Influence of weathering on the leaching behaviour of zinc and PAH from synthetic sports surfaces
(2017)
Synthetic materials used for outdoor sports grounds consist of a mix of inorganic, organic and polymeric compounds that show ageing due to weathering and a complex leaching behaviour by percolation of rainwater, which can limit its lifetime. Additionally, weathering exposure induces degradation processes in the polymers, which leads to the formation of new surfaces allowing water to access additional reservoirs of leachable compounds. A laboratory test comprising artificial weathering, ozonisation and subsequent leaching was developed to investigate this behaviour in a reproducible and controllable way. The experiments showed a general decline of Zn, polycyclic aromatic hydrocarbons (PAH) and total organic carbon (TOC) concentrations after an initial increase. Within this general trend, the course of concentration over exposure duration is very specific for individual sample materials and the analyte under investigation. The results indicate that weathering and degradation behaviour cannot be predicted from initial material conditions. Thus, weathering experiments are recommended to fill this gap of knowledge.
In this paper, we demonstrate the effects of radiation exposures of polymeric materials with UV-A 340 nm lamps (ISO 4892-3, Type 1A) at -10 °C in comparison to an irradiation at +50 °C using a Global UV Test 200 fluorescent lamp device from Weiss Umwelttechnik GmbH, which incorporates an active cooling appliance. While the effects at -10 °C actually are lower than at + 50°C their extent was clearly beyond expectations.
Active thermography with flash and halogen light excitation is used as a method for non-destructive testing of 3D-printed polymer components. Test specimens with artificial defects have been generated, using laser sintering and fused layer modeling. These test specimens have been investigated in different measurement configurations with both excitation methods. Afterwards, the different measurement conditions were compared regarding their capability to detect the defects. Furthermore, advanced analysis methods are used, to fully exploit the capabilities of these techniques.
Additively manufactured test specimens made of polyamide 12 (PA 12) by Laser Sintering (LS) as well as of acrylnitril-butadien-styrol (ABS) by Fused Layer Modeling (FLM), were tested with active thermography. For this, two different excitation methods (flash and impulse excitation) were used and compared, regarding the suitability for the detection of constructed and imprinted defects. To increase the quality of the thermograms, data processing methods like thermal signal reconstruction (TSR) and Fourier-Transformation were applied. Furthermore, the long-term stability of the probes towards environmental stress, like UV-radiation, heat, water contact and frost is being investigated in the presented project with artificial weathering tests.
Additively manufactured test specimens made of polyamide 12 (PA 12) by Laser Sintering as well as of acrylonitrile butadiene styrene (ABS) by Fused Layer Modelling, were characterised with active thermography directly after manufacturing and after artificial weathering. For this, two different excitation methods (flash and pulse heating) were used and compared, regarding their suitability for the detection of constructed and imprinted defects inside the test specimens. To increase the quality of the thermograms, data processing methods like thermal signal reconstruction (TSR) and Fourier Transformation after TSR were applied. To further investigate the long-term stability of the additively manufactured test specimens towards environmental stress, like UV radiation, heat, humidity, water contact and frost with active thermography, an artificial weathering test over 2000 hours (~3 months) was applied to the specimens. The monitoring of the changes in the optical properties of the weathered plastics was supplemented by spectral reflectance and UV/VIS spectroscopy.