Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
Dokumenttyp
- Posterpräsentation (808) (entfernen)
Sprache
- Englisch (672)
- Deutsch (135)
- Französisch (1)
Schlagworte
- Corrosion (36)
- Additive manufacturing (31)
- Mechanochemistry (24)
- Additive Manufacturing (20)
- Glass (20)
- Nanoparticles (20)
- Crystallization (17)
- Fluorescence (15)
- Degradation (14)
- In situ (14)
Organisationseinheit der BAM
- 6 Materialchemie (208)
- 5 Werkstofftechnik (99)
- 8 Zerstörungsfreie Prüfung (98)
- 6.3 Strukturanalytik (65)
- 8.5 Röntgenbildgebung (62)
- 6.6 Physik und chemische Analytik der Polymere (56)
- 9 Komponentensicherheit (54)
- 6.1 Oberflächen- und Dünnschichtanalyse (49)
- 1 Analytische Chemie; Referenzmaterialien (47)
- 4 Material und Umwelt (36)
- 7 Bauwerkssicherheit (34)
- 5.1 Mikrostruktur Design und Degradation (28)
- 1.2 Biophotonik (26)
- 6.0 Abteilungsleitung und andere (26)
- 5.4 Multimateriale Fertigungsprozesse (22)
- 5.2 Metallische Hochtemperaturwerkstoffe (20)
- 9.4 Integrität von Schweißverbindungen (20)
- 4.1 Biologische Materialschädigung und Referenzorganismen (19)
- 5.6 Glas (19)
- 6.2 Material- und Oberflächentechnologien (19)
- 9.3 Schweißtechnische Fertigungsverfahren (19)
- 2 Prozess- und Anlagensicherheit (14)
- 6.5 Synthese und Streuverfahren nanostrukturierter Materialien (14)
- 7.1 Baustoffe (13)
- 8.0 Abteilungsleitung und andere (13)
- 6.7 Materialsynthese und Design (12)
- 8.3 Thermografische Verfahren (12)
- 3 Gefahrgutumschließungen; Energiespeicher (11)
- 4.2 Material-Mikrobiom Wechselwirkungen (11)
- 7.6 Korrosion und Korrosionsschutz (11)
- 9.6 Additive Fertigung metallischer Komponenten (9)
- 1.9 Chemische und optische Sensorik (8)
- 5.3 Polymere Verbundwerkstoffe (8)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (8)
- 8.4 Akustische und elektromagnetische Verfahren (8)
- 1.4 Prozessanalytik (6)
- 9.0 Abteilungsleitung und andere (6)
- 2.5 Konformitätsbewertung Explosivstoffe/Pyrotechnik (5)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (5)
- 4.5 Kunst- und Kulturgutanalyse (5)
- 5.5 Materialmodellierung (5)
- 8.1 Sensorik, mess- und prüftechnische Verfahren (5)
- 9.5 Tribologie und Verschleißschutz (5)
- 1.6 Anorganische Referenzmaterialien (4)
- 2.0 Abteilungsleitung und andere (4)
- 9.2 Versuchsanlagen und Prüftechnik (4)
- 1.5 Proteinanalytik (3)
- 2.1 Sicherheit von Energieträgern (3)
- 4.0 Abteilungsleitung und andere (3)
- 7.2 Ingenieurbau (3)
- 8.2 Zerstörungsfreie Prüfmethoden für das Bauwesen (3)
- 8.6 Faseroptische Sensorik (3)
- VP Vizepräsident (3)
- VP.1 eScience (3)
- 1.1 Anorganische Spurenanalytik (2)
- 2.2 Prozesssimulation (2)
- 3.2 Gefahrguttanks und Unfallmechanik (2)
- 3.4 Sicherheit von Lagerbehältern (2)
- 1.0 Abteilungsleitung und andere (1)
- 1.8 Umweltanalytik (1)
- 3.0 Abteilungsleitung und andere (1)
- 3.3 Sicherheit von Transportbehältern (1)
- 3.6 Elektrochemische Energiematerialien (1)
- 5.0 Abteilungsleitung und andere (1)
- 6.4 Materialinformatik (1)
- 7.4 Baustofftechnologie (1)
- MP Mitglied des Präsidiums (1)
- MP.0 Mitglied des Präsidiums und andere (1)
- P Präsident (1)
- PST Präsidiale Stabsstelle (1)
Eingeladener Vortrag
- nein (1)
The geometry of the melt pool in laser beam welding plays a major role to understand the dynamics of the melt and its solidification behavior. In this study, a butt configuration of 20 mm thick structural steel and transparent quartz glass was used to observe the weld pool geometry in the partial penetration mode by means of a high-speed camera. The observations show that the dimensions of the weld pool vary depending on the depth. The areas close to the weld pool surface take a teardrop-shape. A bulge-region and its temporal evolution were observed approximately in the weld pool root. Additionally, a 3D transient thermal-fluid numerical simulation was performed to obtain the weld pool shape and to understand the formation mechanism of the observed bulging effect. The model considers the local temperature field, the effects of phase transition, thermo-capillary convection, natural convection and temperature-dependent material properties. The numerical results showed good accordance and were furthermore used to improve the understanding of the experimentally observed bulging effect.
The motivation and the measurement setup for large fast-scanning piezoresistive cantilevers are presented. The theory behind the measurements of mechanical properties through contact resonance is explained. Results of such measurements on two kinds of polymer are compared to results from force distance curves. Noise, time-dependency and dependency of the results on the vibration mode are identified as challenges of contact resonance.
Mg is a very promising material for lightweight construction and biomedical applications. However, the applicability of Mg and its alloys is hindered by its high corrosion susceptibility. Moreover, due to the toxicity of most inorganic conversion coating systems, the development of novel pre-treatment strategies for technical alloys are of vital importance. The aim of this study is to develop polymeric bilayer thin films for corrosion protection of Mg-alloys. As polymer matrix, poly(4-vinyl pyridine) (P4VP) was selected due to its semiconducting properties and protonic conductivity. In contrast to ICPs with electronic conductivity, the pH-dependant, reversible protonation/de-protonation capability of the P4VP has been utilized to synthesize environment-responsive coatings. Polyacrylicacid (PAA) was tested as crosslinking layers to improve interfacial interactions between the polymeric layers. The macroscopic corrosion properties of the bilayer coatings were investigated by means of electrochemical methods such as linear sweep voltammetry (LSV) and electrochemical impedance spectroscopy (EIS) in corrosive media simulating technical and biomedical applications. The presentation summarizes our recent results on the synthesis and characterization of this novel coating system with a special focus on their interfacial stability and corrosion protection properties.
Mg is a very promising material for lightweight construction and biomedical applications. However, the applicability of Mg and its alloys is hindered by its high corrosion susceptibility. Moreover, due to the toxicity of most inorganic conversion coating systems, the development of novel pre-treatment strategies for technical alloys are of vital importance. Recently, the application of intrinsically conducting polymers (ICPs) have been introduced as an alternative approach for corrosion protection of Mg alloys. ICPs with electronic conductivity are known to be able to passivate small defects, however they fail in the presence of large defects due to fast coating reduction and increased cation transport if macroscopically extended percolation networks exist.
The aim of this study is to develop graphene-polymer nanocomposite thin films for corrosion protection of Mg-alloys. As polymer matrix, poly(4-vinyl pyridine) (P4VP) was selected due to its semiconducting properties and protonic conductivity. In contrast to ICPs with electronic conductivity, the pH-dependant, reversible protonation/de-protonation capability of the P4VP has been utilized to synthesize environment-responsive coatings. The presentation summarizes our recent results on the synthesis and characterization of this novel coating system with a special focus on their interfacial stability and corrosion protection properties.
Degradation of thermal barrier coatings (TBCs) in gas‐turbine engines due to calcium–magnesium–aluminosilicate (CMAS) glassy deposits from various sources has been a persistent issue since many years. In this study, state of the art electron microscopy was correlated with X‐ray refraction techniques to elucidate the intrusion of CMAS into the porous structure of atmospheric plasma sprayed (APS) TBCs and the formation and growth of cracks under thermal cycling in a burner rig. Results indicate that the sparse nature of the infiltration as well as kinetics in the burner rig are majorly influenced by the wetting behavior of the CMAS. Despite the obvious attack of CMAS on grain boundaries, the interaction of yttria‐stabilized zirconia (YSZ) with intruded CMAS has no immediate impact on structure and density of internal surfaces. At a later stage the formation of horizontal cracks is observed in a wider zone of the TBC layer.
aRTist is an easy-to-use and practical simulation tool to generate realistic radiographic images from CAD objects. A dedicated add-on module makes CT simulation easy (virtual computer tomography). Just choose the number of projections.
Unlike in the practice, simulation can separately image the primary and scatter radiation. This allows studying the scattering artefacts in CT (gray-level variations in regions of homogeneous material).
CEQAT-DGHS Interlaboratory tests for method validation and measurement uncertainty determination
(2019)
An explosion in a chemical plant or a fire on a dangerous goods vessel - the reason for such accidents can be numerous. Prevention starts in the laboratory where chemicals are tested for their hazardous properties in order to be able to assess the risks involved in their handling. For this purpose, test methods have been developed and published. They are applied globally nowadays. Safety experts, manufacturers, suppliers, importers, employers or consumers must be able to rely on the validity of safety-related test methods and on correct test results and assessments in the laboratory.
Interlaboratory tests play a decisive role in assessing the reliability of test results. Participation in interlaboratory tests is not only a crucial element of the quality assurance of laboratories; as such it is explicitly recommended in DIN EN ISO/IEC 17025. In addition, interlaboratory tests are also used to develop and validate test methods and can be used for the determination of the measurement uncertainty.
Interlaboratory tests on different test methods have been performed by Bundesanstalt für Materialforschung und –prüfung (BAM) and Physikalisch-Technische Bundesanstalt (PTB) in collaboration with the QuoData GmbH during the last 10 years. Significant differences between the results of the participating laboratories were observed in all interlaboratory tests. The deviations of the test results were not caused only by laboratory faults but also by deficiencies of the test method (see interlaboratory test reports of the CEQAT-DGHS Centre for quality assurance for testing of dangerous goods and hazardous substances: www.ceqat-dghs.bam.de).
In view of the interlaboratory test results the following conclusions can be drawn:
• To avoid any discrepancy on classification and labelling of chemicals it should become state of the art to use validated test methods and the results accompanied by the measurement uncertainty.
• A need for improvement is demonstrated for all examined test methods. Thus, interlaboratory tests shall initially aim at the development, improvement and validation of the test methods (including the determination of the measurement uncertainty) and not on proficiency tests.
• The laboratory management and the practical execution of the tests need to be improved in many laboratories.
• The term "experience of the examiner" must be seen critically: A "long experience with many tests" is not necessarily a guarantee for correct results.
In this poster we will present some results of a research projects dealing with Arabic recipes of black inks. To improve conservation practices of Arabic manuscripts we have assessed the feasibility of the recipes collected from many Arabic sources on bookmaking and reproduced the most common inks. Ink samples were then artificially aged and analysed using an array of analytical techniques, mostly non-invasive, in order to build a database of Arabic inks and their ingredients and also to verify the detection limits of the portable equipment employed.
First, we will provide an overview of the sources [1-2] employed in the study – dating from 9th to 14th century, although the manuscripts in which they can be found dates up to the 20th century – with an eye on the ink typologies (real and perceived by the compilers). Then we will show how, by reproducing the recipes, it was possible to shed light on some oddities in the procedures and the choice of ingredients. In the end we will discuss problems concerning the identification of ink types and ingredients using reflectography (in Vis, IR and UV), X-Ray Fluorescence, Infrared and Raman spectroscopy. The focus will be in particular on mixed inks – both in the form of carbon inks with the addition of tannins and of a mixture of carbon and iron gall inks – which are particularly difficult to detect [3]. We will also examine the results of iron gall inks made with iron filings or nails instead of vitriol and the various precursor used to extract gallic acid that are mentioned in the sources as surrogates of gall nuts.
[1] A. Schopen, Tinten und Tuschen des arabisch-islamischen Mittelalters, Göttingen: Vandenhoeck & Ruprecht, 2004
[2] S. Fani, Le arti del libro secondo le fonti arabe originali. I ricettari arabi per la fabbricazione degli inchiostri (sec. IX-XIII): loro importanza per una corretta valutazione e conservazione del patrimonio manoscritto, PhD thesis, Napoli: Università L’Orientale, 2013
[3] C. Colini et. al, Manuscript cultures, 11 (2018) 43-50
In this poster we will present some results of a research projects dealing with Arabic recipes of black inks [1-2]. To improve conservation practices of Arabic manuscripts we have assessed the feasibility of the recipes collected from many Arabic sources on bookmaking and reproduced the most common inks. Ink samples were then artificially aged and analysed using an array of analytical techniques, mostly non-invasive, in order to build a database of Arabic inks and their ingredients and also to verify the detection limits of the portable equipment employed.
We will show procedures and problems concerning the identification of ink types and ingredients using reflectography (in Vis, IR and UV), X-Ray Fluorescence, Infrared and Raman spectroscopy. The focus will be in particular on squid ink [3] and mixed inks – both in the form of carbon inks with the addition of tannins and of a mixture of carbon and iron gall inks – which are particularly difficult to detect [4]. We will also examine the results of iron gall inks made with iron filings or nails instead of vitriol, the various precursor used to extract gallic acid that are mentioned in the sources as surrogates of gall nuts.
[1] A. Schopen, Tinten und Tuschen des arabisch-islamischen Mittelalters, Göttingen: Vandenhoeck & Ruprecht, 2004
[2] S. Fani, Le arti del libro secondo le fonti arabe originali. I ricettari arabi per la fabbricazione degli inchiostri (sec. IX-XIII): loro importanza per una corretta valutazione e conservazione del patrimonio manoscritto, PhD thesis, Napoli: Università L’Orientale, 2013
[3] S. Centeno, J. Shamir Journal of Molecular Structure, 873 (2008), 149-159
[4] C. Colini et. al, Manuscript cultures, 11 (2018) 43-50
Virtual-lab-based determination of a macroscopic yield function for additively manufactured parts
(2019)
This work aims for a yield function description of additively manufactured parts of S316L steel at the continuum-mechanical macro-scale by means of so-called virtual experiments using a crystal plasticity (CP) model at meso-scale. Additively manufactured parts require the consideration of the specific process-related microstructure, which prevents this material to be macroscopically treated as isotropic, because of crystallographic as well as topological textures. From virtual experiments, yield loci under various loading conditions are simulated. The scale bridging from meso- to macro-scale is realised by the identification of the simulated yield loci as a modified anisotropic Barlat-type yield model representation.
The church of Koszewko (Poland) is a brick building edified in the 15th century built on cobblestone foundations. There are five windows in the sanctuary. Three of them enclose heraldic panels from the Küssow’s family from the 15th century which are surrounded with Goethe glass from the 18th century to complete the windows. The colored heraldic panels are strongly damaged and corroded with massive paint layer losses, glass- and leadbreakages. Those medieval glass fragments have been shortly discovered and are of particular interest for Poland since only few medieval glazing have been conserved.
The damages as well as the glass compositions have been investigated with ESEM/EDX. Two categories of medieval glass compositions have been identified. The blue glass is particularly sensible to corrosion because of his high content in K2O. The colorless and the red glass samples belong to a stable glass type. Due to the thickness of the gel layer, it is easy to see that the degradation is strongly proceeded. The protection of those medieval stained-glass panels is absolute necessary.
The medieval panels have been restored and surrounded from a copper frame. Then they have been fixed on the wood frame in the church. The exterior glazing has been closed with a panel of Goethe glass. The gap between the Goethe- and the medieval glass is about 3 cm. The Goethe glass panel has been stabilized with a film based on polyester to protect the medieval glasses against any damages. In this way, a low cost protective glazing has been installed for a long-term conservation of each medieval stained-glass panels. The climate measurements over the period of one year on the restored windows are in process. The temperature and the relative humidity are recorded in the church interior, in the gap between the original and the Goethe glass and outdoors.
Despite of the significant advances in additive manufacturing (AM) process optimization there is still a lack of experimental results and understanding regarding the mechanical behavior and its relationship with the microstructural features of AM-parts, especially in loading conditions typical for safety-relevant applications. Within the scope of the presented ongoing investigations, a basic microstructural characterization, tensile tests at room and elevated temperature (400°C) as well as a characterization of the fatigue behavior of additively manufactured Ti-6Al-4V in the low cycle fatigue regime are carried out in the as-built state. After failure, different techniques are used to describe the failure mechanisms of the specimens. The AM-Specimens are provided by the Fraunhofer institute for production systems and design technology and investigated at the BAM following the philosophy of the TF-Project AGIL.
µCT is used to validate the capability of online monitoring for in-situ detection of defects during the L-PBF build process, which is a focus of the TF project ProMoAM.
Our first experiments show that online monitoring using thermography and optical tomography cameras are able to detect defects in the built part. But further research is needed to understand root cause of the correlation.
The Influence of the Temperature Gradient on the Distribution of Residual Stresses in AM AISI 316L
(2019)
Steep temperature gradients and solidification shrinkage are the main contributors to the formation of residual stresses in additively manufactured metallic parts produced by laser beam melting. The aim of this work was to determine the influence of the temperature gradient.
Diffraction results show a similar pattern for both specimens, indicating the shrinkage to be more dominant for the distribution of residual stresses than the temperature gradient. Thermography results imply that a higher energy input result in higher compressive residual stresses in the bulk.
Ellipsometry has become a powerful measurement tool in semiconductor industry since the sixties of the last century.
Early standardization activities focused exclusively on SiO2/Si (ASTM F 576-01, SEMI 3624). The first generic standard dealing with ellipsometry is DIN 50989-1:2018 Ellipsometry – Part 1: Principles. Standardization is a prerequisite for accreditation according to DIN EN ISO/IEC 17025 and the evaluation of uncertainty budgets.
Over the last years, the weight of modern car bodies has risen significantly due to the increasing customers’ demand for comfort and safety equipment. However, this ongoing trend leads to an increasing fuel consumption and thus to higher carbon dioxide emissions. In order to counteract these problems, hot stamping has been established in the automotive industry as a key technology for lightweight construction, regarding the manufacturing of safety-relevant car body components. Hot stamped parts are commonly made out of boron-manganese steel 22MnB5, which is initially austenized and subsequently formed and quenched in one process step. As a result, geometrical complex structures with an ultimate tensile strength of 1500 MPa are generated. The surfaces of the workpieces are coated with an Al-Si layer to avoid oxide scale formation and to ensure corro-sion protection. However, the coating system leads to an increased adhesive wear on the tool sur-face due to the high thermo-mechanical tool stresses. Therefore, a time and cost consuming rework of the hot stamping tools is required. The aim of this study is to increase the tribological perfor-mance of hot stamping tools by using a laser implantation process. This technique allows the ma-nufacturing of separated, elevated and dome-shaped microstructures on the tool surface in conse-quence of a localized dispersing of hard ceramic particles by pulsed laser radiation. The generated surface features offer great potential for reducing the tribological load, due to their high hardness and wear resistance. For this purpose, the friction coefficient of unmodified and laser implanted tool surfaces were examined and compared by using a modified pin-on-disk test. In addition, the surfaces were analyzed by optical measurements in order to quantify the amount of wear.
As a part of ProMoAM project, we are optimizing a prototype X-ray backscatter to reach NDT requirements, and thereafter to apply it for process monitoring. Moreover, we studied the capability of a radiography approach to detect artificial defects in AM components made by laser powder bed fusion (L-PBF).
Analysis of elemental composition of Fe1-xNix and Si1-xGex alloy thin films by EPMA and µ-XRF
(2019)
The present study reports on measurements on thin Fe-Ni films on silicon and first-time results of analysis on Si-Ge thin films deposited on a non-conductive aluminium oxide Substrate by electron probe microanalysis (EPMA). Standard-based and standardless EPMA (with EDS) results were used in combination with the thin film analysis software Stratagem for the quantification.
Further, X-ray fluorescence analysis (XRF) can be used for the determination of elemental composition and thickness of such films as well. In this case, XRF with a μ-focus X-ray source (μ-XRF) attached to a SEM was applied. For quantification, a fundamental parameter (FP) approach has been used to calculate standard-based and standardless results.
Both thin film systems have been chosen as samples of an international round robin test (RRT) organised in the frame of standardisation technical committee ISO/TC 201 ‘Surface chemical analysis’, under the lead of KRISS. The main objective of the RRT is to compare the results of atomic fractions of Fe1-xNix and Si1-xGex alloy films obtained by different surface Analysis techniques, such as X-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES), and secondary ion mass spectrometry (SIMS) applied in the depth-profiling operation mode.
Five samples of different atomic fractions of each thin film system, i.e., Fe1-xNix and Si1-xGex, have been grown by ion beam sputter deposition on silicon and Al2O3 wafers, respectively. Reference FeNi and SiGe films with well-known elemental composition and thickness have been also supplied for standard-based analysis. An excellent agreement has been obtained between the atomic fractions determined by EPMA and µ-XRF with the KRISS certified values.
The movement of the macroscopic magnetic moment in ferromagnetic systems can be described by the Landau-Lifshitz (LL) or Landau-Lifshitz-Gilbert (LLG) equation. These equations are strictly valid only at absolute zero temperature. To include temperature effects a stochastic version of the LL or LLG equation for a spin density of one per unit cell can be used instead. To apply the stochastic LL to micromagnetic simulations, where the spin density per unit cell is generally higher, a conversion regarding simulation cell size and temperature has to be established. Based on energetic considerations, a conversion for ferromagnetic bulk and thin film systems is proposed. The conversion is tested in micromagnetic simulations which are performed with the Object Oriented Micromagnetic Framework (OOMMF). The Curie temperatures of bulk Nickel, Cobalt and Iron systems as well as Nickel thin-film systems with thicknesses between 6.3 mono layer (ML) and 31ML are determined from micromagnetic simulations. The results show a good agreement with experimentally determined Curie temperatures of bulk and thin film systems when temperature scaling is performed according to the presented model.
3D coherence scanning interferometry (CSI) is anoptical, non-contact and rapide measurement technique using a defined bandwidth of white light at normal incidence. White light interference microscopy (WLIM) providest here-dimensional surface topometry data up to a resolution of 0.4 µm lateral and 0.1 nm vertical. Three operating modi, surface, films and advanced films, enable measurements of step heights, roughness, wear volume, cone angle, surface pattern and layer thickness. Traceability to SI system is ensured by certified standards (PTB/NIST) within a DAkkS DIN EN ISO/IEC 17025:2018 accredited lab.
Fresnoite glass with excess SiO2 exhibits oriented surface crystallization, in contrast to the stoichiometric glass composition. Recent EBSD studies documented that the crystals in BTS (2BaO-TiO2-xSiO2, x=0-3) can occur in a distinct [101]-orientation perpendicular to the surface and claimed that this orientation is not a result of growth selection. During these previous studies, however, the effect of surface preparation and surrounding atmosphere during the crystallization experiments were not considered. As these parameters may influence crystal orientation, we studied the surface crystallization of a BTS glass (2BaO-TiO2–2.75SiO2) under controlled conditions with the help of light, electron and polarisation microscopy as well as EBSD. Heat treatments for one hour at 840°C of fractured BTS glass surfaces in air resulted in a large number of not-separable surface crystals. This large number of crystals can be caused by dust particles, which act as nucleation agents. As crystal growth velocity could further be influenced by humidity, our experiments are performed in a filtered and dried air atmosphere. The crystal morphology and orientation will be analysed in dependence of the sample preparation and a differing surrounding atmosphere.
Characterization of early crystallization stages in surface-crystallized diopside glass-ceramics
(2019)
Structure formation in glass-ceramics by means of surface crystallization is a challenging open question and remains elusive to definite answers. In several glass-ceramic systems, oriented crystal layers have been observed at the immediate surface, including diopside and some fresnoite systems. However, it is still open to debate, whether oriented surface crystallization is the result of oriented nucleation or growth selection effects. In the same vein, there is still discussion whether surface nucleation is governed by surface chemistry effects or by defects serving as active nucleation sites.
In order to help answer these questions, annealing experiments at 850°C have been performed on a MgO·CaO·2SiO2 glass, leading to the crystallization of diopside at the surface. Different annealing durations and surface treatment protocols (i.a. lapping with diamond slurries between 16 µm and 1 µm grain size) have been applied. Particular focus has been put on earliest crystallization stages, with crystal sizes down to about 200 nm. The resultant microstructure has been analyzed by electron backscatter diffraction (EBSD) and two different kinds of textures have been observed, with the a- or b-axis being perpendicular to the sample surface and the c-axis lying in the sample plane. Even at shortest annealing durations, a clear texture was present in the samples. Additionally, selected samples have been investigated with energy-dispersive x-ray spectroscopy in the scanning transmission electron microscope (STEM-EDX). The diopside crystals have been found to exhibit distinguished submicron structure variations and the glass around the crystals was shown to be depleted of Mg.
The characteristics of TiO2 coatings can greatly influence their final performance in large-scale applications. In the present study self-assembly of TiO2 nanoparticles (NPs) in multiple layers was selected as a deposition procedure on various substrates. For this, the main prerequisite constitutes the surface modification of both NPs and substrate with e.g. silane coupling agents. A set of functionalized TiO2 NPs has been produced by reaction with either (3- aminopropyl)triethoxysilane (APTES) or (3-aminopropyl)phosphonic acid (APPA) to functionalize the NP surface with free amino-groups. Then, the complementary functionalized NP set can be obtained from an aliquot of the first one, through the conversion of free surface amino-groups to aldehydes by reaction with glutaraldehyde (GA). Several types of TiO2 NPs differing in size, shape and specific surface area have been functionalized. FTIR, TGA, SEM/EDS, XPS, Auger electron spectroscopy (AES) and ToF-SIMS analyses have been carried out to evaluate the degree of functionalization, all the analytical methods employed demonstrating successful functionalization of TiO2 NP surface with APTES or APPA and GA.
Die Abbildung von Bruchflächen im REM liefert hochaufgelöste Bilddaten, die für die mikrofraktografische Bewertung von Bruchmechanismen unerlässlich sind. Durch den Abbildungsprozess im REM gehen räumliche Informationen im Normalfall größtenteils verloren. Mit der Verwendung eines segmentierten Rückstreudetektors ist dagegen die Erzeugung eines 3D-Oberflächenmodells während der Bildaufnahme praktisch in Echtzeit möglich. Die hier beschriebene Untersuchung soll die Anwendbarkeit des Verfahrens auf Bruchflächen zeigen. Zukünftig können Topografiedaten dazu beitragen, Bruchflächen besser zu interpretieren.
Introduction/purpose:
Multi-principal-element alloys (MPEAs), also known as complex concentrated alloys (CCAs), have recently come to the attention of the scientific community due to some interesting and unexpected microstructures, and their potential for improving properties such as, e.g. mechanical strength and oxidation resistance in high temperature structural applications. The AlMo0.5NbTa0.5TiZr refractory (r)CCA is one such candidate, showing a two-phase microstructure after a two-stage heat treatment under argon atmosphere at a controlled cooling rate. Since the application conditions intended for this alloy require a long-term high temperature (> 700 °C) mechanical and oxidation resistance, it becomes necessary to assess the possible phase development in this regime.
Methods:
In this contribution, the CALPHAD method is used to calculate phase equilibria for the AlMo0.5NbTa0.5TiZr CCA in the presence and absence of oxygen. Equilibrium phase amount evolution with temperature and Scheil Model for solidification (e.g. Fig.1a and Fig.1b, respectively) are analyzed, which are obtained using the databases TCNI9 and TTNI7 and the Gibbs energy minimizer in the Thermo-Calc software.
Results:
The diagrams reveal that two BCC-based phases could form during alloy solidification, where one phase would be enriched with Mo, Nb and Ta while the other phase, with Al, Ti and Zr. Activity oxides diagrams show that a stable form of aluminum oxide (α-Al2O3, Pearson symbol: hR10, corundum) can be formed. Results obtained by both databases, as well as discrepancies between property phase and Scheil approaches are discussed on the base of experimental results.
Conclusions:
A modeling tool is used to support alloy characterization and development, providing also the possibility to feedback information to improve existing thermodynamic databases.
19th and 20th centuries glass paint layers consist of a colour body and a colourless lead silicate flux, in which borax or boric acid was added as further component to improve the paint ability and to reduce the firing temperature for multiple layers of paint. Model glasses were used in laboratory tests to investigate the stability of glass paints with additions of boron oxide. To determine boron in paint layers, a LIBS-system with pulsed NdYAG-laser was used.
Water as side effect of reinforcing boehmite filler Local changes in anhydride cured epoxy resin
(2019)
Nanocomposites offer wide opportunities for lightweight constructions and enable reduction of weight and volume. Beside macroscopic toughening nanoparticle reinforced polymers show a soft interface around boehmite (AlOOH) filler nanoparticles. A related strong interaction between boehmite and the anhydride cured resin system is widely suspected in literature but not determined by structural Analysis. Determination of the molecular structure is important to allow simulations approaching the real system and predict future reinforcing effects.
DRIFT (diffuse refletance infrared fourier transformed) spectra of the boehmite reinforced anhydride cured epoxy show significant changes in the molecular structure compared to the neat polymer. Further investigations of the interactions between the single components of the resin system and the boehmite filler pointed out reactions between released water released from the boehmite filler and the anhydride hardener or amine accelerator. This leads to the discussion of competing polymerisation mechanisms that highly influence the polymer properties. Ongoing experiments and literature research approve that this impact of water is able to locally change the stoichiometrie, alter the curing mechanism or support an inhomogeneous crosslink density.
In this joint project, standardized measurement methods for hybrid
mixtures are developed, which serve to determine safety
characteristics for explosion protection.
A hybrid mixture is a multi-phase System consisting of fuel gas or
vapor, as well as air and flammable dust. This combination can occur
for instance in drying processes or during heterogenous reaction
processes.
TIG welding process was monitored using LIBS for the in situ measurement of chemical compositions in austenitic stainless steels. This research aims to prototype a real-time chemical composition analysis system for welding applications and prove the feasibility of such a quality control loop.
The chemical compositions of the weld pool, considering the welding metallurgy, is the most critical parameter for any occurring weld defects, e.g. hot cracking. Hence, controlling the weld pool chemical composition allows governing of the weld pool solidification behavior by monitoring and adjusting the respective welding parameters, e.g. welding current.
LIBS measurements were conducted during a TIG-welding process. The effect of the welding plasma on the LIBS signal was thoroughly investigated by varying various LIBS settings, e.g. delay and exposure time. Quantification of the main alloying elements Cr and Ni in the weld pool during welding was achieved by univariate calibration procedure.
Heating oil storage tanks made of polyethylene grades have been on the market in Germany since the early 1970s. To ensure safety, their replacement is recommended by tank manufacturers after a period of 30 years. Polyethylene is subject to ageing by alteration of the properties during its life cycle. The degree of degradation and the nature of the process mainly depend on the chemical alteration of the polyethylene, the wall thickness of the tank and the environmental conditions. There are no data available on the long-term behaviour of the polyethylene grades, especially after a service life of more than 30 years.
The aim of this investigation was to find a suitable test method to determine the factual degree of damage in comparison to the uncontaminated polyethylene grades. Material data of the used polyethylene grades are available because the BAM was the competent authority for the tests and expert reports for the approval of these tanks until the middle of the 1990s. Therefore, tank sections from the bottom, the shell and the roof of 22 individual storage tanks produced of polyethylene grades A and B have been examined by Melt Flow Rate (MFR) and Attenuated Total Reflectance (ATR). Their service life was in the range between 20 and 41 years.
The MFR measurements of the tank sections showed differences in the values depending on the weight which was used (5 kg or 21.6 kg). An increase of the MFR was determined for the samples of polyethylene grade A, whereas a reduction of the MFR values was measured for most samples of polyethylene grade B. This grade is mainly subject to the internal ageing by cross-linkages, increased degree of branched molecules and loss of the plasticizer.
ATR analysis exhibits an absorption band at 909 cm‒1 predominantly in samples of polyethylene grade A indicating chain scission and concomitantly formed terminal vinyl groups. This absorption band can be used for the characterization of the ageing of the polyethylene grades.
In special cases of angle beam ultrasonic measurement the applied transducer has to withstand extreme temperatures. Since the irradiation angle depends on the speed of sound in both the wedge material and the tested object, the developer must take into account the speed of Sound in a wedge material over the whole temperature range of transducers application.
The influence of prestraining on the aging response of an Al-Cu-Li alloy is investigated by preparation of different strain states (3 %, 4 %, 6 %) of the initial aging state. The Brinell hardness of the subsequently aged samples (up to 60 h aging time) was measured and it was found that the increasing dislocation concentration in the 3 different initial states leads to faster hardness increases and slightly higher maximum hardness.
Small-angle scattering (SAS) offers a reliable route to characterize the nanostructure of large amounts of material with a minimum of tedium, for example, easily extracting size distributions and volume fractions. There are a variety of analysis programs available while the evaluation of SAS measurements has been dominated by the classical curve fitting approach. SASfit represents such a classical curve fitting toolbox: it is one of the mature programs for SAS data analysis and has been available and used for many years. The latest developments will be presented and a scattering function of a mass fractal model of branched polymers in solution is provided as an example for implementing a plug-in.
Alternatively to classical curve fitting, part two presents the latest developments of the user-friendly open-source Monte Carlo regression package McSAS. The form-free Monte Carlo nature of McSAS means, it is not necessary to provide further restrictions on the mathematical form of the parameter distribution: without prior knowledge, McSAS is able to extract complex multimodal or odd- shaped parameter distributions from SAS data. The headless mode is presented by an example of operation within interactive programming environments such as a Jupyter notebook.
Fiber reinforced polymers (FRPs) are a well established material in lightweight applications, e.g. in automotive, aerospace or wind energy. The FRP components are subjected to multiaxial mechanical as well as hygrothermal loads. Common operation temperatures are in the range of 213 K and 373 K (-60 °C and 100 °C) at a relative humidity of 10% to 90%. In spacecraft applications, the environmental conditions are even more extreme. However, the correlation between multiaxial mechanical loading and harsh environment conditions have to-date not been investigated in detail. The project aims to investigate the fatigue behavior of FRPs dependent on multiaxial mechanical loading, temperature, and humidity. Extensive experimental testing is performed on flat plate and cylindrical tube specimens, accompanied by numerical and analytical calculations.
Polymeric core-shell particles were synthesized in a semi-batch emulsion polymerization process. The shell of the particles consist of PVDF with a high amount of beta-phase. Small-angle X-ray scattering (SAXS) was used to quantify the size of the cores of the particles and the thickness of the shell.
Absorption edge tomography is a method which exploits the sudden change of the attenuation coefficient, when the photon energy crosses the absorption edge of an element. The beamline BAM line at BESSY II, which is operated by the Federal Institute for Materials Research and Testing, can provide a monochromatized beam in a photon energy range from 5 keV up to 80 keV with a bandwidth of 2%. Together with the microtomography setup, this enables differential tomography sensitive to any element with N >= 24 (Cr) by using an appropriate K- or L-edge in this range. Here, a polymer filament embedding metal organic framework (MOF) was prepared and used for 3D printing. Absorption edge tomography at the copper K edge was employed to perform a non-destructive 3D characterization of the microstructure of the embedded MOF. Data fusion was then used to determine the size distribution of the embedded MOF.
The porosity and the surface roughness are recently discussed problems for SLM parts. The influence of SLM process parameters on porosity is well studied for different materials. Nevertheless, the build angle (i.e. the angle between part orientation and build plate) needs to be understood as an additional SLM process parameter, as it has been shown, that the microstructure and hence the mechanical performance of various materials depend on the build angle. The inherent build angle of each strut as a part of a lattice structure is the motivation to investigate the influence of the build angle on the porosity and roughness on round-shaped (1 mm diameter) struts by means of CT. Conventional Coordinate Measuring Machine (CMM) has the limitation towards small and round shaped samples. The need for Computed Tomography (CT) regarding investigations of SLM parts will increase because no other non-destructive technique allows the assessment of complex geometries with inner laying surfaces. We used CT to assess the pores and the strut surface. Seven struts out of the nickel alloy Inconel 625 with build angles from 30° to 90° were studied. It was found that the number of pores is smaller, and the size of pores is larger for the 90° strut. In case of 30° strut, the number of pores is increased towards down-skin side, additionally, this strut orientation showed to have the largest number of attached powder particles. The elongated pores exist exclusively near the strut surface. While the roughness at the down-skin surface is highly depending of the biud angle, the roughness at the up-skin surface is the same for all struts. The mechanisms of pore and surface roughness formation is not mainly driven by gravity.
Using non-optimum combination of manufacturing parameters in selective laser melting (SLM) may lead to reduction of quality of component: defects generation, distortion of geometry and even cracking. Usually, the optimization of parameters is performed by changing volumetric energy density (Ev) and selecting parameters giving low porosity values. However, not only low porosity but also stable microstructure and low residual stresses will help to achieve advanced mechanical behavior of the component.
In present work, we investigated cuboid-shaped Ti-6Al-4V samples produced with different manufacturing parameters. The parameters leading to the same Ev were considered as well as parameters which are not included in Ev. Residual stresses in subsurface region were investigated by synchrotron X-ray diffraction, which allows to penetrate around 100 µm from the surface therefore overcome the problem of high roughness of SLM components without additional sample preparation. Only tensile stresses were found along the building direction, that can play critical role especially during cyclic loading. In parallel, using X-ray computed tomography we also observe that porosity is mainly concentrated in the contour region, except in case where the laser speed is small. However, by using some process parameters it was possible to decrease residual stresses and obtain uniform α+β Ti microstructure and relatively low porosity. Additionally, it was found that not included in Ev (e.g., base plate position, focus distance) should be considered as additional manufacturing parameters during SLM process.
The environmental pollution with plastic debris is one of the great challenges scientists are facing in recent times Due to degradation by UV radiation and other environmental factors, larger pieces of plastic can decompose into microscale fragments which can enter human foodstuff through the food chain or by environmental entry Recent publications show a contamination of various food products with microplastic particles suggesting a widespread exposure Thus, orally ingested plastic particles pose a potential health risk to humans In this study, we investigated the impact of artificial digestive juices on the size and shape of the three environmentally relevant microplastic particles polystyrene (PS), polypropylene (PP) and polyvinyl chloride (PVC).
Dose enhancement by gold nanoparticles (AuNP) was shown to increase the biological effectiveness of radiation damage in biomolecules and tissue. Most of the current studies focus on external beam therapy on combination with AuNP. Here we present a Monte-Carlo study (Geant4) to characterise radioactive AuNP. Radioactive ¹⁹⁸Au emits beta and gamma rays and is considered for applications with solid tumours. To effectively apply ¹⁹⁸AuNP their energy deposit characteristics have to be determined in terms of intrinsic and extrinsic properties e.g. AuNP diameter, AuNP density, and their clustering behaviour. After each decay process, the energy deposit, inelastic scattering events, kinetic energy spectrum of secondary particles within the AuNP themselves and in a spherical target volume of water up to 1 μm radius were determined. Simulations were performed for AuNP radii ranging from 2.5 nm to 20 nm radius, different cluster sizes and densities. The results show an increase of the energy deposit in the vicinity of the AuNP up to 150 nm. This effect nearly vanishes for distances up to one micron. For the case of AuNP clusters and the same activity, the enhancement of the energy deposit increases with the relative gold mass percentage and therefore can be adjusted by changing AuNP radius or clustering behaviour.
Porous materials play an important role in several fields of technology, especially for energy applications like photovoltaics, electrolysis or batteries. The activity of porous films is affected by properties like porosity, film thickness, chemical composition of the material as well as the crystallinity of the framework. The complex morphology of such porous films constitutes a challenge even for modern analytical techniques and requires new approaches employing the combination/complementation of data of different analytical methods. In this contribution we characterize thin mesoporous iridium-titanium mixed oxide film properties by Electron Probe Microanalysis (EPMA) with energy dispersive X-ray spectroscopy (EDS) at an SEM.
The WelDX research project aims to foster the exchange of scientific data inside the welding community by developing and establishing a new open source file format suitable for documentation of experimental welding data and upholding associated quality standards. In addition to fostering scientific collaboration inside the national and international welding community an associated advisory committee will be established to oversee the future development of the file format. The proposed file format will be developed with regards to current needs of the community regarding interoperability, data quality and performance and will be published under an appropriate open source license.
By using the file format objectivity, comparability and reproducibility across different institutes and experimental setups can be improved.
Polyolefins as polypropylene are widely used in packaging, automotive, consumer goods, construction, infrastructure, agricultural film and other film and sheet applications. Due to their molecular structure, polyolefins inherently burn well. The wide and growing usage implements that fire retardancy of polyolefin products is necessary and gains more attention. Sulfurous additives with synergistic flame retarding effects were shown in polymers like polystyrene and polyolefins by Bellin et al. and Fuchs et al. earlier. For polystyrene compounds, Braun et al. revealed that thermal degradation in the presence of phosphorus and sulfurous additives changes massively. The total release, the composition, and the onset temperature of evolved decomposition products changes.
For polypropylene, mixtures containing triphenyl phosphate (TPP), sulfur (S8) and poly(tertbutylphenol) disulphide (PBDS) (Table 1) were prepared and investigated via thermogravimetric analysis coupled to Fourier transformed infrared spectroscopy (TGA-FTIR).
The life time of mechanical components in high temperature applications is basically determined by their workings. Corrosion determines the loss of material corresponding to the loss of the effective load-bearing section and consequently increasing stress levels. To improve the material selection for such applications a numerical life prediction corrosion model for different alloys and environments is needed. Based on the ferritic alloys FeCr and FeCrCo a first quantitative model is to be developed. For this purpose, the alloys are aged at 600°C, 650°C and 700°C in synthetic air under normal pressure for between 10 and 240 hours. The first objective is to establish a quantitative relationship between the oxidation rate as a function of composition and microstructure of the alloys. The influence of the inner interface as an essential parameter for transport by diffusion on the oxidation kinetics is discussed in this presentation.
The advantages of treating prefabricated components made of Ultra-High-Performance Concrete (UCPC) at 90 °C are largely recognized, while hydrothermal treatment at 185 °C and the corresponding saturation pressure of 1.1 MPa, in contrast, is not applied in building practice so far and was studied only by a few researchers.
In the research presented, the parameters pre-storage-time before treatment and dwell time in the autoclave were systematically varied. The results illustrate in which way compressive strength increases with the duration of treatment. Already samples which were only heated up and immediately cooled down show an increase in strength compared to the 28-day reference of about 10 %. After 20 h the maximum increase of about 25 % is reached. Interestingly the compressive strength of samples treated very long hardly decreases. It can be therefore concluded that for the composition investigated the achievable mechanical strength is not severely sensitive regarding the duration of the treatment.
Also, pre-storage times before autoclaving longer than 0.5 days showed no significant impact on strength development. The phase composition measured by XRD exhibits significant changes compared to the reference. The amount of ettringite and portlandite have vanished, the cement clinker phases are substantially decreased and hydroxylellestadite and hydrogarnet are formed as new phases. The increase in strength can be assigned to an improved pozzolanic and hydraulic reaction. Contradictory to literature, there was found no obermorite, a mineral which is known to be susceptible for disintegration at Long autoclaving duration. This explains why no significant strength loss appeared.
Alkali-silica reaction (ASR) is a serious Problem concerning the deterioration of concrete. This leads to significant maintenance and reconstruction costs for concrete infrastructures all over the world. The geographical regions, which play a major role in concrete deterioration, are for example coastal Areas or in general, areas with a high air humidity/salinity due to closeness of rivers or lakes.
These exemplary results show, the application of Raman spectroscopy establishes a valuable approach for characterizing the chemical and structural composition of ASR-products. The results prove the potential to trace the kind of reaction products, developing in dependence on the aggregate and to follow up its local alteration from origin of the gel.
The ferritic steel 13CrMo4-5 due to good properties with relation to attractive price is frequently use in power plants industry. According EN10028-2 this steel can be used up to 570 °C because of its creep behavior but its corrosion resistance limits the use frequently to lower temperatures, depending on gas temperature and slag formation. The corrosion test were performed in environment containing mixture of gases like: O2, COx, SOx and ashes, with elements e.g. Na, Cl, Ca, Si, C, Fe, Al. Exposure time was respectively 240 h, 1000 h and 4500 h in temperature 600 °C. The oxide scale on the 13CrMo4-5 steel was significant thicker than for In686 coating and the difference increase according for longer exposure time.
The microstructure, chemical and phase composition of the oxide scales were investigated by means of a light microscope, the electron scanning and transmission microscopes (SEM,TEM) equipped with the EDS detectors.
During the last years Additive Manufacturing (AM) became increasingly important. That becomes clear, while looking at the advantages like a high degree of freedom concerning the geometry of the parts, low waste rates and a reduction of postprocessing, to name just three. Laser Metal Deposition (LMD) is one of those AM- methods. It can be used for different kinds of applications, e.g. repair weldings of used parts, coatings to increase the corrosion resistance or to build up new components. But for all applications, the production of defect free parts is crucial. Therefore, different kinds of non-destructive monitoring techniques were tested for the LMD-process to identify their potential to detect imperfections in-situ.
Die Ursachen für Chemikalienunfälle können vielfältig sein. Prävention beginnt bereits im Prüflabor, wenn Chemikalien auf ihre gefährlichen Eigenschaften getestet werden. Dazu sind Prüfmethoden entwickelt und veröffentlicht worden, die heute weltweit Anwendung finden. Auf die Validität der Prüfmethode und richtige Durchführung der Prüfung im Laboratorium müssen sich Sicherheitsfachkräfte, Transporteure oder Händler verlassen können. Anhand der in den letzten 10 Jahren im Rahmen des CEQAT-DGHS von BAM und PTB durchgeführten Ringversuche (RV) wird gezeigt, dass bei allen bisher untersuchten Prüfmethoden ein Verbesserungsbedarf besteht. Die RV müssen daher zunächst auf die Methodenverbesserung und -validierung abzielen und nicht auf Leistungstests. Das Labormanagement und die praktische Durchführung der Prüfung sind in vielen Laboratorien verbesserungsbedürftig. Der Begriff „Erfahrung der Prüfer“ ist kritisch zu sehen: Eine „lange Erfahrung mit vielen Prüfungen“ ist nicht unbedingt ein Garant für richtige Ergebnisse.
Crack propagation in polymers: Separation of surface energy and irreversible deformation energy
(2019)
Fiber-reinforced-polymers (FRPs) are in current research focus in the lightweight construction industry, because of their extraordinary characteristics (stiffness and strength-to-density relation). The structure of polymer matrix and the interaction with reinforcement are crucial for optimization of the mechanical and thermal properties of FRPs. Due to the macromolecular chain structure, the mechanical properties of a polymer strongly vary with temperature: Below the glass transition, the chain segments of a polymer are “frozen”. Regarding fracture, the total changed energy during fracture if only dissipates for the generation of the new surfaces. However, in the region of the glass transition, the polymer chain segments start to get “unfrozen”, and the energy is not only required for generating new surfaces, but also for irreversibly deformation. This irreversible deformation is affected by the global temperature and the local temperature near the crack tip, which is affected by the local strain rate and crack propagation velocity.
Hence, in this research project, the irreversible deformation of neat and reinforced polymers will be controlled by changing the global temperature as well as the local temperature. With using different fracture experiments, the amount of energy required for creating new surfaces and for the irreversible deformation will be separated. This poster is the summary of the first part of the whole project. In the first part, the basic crack propagation theory for neat polymers is established and the special fracture experiment sample is prepared and tested at room temperature. In addition, the fracture experiment at room temperature is validated numerically.
Behälter aus hochdichtem Polyethylen (PE-HD) werden zur Lagerung und für den Transport von Kraftstoffen eingesetzt. Beim Kontakt beider Medien diffundiert der Kraftstoff in das Polymer, erhöht dessen Volumen und Duktilität und ändert damit das Fließverhalten des Polymers unter Zugbelastung. Zudem weist PE-HD in Luft im verstreckten Bereich das sogenannte strain-whitening (Lichtstreuung) auf, während in Diesel gelagertes PE-HD optisch transparent wird. Zur Untersuchung dieses Phänomens wurden ortsaufgelöste Röntgenrefraktion und –diffraktion (Topographie) eingesetzt. Aus Sicht der molekularen Struktur (Diffraktion) weisen die beiden Probentypen keine Unterschiede auf: im verstreckten Bereich liegt eine „Fasertextur“ der Polymerketten in Belastungsrichtung vor, im unverstreckten Bereich nahezu ideale Isotropie. Die für mikroskopische Strukturen empfindliche Röntgenrefraktion zeigt außerdem für die Probe in Luft im verstreckten Bereich eine ausgeprägte Orientierung von Grenzflächen in Zugrichtung, während die in Diesel gelagerte Probe keine Grenzflächen zeigt. In Analogie zum optischen Verhalten bewirken die ähnlichen Brechungsindizes beider Medien im Röntgenbereich, dass eindiffundierter Diesel als Immersionsflüssigkeit die Brechungseigenschaften herabsetzt.
The introduction of the 5G technology and automotive radar applications moving into higher frequency ranges trigger further miniaturization of LTCC technology (low temperature co-fired ceramics). To assess dimensional tolerances of inner metal structures of an industrially produced LTCC multilayer, computer tomography (CT) scans were evaluated by machine learning segmentation.
The tested multilayer consists of several layers of a glass ceramic substrate with low resistance silver-based vertical interconnect access (VIA). The VIAs are punched into the LTCC green tape and then filled with silver-based pastes before stacking and sintering. These geometries must abide by strict tolerance requirements to ensure the high frequency properties.
This poster presents a method to extract shape and size specific data from these VIAs. For this purpose, 4 measurements, each containing 3 to 4 samples, were segmented using the trainable WEKA segmentation, a non-commercial machine learning tool. The dimensional stability of the VIA can be evaluated regarding the edge-displacement as well as the cross-sectional area. Deviation from the ideal tubular shape is best measured by aspect ratio of each individual layer. The herein described method allows for a fast and semi-automatic analysis of considerable amount of structural data. This data can then be quantified by shape descriptors to illustrate 3-dimensional information in a concise manner. Inter alia, a 45 % periodical change of cross-sectional area is demonstrated.
Homogeneous introduction of organic additives is a key of ceramic powder processing. Addition of organics to ceramic slurries holds advantages compared to dry processing like organic content reduction and a more homogeneous additive distribution on the particle surface.
Investigations of the alumina slurries were primarily based on zeta potential measurements and sedimentation analysis by optical centrifugation. Both methods were combined to determine a suitable additive type, amount and composition, whereas the spray drying suitability has been ensured by viscosity measurements. Granules, yielded by spray drying of such ideally dispersed alumina slurries, are mostly hollow and possess a hard shell. Those granules cannot easily be processed and can only hardly be destroyed in the following shaping step, leading to sinter bodies with many defects and poor strength and density.
The precise slurry destabilization, carried out after ideally dispersing the ceramic powder, shows a strong influence on the drying behavior of the granules and hence on the granule properties. A promising degree of destabilization and partial flocculation was quantified by optical centrifugation and resulted in improved granule properties. Spray drying the destabilized alumina slurries yielded homogeneous “non-hollow” granules without the above mentioned hard shell. Sample bodies produced of these granules exhibited a reduction of defect size and number, leading to better results for sinter body density and strength.
The positive effect of the slurry destabilization has been further improved, by exchanging the atomizing unit from a two-fluid one to an ultrasound atomizer with only minor slurry adjustments necessary. The controlled destabilization and ultrasound atomization of the ceramic slurry show excellent transferability for zirconia and even ZTA (zirconia toughened alumina) composite materials.
Sicherheitstechnische Kenngrößen des Explosionsschutzes für hybride Stoffgemische – Das Verbundvorhaben „NEX-HYS“ Im Rahmen des WIPANO-Programms (Wissens- und Technologietransfer durch Patente und Normen), gefördert vom BMWi, ist ein Verbundvorhaben zur Bestimmung sicherheitstechnischer Kenngrößen hybrider Gemische begonnen worden. Teilnehmer sind die OvGU Magdeburg (Koordination), die BAM, die PTB, die INBUREX GmbH und das DIN. Hybride Gemische, z.B. Staub-Brenngas-Luft-Gemische, spielen in der Prozesstechnik bei Trocknungs- und Transportprozessen eine wichtige Rolle. Für diese Gemische lassen sich die sicherheitstechnischen Kenngrößen nach den vorhandenen Normen nicht bestimmen. Aus bisherigen Forschungsarbeiten ist allerdings bekannt, dass hybride Gemische teilweise zündempfindlicher sind, erweiterte Explosionsbereiche aufweisen und die Auswirkungen von Explosionen heftiger ausfallen können als bei Brennstoffen, die nur in einem Aggregatzustand vorliegen.
Ziel des Verbundprojektes ist es, labortechnische Verfahren zur Bestimmung sicherheitstechnischer Kenngrößen (STK) für hybride Gemische bis zur Normungsreife zu entwickeln und mittelfristig eine europäische Normung für hybride Gemische im CEN TC305 zu initiieren. Folgende, technisch wichtige Kenngrößen sollen bearbeitet werden: Untere Explosionsgrenze, Sauerstoffgrenzkonzentration, maximaler Explosionsdruck, maximaler zeitlicher Druckanstieg und Mindestzündtemperatur.
Um eine schnelle allgemeine Verfügbarkeit der Ergebnisse zu gewährleisten, ist im Rahmen des Vorhabens die Erstellung einer DIN SPEC (Vornorm) geplant.
Im Poster wird das Verbundvorhaben mit den einzelnen Arbeitspaketen dargestellt und diskutiert.
Chromia forming high alloyed ferritic-austenitic steels are being used as boiler tube materials in biomass and coal-biomass co-fired power plants. Despite thermodynamic and kinetic boundary conditions, microstructural features such as grain orientation, grain sizes or surface deformation contribute to the oxidation resistance and formation of protective chromium-rich oxide layers. This study elucidates the impact of microstructure such as the grain size and number of carbide precipitates on high temperature oxidation at 650°C in 0.5% SO2 atmosphere. Cold-rolled Fe-16Cr-0.2C material was heat-treated to obtain two additional microstructures. After exposure to hot and reactive gases for 10 h < t < 1000 h layer thicknesses and microstructure of oxide scales are observed by scanning electron microscopy and Energy-dispersive X-ray spectroscopy. The two heat treated alloys showed reasonable oxidation resistance after 1000 h of exposure. The oxidation rate was substantially higher for the alloy with a duplex matrix after heat treatment compared to the fine-grained material.
Using non-optimum combination of manufacturing parameters in selective laser melting (SLM) may lead to reduction of quality of component: defects generation, distortion of geometry and even cracking. Usually, the optimization of parameters is performed by changing volumetric energy density (Ev) and selecting parameters giving low porosity values. However, not only low porosity but also stable microstructure and low residual stresses will help to achieve advanced mechanical behavior of the component.
In present work, we investigated cuboid-shaped Ti-6Al-4V samples produced with different manufacturing parameters. The parameters leading to the same Ev were considered as well as parameters which are not included in Ev. Residual stresses in subsurface region were investigated by synchrotron X-ray diffraction, which allows to penetrate around 100 µm from the surface therefore overcome the problem of high roughness of SLM components without additional sample preparation. Only tensile stresses were found along the building direction, that can play critical role especially during cyclic loading. The pore shape and spatial distribution obtained by computed tomography varied for samples produced with the same Ev. However, by using some process parameters it was possible to decrease residual stresses and obtain uniform α+β Ti microstructure and relatively low porosity. Additionally, it was found that not included in Ev (e.g., base plate position, focus distance) should be considered as additional manufacturing parameters during SLM process.
Quality Aspects of Additively Manufactured Medical Implants - Defect Detection in Lattice Parts
(2019)
Additive Manufacturing technologies are developing fast to enable a rapid and flexible production of parts. Tailoring products to individual needs is a big advantage of this technology, which makes it of special interest for the medical device industry and the direct manufacturing of final products. Due to the fast development, standards to assure reliability of the AM process and quality of the printed products are often lacking. The EU project Metrology for Additively Manufactured Medical Implants (MetAMMI) is aiming to fill this gap by investigating alternative and cost efficient non-destructive measurement methods.
Toxicological studies have shown that some types of carbon nanotubes may provoke asbestos-like effects including chronic inflammation and lung cancer. Inhaled carbon nanotubes may reach the deep lung tissue. Alveolar macrophages are responsible to remove such foreign objects from the alveoli in a process called phagocytosis. If a macrophage fails to uptake a nanotube completely, cell lesions give rise to inflammation. It is currently assumed that short, long and flexible, and granularly agglomerated (tangled) nanofibres are clearable by macrophages, whereas biodurable long and rigid nanotubes persist in the lung tissue. The flexural rigidity of nanofibres is therefore believed to an important material property that governs fibre toxicity and needs to be investigated. The present work aims at determining the rigidity of nanofibres by detecting their resonance frequencies using a Dynamic Scanning Electron Microscope (DySEM) setup. By depositing and fixing a nanofibre to an oscillating support, it can be excited to vibrations and treated as a cantilevered beam. This way, its elastic modulus can be determined via Euler-Bernoulli’s beam theory. Multi-walled carbon nanotubes (MWCNTs) were deposited on high frequency piezoelectric quartz crystals mounted on a scanning electron microscope (SEM) holder. When introduced into the SEM chamber and connected to a frequency-sweeping waveform generator, the quartz crystal actuates the deposited fibre. A lock-in amplified processes the secondary electron detector signal resulting from the electron beam modulated by the vibrating nanofibre. Whenever a fibre resonance is detected, the SEM image of the fibre is stored to identify the fibre oscillation mode. The found resonance frequencies and modes allow determining the elastic modulus according. Since the frequency spacing of resonances is predicted by Euler-Bernoulli, the mode number can be checked and elastic modulus values be averaged. A significant number of MWCNTs have been classified according to their level of rigidity. The applicability and reliability of the method will be discussed.
Toxicological studies have shown that some types of carbon nanotubes may provoke asbestos-like effects including chronic inflammation and lung cancer. Inhaled carbon nanotubes may reach the deep lung tissue. Alveolar macrophages are responsible to remove such foreign objects from the alveoli in a process called phagocytosis. If a macrophage fails to uptake a nanotube completely, cell lesions may give rise to inflammation. It is currently assumed that short, flexible and long as well as granularly agglomerated (tangled) nanofibres are clearable by macrophages, whereas biodurable long and rigid nanotubes may persist in lung tissue. The flexural rigidity of nanofibres is therefore believed to be an important material property that governs fibre toxicity and needs to be investigated. The present work aims at determining the rigidity of nanofibres by detecting their resonance frequencies using a Dynamic Scanning Electron Microscope (DySEM) setup. By depositing and fixing a nanofibre to an oscillating support, it can be excited to vibrations and treated as a cantilevered beam. This way, its elastic modulus can be determined via Euler-Bernoulli’s beam theory. Multi-walled carbon nanotubes (MWCNTs) were deposited on high frequency piezoelectric quartz crystals mounted on a scanning electron microscope (SEM) holder. When introduced into the SEM chamber and connected to a frequency-sweeping waveform generator, the quartz crystal actuates the deposited fibre. A lock-in amplified processes the secondary electron detector signal resulting from the electron beam modulated by the vibrating nanofibre. Whenever a fibre resonance is detected, the SEM image of the fibre is stored to identify the fibre oscillation mode. The found resonance frequencies and modes allow determining the elastic modulus accordingly. Since the frequency spacing of resonances is predicted by Euler-Bernoulli, the mode number can be identified and elastic modulus values be averaged. A significant number of individual MWCNTs were classified according to their level of rigidity. The applicability and reliability of the method will be discussed.
Toxicological studies have shown that some types of carbon nanotubes may provoke asbestos-like effects including chronic inflammation and lung cancer. Inhaled carbon nanotubes may reach the deep lung tissue. Alveolar macrophages are responsible to remove such foreign objects from the alveoli in a process called phagocytosis. If a macrophage fails to uptake a nanotube completely, cell lesions may give rise to inflammation. It is currently assumed that short, flexible and long as well as granularly agglomerated (tangled) nanofibres are clearable by macrophages, whereas biodurable long and rigid nanotubes may persist in lung tissue. The flexural rigidity of nanofibres is therefore believed to be an important material property that governs fibre toxicity and needs to be investigated. The present work aims at determining the rigidity of nanofibres by detecting their resonance frequencies using a Dynamic Scanning Electron Microscope (DySEM) setup. By depositing and fixing a nanofibre to an oscillating support, it can be excited to vibrations and treated as a cantilevered beam. This way, its elastic modulus can be determined via Euler-Bernoulli’s beam theory. Multi-walled carbon nanotubes (MWCNTs) were deposited on high frequency piezoelectric quartz crystals mounted on a scanning electron microscope (SEM) holder. When introduced into the SEM chamber and connected to a frequency-sweeping waveform generator, the quartz crystal actuates the deposited fibre. A lock-in amplified processes the secondary electron detector signal resulting from the electron beam modulated by the vibrating nanofibre. Whenever a fibre resonance is detected, the SEM image of the fibre is stored to identify the fibre oscillation mode. The found resonance frequencies and modes allow determining the elastic modulus accordingly. Since the frequency spacing of resonances is predicted by Euler-Bernoulli, the mode number can be identified and elastic modulus values be averaged. A significant number of individual MWCNTs were classified according to their level of rigidity. The applicability and reliability of the method will be discussed.
The particle size distribution is considered the most relevant information for nanoscale property identification and material characterization. The current OECD test guideline on particle size and size distribution (TG 110) is not applicable to ‘nano-sized’ objects. In this project we thus develop a new OECD test guideline for the measurement of the size and size distribution of particles and fibers with at least one dimension in the nanoscale. A fiber is defined as an object having an aspect ratio of length/diameter l/d >3. The width and length of each fiber should be measured concurrently.
In order to measure the particle size distributions, many techniques are available. 9 methods for particles and 2 methods for fibres have been tested in a prevalidation study and appropriate methods will be compared in an interlaboratory round robin test starting in February 2019.
Within the perspective of increasing reliability of AM processes, real-time monitoring allows part inspection while it is built and simultaneous defect detection. Further developments of real-time monitoring can also bring to self-regulating process controls. Key points to reach such a goal are the extensive research and knowledge of correlations between sensor signals and their causes in the process.
Glass strength and fatigue is limited by surface cracks. As subcritical crack growth (SCCG) is governed by ambient humidity, stress corrosion at the crack tip is widely accepted to be the underlying mechanism. However, as water is known to have decisive effect on glass properties and can rapidly enter the crack tip near glass region, SCCG could be affected by such water related phenomena. We tried to mimic these effects studying water dissolution and speciation, mechanical properties, and SCCG in water-bearing glasses. For this purpose, glasses up to 8 wt% water have been prepared by means of high-pressure melting of glass powder - water mixtures.
As part of this effort, SCCG in dry and hydrous commercial micros¬cope slide glass (CW = 6 wt%) was studied in double cantilever beam (DCB) geometry and sub-Tg relaxation was measured by Dynamic Mechanical Analysis (DMA).
For SCCG in ambient air (24% r.h.), SCCG was promoted by the presence of 6wt% bulk water with respect to the dry glass. On the other hand, stress intensity values, KI, required to cause slow crack growth (v < 10-6 ms-1) resemble literature findings for float glass of similar composition in liquid water, which might represent the maximum possible promoting effect of ambient water on SCCG.
For SCCG in vacuum (10-3 mbar), dissolved bulk water causes even more pronounced effects. Most strikingly, it strongly decreases the slope of the log v(KI)-curve, which is a measure of dissipated energy during fracture. A strong increase of sub-Tg relaxation with increasing water content was confirmed by DMA. As a consequence, slow crack growth occurs at KI values as measured in the dry glass whereas fast crack growth occurs at much larger KI than that of the dry glass. Kinks and shoulders shown by the inert log v(KI)-curve indicate that bulk water does not simply affect bulk mechanical properties.
Additive manufacturing (AM) opens the route to a range of novel applications. However, the complexity of the manufacturing process poses a challenge to produce defect-free parts with a high reliability. Since process dynamics and resulting microstructures of AM parts are strongly influenced by the involved temperature fields and cooling rates, thermography is a valuable tool for process monitoring. Another approach to monitor the energy input into the part during process is the use of optical tomography.
Common visual camera systems reach much higher spatial resolution than infrared thermography cameras, whereas infrared thermography provides a much higher temperature dynamic. Therefore, the combined application increases the depth of information. Here, we present first measurement results using a laser beam melting setup that allows simultaneous acquisition of thermography and optical tomography from the same point of view using a beam splitter. A high-resolution CMOS camera operating in the visible spectral range is equipped with a near infrared bandpass filter and images of the build plate are recorded with long-term exposure during the whole layer exposing time. Thus, areas that reach higher maximum temperature or are at elevated temperature for an extended period of time appear brighter in the images. The used thermography camera is sensitive to the mid wavelength infrared range and records thermal videos of each layer exposure at an acquisition rate close to 1 kHz.
As a next step, we will use computer tomographic data of the built part as a reference for defect detection.
This research was funded by BAM within the focus area Materials.
The assessment of high cycle fatigue in additive manufactured (AM) components is a challenge due to complex microstructure, anisotropic material behavior, residual stresses and porosity / lack-of-fusion defects. Due to the statistical distribution of defects, a high scatter band of S-N-curves is expected. The fracture mechanics-based fatigue assessment of additive manufactured components must consider the propagation of short cracks emanating from defects.
In this work, the fatigue crack propagation resistance in the short and large crack regimes of additive and conventionally manufactured AISI 316L stainless steel is examined experimentally based on the cyclic R-curve. However, remaining residual stresses in the AM specimen lead to unexpected and dramatic crack-growth during the pre-cracking procedure.
Microbial modelling of sulfate-reducing bacteria (SRB) and methanogenic archaea (ME) using iron
(2019)
Sulfate reducing bacteria (SRB) and methanogenic archaea (MA) are commonly found in the oil and gas environments. The formation of hydrogen sulfide (HS-) is particularly concerning for the petroleum industry due to its corrosiveness. However, the activities of SRB are limited to the concentration of sulfate present in the environment, whereas methanogens can utilize substrates such as H¬2 for methanogenesis. MA is commonly found in sulfate-free environments, such as deep sediments, and are known to form interspecies electron transfer relationships with SRB. Recently, SRB and MA capable of microbiologically influenced corrosion (MIC) by using elemental iron as a direct electron source (EMIC) have gained increased attention. On the iron surface, EMIC-SRB can outcompete EMIC-MA in the presence of sulfate, but this changes as sulfate depletes. The formation of FeS on the metal surface can be further utilized by MA for methanogenesis as it provides a conductive path. However, the possible kinetics involved of the overall process are currently unknown.
We obtained a co-culture of EMIC-SRB and EMIC-MA to investigate the growth rates and electrical potential changes under different environmental conditions, including changes in pH, temperature and salinity. Results indicate that under neutral conditions and using iron as the sole substrate, methane production (up to 5 mM) starts after sulfate was depleted. Electrochemical measurements will be conducted on the co-culture under different conditions to determine the changes in the electrical potential in correlation with the sulfate and methane concentration. Fluorescence and electron microscope images of the biofilm structure will be used to visualize cell distribution and morphology. This study embarks the first step of understanding the relationship between EMIC-SRB and EMIC-MA. Such knowledge is important for the field of microbial electrophysiology and can be further explored for industrial applications.
A central challenge to ensure the sustainable production and use of nanotechnologies is to understand and effectively control the risks along the industrial innovation value chain. Knowledge about nanotechnology processes and nanosafety issues (hazards, fate, risk...) is growing rapidly but the effective use of this knowledge for risk management by market actors is lagging behind.
EC4SafeNano (European Centre for Risk Management and Safe Innovation in Nanomaterials and Nanotechnologies) promotes a harmonized vision of expertise in risk assessment and management for the public and private sectors to enable the safe development and commercialization of nanotechnology.
EC4SafeNano is operated together by major European risk institutes with the support of numerous associated partners, gathering all stakeholders involved in Nanomaterials and Nanotechnologies (regulators, industry, society, research, service providers...).
In a case study the surface chemical transformations upon 2 different ageing procedures (long-term UV irradiation or swimming pool water) of a representative set of titanium dioxide nanoparticles has been investigated. The materials have been analyzed by various analytical techniques. Each method addresses different aspects of the complex endpoint surface chemistry. The multi technique approach allows evaluation of the capabilities and limitations of the applied methods regarding their suitability to address the endpoint surface chemistry and their sensitivity to identify even small surface chemical transformations.
Results:
- To obtain a comprehensive picture, it is insufficient to concentrate on a single analysis technique.
- By using time-of-flight secondary ion mass spectrometry (ToF-SIMS) in combination with principal component analysis (PCA) it was possible to identify even subtle changes in the surface chemistry of the investigated materials.
- A general trend that was observed for the UV-aged samples is the decrease of organic material on the nanomaterial surface.
This project has received funding from the European Union’s Horizon 2020 research and innovation programme under grant agreement No 723623.
The understanding of process-microstructure-property-performance (PMPP) relationships in additive manufacturing (AM) of metals is highly necessary to achieve wide-spread industrial application and replace conventionally manufactured parts, especially regarding safety-relevant applications. To achieve this understanding, reliable data and knowledge regarding material’s microstructure-property relationships (e.g. the role of defects) is needed, since it represents the base for future more targeted process optimizations and more reliable calculations of performance. However, producing reliable material data and assessing the AM material behaviour is not an easy task: big challenges are e.g. the actual lack of standard testing methods for AM materials and the occasional difficulties in finding one-to-one comparable material data for the conventional counterpart.
This work aims to contribute to end this lack of reliable material data and knowledge for the low cycle fatigue behaviour of the most used titanium alloy in aerospace applications (Ti-6Al-4V). For this purpose, two sets of test specimens were investigated. The first set was manufactured from cylindrical rods produced by an optimized DED-L process and the second was manufactured from a hot formed round bar. The test specimens were cyclically loaded until failure in the low-cycle-fatigue (LCF) regime. The tests were carried out according to ISO 12106 between 0.3 to 1.0 % axial strain amplitude from room temperature up to 400°C. The LCF behaviour is described and compared between materials and with literature values based on cyclic deformation curves and strain-based fatigue life curves. Besides, the parameters of Manson-Coffin-Basquin relationship were calculated. The microstructures (initial and after failure) and fracture surfaces were comparative characterized. Thereby, the focus lied on understanding the role of grain morphology and defects on the failure mechanisms and fatigue lifetimes. For this latter characterization, optical microscopy (OM), scanning electron microscopy (SEM) and micro computed tomography (µCT) were used.
The present study addresses the capability of measurement of relative particle number concentration by scanning electron microscopy for model bimodal silica and gold samples prepared in the frame of the European research project “nPSize - Improved traceability chain of nanoparticle size measurements” as candidate reference nanoparticles.
In this paper one refined approach is applied to determine the exact orientation of bipyramidal TiO2 nanoparticles prepared with good dispersion as almost isolated particles on a carbon TEM grid. The advantages of the recently developed high-throughput Transmission Kikuchi Diffraction (TKD) are used to identify quickly and reliably the geometrical orientation of the crystalline TiO2 nanoparticle bipyramids (anatase) on a statistically relevant number of particles.
In this contribution different ways are explored with the aim to generate suitable training data for ‘non-ideal’ samples using various approaches, e.g., computer-generated images or unsupervised learning algorithms such as generative adversarial networks (GANs). We used these data to train simple CNNs to produce segmentation masks of SEM images and tested the trained networks on real SEM images of complex nanoparticle samples. The novel use of CNN for the automated analysis of the size of nanoparticles of complex shape and with a high degree of agglomeration has proved to be a promising tool for the evaluation of particle size distribution on a large number of constituent particles. Further development and validation of the preliminary model, respectively larger training and validation data sets are necessary.
Nanoparticles (NP) have become important materials for a variety of chemical technologies. The enhance surface-area-to-volume ratio of NPs is very high, making them excellent for use as catalyst, in analytical assays, and for antimicrobial applications.
Nickel NPs have exhibited immense potential as important catalyst for the Sabatier reaction, i.e. converting waste to energy via transformation of CO2 into CH4, and could replace the rare earth elements such as Ru, PT, or Rh. In this work we describe the solvothermal synthesis of monometallic and bimetallic nickel nanoparticles.
Monodisperse monometallic Ni nanoparticles were synthesized using Oleylamin as solvent and reducing agent. The nanoparticles were investigated using small angle scattering (SAXS), scanning transmission electron microscopy (STEM) and energy dispersive X-ray spectroscopy (EDX), showing that the catalytically active sites are accessible. However, Ni has a high propensity to undergo oxidation, and becoming deactivated by coke formation. Hence, we further explore the preparation of bimetallic NPs, where a second metal is added to stabilize the Ni.
Bimetallic Cu-Ni NPs were synthesized by simultaneous solvothermal reduction. These bimetallic NPs exhibit excellent catalytic properties are promising candidates to be used as catalysts for efficient energy storage.
Influence of the scanning strategy on the residual stress state in IN718 additive manufactured parts
(2020)
Laser Powder Bed Fusion (L-PBF) is an additive manufacturing technique enabling the design of complex geometries that are unrivalled by conventional production technologies. Nevertheless, L-PBF process is known to induce a high amount of residual stresses (RS) due to the high temperature gradients present during powder melting by laser. High tensile residual stresses are to be found the edges whereas the bulk material shows balancing compressive RS. Literature shows that the RS is highly sensitive to the process parameters. In particular, this study presents the characterization of the RS state in two L-PBF parts produced with a rastering scan vector that undergoes 90° or 67° rotation between subsequent layers.
Modern air-liners and wind turbine rotor blades are made up primarily of fiber reinforced plastics. Failure of these materials heavily impairs the serviceability and the operational safety. Consequently, knowledge of the failure behavior under static and cyclic loads is of great interest to estimate the operational strength and to compare the performance of different materials. Ideally, the damage evolution under operational load is determined with in-situ non-destructive testing techniques. Here, we report in-situ synchrotron X-ray imaging of tensile stress induced cracks in carbon fiber reinforced plastics due to inter-fiber failure. An inhouse designed compact tensile testing machine with a load range up to 15 kN was integrated into the beamline. Since conventional radiographs do not reveal sufficient contrast to distinguish cracks due to inter-fiber failure and micro cracking from fiber bundles, the Diffraction Enhanced Imaging (DEI) technique is applied in order to separate primary and scattered (refracted) radiation by means of an analyzer crystal. This technique allows fast measurements over large fields-of-view and is ideal for in-situ investigations.
Background, Motivation and Objective
Nanomaterials are at the core of some of the 21st century’s most promising technologies. In order to utilize and rationally design materials at the nanoscale the reliable characterization of their physico-chemical properties is highly important. Furthermore, the European Commission has taken measures via the REACH Regulations to control the classification of nanomaterials. REACH Annexes which entered into force in January 2020 require manufacturers to register nanomaterials that are traded in larger quantities (at least 1 ton). Every powder or dispersion where 50% (number distribution) of the constituent particles have sizes ≤ 100 nm in at least one dimension are defined as a nanomaterial. This creates a need for both industrial manufacturers and research and analytical service facilities to reliably characterize potential nanomaterials. Currently, BAM is working on developing reference nanoparticles, which shall expand the scarce list of worldwide available nano reference materials certified for particle size distribution, but also targeting other key parameters such as shape, structure (including porosity) and functional properties. Thus, candidate materials are considered to complement the already available spherical and monodisperse silica, Au and polystyrene reference nanoparticles, e.g. iron oxide and titanium oxide, with an average atomic number between those of silica and gold. Particularly for the imaging by electron microscopies, new nanoparticles of well-defined size in the range of 10 nm are decisive for the accurate particle segmentation by setting precise thresholds.
Statement of Contribution/Methods
Synthesis: Highly monodisperse iron oxide nanoparticles can be synthesized in large quantities by thermal decomposition of iron oleate or iron acetylacetonate precursors in high boiling solvents such as octadecene or dioctyl ether in the presence of oleic acid and oleylamine as capping agents.
Scanning Electron Microscope: An SEM of type Supra 40 from Zeiss has been used including the dedicated measurement mode transmission in SEM (STEM-in-SEM) with a superior material contrast for the nanoparticle analysis. The software package ImageJ has been used for the analysis of the STEM-in-SEM images and to determine the particle size distribution.
Dynamic Light scattering (DLS): Particles in suspension were measured in comparison by means of Zetasizer Nano (Malvern Panalytical; cumulants analysis) and NanoFlex (Microtrac; frequency power spectrum).
Results/Discussion
In this study iron oxide nanoparticles synthesized at BAM and pre-characterized by DLS, SEM (including the transmission mode STEM-in-SEM) are presented. The particles are spherical and highly monodisperse with sizes slightly larger than 10 nm.
Novel Technique for On-Line Monitoring of the Curing Process of Fiber Reinforced Polymer Composites
(2020)
A specially designed experimental set up has been integrated into a commercially available FT IR Spectrometer for ATR experiments on Epoxy Systems. Representative data of far infrared spectra measured during the curing process at different temperatures of an epoxy system will be presented in dependency of the curing situation. The experiments and the selected set up are discussed to demonstrate its potential for future monitoring and ageing control applications during a manufacturing process of polymer composites.
A series of different nanoparticle suspensions (Gold, Latex, and SiO2 in varying concentrations) were microprinted onto TEM grids in a 4 x 4 array in the concentration range 7x10^8 to 1x10^11 NP/mL and imaged with SEM and TSEM. Concentrations and printing conditions (temperature, relative humidity) were varied in order to minimize the coffee ring effect.
Development and characterization of starch film and the incorporation of silver nanoparticles
(2020)
Starch is one of the biopolymers being used for bioplastic synthesis. For production, starch can be combined with different plasticizers, starches from different plant sources and even with nanomaterials to improve or to add film properties. The challenge of adding these, e.g. in the form of silver nanoparticles (AgNp) is to determine the concentration so as to avoid impairing the properties of the film, agglomeration or altering the visual characteristics of the film. In this study, a starch film synthesis route and the incorporation of silver nanoparticles has been proposed in order not to alter the properties of the film while maintaining the transparency and a clear colour of the starch film. The results showed that the proposed synthesis route is promising, efficient, reproducible, fast and the film has good mechanical properties.
Rapid cooling rates and steep temperature gradients are characteristic of additively manufactured parts and important factors for the residual stress formation. This study examined the influence of heat accumulation on the distribution of residual stress in two prisms produced by Laser Powder Bed Fusion (LPBF) of austenitic stainless steel 316L. The layers of the prisms were exposed using two different border fill scan strategies: one scanned from the centre to the perimeter and the other from the perimeter to the centre. The goal was to reveal the effect of different heat inputs on samples featuring the same solidification shrinkage. Residual stress was characterised in one plane perpendicular to the building direction at the mid height using Neutron and Lab X-ray diffraction. Thermography data obtained during the build process were analysed in order to correlate the cooling rates and apparent surface temperatures with the residual stress results. Optical microscopy and micro computed tomography were used to correlate defect populations with the residual stress distribution. The two scanning strategies led to residual stress distributions that were typical for additively manufactured components: compressive stresses in the bulk and tensile stresses at the surface. However, due to the different heat accumulation, the maximum residual stress levels differed. We concluded that solidification shrinkage plays a major role in determining the shape of the residual stress distribution, while the temperature gradient mechanism appears to determine the magnitude of peak residual stresses.
Aluminum is an often-used building material in modern architecture. In recent years buildings from the 1950th and 1960th are increasingly subject of conservation works including the aluminum parts. Typical surface damages are signs of corrosion caused by weathering processes or scratches in the anodized layer due to extensive wear. To repair damaged aluminum surfaces, there are usually two options: smaller areas are repaired by using a touch-up pen, for larger damages it is necessary to remove the anodized layer completely. Both possibilities are disadvantageous for the objects; the touch-up pen often does not match the color together with an insufficient corrosion protection, while newly anodized layers often differ in color and gloss from the original surface.
For this reason, a research project was initiated to develop a mobile method to repair anodized aluminum parts. The first step focusses on the mobile anodization process by using the electrolyte with a gel substrate. Different cathodic materials are to be tested together with appropriate cooling material. The anodized area should be isolated to protect undamaged areas. Examinations of the produced layers are conducted by using Keyence microscope, eddy current testing and ESEM analysis. Further steps are to transform the coloring and sealing process for mobile application. Color could be applied by using a brush or by spray while the sealing process could be performed with water vapor. An heatable putty knife could be used, if heating up the area will be necessary. Once the application process is developed, the anodization will be tested on samples with artificial damages, fixed in horizontal and vertical positions. The stability of the anodized surface will be examined by accelerated ageing in a climate chamber and outdoor weathering.
The electrolyte (diluted sulfuric acid) was combined with a gel binder to enable a mobile application. Several thickening agents were tested concerning their conductivity and stability in acid systems. Anodization tests with different cathodic material and shapes were conducted. The temperature during anodization was controlled and adjusted if necessary. The anodized area was restricted by using either a lacquer, an adhesive or a removable silicon barrier. The fist results show the feasibility of the method on enclosed areas. The achieved thickness was measured by eddy current testing and the structure was controlled by ESEM analysis. The examinations show a connection between thickness and porosity of the anodized layers and the temperature during the application process.
Next steps are testing mobile coloring and sealing methods followed by mobile anodization on artificial damaged areas.
An alternative method for lithium isotope amount ratio analysis is proposed by combining atomic absorption spectrometry with spectra data analysis by machine leaning. It is based on the well-known isotope shift of around 15 pm for the electronic transition at wavelength 670.7845 nm which can be measured by a high-resolution continuum source atomic absorption spectrometer (HR-CS-AAS). For isotope amount ratio analysis, a scalable three boosting machine learning algorithm (XGBoost) was employed and calibrated with a set of samples with a 6Li isotope amount fraction ranging from 99% to 6%. The absolute Li isotope amount fractions of these calibration samples were previously measured by multi-collector inductively coupled plasma mass spectrometry (MC-ICP-MS) and used as ab-initio data for the machine learning algorithm. Validation of the machine leaning model was performed with two standard reference materials (LSVEC and IRMM-016). The procedure was employed for the isotope amount ratio determination of a set of stock chemicals (Li2CO3, LiNO3, LiCl, LiOH, and LiF) as well as a BAM candidate LiMNC cathode reference material. Achieved uncertainties are one order of magnitude higher than those obtained by MC-ICP-MS. This precision and accuracy is nonetheless sufficient to resolve natural occurring variations in Lithium isotope ratios. Also, the LiMNC material was analyzed by HR-CS-AAS with and without matrix purification. The results are comparable within statistical error.
Packages for the transport of high-level radioactive material must withstand severe hypothetical accidents. Regulatory test conditions shall cover these severe accident conditions and consist of mechanical tests and a following thermal test. To withstand the mechanical tests heavy weight packages are often designed with impact limiters consisting of wood encapsulated in steel sheets. The thermal test is defined precisely in the IAEA-regulations as a 30 minute fully engulfing 800 °C fire. After the fire phase a pre-damaged impact limiter might continue burning or smouldering and influence the cask thermal behaviour with its energy release. The energy transferred from the impact limiter to the cask is of importance for the safety of transport packages. A full-scale fire test with an impact limiter of 2.3 m in diameter and filled with spruce wood was designed and performed. The impact limiter continued burning for 3 days. Energy transfer and temperature measurements were performed.
The 5G technology promises real time data transmission for industrial processes, autonomous driving, virtual and augmented reality, E-health applications and many more. The Low Temperature Co-fired Ceramics (LTCC) technology is well suited for the manufacturing of microelectronic components for such applications. Still, improvement of the technology such as further miniaturization is required. This study focuses on the characterization of inner metallization of LTCC multilayer modules, especially on the vertical interconnect access (VIA). Critical considerations for this characterization are delamination, pore clustering in and at the edge of the VIA, deformation, and stacking offset. A LTCC multilayer consisting of a glassy crystalline matrix with silver based VIAs was investigated by synchrotron x-ray tomography (CT). The aim of this study is to propose a multitude of structural characteristic values to maximize the information gained from the available dataset. Data analysis has been done with the open source software ImageJ as well as several additional plugins. The high-resolution CT data was evaluated through 2D slices for accessibility reasons. The segmentation of all 2000 slices to assess the different regions e.g. pores, silver and glass ceramic was done by a supervised machine learning algorithm. A quantitative evaluation of shape, deformation, and porosity of the VIA with respect to its dimensions is presented and the suitability of the characterization approach is assessed.
Biofilm formation in industrial or medical settings is usually unwanted and leads to serious health problems and high costs. Inhibition of initial bacterial adhesion prevents biofilm formation and is, therefore, a major mechanism of antimicrobial action of surfaces. Surface topography largely influences the interaction between bacteria and surfaces which makes topography an ideal base for antifouling strategies and eco-friendly alternatives to chemical surface modifications. Femtosecond laser-processing was used to fabricate sub-micrometric surface structures on silicon and stainless steel for the development of antifouling topographies on technical materials.
Der weit verbreitete austenitische Stahl 316L soll auch mittels additiver Fertigung verarbeitet werden (316L-AM). Zur Entwicklung optimaler Aufbauverfahren ist ein detailliertes Verständnis des Gefüges notwendig. Das additiv aufgebaute Gefüge zeigt eine Mikrostruktur, die geprägt ist von sehr hohen Abkühlraten und gerichtetem Kornwachstum. Mittels klassischer Metallographie können die Charakteristika des Gefüges wie Körner, Subkörner und Schmelzlinien sichtbar gemacht werden. Mittels EBSD werden Kristallorientierungen ermittelt und bildhaft aufbereitet. Die Feinstruktur der Körner wird im REM in der Übersicht aufgelöst. Erst im TEM kann bei hoher Vergrößerung die Natur der Zellstruktur quantitativ ermittelt werden.
A heat treated glass that formed crystals under controlled conditions can be a glass ceramic. A proper understanding of crystallization in glassy melts is needed yet still lacking. Involved processes include the mobility of Elements within the glass during heat treatment and the reorganization of atomic bonds during crystallization. This change in coordination number of certain elements is easily observable in bulk glass samples during heat treatment with XAS. Our plan was to monitor these reorganization processes in situ at the immediate surface during heat treatment with PEEM to get time and spatial resolved data.
Eine umfangreich ausgestaltete Trinkwasseraufbereitung als Multibarrieren-System ist notwendig, wenn das Rohwasser direkt aus Fließgewässern entnommen wird (z. B. für das Mülheimer Verfahren). Eine der Barrieren wird, als gezielte Behandlungs- oder Sicherheitsstufe, oft als Filter mit granulierter Aktivkohle (GAK-Filter) realisiert. Ihre Standzeit kann bei geringer Wasserbelastung (DOC < 2 mg/L), z. B. bei der Landeswasserversorgung Langenau, bis zu 5 Jahre betragen. Bei Rohwasser mit höherem Organikgehalt (DOC > 7 mg/L), wie bei der Nordwasser in Rostock, wird hingegen mindestens alle drei Jahre die GAK in den Filterkolonnen ausgetauscht.
Die Rest-Adsorptionskapazität der GAK kann durch verschiedene Verfahren abgeschätzt werden, ist aber nach wie vor Gegenstand aktueller Forschung. Die weitergehende Charakterisierung der beladenen GAK kann hierbei helfen.
Auf dem Poster sollen erste Ergebnisse zu den in Langenau und Rostock eingesetzten Aktivkohlen präsentiert werden. Hierzu wurden die frischen und nach unterschiedlichen Laufzeiten beladenen GAK untersucht. Die Zusammensetzung der Anorganik und der adsorbierten Organik, welche mittels Zersetzungs¬gasanalyse charakterisiert wurde, zeigt deutliche Unterschiede. Bspw. nimmt der Calcium-Gehalt der GAK in Langenau kontinuierlich zu, wohingegen dieser in den Proben aus Rostock mit zunehmender Laufzeit zurückgeht. Umgekehrt verhält es sich mit der Organik: Die GAK aus Rostock zeigen Hinweise auf biologische Besiedelung, während diese in Langenau trotz längerer Filterlaufzeit auszubleiben scheint.
Monitoring of Concrete with Embedded Ultrasound Sensors, Coda Waves and a Novel Measurement Device
(2020)
Using embedded ultrasound (US) sensors in civil engineering structures and Coda Wave Interferometry (CWI), DFG research group CoDA aims for developing methods of concrete damage assessment by combination of Micro and macro scale simulations and experiments. BAMs goal within the project is the provision of small and durable measurement equipment on the one hand, and the investigation of damage sensitive parameters and development of an imaging algorithm on the other hand. In this study we focus on the development of the measurement system and the influence of temperature variations on the measurements.
Ultra high performance concrete (UHPC) is known for its high compressive strength of more than 150 MPa and its high durability. Thermal treatment at 90°C can accelerate the strength development so that the 28-days-strength can be achieved immediately after the treatment and an additional increase up to 30 % in some cases. The reason for the strength development is an accelerated hydration of the clinker minerals and an intensified pozzolanic reaction leading to a denser microstructure.
In previous research inhomogeneities in form of a zonation after unprotected thermal treatment were observed and analysed in respect to changes in the microstructure. This zonation is defined by a different microstructure in the core compared to the outer zone in the matter of porosity, mineral phase composition and a significant change in the potassium and sulphur concentration of the zones is measurable.
To isolate different transport mechanisms responsible for these element distributions UHPC samples were thermally treated at 90 °C and the microstructure was investigated under dry conditions and after immersion in water to investigate the influence of dehydration during and rehydration after the thermal treatment on the microstructure. Through durability testing via water absorption, water vapour diffusion, permeability testing and sulfuric acid resistance transport mechanisms like diffusion, migration, capillary suction are under investigation in correlation with the microstructure analysis. For the microstructure analysis measurements with µXRF, mercury intrusion porosity, XRD and SEM were conducted.
Die Porosität sowie die Porengrößenverteilung (PSD) eines Baustoffs sind wichtige petrophysikalische Eigenschaften, die Transportprozesse im Material beeinflussen und im direkten Zusammenhang mit der Schadensanfälligkeit stehen (Frost-Tau-Schäden, Schäden durch Salzeinträge und sauren Regen). Verfahren zur Ermittlung der Porosität stellen die Quecksilberporosimetrie (MIP), das Prinzip der Tauchwägung nach Archimedes (triple weighing method, TWM) und die Nuklear Magnetische Resonanz (NMR) dar.
Das Hauptziel dieser Arbeit ist der Vergleich der drei Methoden für die Porositätsbestimmung. Als Untersuchungsmaterial wurde Sandstein gewählt. Als Baustoff wird Sandstein trotz einer teilweise geringen Festigkeit, aber aufgrund seiner Farbvielfalt häufig für Kulturbauten, Gehwegmaterial und Fassaden eingesetzt. Sandsteine weisen zudem meist eine hohe effektive Porosität (bis zu ca. 30 %) und teilweise breite Porengrößenspektren auf, wodurch Feuchte- und Ioneneinträge begünstigt werden und zu z. B. langfristigen Verfärbungen an Sandsteinfassaden führen können.
Im Rahmen dieser Arbeit werden die Porositäten von 10 verschiedenen Sandsteinen aus Deutschland und Tschechien bestimmt. Für die Untersuchungen mittels TWM und NMR wurden für jede Sandsteinart zwei zylinderförmige Proben unter Unterdruck mit Leitungswasser aufgesättigt. Beim Vergleich der Verfahren liegt der Fokus insbesondere auf NMR und der verwendeten Gerätetechnik, die mit einer minimalen Echozeit von 50 µs ein Wasserstoffsignal in Sandsteinen aus bis zu ca. 2 nm kleine Poren erfassen kann. Darüber hinaus wird das Auflösungsvermögen von MIP und NMR bezüglich der Poren- bzw. Poreneingangsgrößen diskutiert. Für den Vergleich von NMR und MIP werden an ausgewählten Sandsteinproben ebenfalls die zusätzlich ermittelten PSD in Korrelation zueinander gebracht.
Erste Ergebnisse zeigen eine gute Korrelation von NMR- und TWM-Daten, aber teilweise starke Abweichungen zu den mit MIP bestimmten Porositäten. Ergebnisse zu den PSD zeigen teilweise nahezu identische Kurvenverläufe. Jedoch ist die Abschätzung des Umrechnungsfaktors für die NMR-Daten ohne Hinzuziehen von zusätzlichen Referenzverfahren wie Röntgen-Computer-Tomographie oder Spektral Induzierte Polarisation teilweise sehr schwierig.
THz and mid IR spectroscopy of high-molecular PE (HMW) and ultra high-molecular PE (UHMW) reveals modifications of the molecular structure. Characteristic absorption bands are changed if the two materials are exposed by γ-Co60 radiation up to 600 kGy and subsequently stored at an annealing temperature of 398 K until for 729 days. UHMW-PE and HMW-PE behave differently during the ageing process because of their molecular weight and inherent structure distinctions. The spectroscopic data offer characteristic absorption bands, which have been used to describe the complete ageing process in more detail. For instance, the integral absorption in the B1u THz-region can be used to describe quantitatively the reduction of crystallinity. The formation of trans vinylene unsaturation and the decay of vinyl during ageing can be observed in detail in the mid IR range.
This poster presents the focused ion beam preparation methodologies developed within the framework of the EU funded EURAMET project ADVENT (Advanced Energy-Saving Technology).
It summarises the key breakthroughs achieved for various in situ investigation techniques, e.g. in situ experiments at the Synchrotron facility BESSY II (IR-SNOM and XRS), TEM and SMM instrumentation.
The created experimental devices from diverse thin-film semiconductor materials paved the way to dynamic structural studies bearing the potential to determine nanoscale correlations between strain and electric fields and, moreover, for the fundamental development of new in situ capabilities.