Wire arc additive manufacturing enables the production of near-net shape large-volume metallic components leveraging an established industrial base of welding and cladding technology and adapting it for layer-wise material deposition. However, the complex relationship between the process parameters and resulting mechanical properties of the components still remains challenging. In case of high-strength Al-Mg-Si aluminum alloys, no commercial filler wires are yet available due the high susceptibility of solidification cracking as well as the necessary efforts to obtain acceptable mechanical properties. To address this need, we evaluated a novel filler wire based on AlMg0.7Si doped with a Ti5B1 master alloy to foster fine equiaxed grains within the deposited metal. The correlation between the process parameters and component quality was examined by analyzing the size and distribution of pores as well as the grain morphology. Furthermore, we evaluated the influence of different post-weld heat treatment strategies to achieve mechanical properties corresponding to the reference wrought material. We demonstrated that fine equiaxed grains in the weld metal reduced the susceptibility of solidification cracking significantly. The novel AlMg0.7Si-TiB (S Al 6063-TiB) filler wire facilitated wire arc additive manufacturing of high-strength aluminum components with mechanical properties that were almost as superior as the corresponding wrought base material.
The study deals with the influence of the heat input on the thermal cycles and Charpy impact toughness for hybrid laser-arc welding of 25 mm thick structural steel S355J2 using a 20-kW high-power laser in combination with an electromagnetic weld pool support. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured using a pyrometer in combination with an optical fibre in three different locations near to fusion lines corresponding to different heights of the seam. Also, Charpy impact specimens were taken from different parts of the weld joint corresponding to the different heights. The influence of the heat input was investigated for 1.8 kJ mm-1 and 3.2 kJ mm-1. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required values could be reached in dependance on applied heat input.
The application of the electromagnetic stirring from an oscillating magnetic field can improve the metal mixing in wire feed laser beam welding. However, the extra parameters introduced in this technique make the selection of an optimal combination of process parameters more difficult. In the current study, besides the commonly concerned magnetic flux density and frequency, the influence of the magnetic field orientation (magnetic field angle) on the transport of filler metal is studied numerically and experimentally. Ex-situ X-ray fluorescence spectrometer measurements are used to map the metal mixing in the final weld. A three-dimensional transient multi-physical model is developed to reveal the deeper physical essence, considering the coupling between heat transfer, fluid flow, keyhole dynamics, element transport and magnetohydrodynamics. The spatial distribution of the laser energy on the keyhole wall is calculated by a ray tracing algorithm. The results show that the magnetic field with smaller angle with respect to the transverse direction provides better penetration capacity, and its stirring effect can reach the lower part of the molten pool. Therefore, the smaller magnetic field angle produces better metal mixing. A constant downward flow is formed at the lower part of the molten pool when magnetic field of 10° angle is applied, which brings the filler metal to the root region. As the magnetic field angle increases to 40°, the beneficial downward flow changes into a constant upward flow, resulting in a concentration of the filler metal in the upper region. This study provides further insight of the underlying physics in the electromagnetically enhanced laser beam welding, which may guide the optimization of parameters to achieve property homogeneity or to avoid potential defects.
The present contribution is the first research reporting full penetration HLAW joints in 15 mm thick EH36 steel butt T-welds with square grooves on 2F welding position by single-sided welding. The effects of welding parameters were investigated to increase the quality of the joints.
Conditions leading to defect-free full penetration welds fulfilling naval regulations includes a laser power of 12.5 kW, a welding speed of 1.6 m/min and the vertical laser offset distance from the flange of 1 mm. Advanced characterization of selected welds included a microstructural identification by optical microscopy, SEM, and XRD, revealing the presence of acicular, polygonal and Widmanstätten ferrite, lath martensite, and some retained austenite at FZ. Hardness and microhardness mapping tests showed values of 155 HV at base metal and 200 to 380 HV at the fusion zone connecting the web to the flange.
The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high-speed camera, and an infrared camera is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs more frequently during partial penetration above 6 mm and complete penetration above 8 mm penetration depth, respectively. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root.
The application of magnesium (Mg) inevitably involves dissimilar welding with steel. A novel solid state spot welding method, refill friction stir spot welding (refill FSSW), was utilized to weld AZ31 Mg alloy to galvanized DP600 steel. Although Mg/Fe is an immiscible alloy system, defect-free welds with high strength were successfully obtained in a wide parameter window. The results of microstructure, interfacial reactions, and mechanical properties are reported to reveal the underlying joining mechanism. Due to the melting of Zn coating and subsequent Mg-Zn reactions, Mg-Zn eutectic and intermetallic compounds were detected within welds. Heterogeneous interfacial reactions occur along Mg/steel interface, and the relationship between interfacial structure and fracture behavior was investigated. The joining mechanism is associated with Zn coating and Fe-Al layer: 1) the presence of Zn coating is beneficial for achieving high-quality welding between Mg and steel, it protects the interface from oxidation and contributes to brazing of the weld; 2) the Al present in Mg alloy reacts with Fe, resulting in the growth of Fe-Al layer, which contributes to the diffusion bonding in the interface. The overall results clearly show that Refill FSSW is a competitive welding method for joining Mg and galvanized steel.
Additive manufacturing, and therefore directed energy deposition, is
gaining more and more interest from industrial users. However, quality assurance for the components produced is still a challenge. Machine learning, especially using artificial neuronal networks, is a potential method for ensuring a high-quality standard. Based on process Parameters and monitoring data, part quality can be predicted. A further advantage is the ability to constantly learn and adopt to slight process changes.
First tests using artificial neural networks focus on the prediction of track geometry. The results show that even a small data set is enough to provide high accuracy in the predictions. In this work, an artificial neural network for the predictive analysis of relative density in laser powder cladding has been developed. A central composite experimental design is used to generate 19 data sets. Input variables are laser power, feed rate and powder mass flow. Cubes are built up where density is considered as a target value. Several neural networks are trained and evaluated with these data sets. Different topologies and initial weights are considered. The best network reaches a confidence level of around 90 % for the prediction of relative density based on the process parameters. Finally, the optimization of the generalization performance is investigated. To this purpose, methods of variation in error limit as well as cross-validation are applied. In this way, density is predictable by an artificial neural network with an accuracy of about 95 %.
The increasing adoption of Open Science principles has been a prevalent topic in the welding science community over the last years. Providing access to welding knowledge in the form of complex and complete datasets in addition to peer-reviewed publications can be identified as an important step to promote knowledge exchange and cooperation. There exist previous efforts on building data models specifically for fusion welding applications; however, a common agreed upon implementation that is used by the community is still lacking. One proven approach in other domains has been the use of an openly accessible and agreed upon file and data format used for archiving and sharing domain knowledge in the form of experimental data. Going into a similar direction, the welding community faces particular practical, technical, and also ideological challenges that are discussed in this paper. Collaboratively building upon previous work with modern tools and platforms, the authors motivate, propose, and outline the use of a common file format specifically tailored to the needs of the welding research community as a complement to other already established Open Science practices. Successfully establishing a culture of openly accessible research data has the potential to significantly stimulate progress in welding research.
In this study, steel-glass experiments were conducted to observe the melt pool geometry using a high-speed camera. The high-speed recordings and optical flow analysis show that two main flows take place in form of vortices. The lower vortex drives the melt backwards from the front keyhole wall and thus causes an extension of the melt pool, which is called bulging. This bulging promotes solidification cracking by forming a closed area filled with melt and the accumulation of impurities in the final solidification phase, resulting in low-melting phases which are under tensile stress at the end of solidification.
This article is devoted to the study of the bulging effect in deep penetration laser beam welding. The numerical results of the investigations are based upon experimental results from previous studies to reveal the relationship between the bulging effect and the hot cracking formation, as well as the mixing of alloying elements in the weld pool. The widening of the molten pool in its center area can be observed in full penetration as well as in partial penetration welds on 8 mm and 12 mm thick structural steel plates, respectively. The weld pool shape is extracted from the simulations to evaluate the extent of the necking of the solidification line as well as the bulging phenomena and its influence on the hot cracking phenomena. Relying on an earlier numerical study utilizing a fixed keyhole, simulation models considering a dynamic keyhole are developed thereto. Additionally, the mixing behavior of alloying elements during partial penetration is investigated. The link between the bulge and the studied phenomena is found to be significant.