Adhesion and corrosive delamination of epoxy films on chemically etched ZnMgAl-alloy coatings
(2016)
The effect of alkaline and acidic pretreatment steps on the surface chemical
composition and adhesion properties of ZnMgAl-alloy coated steel was
investigated by means of spectroscopic methods, scanning Kelvin probe (SKP)
and peel test measurements.The spectroscopic results indicate that the surface
film composition can be adjusted by the wet-chemical treatment. To study the
corresponding surface adhesive properties, the samples were coated with an
epoxy amine adhesive. Peel tests under humid conditions indicated an
increased interaction between the acidic pre-treated surface and the adhesive.
The results of the SKP analysis show that the acidic cleaned substrates have the
highest resistance to delamination, which can be explained by the shift of the
interfacial electrode potential.
Catalysts based on nickel oxide are some of the most active catalysts for the oxygen evolution reaction (OER) in alkaline media. However, preparing catalytic coatings with high surface area and good accessibility of the active sites remains challenging.
We present a new approach for the synthesis of homogeneous and binder-free nickel oxide coatings comprising a highly accessible ordered mesopore structure. The synthesis is achieved via evaporation induced self assembly utilizing PEOPB-PEO triblock copolymers as pore template and a chemical complex of Ni2+ and citric acid as precursor. Excessive crystallization behaviour of NiO is avoided by thermal conversion of the precursor into an amorphous Ni carbonate intermediate, followed by transition of the carbonate into the metal oxide.
We present a comprehensive analysis of the obtained materials in terms of morphology, crystallinity, surface area, composition, and OER activity of differently calcined catalysts. Retaining a low crystallinity and high surface area during the Synthesis proofs to be the most important factor in obtaining a highly active OER catalyst.