Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (169)
- Beitrag zu einem Tagungsband (108)
- Vortrag (41)
- Forschungsbericht (6)
- Buchkapitel (1)
- Tagungsband (Herausgeberschaft für den kompletten Band) (1)
- Posterpräsentation (1)
- Forschungsdatensatz (1)
Sprache
- Englisch (237)
- Deutsch (83)
- Russisch (6)
- Italienisch (1)
- Mehrsprachig (1)
Schlagworte
- Laser beam welding (69)
- Additive manufacturing (19)
- Solidification cracking (19)
- Laser metal deposition (18)
- Mechanical properties (13)
- Microstructure (13)
- Numerical simulation (13)
- Additive Manufacturing (11)
- Laser welding (11)
- Laserstrahlschweißen (11)
Organisationseinheit der BAM
- 9 Komponentensicherheit (241)
- 9.3 Schweißtechnische Fertigungsverfahren (237)
- 7 Bauwerkssicherheit (6)
- 7.2 Ingenieurbau (4)
- 9.6 Additive Fertigung metallischer Komponenten (3)
- 5 Werkstofftechnik (2)
- 5.2 Metallische Hochtemperaturwerkstoffe (2)
- 7.7 Modellierung und Simulation (2)
- 1 Analytische Chemie; Referenzmaterialien (1)
- 1.9 Chemische und optische Sensorik (1)
Eingeladener Vortrag
- nein (41)
Die Anwendung von Leichtbauprinzipien im Stahlbau, wie z.B. die Verwendung von aufgelösten Tragstrukturen, sog. Jackets-Fundamenten, bietet ein großes Potential zur Reduzierung des Ressourcenverbrauchs, insbesondere im Hinblick auf die benötigte Stahlmenge.
In diesem Vortrag zeigen wir die Potenziale einer vollständigen Digitalisierung der schweißtechnischen Fertigungs- und Prüfkette auf, um eine vollautomatische Fertigung sowie Qualitätsprüfung von Rohrknoten als Schlüsselelement von Jackets-Fundamenten zu ermöglichen. Darüber hinaus wird der Zusammenhang zwischen der Geometrie der Nahtform und der resultierenden Ermüdungsfestigkeit durch numerische Methoden unter Einbeziehung bionischer Prinzipien bewertet. Es wird gezeigt, dass Hohlprofilknoten vollautomatisch unter Berücksichtigung von Geometrietoleranzen geschweißt werden können. Darüber hinaus konnte die Nahtform gemäß den numerischen Modellen hergestellt werden, was ein großes Potenzial für eine verlängerte Lebensdauer bietet. Anschließend werden die Verbesserungen bei der Ressourceneffizienz und die Reduzierung der Kohlendioxidemissionen durch eine Lebenszyklusanalyse bewertet.
Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support
(2019)
Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support
(2019)
Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone.
Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness.Abetter combination of These mechanical properties is ensured by applying a post weld heat treatment.
Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone.
Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness. A better combination of These mechanical properties is ensured by applying a post weld heat treatment.
In this paper, the friction stir welding process was numerically investigated for 6 mm thick aluminum alloy AA2024-T3. The finite element software COMSOL Multiphysics was used to calculate the transient thermal field during welding and the mechanical reaction depending on different mechanical clamping conditions and hardening models subsequently. A thermal pseudo-mechanical (TPM) heat source was implemented.
Softening effects of the material due to precipitation hardening dissolution caused by the frictional heat were accounted for. The transient temperature evolution measured by thermocouple elements at various locations was compared to the numerical results. A good agreement was found for the thermal field. A sensitivity study of the mechanical models showed the strong influence of the clamping conditions and the softening model.
Der Trend zum Leichtbau und die Transformation zur E-Mobilität in der
Automobilindustrie befeuern die Entwicklung neuer hochfester Stähle für den Karosseriebau. Derartige Werkstoffe sind beim Widerstandspunktschweißen besonders rissanfällig (LME). Das Schweißen unter Zug stellt eine effektive Methode um die LME-Anfälligkeit unterschiedlicher Werkstoffe qualitativ zu bestimmen.
Die Anwendung der additiven Fertigung nimmt stark zu. Eine neue Designfreiheit erlaubt es hier den Konstrukteurinnen und Konstrukteuren, die Bauteilfunktion in den Vordergrund der Entwicklungen zu stellen. Leichtbaustrukturen sowie Funktionsintegration machen es möglich, vormals Bauteile aus vielen Einzelkomponenten jetzt in einem einzigen Bauteil zu vereinigen. Experten am Fraunhofer IPK qualifizieren das Laser-Pulver-Auftragschweißen für die additive Fertigung und legen dabei besonderen Wert auf die Automatisierung des Verfahrens.
Manganese alloyed stainless steels represent a cost-effective alternative to conventional CrNi- stainless steels due to strong fl uctuations of the market prices for nickel seen during the last years. In CrMnNi steels, nickel is partially replaced by lower-cost manganese and small amounts of nitrogen for stabilization of the austenitic phase. This also brings benefi ts regarding the mechanical properties, as it results in an increased material strength. Laser beam welding of such materials was investigated for direct comparison with Standard CrNi steels. Main emphasis was laid on fi nding adequate process parameters to achieve a stable welding process and obtain a good weld quality. Two different laser sources, a 4.4 kW Nd:YAG and a 5 kW CO2 laser, were used to weld 1.5 mm stainless steel sheets in continuous wave mode. A high-Mn austenitic (1.4376) and a lean duplex (1.4162) steel, as well as the standard austenitic (1.4301) and duplex (1.4362) grades were selected as test materials. Both butt and lap joint confi gurations were studied. Experiments were carried out systematically, varying the welding speed, laser power and focal point position in order to determine adequate process windows. The infl uence of the shielding gas type and fl ow rate on the process stability and the weld quality were investigated. The effects of weld edge preparation on the weld appearance and quality levels attained were also examined. The obtained welded joints were subjected to radiographic tests for detection of internal imperfections. Also a metallurgical characterization of the samples regarding the resulting phase composition or balance and hardness depending on the welding process parameters was conducted. Furthermore, tensile and potentiodynamic tests were performed to evaluate the mechanical and corrosion properties, respectively. The results provide an insight into the advantages and limitations of the laser beam welding process for joining high-manganese alloyed stainless steels. Conditions for the production of defect-free and corrosion-resistant welds having good mechanical properties could be determined.
The application of magnesium (Mg) inevitably involves dissimilar welding with steel. A novel solid state spot welding method, refill friction stir spot welding (refill FSSW), was utilized to weld AZ31 Mg alloy to galvanized DP600 steel. Although Mg/Fe is an immiscible alloy system, defect-free welds with high strength were successfully obtained in a wide parameter window. The results of microstructure, interfacial reactions, and mechanical properties are reported to reveal the underlying joining mechanism. Due to the melting of Zn coating and subsequent Mg-Zn reactions, Mg-Zn eutectic and intermetallic compounds were detected within welds. Heterogeneous interfacial reactions occur along Mg/steel interface, and the relationship between interfacial structure and fracture behavior was investigated. The joining mechanism is associated with Zn coating and Fe-Al layer: 1) the presence of Zn coating is beneficial for achieving high-quality welding between Mg and steel, it protects the interface from oxidation and contributes to brazing of the weld; 2) the Al present in Mg alloy reacts with Fe, resulting in the growth of Fe-Al layer, which contributes to the diffusion bonding in the interface. The overall results clearly show that Refill FSSW is a competitive welding method for joining Mg and galvanized steel.