Wissenschaftliche Artikel der BAM
Filtern
Dokumenttyp
Sprache
- Englisch (203)
- Deutsch (12)
- Portugiesisch (1)
Schlagworte
- Concrete (17)
- Alkali-activated materials (15)
- Corrosion (15)
- Flame retardant (9)
- Cement (7)
- Fatigue (6)
- Additive manufacturing (5)
- Durability (5)
- Rheology (5)
- Carbon steel (4)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (216) (entfernen)
Paper des Monats
- ja (15)
In general, pH-sensitive colorants such as phenolphthalein are applied on freshly split surfaces of building structures to determine the state of carbonation. For years, it has been known that the aerosols of phenolphthalein are suspected of being carcinogenic. Hence, more work has currently being done on alternative indicators for the use in research and the use on construction sites. Over the past years, mainly pH indicators from other research areas and natural dyes were investigated for their usability to cementitious systems. This paper presents the experimental results of using phenolphthalein solution bound in agar-agar gel. This gel-bound indicator allows the future use of the already known phenolphthalein dye without the health hazards for the user. To demonstrate the flexibility of the gel-bound colorant, different application forms of the indicator were carried out and assessed. In addition, the results obtained by the different methods were statistically evaluated to ensure validity.
The accuracy of the results was confirmed by thermogravimetric analysis and IR spectroscopic studies as reference methods. It has also succeeded to demonstrate the comparability of the results achieved by the gel-bound colorant with the results of the common sprayed application method. As an additional gain in knowledge, comparative results of indicator tests, TGA analysis, and FTIR investigation are shown.
Several studies show that thermal and hydrothermal treatment can further improve the excellent properties of UHPC in terms of mechanical strength and durability. While for the thermal treatment the increase in strength is attributed to an intensified pozzolanic and hydraulic reaction, for the hydrothermal treatment previous studies accredited it mostly to the formation of tobermorite. In the presented study thermal and hydrothermal treatment of UHPC samples was systematically varied and the phase formation analysed related to the strength development of a reference sample cured for 28 days in water. For the thermal treatment the results show that the strength increase depends on the protection against desiccation and can be ascribed to an improved pozzolanic reaction of the siliceous fillers. To achieve a significant enhancement of strength, a pre-storage time of few days and a long dwell time at elevated temperature/pressure are required. For the hydrothermal treatment already heating the specimens up to 185 °C in saturated steam followed by an immediate cooling leads to a substantial increase in compressive strength. Pre-storage time did not affect the result as far as a minimum of several hours is guaranteed. The improved performance is due to an increase in the pozzolanic and hydraulic reaction. Surprisingly, tobermorite was only found within a very thin layer at the surface of the sample, but not in the bulk. Sulphate and aluminium stemming from the decomposition of the ettringite are bound in the newly formed phases hydroxylellestadite and hydrogarnet.
Potentialfeldmessung (PM) ist die beliebteste Methode der Zerstörungsfreien Prüfung (ZfP) zur Lokalisierung von aktiver Betonstahlkorrosion. PM wird durch Parameter wie z. B. Feuchtigkeits- und Chloridgradienten im Bauteil beeinflusst, so dass die Sensitivität gegenüber der räumlich sehr begrenzten, aber gefährlichen Lochkorrosion gering ist. Wir zeigen in dieser Studie, wie zusätzliche Messinformationen mit Multisensor-Datenfusion genutzt werden können, um die Detektionsleistung zu verbessern und die Auswertung zu automatisieren. Die Fusion basiert auf überwachtem maschinellen Lernen (ÜML). ÜML sind Methoden, die Zusammenhänge in (Sensor-) Daten anhand vorgegebener Kennzeichnungen (Label) erkennen. Wir verwenden ÜML um „defekt“ und „intakt“ gelabelte Bereiche in einem Multisensordatensatz zu unterscheiden. Unser Datensatz besteht aus 18 Messkampagnen und enthält jeweils PM-, Bodenradar-, Mikrowellen-Feuchte- und Wenner-Widerstandsdaten. Exakte Label für veränderliche Umweltbedingungen wurden in einer Versuchsanordnung bestimmt, bei der eine Stahlbetonplatte im Labor kontrolliert und beschleunigt verwittert. Der Verwitterungsfortschritt wurde kontinuierlich überwacht und die Korrosion gezielt erzeugt. Die Detektionsergebnisse werden quantifiziert und statistisch ausgewertet. Die Datenfusion zeigt gegenüber dem besten Einzelverfahren (PM) eine deutliche Verbesserung. Wir beschreiben die Herausforderungen datengesteuerter Ansätze in der zerstörungsfreien Prüfung und zeigen mögliche Lösungsansätze.
The susceptibility of concrete structures due to alkali–silica reaction (ASR) can be assessed by means of ASR concrete prism testing at 60 °C, according to RILEM AAR 4.1. There, expansion of concrete prisms indicates alkali-reactivity of the examined concrete mix. This work applies in situ expansion measurement to accelerated concrete prism testing. Automated measuring facilitates both storage without the usually necessary interruptions for manual measurement and acquisition of quasi-continuousexpansion data. A comparative experimental programme showed that conventional testing resulted in stronger expansion and leaching of alkalis than automated testing. Experimental simulation of interruptions, typically associated with manual measurements in conventional testing, could prove the influence of these cooling–heating cycles. Two phenomenological approaches, frequently used for describing reaction kinetics of ASR by linking it to expansion results from ASR-testing, were validated with continuous expansion data of three types of aggregate. Experimental expansion depicted s-shaped curves similar to them of the modelling approaches. However, strong swelling recorded in the beginning of the test was not covered by the model curves. Auxiliary measurement of acoustic emissions and ultrasonic velocity helped characterising mechanisms such as hydration and cracking, which also influence prism expansion. The proposed modification of the measurement procedure provides an extended basis to analyse expansion mechanisms. Regarding data for validation of ASR-expansion models, continuous expansion results are preferable to conventional test results.
Durability Assessment of Structural Sealant Glazing Systems applying a Performance Test Method
(2020)
During the service life of a Structural Sealant Glazing (SSG) facade, its silicone bond is exposed to climatic, chemical, and mechanical loads. While current durability assessment methods schedule separate test programmes for accelerated weathering and fatigue, the presented test applies mechanical loading and weather cycling simultaneously to simulate 50 years of use. Specifically designed medium-scale system specimens resemble a common SSG-bond. Displacement-controlled sinusoidal load cycles in two load directions subject these specimens to tensile, compression and shear loads. Weathering comprises temperature and humidity cycles, UV-radiation, and application of water and detergent. During testing, the forces transmitted by the system specimens are continuously measured for performance assessment. The resulting system response reveals mechanical performance characteristics like elastic moduli and dissipated energies which decrease during exposure, indicating stress relaxation and degradation. Two common structural sealants were tested. After testing, sections of the system specimens were subjected to tensile and shear tests for mechanical characterisation. Strengths and moduli are notably reduced by combined loading compared to those of reference and weathered specimens. Hardness and visual inspections of the bond correlate with the performance and bond characteristics. The approach introduced in this article provides a basis for life cycle assessment of SSG-systems.
During the service life of structural sealant glazing (SSG) facades, the loadbearing capacity of the silicone bonds needs to be guaranteed. Laboratory Tests can assess the durability of SSG-systems based on mechanical characteristics of the bond after simultaneous exposure to both climatic and mechanical loads.
This article studies how the material characteristics of two common structural sealants are affected by laboratory and field exposure. Dynamic mechanical Analysis (DMA) confirms a reduction in the dynamic modulus of exposed Silicone samples. Results from thermogravimetric analysis, Fourier-transform infrared spectroscopy, differential scanning calorimetry, and small-angle X-ray scattering/wide-angle X-ray scattering show differences between the two sealants and indicate no/minor changes in the composition and morphology of the laboratory and field exposed sealants. Mechanical characterization methods, such as DMA, and tensile and shear testing of the structural bond, are shown to be sensitive toward the combined climatic and mechanical loadings, and are hence suitable for studying degradation mechanisms of structural sealants.
Bitumen is a crucial building material in road construction, which is exposed to continuously higher stresses due to higher traffic loads and changing climatic conditions. Therefore, various additives are increasingly being added to the bitumen complicating the characterisation of the bituminous binder, especially concerning the reuse of reclaimed asphalt.
Therefore, this work aimed to demonstrate that the combination of Fourier transform infrared (FTIR) spectroscopy with attenuated total reflexion (ATR) technique and multivariate evaluation is a very wellsuited method to reliable identify and quantify additives in bituminous binders. For this purpose, various unmodified and modified binders, directly and extracted from laboratory and reclaimed asphalts, were investigated with FTIR-ATR spectroscopy. The determined spectra, pre-processed by standard normal variate (SNV) transformation and the determination of the 1st derivation, were evaluated using factor Analysis (FA), linear discriminant analysis (LDA) and partial least square regression (PLSR). With this multivariate evaluation, first, a significant model with a very high hit rate of over 90% was developed allowing for the identification of styrene-butadiene copolymers (SBC), ethylene-copolymer bitumen (ECB) and different waxes (e.g. amide and Fischer-Tropsch wax) even if the additives do not show any additional peaks or the samples are multi-modified. Second, a quantification of the content is possible for SBC, ECB, and Amide wax with a mean error of RMSE B 0.4 wt% and a
coefficient of determination of R2[90%. Based on these results, FTIR identification and quantification of additives in bituminous binders is a very promising method with a great potential.
Alkali-silica reaction (ASR) is a chemical reaction within concrete which can lead over time to cracking and spalling. Due to the complexity of the problem, it still causes damage to concrete constructions worldwide.
The publication aims to illustrate the interdisciplinary research of the German Federal Institute for Materials Research and Testing (BAM) within the last 20 years, considering all aspects of ASR topics from the macro to the micro level. First, methods for characterization and assessment of ASR risks and reaction products used at BAM are explained and classified in the international context. Subsequently the added value of the research approach by combining different, preferably nondestructive, methods across all scales is explained using specific examples from a variety of research projects. Aspects covered range from the development of new test-setups to assess aggregate reactivity, to analysis of microstructure and reaction products using microscopical, spectroscopical and X-ray methods, to the development of a testing methodology for existing concrete pavements including in-depth analysis of the visual damage indicator and the de-icing salt input using innovative testing techniques. Finally, research regarding a novel avoidance strategy that makes use of internal hydrophobization of the concrete mix is presented.
block and mortar types is analysed with particular regard to the influence of varying relative humidity. The uniaxial compressive strength and deformation characteristics of unstabilised earth blocks and mortars as well as of unstabilised earth block masonry are studied in detail and compared to conventional masonry to evaluate whether the structural design can be made accordingly. An increase of 30 % points in relative humidity leads to a reduction of the masonry´s compressive strength between 33 % and 35 % whereas the Young´s modulus is reduced by 24–29 %. However, the ratio between the Young´s modulus and the characteristic compressive strength of earth block masonry ranges between E33/fk = 283–583 but is largely independent of the relative humidity. The results show that the mechanical properties of the investigated unstabilised earth block masonry are sufficient for load-bearing structures, yielding a masonry compressive strength between 2.3 MPa and 3.7 MPa throughout the range of moisture contents
investigated. In general, the design concept of conventional masonry can be adapted for unstabilised earth masonry provided that the rather low Young´s modulus as well as the moisture dependence of both, compressive strength and Young´s modulus, are sufficiently taken into
account.
The RILEM technical committee TC 247-DTA ‘Durability Testing of Alkali-Activated Materials’ conducted a round robin testing programme to determine the validity of various durability testing methods, originally developed for Portland cement based-concretes, for the assessment of the durability of alkali-activated concretes. The outcomes of the round robin tests evaluating sulfate resistance, alkali-silica reaction (ASR) and freeze–thaw resistance are presented in this contribution. Five different alkali-activated concretes, based on ground granulated blast furnace slag, fly ash, or metakaolin were investigated. The extent of sulfate damage to concretes based on slag or fly ash seems to be limited when exposed to an Na2SO4 solution. The mixture based on metakaolin showed an excessive, very early expansion, followed by a dimensionally stable period, which cannot be explained at present. In the slag-based concretes, MgSO4 caused more expansion and visual damage than Na2SO4; however, the expansion limits defined in the respective standards were not exceeded. Both the ASTM C1293 and RILEM AAR-3.1 test methods for the determination of ASR expansion appear to give essentially reliable identification of expansion caused by highly reactive aggregates. Alkali-activated materials in combination with an unreactive or potentially expansive aggregate were in no case seen to cause larger expansions; only the aggregates of known very high reactivity were seen to be problematic. The results of freeze–thaw testing (with/without deicing salts) of alkali-activated concretes suggest an important influence of the curing conditions and experimental conditions on the test outcomes, which need to be understood before the tests can be reliably applied and interpreted.