Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Dokumenttyp
- Beitrag zu einem Tagungsband (21) (entfernen)
Schlagworte
- Laser powder bed fusion (5)
- Additive manufacturing (4)
- Additive Manufacturing (2)
- AlSi10Mg (2)
- Inconel 718 (2)
- Infrared thermography (2)
- Laser Powder Bed Fusion (2)
- (U)HMWPE (1)
- Additive Fertigung (1)
- Additive manufacturing (AM) (1)
Organisationseinheit der BAM
- 9.6 Additive Fertigung metallischer Komponenten (21) (entfernen)
Rapidly advancing technologies and progressive digitisation are posing challenges to the established quality infrastructure (QI). In response, the key stakeholders of the German QI established the initiative QI-Digital aimed at developing new solutions for modern quality assurance. One of the central use cases herein is quality assurance for additive manufacturing, in which a fully interlinked additive manufacturing process chain is established. The intention is to collect and process data from each production step, allowing for a comprehensive digital view of the physical material flow. Within this process chain, prototypes of digital QI tools like machine readable standards and digital quality certificates are being demonstrated, tested, and evolved. This is complemented by research on the process level, comprising the evaluation and refinement of methods for in-situ and ex-situ quality assurance, as well as algorithms for registration, reduction, and analysis of process data. This paper presents the status, goals, and vision for the QI-Digital use case additive manufacturing.
For the wide acceptance of the use of additive manufacturing (AM), it is required to provide reliable testing methods to ensure the safety of the additively manufactured parts. A possible solution could be the deployment of in-situ monitoring during the build process. However, for laser powder bed fusion using metal powders (PBF-LB/M) only a few in-situ monitoring techniques are commercially available (optical tomography, melt pool monitoring), which have not been researched to an extent that allows to guarantee the adherence to strict quality and safety standards.
In this contribution, we present results of a study of PBF-LB/M printed parts made of the nickel-based superalloy Haynes 282. The formation of defects was provoked by local variations of the process parameters and monitored by thermography, optical tomography and melt pool monitoring. Afterwards, the defects were characterized by computed tomography (CT) to identify the detection limits of the used in-situ techniques.
Laser-based Powder Bed Fusion of Metal (PBF-LB/M) is a broadly used metal additive manufacturing (AM) method for fabricating complex metallic parts, whose sizes are however limited by the build envelope of PBF-LB/M machines. Laser welding arises as a valid joining method for effectively integrating these AM parts into larger assemblies.
PBF-LB/M components must usually be stress-relieved before they can be separated from the build plate. An additional heat treatment can be beneficial for obtaining homogeneous mechanical properties across the seam or for the formation of desired precipitations in nickel-based-alloys.
Therefore, the tensile performance of laser welded hybrid (AM/wrought) and AM-AM tensile samples of Inconel 718 is examined after undergoing three different heat treatments and considering three relevant build directions. It can be shown that the build orientation is an influencing factor on weld properties even after two applied heat treatments.
The industrialization of AM is only possible by creating synergy with the tools of Industry 4.0. The system technology of Powder Bed Fusion with Laser beam of Metals (PBF-LB/M) reached a level of high performance in terms of process stability and material spectrum in the past years. However, the digital process chain, starting from CAD via CAM and plant-specific compila-tion of the manufacturing file exhibits media disruptions. The consequence is a loss of metadata. A uniform data scheme of simulation for Design for Additive Manufacturing (DfAM), the PBF-LB/M process itself and quality assurance is currently not realized within industry. There is no entity in the common data flows of the process chains, that enables the integration of these functionalities. As part of the creation of a digital quality infrastructure in the QI-Digital pro-ject, an integration of the CAD/CAM chain is being established. The outcome is a file in an advanced commercially available format which includes all simula-tions and manufacturing instructions. The information depth of this file extends to the level of the scan vectors and allows the automatic optimization and holis-tic documentation. In addition, the KPI for the economic analysis are generated by compressing information into a unique file combined with the application of a digital twin. The implementation and advantages of this solution are demon-strated in a case study on a multi-laser PBF-LB/M system. A build job contain-ing a challenging geometry is thermally simulated, optimized, and manufac-tured. To verify its suitability for an Additive Manufacturing Service Platform (AMSP), the identical production file is transferred to a PBF-LB/M system of another manufacturer. Finally, the achieved quality level of the build job is evaluated via 3D scanning. This evaluation is carried out in the identical entity of the production file to highlight the versatility of this format and to integrate quality assurance data.
Safety-critical applications of products manufactured by laser powder bed fusion (PBF-LB/M) are still limited to date. This is mainly due to a lack of knowledge regarding the complex relationship between process, structure, and resulting properties. The assurance of homogeneity of the microstructure and homogeneity of the occurrence and distribution of defects within complexly shaped geometries is still challenging. Unexpected and unpredicted local inhomogeneities may cause catastrophic failures. The identification of material specific and machine specific process parameter windows for production of fully dense simple laboratory specimens is state of the art. However, the incorporation of changing thermal conditions that a complexly shaped component can be faced with during the manufacturing process is often neglected at the stage of a process window determination. This study demonstrates the tremendous effect of changing part temperatures on the defect occurrence for the broadly used stainless steel alloy AISI 316L. Process intrinsic variations of the surface temperature are caused by heat accumulation which was measured by use of a temperature adjusted mid-wavelength infrared (MWIR) camera. Heat accumulation was triggered by simple yet effective temporal and geometrical restrictions of heat dissipation. This was realized by a variation of inter layer times and reduced cross section areas of the specimens. Differences in surface temperature of up to 800 K were measured. A severe development of keyhole porosity resulted from these distinct intrinsic preheating temperatures, revealing a shift of the process window towards unstable melting conditions. The presented results may serve as a warning to not solely rely on process parameter optimization without considering the actual process conditions a real component is faced with during the manufacturing process. Additionally, it motivates the development of representative test specimens.
Additive manufacturing (AM) processes such as laser powder bed fusion (PBF-LB/M) are rapidly gaining popularity in repair applications. Gas turbine components benefit from the hybrid repair process as only damaged areas are removed using conventional machining and rebuilt using an AM process. However, hybrid repair is associated with several challenges such as component fixation and precise geometry detection. This article introduces a novel fixturing system, including a sealing concept to prevent powder sag during the repair process. Furthermore, a high-resolution camera within an industrial PBF-LB/M machine is installed and used for object detection and laser recognition. Herein, process related inaccuracies such as PBF-LB/M laser drift is considered by detection of reference objects. This development is demonstrated by the repair of a representative gas turbine blade. The final offset between AM build-up and component is analysed. An approximate accuracy of 160 μm is achieved with the current setup.
Based on state-of-the-art research and regulations, the application of the fracture mechanics master curve (MC) concept to ferritic ductile cast iron (DCI) is being investigated in a recently started German joint research project between BAM Berlin and MPA Stuttgart. This paper outlines the research approach and the planned investigations and provides first results.
According to the IAEA guidelines SSG 26, the safety assessment of DCI containers for transport as well as interim and final storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods under dynamic loading conditions. Within fracture mechanics safety assessments for steels in nuclear technology, the probabilistic MC concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. The MC concept allows for an effective statistical consideration of the scatter of the material toughness in the transition regime. Furthermore, the MC can also be used for elevated loading rates as they occur in accident or crash scenarios. However, for DCI, a systematic review of potential modifications to the MC assumptions and procedure according to ASTM E1921 and an associated validation are still lacking. Therefore, a corresponding methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component.
For the experimental program, a DCI material was produced as it is generally used for transport and storage containers. A basic mechanical-technological material characterization consisting of tensile, Charpy, and Pellini tests is planned. A comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens. Moreover, numerical analyses of different specimen geometries and test setups are planned to investigate the influences of stress triaxiality and loading rate. Throughout the experimental program, the microstructure-property relationship will be investigated based on quantitative metallographic and fractographic analyses. Finally, different MC assessment strategies will be considered, and modifications will be made if necessary.
Overview of ongoing research and future prospects on polyethylene neutron shielding materials at bam
(2023)
The extension of the interim storage period of radioactive waste before disposal will cause additional challenges for the nuclear waste management in Germany, so that an extensive knowledge of the long-term performance of casks, including their components and inventories, will be required for future extended storage licenses.
Ultra-high and high molecular weight polyethylenes ((U)HMW-PE) are used for neutron shielding purposes in casks for storage and transport of spent fuel and high-level waste due to their extremely high hydrogen content. During their service life of several decades as cask components, the PE materials are exposed to neutron and gamma radiation from the radioactive inventory of the casks, mechanical assembling stresses and temperature. All these combined effects affect the material properties of such components which in turn may be crucial for some possible accident scenarios.
At the Bundesanstalt für Materialforschung und -prüfung (BAM), the effects of high temperature exposure in combination with subsequent or previous irradiation were investigated with a comprehensive aging program including thermal aging at 125 °C for different aging periods up to 5 years and irradiation with doses ranging from 50 to 600 kGy.
This contribution provides an overview of the ongoing research related to the structural changes of (U)HMW-PE induced by gamma irradiation and high temperature exposure and focuses on current research perspectives at BAM with regard to the prediction of the dynamic behavior of the material during extended interim storage in case of an accident scenario. First results of the coupled effect of temperature, radiation and mechanical loading will be presented. The effect of microstructural changes induced by gamma irradiation and high temperature on the mechanical behavior of (U)HMW-PE will be assessed.
Since there is a continuously growing demand for complex, frequently heavy-sectioned spheroidal graphite cast iron (SGI) castings it is worth paying attention to the chunky graphite (CHG) degeneration which may occur under certain technological circumstances. Although a reference line for preventive actions in terms of general metallurgical and process measures could be drawn to avoid CHG in heavy-sectioned ferritic SGI castings, a broad majority of experts claim the avoidance of CHG in heavy sections cannot yet be rated a hundred percent process safe. A major reason may be seen in the fact that a universal, generally accepted explanation of CHG formation and growth has not yet been established, although several theories have been proposed. Nevertheless, metallurgical aspects are not in the focus of this paper.
This paper is about the current state of methods to detect CHG in SGI on the laboratory and component scales. Capabilities and limits of different metallographic, fractographic and non-destructive computer tomographic methods to recognize and quantify CHG are discussed. With respect to the characteristic fili-gree three-dimensional string-like, multi-branched CHG structure, which is non-isometric and non-dispersed, serious implications on the possibility to quantitatively characterize the amount of CHG must be considered.
In contrary to the metallurgical aspects, the knowledge about the impact of CHG on the materials and com-ponents properties is still surprisingly limited. Therefore, special emphasis of this paper is on the impact of CHG degeneration on the properties of ferritic SGI. Experimental results are reviewed to illustrate the effect of CHG on mechanical strength and ductility properties as well as fracture mechanics properties in terms of crack resistance and fracture toughness.
The present situation is characterized by discussions and uncertainty about the acceptance or rejection of SGI components containing CHG. Addressing this, conclusions from the materials engineering point of view are drawn for quality control, a safe operational strategy in the foundry and component safety.
Das Master Curve (MC) Konzept nach ASTM E1921 wird momentan u.a. in der Kerntechnik für die bruchmechanische Sicherheitsbewertung ferritischer Stähle eingesetzt.
Für ferritisches Gusseisen mit Kugelgraphit (GJS) fehlt jedoch eine Validierung dieser Methode und ggf. eine systematische Überprüfung möglicher Modifikationen grundlegender Ansätze des MC-Konzepts. Aus diesem Grund soll in einem kürzlich gestarteten BMUV-Verbundprojekt zwischen der MPA Stuttgart und der BAM Berlin die Anwendbarkeit des MC-Konzepts auf GJS bei dynamischer Beanspruchung untersucht werden. Ziel ist es, eine effektive und effiziente Methodik bereitzustellen, mit der mittels einer vergleichsweise kleinen Stichprobe bruchmechanischer Kleinproben eine Referenztemperatur T0 zur werkstoffspezifischen Temperaturjustierung der MC ermittelt werden kann.
When it comes to higher accuracies, new technologies and real applications in additive manufacturing, there is one topic which cannot be avoided: The material response on the chosen processing parameters and its agreement and correspondence with literature data of the wrought material grade counterpart. In industrial Additive Manufacturing (AM) standards in terms of printing parameters, protection gas atmospheres or powder handling instructions are not obligatory. Therefore, the question must be answered whether the AM process is reproducible and reliable over different printing companies. This was the motivation to realize a round robin test between 8 European printing companies and academic partners. The consortium had printed and tested fatigue and tensile testing bars under plant-specific conditions. A commonly used cast aluminum alloy, AlSi10Mg, was chosen as test material for the PBF-LB/M process. Differences of the results between the partners and the scatter itself were discussed in detail.
In line with the industrial trend of additive manufacturing, cold spray as a non-laser-based process is becoming increasingly important for many fields of application. For the evaluation of additive manufacturing of winding components made of copper for large electrical high-voltage machines, material and component properties such as electrical conductivity, mechanical load capacity and the component size that can be produced are of particular importance. In this context, the cold spray process offers advantages over laser-based additive manufacturing processes such as laser powder bed fusion (LPBF) or laser cladding by using the kinetic energy of the copper powder particles to generate particle cohesion. To investigate the electrical conductivity as well as the mechanical load capacity of cold spray parts, specimens were machined out of cold sprayed bulk copper deposits. The characteristic values were obtained with regard to the direction of deposition, which is defined by the direction of the robot’s movement. Thus, for the investigation of the component properties, specimens were provided that had been produced both longitudinally and transversely as well as orthogonally to the direction of deposition. The results of the investigations show that both the electrical conductivity and the mechanical load capacity of the specimen have a strong preferential direction of the specimen orientation with respect to the direction of deposition. Furthermore, it could be shown that by increasing the deposition height, there is an increasing oxygen content in the sample material, combined with increasingly significant defect networks. These effects have a negative impact on the electrical conductivity as well as on the mechanical load capacity. As a conclusion, further need for investigation is identified in the optimization of the process parameters as well as in the deposition strategy for the additive manufacturing of large-volume components with cold spray.
Laser welding is an appropriate technique for joining Laser Powder Bed Fusion (L-PBF) parts together and to conventional wrought ones. The potential consists of profiting from synergies between additive and conventional manufacturing methods and overcoming the existing limitations of both. On the one hand, L-PBF is a widely spread metal-based additive manufacturing technique suitable for generating complex parts which can present intrinsic designed cavities, conformal cooling channels, and filigree structures contributing to sustainable manufacturing and efficiency-oriented designs. On the other hand, chamber sizes for producing L-PBF parts are limited, and the process is time-consuming. Thus, its employment is not for every geometry justified. Additionally, they are in most cases individual elements of a larger assembly and need to be joined together to conventionally fabricated parts.
The present research suggests laser welding parameters to adequately bond pairs of wrought and L-PBF processed plates and two L-PBF plates of Inconel 718 in butt position. L-PBF samples are printed in three different build-up orientations. Additionally, the influence of as-built L-PBF roughness qualities and usual pre-weld preparations such as edge milling are examined. The effect of normed pre-weld heat treatments is also contemplated. Identified cracks are analyzed by means of EDS in order to confirm the present phases on the areas of interest. EBSD is also employed to obtain a clear depiction of the crystallographic texture and distribution of the hot cracks.
The quality of the weldment was examined according to existing standards. Substantial differences in seam geometry and microstructure across different edge’s surface qualities and build directions of stress relieved L-PBF parts have not been detected. Nevertheless, even if no other irregularities are present in the seam, variability in liquation cracking susceptibility has been confirmed. This defect is prone to happen when parts made of this nickel-based superalloy are welded together when not enough precautions are taken. It has been determined that grain size and ductility of the material before welding play a crucial role and mitigating or intensifying these imperfections. Moreover, recommendations are presented to avoid this potential welding defect.
Am Beispiel eines abgesetzten zylindrischen Bauteils (Achsschenkel) werden Probleme der analytischen bruchmechanischen Bauteilbewertung diskutiert. Als Basis-philosophie wird ein Fail Safe-Kriterium (kontrolliertes Versagen) angesetzt. Die Forderung ist, dass sich der Achsschenkel, bevor er bricht, in einem Ausmaß plastisch verformen kann, bei dem der Fahrer bemerkt, dass mit seinem Fahrzeug etwas nicht in Ordnung ist. Um das zu gewährleisten, muss der Werkstoff einen bestimmten Riss-widerstand aufweisen. Dazu werden im hier vorgestellten ersten Teil des Projektes mittels FEM Rissspitzenbeanspruchungen in Abhängigkeit von der Auslenkung des Zylinders und angenommener Rissgrößen ermittelt. Diese finden als Zielgrößen in der weiteren Analyse Anwendung. Da eine einfach umzusetzende Lösung angestrebt wird, werden zusätzlich analytische Rechnungen an Ersatzgeometrien (halbunendliche Platte und Vollzylinder), aber mit den realen Spannungen am Bauteil durchgeführt. Es zeigt sich, dass die Ergebnisse wegen des Steifigkeitsunterschieds zwischen Bauteil und Ersatzgeometrie unvertretbar konservativ sind. Alternativ wird ein hybrides Konzept vorgestellt, für das die Modellparameter mittels FEM bestimmt werden. Es liefert sehr genaue Ergebnisse. Im Rahmen der analytischen Rechenvorschrift können die Lösungen auf andere Werkstoffe übertragen werden, ohne dass zusätzliche FEM-Analysen notwendig sind.
Heterogene Fehlstellendichten und Mikrostrukturausbildungen sind große Herausforderungen für den Einsatz des pulverbettbasierten Laserstrahlschmelzens (L PBF) besonders für sicherheitskritische Bauteile. Unter der Vielzahl an Einflussfaktoren auf die Qualität und die mechanischen Eigenschaften von L PBF-Bauteilen hat die Zwischenlagenzeit (ILT) bisher wenig Beachtung gefunden. Sie nimmt ebenso wie die Bauteilgeometrie Einfluss auf die thermische Historie während der Fertigung. Ihr Einfluss auf die intrinsische Vorerwärmung ist in Kombination mit der Bauteilhöhe mittels thermografischer Temperaturmessung untersucht worden. Signifikante Unterschiede in der thermischen Historie konnten dabei mit variierenden Schmelzbaddimensionen, Korngrößen und Fehlstellendichten am Beispiel der austenitischen Stahllegierung AISI 316L in Zusammenhang gebracht werden.
In der Automobilindustrie stellt das Presshärteverfahren eine Schlüsseltechnologie zur ressourceneffizienten Herstellung sicherheitsrelevanter Karosserie-komponenten dar. Während der Umformoperation treten jedoch hohe Reibungs- und Verschleißerscheinungen an den interagierenden Werkzeug- und Werkstückwirkflächen auf, die sowohl die Bauteilqualität als auch die Maschinenstandzeit nachhaltig beeinträchtigen. Um die bestehenden Verfahrensgrenzen zu erweitern, wird daher eine Modifikation der Presshärtewerkzeuge mittels Laserimplantation angestrebt. Hierbei werden in die Werkzeugoberfläche keramische Hartstoffpartikel anhand eines gepulsten Laserstrahles eingebettet, infolgedessen kuppelförmige sowie höchstfeste Strukturen im Mikrometerbereich entstehen. Die Auswahl geeigneter Hartstoffmaterialien stellt jedoch ein entscheidendes und bisweilen limitierendes Kriterium dar, um defektfreie sowie verschleißresistente Oberflächenmodifikationen zu generieren. In diesem Zusammenhang wurden im Rahmen dieser Arbeit unterschiedliche titanbasierte Hartstoffpartikel auf presshärtespezifische Werkzeugstähle laserimplantiert und anschließend mittels modifizierten Pin-on-Disk-Tests hinsichtlich ihres tribologischen Einsatzverhaltens untersucht. Um die Wirksamkeit des Laserimplantationsverfahrens zu evaluieren, wurden zudem Verschleißuntersuchungen an unmodifizierten Werkzeugoberflächen durchgeführt und mit den erzielten Ergebnissen der lokal dispergierten Topographien verglichen.
Within the group of additive manufacturing (AM) technologies for metals, laser powder bed fusion (L-PBF) has a leading position. Nevertheless, reproducibility of part properties has not reached sufficient maturity hindering the use for industrial applications especially for safety-relevant components. This article presents the results of various experimental tests performed with the aluminium alloy AlSi10Mg identifying reasons for the high deviations in mechanical properties. Herein, it is discussed how microstructure is influenced by different process parameters (laser power, scanning speed, energy density, building height) and how it can be adjusted by suitable post process heat treatments. The impact of resulting changes in microstructure is shown by monotonic tensile and cyclic fatigue tests considering specimens manufactured with different L-PBF machines.
In order to reduce weight of vehicles, the interest in multi-material-design has been growing within the last few years. For vehicles the combination of steel and aluminium alloys offers the most promising compromise between weight, strength and formability. Thermal joining of these dissimilar materials is still a challenge to overcome. A possible approach is a new joining technology, whereby a combination of laser beam welding and contactless induced electromagnetic forces are used to displace the generated melt of one joining partner into a notch of the other. This paper presents the working principle and shows numerical analyses to improve the understanding of this joining process. The simulations help to calculate the thermal development of the joining partners, which is important for the formation of intermetallic phases. Furthermore, the calculation of the time required for a complete displacement is possible. The numerical results are validated by experimental results.
Laser powder bed fusion is used to create near net shape metal parts with a high degree of freedom in geometry design. When it comes to the production of safety critical components, a strict quality assurance is mandatory. An alternative to cost-intensive non-destructive testing of the produced parts is the utilization of in-situ process monitoring techniques. The formation of defects is linked to deviations of the local thermal history of the part from standard conditions. Therefore, one of the most promising monitoring techniques in additive manufacturing is thermography. In this study, features extracted from thermographic data are utilized to investigate the thermal history of cylindrical metal parts. The influence of process parameters, part geometry and scan strategy on the local heat distribution and on the resulting part porosity are presented. The suitability of the extracted features for in-situ process monitoring is discussed.