quantitatively measure the chemical composition in the weld seam of various DSS and to identify possible influences of welding parameters on the microstructure of the material. The chemical concentrations of the main alloying elements Cr, Ni, Mn on the surface of the sample during the welding process and the cooling process were measured. Mn and Ni are austenite stabilizers and their content increases during welding by using certain high alloyed filler material. Spectra were recorded every 1.3 s at a spacing of approximately 2 mm. During the cooling process the location of the measurement was not changed. The LIBS method is proofed to be suitable for the quantitative representation of the chemical compositions during the welding process.
The importance of high-temperature materials made of iron aluminides (FeAl) has been increasing in light weight applications, e.g., airplane turbines, due to the high material’s specific strength. However, the highly economic production by means of permanent mold casting involves special microstructures for Fe26Al4Mo0.5Ti1B alloy components leading to difficult machinability for subsequent finishing milling and low surface qualities. Major effects of tool and machining parameter variation incorporating ultrasonic assistance on the milling process and surface integrity are shown. Loads for tool and component surface are significantly adjustable to enable an economic process chain regarding the surface integrity of safety-relevant components.
Many applications in industry require a material-to-material joining process of Duplex Stainless Steels (DSS). Therefore, it is essential to investigate the material’s properties during a welding process to control the weld quality. With the help of Laser-Induced Breakdown Spectroscopy (LIBS), the chemical composition during the Tungsten Inert Gas (TIG) welding process of DSS could be monitored in situ. The chemical composition could be quantitatively measured using pre-established calibration curves. Although the surface temperature and the welding plasma have a high influence on the spectral intensities, reliable composition measurements were possible. The concentration of alloying elements could be mapped during the TIG welding process.
Chemical compositions of a weld can be varying locally as a result of the welding process. These local variations can be due to the vaporization of individual alloying elements. In this work, tungsten inert gas (TIG) bead-on-plate stainless steel welds of EN grade 1.4404 and 1.4435 were investigated using laser-induced breakdown spectroscopy (LIBS) on the completed welds. This study aims to reveal the welding parameters’ influence on the resulting local chemical compositions of the stainless steel welds. We demonstrated Mn vaporize before Cr due to its lower latent enthalpy of vaporization. Hence, Mn accumulates on the heat-affected zone (HAZ) both sides across the weld bead by being swept away through the circulation flow of the welding plasma. Additionally, increasing the heat input tends to enhance the accumulated Mn content on the HAZ as well as increasing the shielding gas flow rate. The results are in good agreement with the literature and proved that LIBS is an effective method to inspect completed welds.
In situ EDXRD study of MAG-welding using LTT weld filler materials under structural restraint
(2017)
Welding using low transformation temperature (LTT) filler materials is an innovative approach to mitigate detrimental welding residual stresses without cost-intensive post weldtreatments. Due to the local Generation of compressive residual stresses in the weld line by means of a delayed martensite transformation a significant enhancement of the cold cracking resistance of highly stressed welded components can be expected. For the effective usage of These materials a deeper understanding of the microstructural evolution inside the weld material is necessary to determine the complex processes that cause the residual stress formation during welding. Solid-state phase transformation kinetics and the evolution of strain in LTT weld filler materials are monitored in-situ at the instrument ID15A at the ESRF in Grenoble, France. The transferability to real components is implemented by using a realistic MAG welding process under consideration of structural restraint. During welding of multilayer joints, the phase Transformation and phase specific strain evolution of each individual layer is investigated in transmission geometry by means of energy-dispersive X-ray diffraction EDXRD using high energy synchrotron Radiation with a counting rate of 2.5 Hz. The measurement results of a 10% Cr / 10% Ni LTT weld filler are compared to data monitored for the conventional weld filler material G89. The in-situ data clearly indicate a strong effect on the local strain evolution and the formation of compressive strain. This results from the restraint volume expansion during the postponed austenite to martensite transformation of the LTT weld filler, which counteracts the thermal shrinkage. In contrast, for the conventional weld filler material the thermal contraction strains lead to tensile residual strain during welding. Furthermore, the results of in-situ observation during welding Show that the transformation kinetic is dependent on the welding sequence.
The roles of microalloying niobium, titanium and vanadium for controlling austenite grain growth, microstructure evolution and hardness were investigated at different simulated heat affected zones (HAZ) for high strength low alloy (HSLA) S690QL steel. High resolution FEG-SEM has been used to characterize fine bainitic ferrite, martensite and nanosized second phases at simulated coarse and fine grain HAZs. It was found that for Ti bearing steel (Ti/N ratio is 2) austenite grain had the slowest growth rate due to the presence of most stable TiN. The fine cuboidal particles promoted intragranular acicular ferrite (IGF) formation. Nb bearing steel exhibited relatively weaker grain growth retardation compared with titanium bearing steels and a mixed microstructure of bainite and martensite was present for all simulated HAZs. IGF existed at coarse grain HAZ of Ti+V bearing steel but it was totally replaced by bainite at fine grain HAZs. Hardness result was closely related to the morphology of bainitic ferrite, intragranular ferrite and second phases within ferrite. The microstructure and hardness results of different simulated HAZs were in good agreement with welded experimental results.
Effect of cooling rate on microstructure and properties of microalloyed HSLA steel weld metals
(2015)
Two high strength Nb/Ti microalloyed S690QL steels were welded with identical filler material, varying welding parameters to obtain three cooling rates: slow, medium and fast cooling. As cooling rate increased, the predominantly acicular ferrite in Nb weld metal (WM) is substituted by bainite, with a consequence of obvious hardness increase, but in Ti WM, no great variation of acicular ferrite at all cooling rates contributed to little increment of hardness. The transition between bainite and acicular ferrite has been analysed from the point view of inclusions characteristics, chemical composition and cooling rate. Excellent Charpy toughness at 233 K was obtained with acicular ferrite as predominantly microstructure. Even with bainite weld of high hardness, the toughness was nearly enough to fulfill the minimal requirements. WM for Ti steel showed to be markedly less sensitive to the variations of cooling rate than that for Nb steel.
Novel martensitic filler materials with specially adjusted martensite start temperatures (Ms) can counteract the cooling specific shrinkage due to expansion effects of the weld metal associated with phase transformations. That can be exploited to create compressive residual stresses in the weld and adjacent areas, i.e. beneficial for increasing fatigue strength. The Ms temperature is shifted via the chemical composition, mainly by the alloying elements nickel and chromium, resulting as well in different retained austenite contents. Investigations were made using different Low Transformation Temperature (LTT) alloys with varying nickel content. The resulting phase transformation temperatures were – for the first time – detected using high energy synchrotron diffraction and Single Sensor Differential Thermal Analysis (SS-DTA). Compared to angle dispersive diffraction, energy dispersive diffraction offers the possibility to measure residual stresses of the martensite and austenite phase parallel fast in one experiment up to depths of 100 µm. The residual stresses show significant distributions dependent on Ms temperature. The effect on the cold cracking behaviour of these alloys was investigated using the Tekken test. Results show that cold cracking can be avoided when appropriate contents of retained austenite are existent.