Analytische Chemie
Filtern
Dokumenttyp
- Zeitschriftenartikel (68)
- Beitrag zu einem Tagungsband (4)
- Buchkapitel (1)
Referierte Publikation
- ja (73) (entfernen)
Schlagworte
- Ultrasound (20)
- Concrete (13)
- LIBS (12)
- Non-destructive testing (12)
- Air-coupled ultrasound (7)
- Material moisture (6)
- Zerstörungsfreie Prüfung (6)
- Embedded sensors (5)
- Nondestructive testing (5)
- Cement (4)
Organisationseinheit der BAM
- 8.2 Zerstörungsfreie Prüfmethoden für das Bauwesen (73) (entfernen)
Paper des Monats
- ja (1)
High-Amplitude Surge of a Pitching Airfoil: Complementary Wind- and Water-Tunnel Measurements
(2018)
RECENT interest in gust response, rotorcraft forward flight and wind energy, among other applications, has focused on streamwise oscillations of nominally two-dimensional airfoils in attached and separated flows. The airfoil may be simultaneously held at constant incidence or execute some maneuver, such as pitch.
The relative freestream is spatially uniform but temporally unsteady, and this can be accomplished in a ground-test facility in two ways. The first method is to vary the output of the prime mover, such as the rotational speed of the impeller or the blower driving a wind tunnel, or (alternatively) to vary the pressure drop in the tunnel, thereby varying the flow speed in the test section, despite nominally constant primemover revolutions per minute. The second method is used to keep the tunnel’s operating speed constant, as well as to move the test article in the streamwise direction, fore and aft (for example, via an electric linear motor), such that the relative freestream speed felt by the test article varies according to some waveform. Typically, the latter approach is chosen in water tunnels, where there is too much tunnel-circuit inertia to vary the flow speed directly but where the usually low tunnel test section flow speeds enable large excursions in the relative freestream by oscillation of the test article. In fact, outright reverse flow is possible by moving the test article in the laboratory frame at a higher speed than the water-tunnel flow speed. In either case, a sinusoidal relative-speed waveform is the most intuitively realizable, and this can be combined with similar oscillations in the airfoil incidence angle or other kinematics. Although the two methods of realizing streamwise oscillations are mechanically distinct, experimental comparisons between an oscillating test article in a water tunnel and a stationary test article in a wind tunnel with a louvermechanismhave demonstrated agreement in themeasured lift and drag histories. Such experimentswere performed by Granlund et al. for a 10% freestream amplitude oscillation and fixed airfoil incidence, comparing a free-surface water tunnel and a closed-circuit wind tunnel. After buoyancy was subtracted from the wind-tunnel data (resulting from the louver pressure drop) and the model inertia subtracted from the water-tunnel data (resulting from acceleration of the test article), the remaining lift and drag histories matched well at the low freestream oscillation amplitude regime. The work of Granlund et al. was later extended to high-advance-ratio streamwise oscillations of 50% amplitude by Greenblatt et al., where the aerodynamic histories of the water-tunnel and wind-tunnel facilities were compared in combined pitch and freestreamoscillations (governed by relative pitch phase), pure pitch oscillations, and purely freestream oscillations. Agreement between the two facilities’ data for fixed-incidence streamwise oscillations was reasonably good, and in fact, better than agreement in just the static lift and drag, evidently owing to differences in blockage and model-support systems. Additionally, Greenblatt et al. determined there was no strong coupling between simultaneous freestream oscillations and pitch oscillations on resultant lift and moment coefficients.
In civil engineering concrete is the most used building material for making infrastructures like bridges and parking decks worldwide. It is as a porous and multiphase material made of aggregates with a defined grain size distribution, cement and water as well as different additives and admixtures depending on the application. Different grain sizes are important to ensure the needed density and compressive strength.
The resulting porous cement matrix contains a mixture of flour grains (aggregates with a grain size below 125 lm) and cement particles (particle size≈50lm). Harmful species like chlorides may penetrate together with water through the capillary pore space and may trigger different damage processes. The damage assessment of concrete structures in Germany is estimated due to the quantification of harmful elements regarding to the cement content only. In the evaluation of concrete using LIBS a two-dimensional scanning is necessary to consider the heterogeneity caused by the aggregates. Therefore, a LIBS system operating with a low energy NdCr:YAG laser, a pulse energy of 3 mJ, a wavelength of 1064 nm, a pulse width of 1.5 ns and a Repetition rate of 100 Hz has been used. Different Czerny-Turner spectrometers with CCD detectors in the UV and NIR range have been used for the detection. Large aggregates (macro-heterogeneity) can be excluded from the evaluation, whereas small aggregates in the range of the laser spot size (flour grains) cannot be spatially resolved. In this work the micro heterogeneity caused by flour grains and their impact on the quantification with LIBS will be discussed. To analyze the effect of changing grain sizes and ratios, the ablation behavior has been determined and compared. Samples with defined grain sizes were made and analyzed using LIBS.
The grain size distributions were analyzed with laser diffraction (LDA).
Monitoring of the absolute water content in porous materials based on embedded humidity sensors
(2018)
Moisture transport monitoring may indicate the onset of deterioration in porous building materials Prior to damage occurring. Most moisture measurement systems provide only qualitative values, require extensive calibration, or are destructive. Thus, non-destructive and calibration-free monitoring Systems are required. Our approach of moisture monitoring is to embed sensors that measure the relative humidity.
In our experiment, screed samples are monitored during the Hydration and evaporation process. Every test sample is equipped with 10 embedded sensors which measure the relative humidity across the sample thickness. Based on Hillerborg’s approach, the relative humidity is converted into the corresponding pore saturation. In our study, the free water is computed without knowledge of the Sorption isotherm. The free water in the pore system is predicted and validated. The predicted weight decrease corresponds conclusively to gravimetrically measured weights. The embedded sensors yield the absolute liquid water content and enable an experimental, non-destructive monitoring of liquid water in porous materials.
This paper reviews state-of-the-art in nondestructive testing (NDT) and semidestructive testing (SDT) methods applicable for imaging the condition of structural timber. Both NDT and SDT imaging reveal defects, damages, and decay, while the extent of wood decay can also be quantified. Combined with an appropriate data interpretation concerning the internal defects, the mechanical properties of the material can also be assessed. The possibilities and limitations of the most relevant individual NDT and SDT methods, also in combination with each other, are outlined and compared. To facilitate comparison, many observations are reported based on the same test specimen.
Processing ultrasonic data by coda wave interferometry to monitor load tests of concrete beams
(2018)
Ultrasonic transmission measurements have been used for decades to monitor concrete elements, mostly on a laboratory scale. Recently, coda wave interferometry (CWI), a technique adapted from seismology, was introduced to civil engineering experiments. It can be used to reveal subtle changes in concrete laboratory samples and even large structural elements without having a transducer directly at the place where the change is taking place. Here, several load tests until failure on large posttensioned concrete beams have been monitored using networks of embedded transducers. To detect subtle effects at the beginning of the experiments and cope with severe changes due to cracking close to failure, the coda wave interferometry procedures had to be modified to an adapted step-wise approach. Using this methodology, we were able to monitor stress distribution and localize large cracks by a relatively simple technique. Implementation of this approach on selected real structures might help to make decisions in infrastructure asset management.
Post-tensioning systems provide safe and efficient construction solutions for long span bridges. Despite the improved grouting practices over the past decade, existing post-tensioning systems may have significant amount of grout defects, which could lead to corrosion of the strands. Condition assessment of post-tensioning systems is necessary to allow bridge owners to take timely, proactive actions to mitigate or prevent further Deterioration and unanticipated tendon failures. A detailed experimental study conducted to assess the performance of nondestructive evaluation techniques in detecting grout defects within internal tendons is presented herein.
Nondestructive evaluation techniques that include Ground Penetrating Radar, Impact Echo, Ultrasonic Tomography, and Ultrasonic Echo are evaluated in terms of detecting the location and severity of fabricated grout defects in a full-scale post-tensioned U-girder mock-up specimen. While Ground Penetrating Radar can identify the location and profile of the internal tendons, particularly metal ducts due to strong reflections, this method did not provide any information about the defect conditions within the tendon. Both Impact Echo and Ultrasonic Echo techniques are effective in identifying the Location of grout defects, but could not differentiate between water, void, or compromised grout conditions. The study clearly demonstrates the need for NDE techniques that are applicable to anchorage regions, and that are capable of estimating the severity and nature of grout defects in internal tendons.
The non-destructive assessment of cracks in concrete is a common task for which non-destructive evaluation solutions have been published. Primarily, these tests have been carried out on artificial cracks that have been created by using notches instead of natural cracks. This study evaluates a procedure designed to create reproducible and controlled cracks in concrete. The procedure is based on using expanding mortar in a series of blind holes. This is done in combination with carefully aligned reinforcement to guide the direction of the crack development. The depth of the crack is also controlled by reinforcement. Crack depth varies statistically in the range of the Maximum aggregate size (16 mm) used for concrete.
The determination of chloride is still one of the main tasks for the evaluation of reinforced concrete structures.
The corrosion of the reinforcement induced by the penetrating chlorides is the dominant damage process affecting the lifetime of concrete structures. In the recent years different research groups demonstrated that LIBS can be a fast and reliable method to quantify chlorine in cement-bound materials. Because chlorine in concrete can only occur as solved ions in the pore solution or bound in salts or hydrated cement phases, the detected emission of chlorine can be correlated with the chloride concentration determined e.g. with potentiometric titration. This work inter alia describes the production of reference samples and possible side effects during the production process. Due to transport processes in the porous matrix of the cement a misinterpretation of the concentrations is possible. It is shown how to overcome these effects and higher precisions of the single measurements can be realised. Using the calibration method, blank sample method and noise method, three different ways of calculating the limit of detection (LOD) and limit of quantification (LOQ) are compared. Due to the preparation of the reference samples a precision of the whole calibration model of sx0 = 0.023 wt% is determined.
The validation of the model is based on different test sets, which are varying in their composition
(different Cl-salts, water-to-cement ratios and additives). The determined mean error of the validation is
0.595 ± 0.063 wt%, which is comparable to standardised methods like potentiometric titration, direct potentiometry
or photometry (0.40 ± 0.06 wt%) [1].
In den letzten Jahren sind im deutschen Bundesautobahnnetz vermehrt AKR-Schäden an Betonfahrbahndecken aufgetreten. Ursächlich hierfür ist die Verwendung alkaliempfindlicher Gesteinskörnung. Dies führt bei gleichzeitiger Anwesenheit von Wasser infolge der Exposition der Fahrbahndecke und des alkalischen Milieus durch den Einsatz alkalireicher Portlandzemente bei der Betonherstellung zu einer Alkali-Kieselsäure-Reaktion (AKR). Zusätzlich wird der AKR-Schädigungsprozess in Betonfahrbahndecken durch den externen Tausalzeintrag (primär NaCl) im Winter begünstigt. Vor diesem Hintergrund kommt der Ermittlung des Tausalzeintrags in den Fahrbahndeckenbeton eine große Bedeutung zu.
Die Analyse des Tausalzeintrags erfolgte bisher ausschließlich nasschemisch an gemahlenen Bohrkernsegmenten. Nachteilig sind hierbei der relativ hohe prüftechnische Aufwand und die eingeschränkte Ortsauflösung. Der alternative Einsatz von LIBS (Laser-induced breakdown spectroscopy) eröffnet in diesem Kontext neue Möglichkeiten. So wird in diesem Beitrag anhand von Bohrkernen aus einem repräsentativen AKR-geschädigten BAB-Abschnitt exemplarisch die Vorgehensweise bei der LIBS-Analyse zur Ermittlung der Na- und Cl-Verteilung an vertikalen Schnittflächen von Bohrkernen aufgezeigt. Da der Tausalzeintrag primär über den Zementstein erfolgt, wurde der verfälschende Na-Grundgehalt der Gesteinskörnung mittels eines Ausschlusskriteriums (Ca-Gehalt) eliminiert. Vergleichend durchgeführte Cl-Mappings mit Mikroröntgenfluoreszenzanalyse sowie nasschemische Analysen belegen die Güte der durchgeführten LIBS-Messungen. Allerdings bedarf es bei der quantitativen Ermittlung des Natriumgehaltes in der Betonfahrbahndecke noch weitergehender Untersuchungen.
Dunkelfärbung der Betonfahrbahndecke im AKR-Kontext - Ursachenanalyse mit innovativer Prüftechnik
(2018)
Die AKR-Schadensevolution von Betonfahrbahndecken ist in der Anfangsphase durch eine Dunkelfärbung der Oberfläche im Fugenbereich gekennzeichnet. Es wird vermutet, dass eine erhöhte Durchfeuchtung der Betonrandzone ursächlich für diese Erscheinung ist. Vor diesem Hintergrund wurde exemplarisch eine Fahrbahnplatte eines repräsentativen Bundesautobahnabschnitts systematisch mit verschiedenartiger zerstörungsfreier Prüftechnik vor Ort untersucht. Die Ergebnisse der zunächst erfolgten großflächigen Durchmusterung mit Radar zeigen, dass in den Bereichen mit einer Dunkelfärbung der Betonfahrbahndecke erhöhte Laufzeiten der Radarimpulse zwischen der
Oberfläche und der Rückseite der Betonfahrbahndecke auftreten, was auf eine erhöhte integrale Durchfeuchtung der Betonfahrbahndecke schließen lässt. Vertiefend durchgeführte NMR-Feuchtemessungen in der Betonrandzone zeigen eine gute Korrelation zwischen erhöhtem Feuchtegehalt und der dunkel gefärbten Fahrbahnoberfläche. Die Ergebnisse beider zerstörungsfreien Prüfmethoden lassen den Schluss zu, dass die Betonfahrbahndecke in der Nähe des Fugenkreuzes eine höhere Durchfeuchtung als im Bereich der Querscheinfuge aufweist. Die geringste Durchfeuchtung besitzt die Betonfahrbahndecke in der Plattenmitte. Die mit den zerstörungsfreien Prüfverfahren ermittelten Befunde stimmen prinzipiell gut mit den punktuell mittels Darr-Wäge-Verfahren an Bohrmehlproben gewonnenen Ergebnissen überein.