Additive Fertigung
Filtern
Erscheinungsjahr
- 2023 (4) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (2)
- Vortrag (2)
Schlagworte
- Additive manufacturing (1)
- AlSi10Mg (1)
- Cyclic R-curve (1)
- Fatigue crack growth (1)
- Fatigue crack propagation (1)
- Finish milling (1)
- Forschung (1)
- Fügetechnik (1)
- Heat treatment (1)
- Microstructure characterization (1)
Organisationseinheit der BAM
- 9.0 Abteilungsleitung und andere (4) (entfernen)
Eingeladener Vortrag
- nein (2)
The microstructure has a great influence on short fatigue crack growth in metallic materials. Laser-based Powder Bed Fusion AlSi10Mg alloys exhibit in the as-built condition a fine fibrous Si structure and a supersaturated solid solution of Si in the α-Al matrix, which is significantly modified by heat treatments starting already at temperatures under 260 °C. This study focuses on the influence of post-process heat treatments on the microstructural evolution and the resulting fatigue crack growth resistance. As compared to the as-built condition, two heat treatments at 265 °C/1 h and at 300 °C/2 h are found to be beneficial to the fatigue crack growth resistance of the investigated material.
The high cooling rates (~106 K/s) occurring during Laser Powder Bed Fusion (PBF-LB/M) of AlSi10Mg induce to the formation of a fine nanometric silicon network in the as-built condition. Such unprecedented microstructure enhances the mechanical strength when compared to equivalent as-cast materials. Nevertheless, PBF-LB/M also leads to high magnitude residual stress (RS) due to the extreme localized temperature gradients. The presence of RS can be detrimental to the fatigue life of engineering components, and great efforts are focused on understanding their generation and evolution after post-process heat treatments. Typically, T6 heat treatments are used to mitigate RS and improve mechanical performances by Mg2Si precipitation during ageing at 160-180°C. Nevertheless, the solutionizing at 500-540°C vanishes the fine silicon network, leading to the formation of micrometric (average of ~2-5 µm) polygonal Si particles, similar to those observed in T6 heat-treated Al-Si cast materials. Therefore, the aim of this work is to evaluate the ability of two so-called low temperature heat treatments (i.e., at 265°C and 300°C) to mitigate RS while retaining the fine as-built microstructure inherent to PBF-LB/M AlSi10Mg. The fatigue behavior of the as-built material is subsequently compared to the two low temperature conditions.
Multi-Principal-Element or High-Entropy Alloys (MPEAs/HEAs) have gained increasing interest in the past two decades largely due to their outstanding properties such as superior mechanical strength and corrosion resistance. However, research studies on their processability are still scarce. This work assesses the effect of different machining conditions on the machinability of these novel alloys, with the objective of advancing the introduction of MPEA systems into industrial applications. The present study focuses on the experimental analysis of finish-milling conditions and their effects on the milling process and resulting surface finish of CoCrFeNi, Al0.3CoCrFeNi and Al0.3CoCrFeNiMo0.2 alloys fabricated via Spark Plasma Sintering. Ball-nose-end milling experiments have been carried out various milling parameters such as cutting speed, feed per cutting edge, and ultrasonic assistance. In situ measurements of cutting forces and temperature on the tool edge were performed during the experiments, and surface finish and tool wear were analyzed afterwards. The results exhibited decreasing cutting forces by means of low feed per cutting edge and reduced process temperatures at low cutting speed, with the use of ultrasonic-assisted milling. It was shown that the machinability of these modern alloys through conventional, as well as modern machining methods such as ultrasonic-assisted milling, is viable, and common theories in machining can be transferred to these novel MPEAs.
Der Vortrag gibt einen kurzen Überblick über die Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige FuE-Bereiche. Fügetechnologien haben dabei wesentliche Bedeutung für die Umsetzung von technischen Komponenten der Wasserstofftechnologien. Forschungsschwerpunkte ergeben sich insbesondere für die Erzeugung und den Transport des Wasserstoffs.