Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Dokumenttyp
- Vortrag (29)
- Beitrag zu einem Tagungsband (15)
- Zeitschriftenartikel (11)
- Posterpräsentation (2)
Referierte Publikation
- nein (57) (entfernen)
Schlagworte
- Laser beam welding (57) (entfernen)
Organisationseinheit der BAM
- 9.3 Schweißtechnische Fertigungsverfahren (57) (entfernen)
Eingeladener Vortrag
- nein (29)
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase of the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verifies the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains that have been solidified and formed previously from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are ana lyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cel lular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.
Notch impact toughness of laser beam welded thick sheets of cryogenic nickel alloyed steel X8Ni9
(2020)
This research work deals with the investigations of the impact toughness of laser beam welded 14.5 mm thick sheets made of cryogenic steel X8Ni9 as a function of preheating. This 9% nickel alloyed steel is widely used in the liquefied natural gas (LNG) industry. An application of highly efficient welding processes such as high-power laser beam welding (LBW) in LNG sector requires an understanding of the interactions between the LBW process parameters and weld properties, in particular the impact toughness. The results show that the original fine-grained martensitic microstructure of the base metal (BM) is significantly changed by melting and crystallization during the LBW, what can lead to a decrease in the impact toughness of the weld metal (WM) below the required level. An optimal preheating temperature range leads to the favorable thermal welding cycle and is of remarkable importance for maintaining the notch impact toughness of laser beam welded joints of these thick steel sheets. A parameter window was identified in which V-notch impact toughness comparable to that of the BM at -196 °C was achieved.
The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high-speed camera, and two thermal imaging cameras is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs above 10 mm penetration depth. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root.
The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high speed camera, and two thermal imaging cameras is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs above 10 mm penetration depth. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding parameters on the formation of end crater defects such as pores, cracks, excessive root-side drop-through and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Strategies with a reduction of the welding speed shows a creation of inadmissible root sagging. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques. A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of 10 mm and then transferred on the 9.5 mm thick pipe sections made of high-strength steel X100Q.
Die Wärmeverteilung des Lasers beim Laserstrahltiefschweißen ist für die Formgebung der Dampfkapillare und für die Schweißbaddynamik entscheidend. In dieser Arbeit werden die Laserwärmeverteilung und deren Einflüsse auf die Schweißbadtiefe sowie -breite numerisch anhand des Ray-Tracing-Verfahrens analysiert. Hierbei wird der La-serstrahl in mehreren Strahlenbündeln bzw. Subrays unterteilt. Diesbezüglich soll der Pfad der Subrays präzis be-rechnet werden, um die Dynamik der Dampfkapillare und des Schweißbades eines realen Schweißprozesses rich-tig abzubilden. Zu diesem Zweck beschäftigt sich die vorliegende Arbeit mit der Genauigkeitsverbesserung der Kontaktposition und der Reflexionsrichtung der Subrays auf der freien Oberfläche anhand der Level-Set-Methode. Um die Güte dieses Simulationsansatzes zu gewährleisten, wurde eine Gegenüberstellung mit den zwei klassischen Ray-Tracing-Verfahren mittels drei verschiedenen Benchmark-Testreihen durchgeführt. Anschließend wurden die Versuchsergebnisse zur Validierung der implementierten numerischen Ansätze verwendet. Im Rahmen dieser Arbeit kann es gezeigt werden, dass unterschiedliche Wärmeverteilung aufgrund der verschiedenen Ray-Tracing-Verfahren deutlich zu erkennen ist, welche wiederum die Schweißbaddynamik sowie die lokalisierte Dampfkapil-lardynamik stark beeinflussen. Ferner wurde es bestätigt, dass die implementierte Level-Set-Methode zu einer ge-naueren Ermittlung der Kontaktposition und der Reflexionsrichtung der Subrays und somit zu einer Verbesserung der simulierten Schmelzkontur führt.
Der Absorptionsgrad metallischer Werkstoffe spielt bei Fügeprozessen mit einer Strahlungsquelle wie dem Hochleistungslaserstrahltiefschweißen eine bedeutende Rolle. Dieser beeinflusst die Menge der absorbierten Laserenergie, welche zum Aufschmelzen sowie zur lokalen Verdampfung des zu verbindenden Materials führt. Eine der wichtigsten Eigenschaften der Laserstrahlabsorption ist die Temperaturabhängigkeit. Dennoch wird sie in vielen Simulationsarbeiten häufig ignoriert und stattdessen ein angepasster Parameter zur Kalibrierung der Ergebnisse implementiert. Diese Vorgehensweise wirkt sich negativ auf die Zuverlässigkeit sowie die Genauigkeit des numerischen Modells sowie auf die Vorhersagbarkeit der Simulationsergebnisse aus. In der vorliegenden Arbeit wird die Temperaturabhängigkeit der Laserabsorption in ein selbstkonsistentes zweiphasiges Modell unter Berücksichtigung der gekoppelten 3D-Fluidströmung und Wärmeübertragung einbezogen. Die berechnete Laserstrahlabsorption wird durch die temperaturabhängigen Materialeigenschaften, die Lasercharakteristik und den Einfallswinkel des Laserstrahls bestimmt. Die freie Oberfläche jeder Phase wird mithilfe der volume-of-fluid Methode, kurz VOF, berechnet und die Laser-Material-Wechselwirkung wird durch ein neulich implementiertes Ray-Tracing-Verfahren modelliert, die auf einem lokalisierten Level-Set-Algorithmus basiert. Anschließend wird die transiente Wärmeeinbringung und die Geometrie der Schweißnaht analysiert und mit dem temperaturunabhängigen Absorptionsmodell verglichen. Es wurde festgestellt, dass die Temperaturabhängigkeit der Laserabsorption entscheidend für die genaue Bestimmung der Wärmeeinbringung und der Schmelzbadgeometrie ist. Das entwickelte Modell wurde anhand der experimentellen Untersuchungen validiert und die Bedeutung der Temperaturabhängigkeit bei der Laserstrahlabsorption wurde für die Simulation des Laserstrahltiefschweißens aufgeklärt.