- nein (4)
Relation of craze to crack length during slow crack growth phenomena in high‐density polyethylene
(2024)
The craze‐crack mechanism occurring in high‐density polyethylene (HDPE) causing slow crack growth and environmental stress cracking is investigated in detail with respect to the relation of crack length and the related craze zone. This is essential for the understanding of the resulting features of the formed fracture surface and their interpretation in the context of the transition from crack propagation to ductile shear deformation. It turns out that an already formed craze zone does not inevitably result in formation of a propagating crack, but could also undergo ductile failure. For the examination, the full notch creep test (FNCT) was employed with a subsequent advanced fracture surface analysis that was performed using various imaging techniques: light microscopy, laser scanning microscopy, scanning electron microscopy, and X‐ray micro computed tomography scan. FNCT specimens were progressively damaged for increasing durations under standard test conditions applying Arkopal, the standard surfactant solution, and biodiesel as test media were used to analyze the stepwise growth of cracks and crazes. From considerations based on well‐established fracture mechanics approaches, a theoretical correlation between the length of the actual crack and the length of the preceding craze zone was established that could be evidenced and affirmed by FNCT fracture surface analysis. Moreover, the yield strength of a HDPE material exposed to a certain medium as detected by a classic tensile test was found to be the crucial value of true stress to induce the transition from crack propagation due to the craze‐crack mechanism to shear deformation during FNCT measurements.
Highlights
- Progress of crack formation in high‐density polyethylene is analyzed by different imaging techniques
- Determined growth rates depend on distinction between craze zone and crack
- The ratio of the present crack to the anteceding craze zone is validated theoretically
- The transition from crack propagation to ductile shear deformation is identified
- An already formed craze zone may still fail by ductile mechanisms
Two-dimensional covalent organic frameworks (COFs) based on phosphinine and thiophene building blocks have been synthesized with two different side groups. The materials are denoted as CPSF-MeO and CPSF-EtO where CxxF correspond to the covalent framework, whereas P and S are related to heteroatoms phosphorous and sulfur. MeO and EtO indicate the substituents, i.e. methoxy and ethoxy.
Their morphologies were studied by scanning electron microcopy and X-ray scattering. The absence of crystalline reflexes in the X-ray pattern reveal that both materials are amorphous and can be considered as glasses. Furthermore, N2 adsorption measurements indicate substantial Brunauer–Emmett–Teller (BET) surface area values pointing to the formation of three-dimensional pores by stacking of the aromatic 2D layer. An analysis of the porosity of both COFs showed a mean radius of the pores to be of ca. 4 nm, consistent with their chemical structure. The COFs form nanoparticles with a radius of around 100 nm. The thermal behavior of the COFs was further investigated by fast scanning calorimetry. These investigations showed that both COFs undergo a glass transition. The glass transition temperature of CPSF-EtO is found to be ca. 100 K higher than that for CPSF-MeO. This large difference in the glass transition is discussed to be due to a change in the interaction of the COF sheets induced by the longer ethoxy group. It might be assumed that for CPSF-EtO more individual COF sheets assemble to larger stacks than for CPSF-MeO. This agrees with the much larger surface area value found for CPSF-EtO compared to CPSF-MeO. To corroborate the results obtained be fast scanning calorimetry dielectric measurements were conducted which confirm the occurrence of a dynamic glass transition. The estimated temperature dependence of the relaxation rates of the dielectric relaxation and their absolute values agrees well with the data obtained by fast scanning calorimetry. Considering the fragility approach to the glass transition, it was further found that CPSF-MeO is a fragile glass former whereas CPSF-EtO behaves as a strong glass forming material. This difference in the fragility points also to distinct differences in the interaction between the 2D COF molecules in both materials.
Polymers with intrinsic microporosity (PIMs) are gaining attention as gas separation membranes. Nevertheless, they face limitations due to pronounced physical aging. In this study a covalent organic framework containing λ5-phosphinine moieties, CPSF-EtO were incorporated as a nanofiller (concentration range 0-10 wt%) into a PIM-1 matrix forming dense films with a thickness of ca. 100 μm. The aim of the investigation was to investigate possible enhancements of gas transport properties and mitigating effects on physical aging. The incorporation of the nanofiller occurred on aggregate level with domains up to 100 nm as observed by T-SEM and confirmed by X-ray scattering. Moreover, the X-ray data show that the structure of the microporous network of the PIM-1 matrix is changed by the nanofiller.
As the molecular mobility is fundamental for gas transport as well as for physical aging, the study includes dielectric investigations of pure PIM-1 and PIM-1/CPSF-EtO mixed matrix membranes to establish a correlation between the molecular mobility and the gas transport properties. Using the time-lag method the gas permeability and the permselectivity were determined for N2, O2, CH4 and CO2 for samples with variation in filler content. A significant increase in the permeability of CH4 and CO2 (50 % increase compared to pure PIM-1) was observed for a concentration of 5 wt% of the nanofiller. Furthermore, the most pronounced change in the permselectivity was found for the gas pair CO2/N2 at a filler concentration of 7 wt%.
Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. These polymers are characterized by a high permeability and reasonable permselectivity. The latter point is somehow surprising because for microporous systems a more Knudson-like diffusion is expected then a size dependent temperature activated sieving process. It was argued in the framework of a random gate model that molecular fluctuations on a time scale from ps to ns are responsible for the permselectivity.
Here series of polymers of intrinsic microporosity (PIMs) as well as microporous polynorbornenes with bulky Si side groups and a rigid backbone are considered. The polymers have different microporosity characterized by high BET surface area values.
First inelastic time-of-flight neutron scattering measurements were carried out to investigate the low frequency density of state (VDOS). The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. It was found that the frequency of the maximum position of the Boson peak correlates with the BET surface area value.
Secondly elastic scans as well as quasielastic neutron scattering measurements by a combination of neutron time-of-flight and backscattering have been out. A low temperature relaxation process was found for both polymers. This process was assigned to the methyl group rotation. It was analysed in terms of a jump diffusion in a three-fold potential. The analysis of the dependence of the elastic incoherent structure factor on the scattering vector yields the number of methyl groups which might be immobilized.
The neutron scattering experiments were accompanied by fast scanning calorimetry and broadband dielectric investigations as well as atomistic molecular dynamic simulations.
The dataset provided in this repository comprises data obtained from a series of full-notch creep tests (FNCT) performed on selected high-density polyethylene (PE-HD) materials (for further details, see section 1 Materials in this document) in accordance with the corresponding standard ISO 16770.
The FNCT is one of the mechanical testing procedures used to characterize polymer materials with respect to their environmental stress cracking (ESC) behavior. It is widely applied for PE-HD materials, that are predominantly used for pipe and container applications. It is based on the determination of the time to failure for a test specimen under constant mechanical load in a well-defined and temperature controlled liquid environment. The test device used here also allows for continuous monitoring of applied force, specimen elongation and temperature.
Inelastic incoherent neutron time-of-flight scattering was employed to investigate the low-frequency vibrational density of states (VDOSs) for a series of glassy Janus-poly(tricyclononenes), which consist of a rigid main chain and flexible alkyl side chains. Here, the length of the flexible side chains was systematically varied from propyl to octyl. Such materials have potential applications as active separation layers in gas separation membranes as a green future technology, especially for the separation of higher hydrocarbons. From the morphological point of view, the Janus polynorbornenes undergo a nanophase separation into alkyl side chain-rich nanodomains surrounded by a rigid polynorbornene matrix. Here, the influence of the nanophase-separated structure on the low-frequency VDOS is investigated from a fundamental point of view. The low-frequency VDOSs of these Janus polynorbornene show excess contributions to the Debye type VDOS known as the Boson peak (BP) for all side chain lengths. Due to the high incoherent scattering cross-section of hydrogen, most of the scattering comes from the alkyl side chain-rich domains.
Compared to conventional glass-forming materials, in the considered Janus polynorbornenes, the BP has a much lower intensity and its frequency position is shifted to higher values. These experimental results are discussed in terms of the nanophase-separated structure where the alkyl chain-rich domains were constrained by the surrounding matrix dominated by the rigid backbone. With increasing alkyl chain length, the size of the alkyl chain-rich domains increases. The frequency position of the BP shifts linearly to lower frequencies with the size of these nanodomains estimated from X-ray measurements. The obtained results support the sound wave interpretation to the BP
Slow crack growth (SCG) under the influence of external fluid media, usually termed environmental stress cracking (ESC), is still one of the most frequent origins of severe damage and failure of polymeric materials. For polyethylene (PE) this is relevant for mass products, like bottles for consumer products, but also for high-performance materials for pipes or industrial packaging, including containers for chemicals and other dangerous goods. Especially for high-density polyethylene (PE-HD) the susceptibility to SGC and ESC is depending on the complex interplay between molecular weight and architecture and the resulting semicrystalline morphology, especially the formation of tie-molecules.
A reliable assessment of the resistance against this damage phenomenon is essential for demanding as well as safety-critical applications and has to take into account suitable testing methodologies and conditions in combination with environmental media reflecting the properties representative for typical fillings and relevant components causing ESC. In this context a better understanding of different influencing factors, such as sorption, swelling or surface activity is necessary together with a detailed characterization of different stages of crack propagation and underlying mechanisms. Therefor well-established testing methods, such as the Full Notch Creep Test (FNCT), were complemented by detailed fracture surface analysis using e.g. LSM and SEM in combination with a time-dependent optical monitoring of the progressing crack growth.
For the crack growth also the ratio of fibrillated craze zone to crack opening is important for the deeper understanding of crack propagation and related material parameters which can be additionally addressed by X-ray computed tomography.
The addition of nanoparticles as reinforcing fillers in elastomers yields nanocomposites with unique property profiles, which opens the door for various new application fields. Major factors influencing the performance of nanocomposites are studied by varying the type and shape of nanoparticles and their dispersion in the natural rubber matrix. The industrial applicability of these nanocomposites is put into focus using two types of graphene and a nanoscale carbon black, all commercially available, and scalable processing techniques in the form of a highly filled masterbatch production via latex premixing by simple stirring or ultrasonically assisted dispersing with surfactant followed by conventional two-roll milling and hot pressing. Different processing and measurement methods reveal the potential for possible improvements: rheology, curing behavior, static and dynamic mechanical properties, swelling, and fire behavior. The aspect ratio of the nanoparticles and their interaction with the surrounding matrix prove to be crucial for the development of superior nanocomposites. An enhanced dispersing method enables the utilization of the improvement potential at low filler loadings (3 parts per hundred of rubber [phr]) and yields multifunctional rubber nanocomposites: two-dimensional layered particles (graphene) result in anisotropic material behavior with strong reinforcement in the in-plane direction (157% increase in the Young's modulus). The peak heat release rate in the cone calorimeter is reduced by 55% by incorporating 3 phr of few-layer graphene via an optimized dispersing process.
Packaging containers for dangerous goods that include aggressive liquids require that any packaging material that is based on high-density polyethylene has a high degree of stability and durability. This work is focused on testing the environmental stress cracking of the high-density polyethylenes used for such containers in contact with crop protection formulations, in particular, two model liquids established in Germany as standardized test media representatives for crop protection formulations containing the various admixtures typical for such products. One of the liquids is water-based and contains mostly surface-active ingredients, while the other is solvent-based and includes some emulsifiers. Originally established for pin impression tests, these model liquids and their individual components were here used for the first time as environmental media in the Full Notch Creep Test, which addresses the resistance against environmental stress cracking. The Full Notch Creep Test was carried out on five high-density polyethylene types with both model liquids, and also on one selected material with its components. The evaluation was focused on the fracture surface structures, which were visualized by a scanning electron microscope and by optical in situ imaging of the notch opening. While the water-based model liquid and its surface-active individual components induced environmental stress cracking with the characteristic pattern for a craze-crack mechanism and so-called brittle fracture on the surface, the solvent-based model liquid and its soluble ingredients exhibited rather ductile failure behavior, caused by the plasticizing effect on the polymer that reduced the yield stress of the high-density polyethylene.
For both cases, fracture surface analysis, together with side views of the crack opening, showed a clear relation between surface pattern, notch deformation (e.g., by blunting), or crack opening due to crack growth with time to failure and the solubility of the liquids in high-density polyethylene.
In the processing of nanocomposites, high shear stresses at elevated tempera-tures orient two-dimensional nanoparticles like graphene. This orientationleads to anisotropic mechanical, thermal or barrier properties of the nanocom-posite. This anisotropy is addressed in this study by comparing graphene (few-layer graphene, FLG) with a nanoscaled carbon black (nCB) at a filler contentof 3 phr, by varying the vulcanization, and by comparing different FLG con-tents. Transmission electron microscopy gives insight into the qualitative ori-entation in the nanocomposite with FLG or nCB. The storage moduli paralleland normal to the orientation reveal the direction dependency of reinforce-ment through dynamic mechanical analysis (DMA). Dimensional swellingmeasurements show a restriction of the expansion parallel to the FLG orienta-tion, and an increased expansion normal to the orientation. The vulcanizationsystem and crosslinking determine the respective level of property values, andhigher crosslinking densities increase the anisotropy in DMA resulting invalues of up to 2.9 for the quantified anisotropy factor. With increasing FLGcontent, the anisotropy increases. A comparison of the results reveals swellingmeasurements as the most suitable method for the determination of anisot-ropy. Compared to recent literature, the presented processing induces higheranisotropy, leading to higher reinforcing effects in the direction of orientation