Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2017 (3) (entfernen)
Dokumenttyp
Sprache
- Englisch (3) (entfernen)
Schlagworte
- Welding (3) (entfernen)
Residual stresses and distortions in welded I-girders for steel construction are relevant when evaluating the stability of steel beams and column members. The application of high strength steels allows smaller wall thicknesses compared to conventional steels. Therefore, the risk of buckling has to be considered carefully. Due to the lack of knowledge concerning the residual stresses present after welding in high strength steel components conservative assumptions of their level and distribution is typically applied. In this study I-girders made of steels showing strengths of 355 MPa and 690 MPa were welded with varying heat input. Due to the dimension of the I-girders and the complex geometry the accessibility for residual stress measurement using X-ray diffraction was limited. Therefore, saw cutting accompanied by strain gauge measurement has been used to produce smaller sections appropriate to apply X-ray diffraction. The stress relaxation measured by strain gauges has been added to residual stresses determined by X-ray diffraction to obtain the original stress level and distribution before sectioning. The combination of both techniques can produce robust residual stress values. From practical point of view afford for strain gauge application can be limited to a number of measuring positions solely to record the global amount of stress relaxation. X-ray diffraction can be applied after sectioning to determine the residual stresses with sufficient spatial resolution.
High-strength steels with yield strengths ≥ 690 MPa are becoming increasingly significant for modern steel constructions. Both quenched and tempered (QT) high-strength steels and steels produced by the thermo-mechanically controlled process (TMCP) are currently available. TMCP-steels are usually provided with a typical mill scale. Apart from the manufacturing process these steels differ also in their chemical composition. The influence of these differences are investigated here with focus on the residual stresses formed during TIG welding. Bead on plate welds have shown characteristic residual stress distributions depending on the type of steel as well as on the heat input and preheat temperature. The following work demonstrates that the fluid flow, induced by the elements present in the mill scale, leads to a deeper penetration of the material. This can also lead to increased residual stresses in the surface of the weld and the HAZ. Furthermore, higher heat input and preheat temperature can induce higher tensile residual stresses − which are evident in the present study.
In situ EDXRD study of MAG-welding using LTT weld filler materials under structural restraint
(2017)
Welding using low transformation temperature (LTT) filler materials is an innovative approach to mitigate detrimental welding residual stresses without cost-intensive post weldtreatments. Due to the local Generation of compressive residual stresses in the weld line by means of a delayed martensite transformation a significant enhancement of the cold cracking resistance of highly stressed welded components can be expected. For the effective usage of These materials a deeper understanding of the microstructural evolution inside the weld material is necessary to determine the complex processes that cause the residual stress formation during welding. Solid-state phase transformation kinetics and the evolution of strain in LTT weld filler materials are monitored in-situ at the instrument ID15A at the ESRF in Grenoble, France. The transferability to real components is implemented by using a realistic MAG welding process under consideration of structural restraint. During welding of multilayer joints, the phase Transformation and phase specific strain evolution of each individual layer is investigated in transmission geometry by means of energy-dispersive X-ray diffraction EDXRD using high energy synchrotron Radiation with a counting rate of 2.5 Hz. The measurement results of a 10% Cr / 10% Ni LTT weld filler are compared to data monitored for the conventional weld filler material G89. The in-situ data clearly indicate a strong effect on the local strain evolution and the formation of compressive strain. This results from the restraint volume expansion during the postponed austenite to martensite transformation of the LTT weld filler, which counteracts the thermal shrinkage. In contrast, for the conventional weld filler material the thermal contraction strains lead to tensile residual strain during welding. Furthermore, the results of in-situ observation during welding Show that the transformation kinetic is dependent on the welding sequence.